新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制
收稿日期: 2020-12-07
修回日期: 2021-01-28
网络出版日期: 2021-06-10
基金资助
国家重点研发计划项目(2018YFA0702900);国家自然科学基金项目(51774265);国家科技重大专项项目(2019ZX06004010);中国科学院2017年度创新交叉团队和中国科学院青年创新促进会项目
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism
Received date: 2020-12-07
Revised date: 2021-01-28
Online published: 2021-06-10
Supported by
National Key Research and Development Program of China(2018YFA0702900);National Natural Science Foundation of China(51774265);National Science and Technology Major Project of China(2019ZX06004010);Program of CAS Interdisciplinary Innovation Team and Youth Innovation Promotion Association, CAS
为解决镍基高温合金的焊接难题,以新型Ni-Co基高温合金为实验材料,采用塑性变形连接的新方法,实现了新型Ni-Co基高温合金的连接。通过OM、EBSD、TEM等分析手段探究了界面的再结晶行为及界面的愈合机制。结果表明,1150℃进行塑性变形连接时,合金的变形抗力小,不易开裂。不同变形量的连接实验表明,在40%的变形量下,合金可以实现界面的完全愈合,其力学性能达到基体同等水平。在塑性变形过程中,界面附近的粗大晶粒首先发生细化,随着变形量的增加,细化的晶粒在连续动态再结晶的辅助作用下,通过界面晶界的迁移消除了原始连接界面,实现界面的愈合。
关键词: Ni-Co基高温合金; 塑性变形连接; 动态再结晶
任少飞 , 张健杨 , 张新房 , 孙明月 , 徐斌 , 崔传勇 . 新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制[J]. 金属学报, 2022 , 58(2) : 129 -140 . DOI: 10.11900/0412.1961.2020.00493
Superalloys with excellent high-temperature resistance and oxidation resistance have been widely used in aviation and energy fields. The new Ni-Co base superalloy is considered a candidate for the next generation of turbine discs due to its higher performance of mechanical properties and microstructure stability at high temperatures. However, tungsten inert gas (TIG) welding, metal inert gas (MIG) welding, and other welding techniques are not suitable for welding the new Ni-Co base superalloy because the Al + Ti content of the alloy reaches 7.5%, while traditional welding techniques (electron beam welding, friction welding, and diffusion welding) also have some disadvantages. For example, friction welding has certain requirements on the shape of the sample, and it is not suitable for welding large-volume alloys. Diffusion welding requires a long heat retention period and a harmful precipitation phase exists at the interface. A new welding method is applied in this study to solve the problem of welding nickel-based superalloy, achieving a better bonding effect. The Gleeble 3500 thermal simulator was used to study the plastic deformation bonding of Ni-Co base superalloys in a temperature range of 1000-1200oC and a strain range of 5%-40% with a strain rate of 0.001 s-1. The recrystallization behavior of the interface was studied by OM, EBSD, and TEM, and the bonding mechanism of the interface was clarified. The results showed that the resistance to deformation of the alloy was low when the plastic deformation bonding was performed at 1150oC, and there was no risk of cracking of the alloy. Plastic deformation bonding experiments with different deformations had shown that the alloy can achieve complete bonding of the interface under the condition of 40% deformation, and its mechanical properties can reach the same level as the matrix. The tensile fracture analysis showed that the fracture profile of the 40% deformed joint was consistent with the base material, showing a ductile fracture pattern. The results of EBSD and TEM showed that the coarse grains near the interface were first refined during the plastic deformation. With the increase of deformation, the refined grain removed the original interface by the migration of the interfacial grain boundaries with the assistance of a continuous dynamics recrystallization process and ultimately led to the bonding of the interface.
| 1 | Lin Y C , Wu X Y , Chen X M , et al . EBSD study of a hot deformed nickel-based superalloy [J]. J. Alloys Compd., 2005, 640: 101 |
| 2 | Yang X W , Li W Y , Li J L , et al . Finite element modeling of the linear friction welding of GH4169 superalloy [J]. Mater. Des., 2015, 87: 215 |
| 3 | Chen X M , Lin Y C , When D X , et al . Dynamic recrystallization behavior of a typical nickel-based superalloy during hot deformation [J]. Mater. Des., 2014, 57: 568 |
| 4 | Qu J L , Xie J F , Bi Z N , et al . Hot deformation characteristics and dynamic recrystallization mechanism of GH4730 Ni-based superalloy [J]. J. Alloys Compd., 2019, 785: 918 |
| 5 | Xiang X M , Jiang H , Dong J X , et al . As-cast microstructure characteristic and homogenization of a newly developed hard-deformed Ni-based superalloy GH4975 [J]. Acta Metall. Sin., 2020, 56: 988 |
| 5 | 向雪梅, 江 河, 董建新 等 . 难变形高温合金GH4975的铸态组织及均匀化 [J]. 金属学报, 2020, 56: 988 |
| 6 | Zhang Y , Li X X , Wei K , et al . Hot Deformation characteristics of novel wrought superalloy GH4975 extruded rod used for 850oC turbine disc [J]. Acta Metall. Sin., 2020, 56: 1401 |
| 6 | 张 勇, 李鑫旭, 韦 康 等 . 850℃涡轮盘用新型变形高温合金GH4975挤压棒材热变形规律研究 [J]. 金属学报, 2020, 56: 1401 |
| 7 | Bi Z N , Qin H L , Dong Z G , et al . Residual stress evolution and its mechanism during the manufacture of superalloy disk forgings [J]. Acta Metall. Sin., 2019, 55: 1160 |
| 7 | 毕中南, 秦海龙, 董志国 等 . 高温合金盘锻件制备过程残余应力的演化规律及机制 [J]. 金属学报, 2019, 55: 1160 |
| 8 | Cui C Y , Gu Y F , Ping D H , et al . Microstructural evolution and mechanical properties of a Ni-based superalloy, TMW-4 [J]. Metall. Mater. Trans., 2009, 40A: 282 |
| 9 | Cui C Y , Gu Y F , Yuan Y , et al . Enhanced mechanical properties in a new Ni-Co base superalloy by controlling microstructures [J]. Mater. Sci. Eng., 2011, A528 : 5465 |
| 10 | Yuan Y , Gu Y F , Zhong Z H , et al . Creep mechanisms of a new Ni-Co-base disc superalloy at an intermediate temperature [J]. J. Microsc., 2012, 248: 34 |
| 11 | Yuan Y , Gu Y F , Cui C Y , et al . A novel strategy for the design of advanced engineering alloys—Strengthening turbine disk superalloys via twinning structures [J]. Adv. Eng. Mater., 2011, 13: 296 |
| 12 | Gu Y F , Cui C Y , Yuan Y , et al . Research progress in a high performance cast & wrought superalloy for turbine disc applications [J]. Acta Metall. Sin., 2015, 51: 1191 |
| 12 | 谷月峰, 崔传勇, 袁 勇 等 . 一种高性能航空涡轮盘用铸锻合金的研究进展 [J]. 金属学报, 2015, 51: 1191 |
| 13 | Ye X , Hua X M , Wang M , et al . Controlling hot cracking in Ni-based Inconel-718 superalloy cast sheets during tungsten inert gas welding [J]. J. Mater. Process. Technol., 2015, 222: 381 |
| 14 | Han K , Wang H Q , Shen L , et al . Analysis of cracks in the electron beam welded joint of K465 nickel-base superalloy [J]. Vacuum, 2018, 157: 21 |
| 15 | Osoba L O , Ding R G , Ojo O A . Microstructural analysis of laser weld fusion zone in Haynes 282 superalloy [J]. Mater. Charact., 2012, 65: 93 |
| 16 | Ravisankar B , Krishnamoorthi J , Ramakrishnan S S , et al . Diffusion bonding of SU 263 [J]. J. Mater. Process. Technol., 2009, 209: 2135 |
| 17 | Sah I , Kim D , Lee H J , et al . The recovery of tensile ductility in diffusion-bonded Ni-base alloys by post-bond heat treatments [J]. Mater. Des., 2013, 47: 581 |
| 18 | Zhang G , Chandel R S , Seow H P . Solid state diffusion bonding of Inconel 718 [J]. Sci. Technol. Weld. Joining., 2001, 6: 235 |
| 19 | Xiong J T , Yuan L , Zhu Y , et al . Diffusion bonding of nickel-based superalloy GH4099 with pure nickel interlayer [J]. J. Mater. Sci., 2019, 54: 6552 |
| 20 | Uday M B , Ahmad Fauzi M N , Zuhailawati H , et al . Advances in friction welding process: A review [J]. Sci. Technol. Weld. Joining, 2010, 15: 534 |
| 21 | Xie B J , Sun M Y , Xu B , et al . Dissolution and evolution of interfacial oxides improving the mechanical properties of solid state bonding joints [J]. Mater. Des., 2018, 157: 437 |
| 22 | Jiang H Y , Sun M Y , Wu M F , et al . Microstructure and properties of 7075 aluminum alloy hot compress bonding joint [J]. Heat Treat. Met., 2020, 45(2): 46 |
| 22 | 江海洋, 孙明月, 吴铭方 等 . 7075铝合金热变形连接接头的组织与性能 [J]. 金属热处理, 2020, 45(2): 46 |
| 23 | Zhang J Y , Xu B , Tariq N H , et al . Microstructure evolutions and interfacial bonding behavior of Ni-based superalloys during solid state plastic deformation bonding [J]. J. Mater. Sci. Technol., 2020, 46: 1 |
| 24 | Sun M Y , Xu B , Xie B J , et al . Research advances on homogenization manufacturing of heavy components by metal additive forging [J]. Chin. Sci. Bull., 2020, 65: 3043 |
| 24 | 孙明月, 徐 斌, 谢碧君 等 . 大锻件均质化构筑成形研究进展 [J]. 科学通报, 2020, 65: 3043 |
| 25 | Zhou L Y , Feng S B , Sun M Y , et al . Interfacial microstructure evolution and bonding mechanisms of 14YWT alloys produced by hot compression bonding [J]. J. Mater. Sci. Technol., 2019, 35: 1671 |
| 26 | Zhang J Y , Sun M Y , Xu B , et al . Evolution of the interfacial microstructure during the plastic deformation bonding of copper [J]. Mater. Sci. Eng., 2019, A746 : 1 |
| 27 | Xie B J , Sun M Y , Xu B , et al . Oxidation of stainless steel in vacuum and evolution of surface oxide scales during hot-compression bonding [J]. Corros. Sci., 2019, 147: 41 |
| 28 | Zhao G D , Yu L X , Qi F , et al . The minor precipitation at the final stage of U720Li solidification [J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 518 |
| 29 | Liu P , Zhang R , Yuan Y , et al . Hot deformation behavior and workability of a Ni-Co based superalloy [J]. J. Alloys Compd., 2020, 83: 154618 |
| 30 | Liu F F , Chen J Y , Dong J X , et al . The hot deformation behaviors of coarse, fine and mixed grain for Udimet 720Li superalloy [J]. Mater. Sci. Eng., 2016, A651: 102 |
| 31 | Wu Y S , Liu Z , Qin X Z , et al . Effect of initial state on hot deformation and dynamic recrystallization of Ni-Fe based alloy GH984G for steam boiler applications [J]. J. Alloys Compd., 2019, 795: 370 |
| 32 | Paggi A , Angella G , Donnini R . Strain induced grain boundary migration effects on grain growth of an austenitic stainless steel during static and metadynamic recrystallization [J]. Mater. Charact., 2015, 107: 174 |
| 33 | Sakai T . Dynamic recrystallization microstructures under hot working conditions [J]. J. Mater. Process. Technol., 1995, 53: 349 |
| 34 | Cao Y , Di H S , Zhang J C , et al . Research on dynamic recrystallization behavior of Incoloy 800H [J]. Acta Metall. Sin., 2012, 48: 1175 |
| 34 | 曹 宇, 邸洪双, 张洁岑 等 . 800H合金动态再结晶行为研究 [J]. 金属学报, 2012, 48: 1175 |
| 35 | Hu G X , Cai X , Rong Y H . Fundamentals of Materials Science [M]. Shanghai: Shanghai Jiao Tong University Press, 2010: 5 |
| 35 | 胡赓祥, 蔡 珣, 戎咏华 . 材料科学基础 [M]. 上海: 上海交通大学出版社, 2010: 5 |
| 36 | Xie B C , Yu H , Sheng T , et al . DDRX and CDRX of an as-cast nickel-based superalloy during hot compression at γ′ sub-/super-solvus temperatures [J]. J. Alloys Compd., 2019, 803: 16 |
| 37 | Hu W , Ponge D , Gottstein G . Origin of grain boundary motion during diffusion bonding by hot pressing [J]. Mater. Sci. Eng., 1995, A190: 223 |
| 38 | Mandal S , Jayalakshmi M , Bhaduri A K . et al . Effect of strain rate on the dynamic recrystallization behavior in a nitrogen-enhanced 316L(N) [J]. Metall. Mater. Trans.,2014, 45A: 5645 |
| 39 | Bellier S P , Doherty R D . The structure of deformed aluminium and its recrystallization—Investigations with transmission Kossel diffraction [J]. Acta. Metall., 1977, 25: 521 |
| 40 | Sakai T , Belyakov A , Kaibyshev R , et al . Dynamic and post-dynamic recrystallization under hot, cold and severe plastic deformation conditions [J]. Prog. Mater. Sci., 2014, 60: 130 |
| 41 | Zhong X T , Wang L , Liu F . Study on formation mechanism of necklace structure in discontinuous dynamic recrystallization of Incoloy 028 [J]. Acta Metall. Sin., 2018, 54: 969 |
| 41 | 钟茜婷, 王 磊, 刘 峰 . Incoloy 028合金不连续动态再结晶中链状组织形成机理研究 [J]. 金属学报, 2018, 54: 969 |
/
| 〈 |
|
〉 |