新一代马氏体耐热钢G115的研究进展
收稿日期: 2021-05-07
修回日期: 2021-12-01
网络出版日期: 2021-12-20
基金资助
国家自然科学基金项目(U1960204)
Research Progress of a Novel Martensitic Heat-Resistant Steel G115
Received date: 2021-05-07
Revised date: 2021-12-01
Online published: 2021-12-20
Supported by
National Natural Science Foundation of China(U1960204)
提高火电机组中耐热锅炉的蒸汽温度和压力参数可以有效提升燃煤效率,减少有害气体排放。受煤炭资源紧缺和温室效应的双重影响,发展650℃及更高温度超超临界(ultra super-critical,USC)机组中的耐热锅炉材料已迫在眉睫。我国在600℃ USC机组用耐热材料P92钢基础上研发的马氏体耐热钢G115有望成为优选材料之一。本文介绍了G115钢的成分特点、形貌特征,综述了其在组织稳定性、蠕变性能、抗疲劳性能、抗蒸汽氧化性能以及工业管材制备等方面的研究进展,重点归纳了G115钢中富Cu相的作用,展望了未来研究重点,以期为更深入研究G115钢提供可行思路。
何焕生 , 余黎明 , 刘晨曦 , 李会军 , 高秋志 , 刘永长 . 新一代马氏体耐热钢G115的研究进展[J]. 金属学报, 2022 , 58(3) : 311 -323 . DOI: 10.11900/0412.1961.2021.00185
Improving the steam temperature and the pressure of the boiler applied in the thermal power could enhance the coal-fired efficiency and reduce the emission of harmful gases. Due to the dual impact of dwindling fossil resources and an exacerbated global greenhouse effect, it is critical to develop new heat-resistant boiler materials for ultra super-critical (USC) units at temperatures of 650oC and higher. With great thermal conductivity, good fatigue resistance, and low cost, martensitic heat-resistant steel G115, based on P92 steel applied in 600oC USC units, is a promising steel to be applied to this among all candidate materials. This paper introduces the main chemical composition and the microstructure feature of G115 steel, and the research progress in the areas of microstructure stability, creep performance, fatigue resistance, steam oxidation resistance, and industrial pipe production are summarized, with a focus on the role of Cu-rich phase in G115 steel. Finally, some key points on G115 steel are proposed to provide ideas for future research.
| 1 | Wu Z Q , Bai Y , Ma L T , et al . Research and development of martensitic creep-resistant steels for 650oC [J]. Iron Steel, 2015, 50(5): 1 |
| 1 | 吴增强, 白 银, 马龙腾 等 . 650℃马氏体耐热钢研究及其进展 [J]. 钢铁, 2015, 50(5): 1 |
| 2 | Sklenicka V , Kucharova K , Svobodova M , et al . The effect of a prior short-term ageing on mechanical and creep properties of P92 steel [J]. Mater. Charact., 2018, 136: 388 |
| 3 | Jin X , Zhu B Y , Li Y F , et al . Effect of the microstructure evolution on the high-temperature strength of P92 heat-resistant steel for different service times [J]. Int. J. Press. Vessels Pip., 2020, 186: 104131 |
| 4 | Masuyama F . History of power plants and progress in heat resistant steels [J]. ISIJ Int., 2001, 41: 612 |
| 5 | Liu Z D , Chen Z Z , He X K , et al . Systematical innovation of heat resistant materials used for 630~700oC advanced ultra-supercritical (A-USC) fossil fired boilers [J]. Acta Metall. Sin., 2020, 56: 539 |
| 5 | 刘正东, 陈正宗, 何西扣 等 . 630~700℃超超临界燃煤电站耐热管及其制造技术进展 [J]. 金属学报, 2020, 56: 539 |
| 6 | Wang J Z , Liu Z D , Bao H S , et al . Study of steel and alloys for ultra-supercritical power plant in China [J]. Iron Steel, 2015, 50(8): 1 |
| 6 | 王敬忠, 刘正东, 包汉生 等 . 中国超超临界电站锅炉关键材料用钢及合金的研究现状 [J]. 钢铁, 2015, 50(8): 1 |
| 7 | Chi C Y , Yu H Y , Xie X S . Research and development of austenitic heat-resistant steels for 600oC superheat/reheater tubes of USC power plant boilers [J]. World Iron Steel, 2012, 12(4): 50 |
| 7 | 迟成宇, 于鸿垚, 谢锡善 . 600℃超超临界电站锅炉过热器及再热器管道用先进奥氏体耐热钢的研究与发展 [J]. 世界钢铁, 2012, 12(4): 50 |
| 8 | Gao Q Z . Phase transformation behaviors and welding of the modified high Cr ferritic heat-resistant steel [D]. Tianjin: Tianjin University, 2012 |
| 8 | 高秋志 . 新型高Cr铁素体耐热钢相变行为及焊接性 [D]. 天津: 天津大学, 2012 |
| 9 | Li H . Research on the high temperature oxidation and corrosion properties of new martensitic heat resistant steel [D]. Harbin: Harbin Engineering University, 2019 |
| 9 | 李 洪 . 新型马氏体耐热钢的高温氧化和腐蚀性能研究 [D]. 哈尔滨: 哈尔滨工程大学, 2019 |
| 10 | Kim B K , Tan L , Xu C , et al . Microstructural evolution of NF709 (20Cr-25Ni-1.5MoNbTiN) under neutron irradiation [J]. J. Nucl. Mater., 2016, 470: 229 |
| 11 | Zhang Z , Hu Z F , Tu H Y , et al . Microstructure evolution in HR3C austenitic steel during long-term creep at 650oC [J]. Mater. Sci. Eng., 2017, A681: 74 |
| 12 | Dudova N , Mishnev R , Kaibyshev R . Creep behavior of a 10%Cr heat-resistant martensitic steel with low nitrogen and high boron contents at 650?oC [J]. Mater. Sci. Eng., 2019, A766: 138353 |
| 13 | Rojas D , Garcia J , Prat O , et al . Effect of processing parameters on the evolution of dislocation density and sub-grain size of a 12%Cr heat resistant steel during creep at 650oC [J]. Mater. Sci. Eng., 2011, A528: 1372 |
| 14 | Yin F S , Jung W S , Chung S H . Microstructure and creep rupture characteristics of an ultra-low carbon ferritic/martensitic heat-resistant steel [J]. Scr. Mater., 2007, 57: 469 |
| 15 | Gao Q Z , Dong X , Li C , et al . Microstructure and oxidation properties of 9Cr-1.7W-0.4Mo-Co ferritic steel after isothermal aging [J]. J. Alloys Compd., 2015, 651: 537 |
| 16 | Liu Z , Xie X . The Chinese 700oC A-USC development program [A]. Materials for Ultra-Supercritical and Advanced Ultra-Supercritical Power Plants [M]. United Kingdom: Woodhead Publishing, 2017: 715 |
| 17 | Xiao B , Xu L Y , Cayron C , et al . Solute-dislocation interactions and creep-enhanced Cu precipitation in a novel ferritic-martensitic steel [J]. Acta Mater., 2020, 195: 199 |
| 18 | Abe F . New martensitic steels [A]. Materials for Ultra-Supercritical and Advanced Ultra-Supercritical Power Plants [M]. United Kingdom: Woodhead Publishing, 2017: 323 |
| 19 | Liu Z D , Cheng S C , Bao H S , et al . Steel for steam-temperature ultra-supercritical thermal power unit and preparation method thereof [P] Chin Pat., 201210574445.1, 2013 |
| 19 | 刘正东, 程世长, 包汉生 等 . 蒸汽温度超超临界火电机组用钢及制备方法 [P]. 中国专利, 201210574445.1, 2013) |
| 20 | Liu C X , Mao C L , Cui L , et al . Recent progress in microstructural control and solid-state welding of reduced activation ferritic/martensitic steels [J]. Acta Metall. Sin., 2021, 57: 1521 |
| 20 | 刘晨曦, 毛春亮, 崔 雷 等 . 低活化铁素体/马氏体钢组织调控及其固相连接研究进展 [J]. 金属学报, 2021, 57: 1521 |
| 21 | Wang H , Yan W , van Zwaag S , et al . On the 650oC thermostability of 9-12Cr heat resistant steels containing different precipitates [J]. Acta Mater., 2017, 134: 143 |
| 22 | Xu Y T , Nie Y H , Wang M J , et al . The effect of microstructure evolution on the mechanical properties of martensite ferritic steel during long-term aging [J]. Acta Mater., 2017, 131: 110 |
| 23 | Faulkner R G , Williams J A , Sanchez E G , et al . Influence of Co, Cu and W on microstructure of 9%Cr steel weld metals [J]. Mater. Sci. Technol., 2003, 19: 347 |
| 24 | Helis L , Toda Y , Hara T , et al . Effect of cobalt on the microstructure of tempered martensitic 9Cr steel for ultra-supercritical power plants [J]. Mater. Sci. Eng., 2009, A510-511: 88 |
| 25 | Liu Z , Wang X T , Dong C . Effect of boron on G115 martensitic heat resistant steel during aging at 650oC [J]. Mater. Sci. Eng., 2020, A787: 139529 |
| 26 | Wen X L , Zhang Q Q , Chen L . A state-of-the-art review of chemical component study of the candidate steel for 650oC ultra-supercritical boiler tube [J]. Mater. Rev., 2018, 32: 2167 |
| 26 | 文新理, 章清泉, 陈 列 . 650℃第三代超超临界锅炉管候选钢种的化学成分研究现状 [J]. 材料导报, 2018, 32: 2167 |
| 27 | Chi C Y , Yu H Y , Dong J X , et al . The precipitation strengthening behavior of Cu-rich phase in Nb contained advanced Fe-Cr-Ni type austenitic heat resistant steel for USC power plant application [J]. Prog. Nat. Sci.: Mater. Int., 2012, 22: 175 |
| 28 | Tan S P , Wang Z H , Cheng S C , et al . Effect of Cu content on aging precipitation behaviors of Cu-Rich Phase in Fe-Cr-Ni alloy [J]. J. Iron Steel Res. Int., 2010, 17: 63 |
| 29 | Zeng Y P , Jia J D , Cai W H , et al . Effect of long-term service on the precipitates in P92 steel [J]. Int. J. Miner. Metall. Mater., 2018, 25: 913 |
| 30 | Li J R , Zhang C L , Jiang B , et al . Effect of large-size M23C6-type carbides on the low-temperature toughness of martensitic heat-resistant steels [J]. J. Alloys Compd., 2016, 685: 248 |
| 31 | Xu Y T , Zhang X Y , Tian Y B , et al . Study on the nucleation and growth of M23C6 carbides in a 10% Cr martensite ferritic steel after long-term aging [J]. Mater. Charact., 2016, 111: 122 |
| 32 | Pandey C , Mahapatra M M , Kumar P , et al . Some studies on P91 steel and their weldments [J]. J. Alloys Compd., 2018, 743: 332 |
| 33 | Abe F , Taneike M , Sawada K . Alloy design of creep resistant 9Cr steel using a dispersion of nano-sized carbonitrides [J]. Int. J. Press. Vessels Pip., 2007, 84: 3 |
| 34 | Kipelova A , Kaibyshev R , Belyakov A , et al . Microstructure evolution in a 3%Co modified P911 heat resistant steel under tempering and creep conditions [J]. Mater. Sci. Eng., 2011, A528: 1280 |
| 35 | Yang L X . Multi-scale characterization of Cu and correlation study on composition-structure-properties of ultra supercritical heat resistant steel G115 [D]. Beijing: Central Iron & Steel Research Institute, 2018 |
| 35 | 杨丽霞 . 超超临界耐热钢G115中Cu的跨尺度表征及其成分-组织结构-性能相关性研究 [D]. 北京: 钢铁研究总院, 2018 |
| 36 | H?ttestrand M , Andrén H O . Microstructural development during ageing of an 11% chromium steel alloyed with copper [J]. Mater. Sci. Eng., 2001, A318: 94 |
| 37 | Ma L T , Bai Y , Liu Z D . The Laves phase evolution of 9Cr-3W-3Co steel under long term isothermal treatment [J]. Steel Res. Int., 2017, 88: 1600412 |
| 38 | Kipelova A , Belyakov A , Kaibyshev R . Laves phase evolution in a modified P911 heat resistant steel during creep at 923 K [J]. Mater. Sci. Eng., 2012, A532: 71 |
| 39 | Rojas D , Garcia J , Prat O , et al . 9%Cr heat resistant steels: Alloy design, microstructure evolution and creep response at 650oC [J]. Mater. Sci. Eng., 2011, A528: 5164 |
| 40 | Ma L T , Wang Y F , Di G B . Study on the microstructure evolution and tungsten content optimization of 9Cr-3W-3Co steel [J]. Materials, 2018, 11: 2080 |
| 41 | Liu Z , Liu Z D , Wang X T , et al . Investigation of the microstructure and strength in G115 steel with the different concentration of tungsten during creep test [J]. Mater. Charact., 2019, 149: 95 |
| 42 | Yan P , Liu Z D , Bao H S , et al . Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions [J]. Mater. Sci. Eng., 2013, A588: 22 |
| 43 | Liu Z , Liu Z D , Wang X T , et al . The microstructural evolution and mechanical property in G115 steels during long-term aging at 650oC [J]. Mater. Res. Express, 2019, 6: 116 |
| 44 | Guo X F , Jiang Y , Gong J M , et al . The influence of long-term thermal exposure on microstructural stabilization and mechanical properties in 9Cr-0.5Mo-1.8W-VNb heat-resistant steel [J]. Mater. Sci. Eng., 2016, A672: 194 |
| 45 | Saini N , Mulik R S , Mahapatra M M . Study on the effect of ageing on laves phase evolution and their effect on mechanical properties of P92 steel [J]. Mater. Sci. Eng., 2018, A716: 179 |
| 46 | Duan P , Liu Z D , Li B , et al . Study on microstructure and mechanical properties of P92 steel after high-temperature long-term aging at 650oC [J]. High Temp. Mater. Processes, 2020, 39: 545 |
| 47 | Gao Q Z , Zhang Y N , Zhang H L , et al . Precipitates and particles coarsening of 9Cr-1.7W-0.4Mo-Co ferritic heat-resistant steel after isothermal aging [J]. Sci. Rep., 2017, 7: 5859 |
| 48 | Liu Z , Liu Z D , Wang X T , et al . Evolution of the microstructure in aged G115 steels with the different concentration of tungsten [J]. Mater. Sci. Eng., 2018, A729: 161 |
| 49 | Xiao B , Xu L Y , Zhao L , et al . Creep properties, creep deformation behavior, and microstructural evolution of 9Cr-3W-3Co-1CuVNbB martensite ferritic steel [J]. Mater. Sci. Eng., 2018, A711: 434 |
| 50 | Heo Y U , Kim Y K , Kim J S , et al . Phase transformation of Cu precipitates from bcc to fcc in Fe-3Si-2Cu alloy [J]. Acta Mater., 2013, 61: 519 |
| 51 | Isheim D , Gagliano M S , Fine M E , et al . Interfacial segregation at Cu-rich precipitates in a high-strength low-carbon steel studied on a sub-nanometer scale [J]. Acta Mater., 2006, 54: 841 |
| 52 | Liang Y , Yan W , Shi X B , et al . On Laves phase in a 9Cr3W3CoB martensitic heat resistant steel when aged at high temperatures [J]. J. Mater. Sci. Technol., 2021, 85: 129 |
| 53 | Yan P , Liu Z D . Toughness evolution of 9Cr-3W-3Co martensitic heat resistant steel during long time aging [J]. Mater. Sci. Eng., 2016, A650: 290 |
| 54 | Zhang H J , Zhou R C , Tang L Y , et al . Study on microstructure and mechanical properties of P92 steel aged at 650oC [J]. Proc. CSEE, 2009, 29(suppl.): 174 |
| 54 | 张红军, 周荣灿, 唐丽英 等 . P92钢650℃时效的组织性能研究 [J]. 中国电机工程学报, 2009, 29(): 174 |
| 55 | Isik M I , Kostka A , Eggeler G . On the nucleation of Laves phase particles during high-temperature exposure and creep of tempered martensite ferritic steels [J]. Acta Mater., 2014, 81: 230 |
| 56 | Yu Y H , Liu Z D , Zhang C , et al . Correlation of creep fracture lifetime with microstructure evolution and cavity behaviors in G115 martensitic heat-resistant steel [J]. Mater. Sci. Eng., 2020, A788: 139468 |
| 57 | Mishnev R , Dudova N , Fedoseeva A , et al . Microstructural aspects of superior creep resistance of a 10%Cr martensitic steel [J]. Mater. Sci. Eng., 2016, A678: 178 |
| 58 | Xiao B , Xu L Y , Zhao L , et al . Microstructure evolution and fracture mechanism of a novel 9Cr tempered martensite ferritic steel during short-term creep [J]. Mater. Sci. Eng., 2017, A707: 466 |
| 59 | Xiao B , Xu L Y , Tang Z X , et al . A physical-based yield strength model for the microstructural degradation of G115 steel during long-term creep [J]. Mater. Sci. Eng., 2019, A747: 161 |
| 60 | Xiao B , Xu L Y , Zhao L , et al . Deformation-mechanism-based creep model and damage mechanism of G115 steel over a wide stress range [J]. Mater. Sci. Eng., 2019, A743: 280 |
| 61 | Jiang C C , Dong Z , Song X L , et al . Long-term creep rupture strength prediction for a new grade of 9Cr martensitic creep resistant steel (G115)—An application of a new tensile creep rupture model [J]. J. Mater. Res. Technol., 2020, 9: 5542 |
| 62 | Jing H Y , Luo Z X , Xu L Y , et al . Low cycle fatigue behavior and microstructure evolution of a novel 9Cr-3W-3Co tempered martensitic steel at 650?°C [J]. Mater. Sci. Eng., 2018, A731: 394 |
| 63 | Luo Z X . Low cycle fatigue behavior and microstructure evolution of G115 martensitic steel at high temperature [D]. Tianjin: Tianjin University, 2018 |
| 63 | 罗振轩 . G115马氏体耐热钢高温低周疲劳行为及微观组织研究 [D]. 天津: 天津大学, 2018 |
| 64 | Tang Z X , Jing H Y , Xu L Y , et al . Temperature effect on dwell-fatigue crack propagation behavior of novel tempered martensitic ferritic steel G115 [J]. Eng. Fract. Mech., 2020, 237: 107250 |
| 65 | Tang Z X , Jing H Y , Xu L Y , et al . Creep-fatigue crack growth behavior of G115 steel under different hold time conditions [J]. Int. J. Fatigue, 2018, 116: 572 |
| 66 | Xu L Y , Rong J Y , Zhao L , et al . Creep-fatigue crack growth behavior of G115 steel at 650?oC [J]. Mater. Sci. Eng., 2018, A726: 179 |
| 67 | Tang Z X , Jing H Y , Xu L Y , et al . Investigating crack propagation behavior and damage evolution in G115 steel under combined steady and cyclic loads [J]. Theor. Appl. Fract. Mech., 2019, 100: 93 |
| 68 | Tang Z X , Jing H Y , Xu L Y , et al . Investigation of creep-fatigue crack growth of G115 steel using a novel damage model [J]. Int. J. Mech. Sci., 2020, 183: 105827 |
| 69 | Bai Y , Chen Z Z , Liu Z D , et al . Effect of temperature on steam oxidation behavior of G115 steel [J]. J. Iron Steel Res., 2020, 32: 52 |
| 69 | 白 银, 陈正宗, 刘正东 等 . 蒸汽温度对G115钢氧化行为的影响 [J]. 钢铁研究学报, 2020, 32: 52 |
| 70 | Liu Z D , Chen Z Z , Bao H S , et al . Development and Engineering of a New Generation of Martensitic Heat Resistant Steel G115 [M]. Beijing: Metallurgical Industry Press, 2020: 263 |
| 70 | 刘正东, 陈正宗, 包汉生 等 . 新一代马氏体耐热钢G115研发及工程化 [M]. 北京: 冶金工业出版社, 2020: 263 |
| 71 | Singh Raman R K , Khanna A S , Tiwari R K , et al . Influence of grain size on the oxidation resistance of 2 1 4 Cr-1Mo steel [J]. Oxid. Met., 1992, 37: 1 |
| 72 | Bai Y , Liu Z D , Xie J X , et al . Effect of pre-oxidation treatment on the behavior of high temperature oxidation in steam of G115 steel [J]. Acta Metall. Sin., 2018, 54: 895 |
| 72 | 白 银, 刘正东, 谢建新 等 . 预氧化处理对G115钢高温蒸气氧化行为的影响 [J]. 金属学报, 2018, 54: 895 |
| 73 | Shen K , Cai W H , Du S M , et al . Effect of shot peening on high-temperature steam oxidation behavior of martensitic heat-resistant steel [J]. Heat Treat. Met., 2021, 46(2): 66 |
| 73 | 谌 康, 蔡文河, 杜双明 等 . 喷丸对马氏体耐热钢高温蒸汽氧化行为的影响 [J]. 金属热处理, 2021, 46(2): 66 |
| 74 | Dong M , Xie X Y , Zhu Y C , et al . Preparation of FeAl penetration layer on G115 and T92 steel surface and its oxidation resistance to high temperature steam [J]. Trans. Mater. Heat Treat., 2021, 42(5): 135 |
| 74 | 董 猛, 谢逍原, 朱阳存 等 . G115和T92钢表面FeAl渗层制备及其抗高温水蒸汽氧化性能 [J]. 材料热处理学报, 2021, 42(5): 135 |
| 75 | Liu Z D , Chen Z Z , Bao H S , et al . Argon arc welding wire for heat resistant steel G 115 [P] Chin Pat., 201611250159.4, 2017 |
| 75 | 刘正东, 陈正宗, 包汉生 等 . G115耐热钢用氩弧焊焊丝 [P]. 中国专利, 201611250159.4, 2017) |
| 76 | Li H , She Y T , Li X Y , et al . TIG welding wire of steel for steam temperature ultra supercritical thermal power unit and its preparation method [P]. Chin Pat., 201610961348.2, 2017 |
| 76 | 李 浩, 佘英堂, 李欣雨 等 . 蒸汽温度超超临界火电机组用钢的TIG焊焊丝及其制备方法 [P]. 中国专利, 201610961348.2, 2017) |
| 77 | Xu L Y , Pang H N , Zhao L , et al . Microstructure and mechanical properties of CMT + P welding process on G115 steel [J]. Trans. China Weld. Inst., 2020, 41(8): 1 |
| 77 | 徐连勇, 庞红宁, 赵 雷 等 . G115钢CMT+P焊接工艺及组织和性能 [J]. 焊接学报, 2020, 41(8): 1 |
| 78 | Qi X Q , Liu Z H , Li X . Effect of different tempering temperature on the microstructure and properties of G115 steel weld [J]. J. Phys.: Conf. Ser., 2021, 1865: 032023 |
| 79 | Matsunaga T , Hongo H , Tabuchi M , et al . Suppression of grain refinement in heat-affected zone of 9Cr-3W-3Co-VNb steels [J]. Mater. Sci. Eng., 2016, A655: 168 |
| 80 | Li L P , Liang J , Zhao L , et al . Effect of PWHT temperature on microstructure and mechanical properties of G115/T92 dissimilar steel welded joint [J]. Heat Treat. Met., 2019, 44(2): 68 |
| 80 | 李林平, 梁 军, 赵 雷 等 . 焊后热处理温度对G115/T92异种钢接头组织及力学性能的影响 [J]. 金属热处理, 2019, 44(2): 68 |
| 81 | Li L P , Liang J , Zhao L , et al . Microstructure and mechanical properties of G115/T92 dissimilar welded joints [J]. Trans. Mater. Heat Treat., 2018, 39(9): 138 |
| 81 | 李林平, 梁 军, 赵 雷 等 . G115/T92异种钢焊接接头的显微组织及力学性能 [J]. 材料热处理学报, 2018, 39(9): 138 |
| 82 | Yang M H , Zhang Z , Liu Y R , et al . Fine-grain heat affected zone softening of G115/Sanicro25 dissimilar steel welded joints after post-weld heat treatment [J]. Int. J. Press. Vessels Pip., 2020, 188: 104253 |
| 83 | Xiong J K , Li T , Yuan X J , et al . Improvement in weldment of dissimilar 9% Cr heat-resistant steels by post-weld heat treatment [J]. Metals, 2020, 10: 1321 |
| 84 | Zhang Y Y , Gou G Q . Microstructure and properties of 9Cr-3W-3Co steel joint by shielded metal arc welding [J]. AIP Adv., 2020, 10: 045034 |
| 85 | Li T . Study on mechanical characteristics and microstructure of TIG welding on dissimilar 9%Cr heat-resistant steels [D]. Chongqing: Chongqing University, 2020 |
| 85 | 李 婷 . 异种9%Cr马氏体耐热钢TIG熔化焊组织及性能研究 [D]. 重庆: 重庆大学, 2020 |
| 86 | Liu Z D . Industrially integrated metallurgical processing of novel G115(R) martensitic heat resistant steel pipes [A]. Proceedings of the 12th Academic Conference on chemical, metallurgical and material engineering, Chinese Academy of Engineering [C]. Zhengzhou, 2018: 348 |
| 86 | 刘正东 . G115(R)马氏体耐热钢管研制 [A]. 中国工程院化工、冶金与材料工程第十二届学术会议论文集 [C]. 郑州, 2018: 348 |
| 87 | Lei B W , Li Y Q , Pang H P , et al . Manufacturing technology of novel heat resistant steel G115 large-diameter heavy wall seamless pipe [J]. Met. Funct. Mater., 2020, 27(5): 14 |
| 87 | 雷丙旺, 李永清, 庞海平 等 . 新型马氏体耐热钢G115大口径厚壁无缝钢管制造技术 [J]. 金属功能材料, 2020, 27(5): 14 |
| 88 | Cong X Z , Peng X N , Peng X K , et al . Heat treatment for G115 large diameter pipe fittings [J]. Heat Treat. Met., 2021, 46(3): 90 |
| 88 | 丛相州, 彭杏娜, 彭先宽 等 . G115钢大口径管件的热处理 [J]. 金属热处理, 2021, 46(3): 90 |
| 89 | Li H Z , Liang J , Xu L Y , et al . Effect of cyclic normalization on microstructure and impact toughness of 9Cr3W3Co steel [J]. Trans. Mater. Heat Treat., 2017, 38(10): 67 |
| 89 | 李海昭, 梁 军, 徐连勇 等 . 循环正火处理对9Cr3W3Co钢组织及冲击韧性的影响 [J]. 材料热处理学报, 2017, 38(10): 67 |
| 90 | Ma L T , Liu Z D , Bai Y . Effect of doubled normalization on microstructure and impact toughness of 9Cr3W3Co steel [J]. Heat Treat. Met., 2017, 42(3): 18 |
| 90 | 马龙腾, 刘正东, 白 银 . 二次正火处理对9Cr3W3Co钢微观组织和冲击韧性的影响 [J]. 金属热处理, 2017, 42(3): 18 |
| 91 | Peng X N , Cong X Z , Peng X K , et al . Experimental study on hot press bending process for G115 steel [J]. Forg. Stamping Technol., 2021, 46(2): 142 |
| 91 | 彭杏娜, 丛相州, 彭先宽 等 . G115钢热压弯成形工艺试验研究 [J]. 锻压技术, 2021, 46(2): 142 |
/
| 〈 |
|
〉 |