研究论文

微弧氧化6082-T6铝合金的高周疲劳性能及残余应力松弛机理

  • 苏凯新 ,
  • 张继旺 ,
  • 张艳斌 ,
  • 闫涛 ,
  • 李行 ,
  • 纪东东
展开
  • 1.西南交通大学 牵引动力国家重点实验室 成都 610031
    2.西南交通大学 机械工程学院 成都 610031
    3.保德利电气设备有限责任公司 宝鸡 721000
苏凯新,男,1996年生,博士生

收稿日期: 2020-12-29

  修回日期: 2021-01-29

  网络出版日期: 2021-06-29

基金资助

国家自然科学基金项目(52075457)

High-Cycle Fatigue Properties and Residual Stress Relaxation Mechanism of Micro-Arc Oxidation 6082-T6 Aluminum Alloy

  • Kaixin SU ,
  • Jiwang ZHANG ,
  • Yanbin ZHANG ,
  • Tao YAN ,
  • Hang LI ,
  • Dongdong JI
Expand
  • 1.State Key Laboratory of Traction Power, Southwest Jiaotong University, Chengdu 610031, China
    2.School of Mechanical Engineering, Southwest Jiaotong University, Chengdu 610031, China
    3.Bj -baodeli Electrical Equipment Co. , Ltd. , Baoji 721000, China
ZHANG Jiwang, Tel: (028)87600843, E-mail: zhangjiwang@swjtu.edu.cn

Received date: 2020-12-29

  Revised date: 2021-01-29

  Online published: 2021-06-29

Supported by

National Natural Science Foundation of China(52075457)

摘要

为研究微弧氧化(MAO)处理对高速铁路接触网腕臂用6082-T6铝合金高周疲劳性能的影响,开展了6082-T6铝合金未处理(UP)及MAO处理试样的旋转弯曲疲劳实验,获得了循环应力与疲劳寿命(S-N)曲线。采用激光共聚焦显微镜、纳米压痕仪、XRD和SEM研究了试样的表面形貌及粗糙度、剖面形貌、剖面纳米硬度和弹性模量梯度分布、膜层相成分以及疲劳断口形貌,采用X射线残余应力分析仪获得了不同循环应力下MAO试样膜层-基体界面残余应力的松弛行为。实验结果表明:微弧氧化处理试样的表面形貌严重恶化,并且在膜层与基体交界处存在较大的残余拉应力,导致疲劳性能大幅度降低。此外,当循环应力和基体残余拉应力(平衡膜层的残余应力)之和大于基体材料的循环屈服强度时,膜层-基体界面残余拉应力出现松弛。最后,采用失配应变理论分析了膜层-基体界面残余拉应力的形成机理及其在外加循环应力作用下的松弛机理,深入讨论了在高循环应力和低循环应力作用下,膜层对基体疲劳性能的影响。

本文引用格式

苏凯新 , 张继旺 , 张艳斌 , 闫涛 , 李行 , 纪东东 . 微弧氧化6082-T6铝合金的高周疲劳性能及残余应力松弛机理[J]. 金属学报, 2022 , 58(3) : 334 -344 . DOI: 10.11900/0412.1961.2020.00528

Abstract

Recently, the fatigue failure of aluminum alloy components of high-speed railway catenary is becoming increasingly serious, which causes a threat to the normal operation of high-speed trains. In this study, the effect of micro-arc oxidation (MAO) coating on the high-cycle fatigue properties of 6082-T6 aluminum alloy for the catenary cantilever of the high-speed railway was studied. First, the rotating bending fatigue tests of untreated (UP) and MAO specimens of 6082-T6 aluminum alloy were performed. Then, the surface morphology and roughness, cross-section morphology, nanoindentation hardness, and elastic modulus gradient distribution, phase composition of MAO coating, and fatigue fracture morphology of the fatigue samples were studied by a confocal laser microscope, nanoindentation, XRD, and SEM. The experimental results showed that after MAO treatment, a large number of micro-cracks and pores were formed on the surface of the samples, and the morphology of the samples severely deteriorated. The XRD results indicated that the closer the coating surface, the stronger was the diffraction peaks of α-Al2O3 and γ-Al2O3. Besides, there was the higher tensile residual stress at the coating-substrate interface, which led to a significant reduction in fatigue properties. The fatigue strength decreased by 26.7% at 2 × 107 cyc. Finally, the formation and relaxation mechanisms of tensile residual stress under cyclic stress were analyzed using mismatch strain theory, and the effects of the coating on the fatigue properties of the substrate under high and low cyclic stresses were discussed further.

参考文献

1 Starke E A, Staley J T. Application of modern aluminum alloys to aircraft [J]. Prog. Aeosp. Sci., 1996, 32: 131
2 Heinz A, Haszler A, Keidel C, et al. Recent development in aluminium alloys for aerospace applications [J]. Mater. Sci. Eng., 2000, A280: 102
3 Krishna L R, Somaraju K R C, Sundararajan G. The tribological performance of ultra-hard ceramic composite coatings obtained through microarc oxidation [J]. Surf. Coat. Technol., 2003, 163-164: 484
4 Krishna L R, Purnima A S, Sundararajan G. A comparative study of tribological behavior of microarc oxidation and hard-anodized coatings [J]. Wear, 2006, 261: 1095
5 Lonyuk B, Apachitei I, Duszczyk J. The effect of oxide coatings on fatigue properties of 7475-T6 aluminium alloy [J]. Surf. Coat. Technol., 2007, 201: 8688
6 Wasekar N P, Jyothirmayi A, Sundararajan G. Influence of prior corrosion on the high cycle fatigue behavior of microarc oxidation coated 6061-T6 Aluminum alloy [J]. Int. J. Fatigue, 2011, 33: 1268
7 Nie X, Meletis E I, Jiang J C, et al. Abrasive wear/corrosion properties and TEM analysis of Al2O3 coatings fabricated using plasma electrolysis [J]. Surf. Coat. Technol., 2002, 149: 245
8 Barik R C, Wharton J A, Wood R J K, et al. Corrosion, erosion and erosion-corrosion performance of plasma electrolytic oxidation (PEO) deposited Al2O3 coatings [J]. Surf. Coat. Technol., 2005, 199: 158
9 Wen L, Wang Y M, Zhou Y, et al. Corrosion evaluation of microarc oxidation coatings formed on 2024 aluminium alloy [J]. Corros. Sci., 2010, 52: 2687
10 Gecu R, Yurekturk Y, Tekoglu E, et al. Improving wear resistance of 304 stainless steel reinforced AA7075 aluminum matrix composite by micro-arc oxidation [J]. Surf. Coat. Technol., 2019, 368: 15
11 Kong D J, Liu H, Wang J C. Effects of micro arc oxidation on fatigue limits and fracture morphologies of 7475 high strength aluminum alloy [J]. J. Alloys Compd., 2015, 650: 393
12 Dai W B, Liu Z H, Li C Y, et al. Fatigue life of micro-arc oxidation coated AA2024-T3 and AA7075-T6 alloys [J]. Int. J. Fatigue, 2019, 124: 493
13 Wang Y M, Zhang P F, Guo L X, et al. Effect of microarc oxidation coating on fatigue performance of Ti-Al-Zr alloy [J]. Appl. Surf. Sci., 2009, 255: 8616
14 Khan R H U, Yerokhin A, Li X, et al. Surface characterisation of DC plasma electrolytic oxidation treated 6082 aluminium alloy: Effect of current density and electrolyte concentration [J]. Surf. Coat. Technol., 2010, 205: 1679
15 Leoni A, Apachitei I, Riemslag A C, et al. In vitro fatigue behavior of surface oxidized Ti35Zr10Nb biomedical alloy [J]. Mater. Sci. Eng., 2011, C31: 1779
16 Madhavi Y, Krishna L R, Narasaiah N. Influence of micro arc oxidation coating thickness and prior shot peening on the fatigue behavior of 6061-T6 Al alloy [J]. Int. J. Fatigue, 2019, 126: 297
17 Oliver W C, Pharr G M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments [J]. J. Mater. Res., 1992, 7: 1564
18 Lin J, Ma N S, Lei Y P, et al. Measurement of residual stress in arc welded lap joints by cosα X-ray diffraction method [J]. J. Mater. Process. Technol., 2017, 243: 387
19 Dai W B, Li C Y, He D, et al. Influence of duty cycle on fatigue life of AA2024 with thin coating fabricated by micro-arc oxidation [J]. Surf. Coat. Technol., 2019, 360: 347
20 Li J, Sun Q, Zhang Z P, et al. Theoretical estimation to the cyclic yield strength and fatigue limit for alloy steels [J]. Mech. Res. Commun., 2009, 36: 316
21 B?umel A, Seeger T. Materials Data for Cyclic Loading [M]. Amsterdam: Elsevier, 1990: 1
22 Wasekar N P, Ravi N, Babu P S, et al. High-cycle fatigue behavior of microarc oxidation coatings deposited on a 6061-T6 Al alloy [J]. Metall. Mater. Trans., 2010, 41A: 255
23 Gu W C, Lv G H, Chen H, et al. Characterisation of ceramic coatings produced by plasma electrolytic oxidation of aluminum alloy [J]. Mater. Sci. Eng., 2007, A447: 158
24 Krishna L R, Gupta P S V N B, Sundararajan G. The influence of phase gradient within the micro arc oxidation (MAO) coatings on mechanical and tribological behaviors [J]. Surf. Coat. Technol., 2015, 269: 54
25 Xue W B, Deng Z W, Chen R Y, et al. Distribution of hardness and elastic modulus near the interface between aluminum alloy substrate and microarc oxidation coating [J]. Acta Metall. Sin., 1999, 35: 638
25 薛文斌, 邓志威, 陈如意等. 铝合金微弧氧化膜与基体界面区的硬度和弹性模量分布 [J]. 金属学报, 1999, 35: 638
26 Malyshev V. Mikrolichtbogen-oxidation: EIN neuartiges verfahren zur verfestigung von aluminiumoberfl?chen [J]. Metalloberflaeche, 1995, 49: 606
27 Dai W B, Li C Y, He D, et al. Mechanism of residual stress and surface roughness of substrate on fatigue behavior of micro-arc oxidation coated AA7075-T6 alloy [J]. Surf. Coat. Technol., 2019, 380: 125014
28 Su K X, Zhang J W, Li H, et al. Analysis on the fatigue properties of shot-peened Al-Si-Mg alloy and its fatigue life prediction [J]. J. Mater. Eng. Perform., 2020, 29: 5114
29 Schijve J. Fatigue of Structures and Materials [M]. New York: Springer Science & Business Media, 2001: 1
30 Hadzima B, Novy F, Tr?ko L, et al. Shot peening as a pre-treatment to anodic oxidation coating process of AW 6082 aluminum for fatigue life improvement [J]. Int. J. Adv. Manuf. Technol., 2017, 93: 3315
31 Krishna L R, Madhavi Y, Sahithi T, et al. Influence of prior shot peening variables on the fatigue life of micro arc oxidation coated 6061-T6 Al alloy [J]. Int. J. Fatigue, 2018, 106: 165
32 Freund L B, Suresh S. Thin Film Materials: Stress, Defect Formation and Surface Evolution [M]. Cambridge: Cambridge University Press, 2004: 1
33 Dai W B, Hao J, Li C Y, et al. Residual stress relaxation and duty cycle on high cycle fatigue life of micro-arc oxidation coated AA7075-T6 alloy [J]. Int. J. Fatigue, 2020, 130: 105283
34 Kim J C, Cheong S K, Noguchi H. Residual stress relaxation and low- and high-cycle fatigue behavior of shot-peened medium-carbon steel [J]. Int. J. Fatigue, 2013, 56: 114
35 Zhong W, Ding Y L, Song Y S, et al. Relaxation effect of welding residual stress in deck-to-rib joints [J]. J. Zhejiang Univ. (Eng. Sci.), 2020, 54: 83
35 钟 雯, 丁幼亮, 宋永生等. 顶板-纵肋焊接细节残余应力的松弛效应 [J]. 浙江大学学报(工学版), 2020, 54: 83
36 Zhang J W, Lu L T, Shiozawa K, et al. Analysis on fatigue property of microshot peened railway axle steel [J]. Mater. Sci. Eng., 2011, A528: 1615
37 Ishihara S, Saka S, Nan Z Y, et al. Prediction of corrosion fatigue lives of aluminium alloy on the basis of corrosion pit growth law [J]. Fatigue Fract. Eng. Mater. Struct., 2006, 29: 472
文章导航

/