装甲防护陶瓷-金属叠层复合材料界面研究进展
收稿日期: 2021-01-29
修回日期: 2021-05-11
网络出版日期: 2021-05-26
基金资助
国家自然科学基金项目(52074246);国防基础科研重点项目(JCKY2020408B002);山西省科技重大专项项目(20181101014)
Current Research Status of Interface of Ceramic-Metal Laminated Composite Material for Armor Protection
Received date: 2021-01-29
Revised date: 2021-05-11
Online published: 2021-05-26
Supported by
National Natural Science Foundation of China(52074246);National Defense Basic Scientific Research Key Program of China(JCKY2020408B002);Major Science and Technology Project of Shanxi Province(20181101014)
将陶瓷与金属以一定顺序逐层叠加,可制成叠层结构的复合材料,兼具陶瓷高强度、高硬度、低密度及金属强延展性的特点,从而应用于防弹装甲材料。但叠层材料存在界面结合弱、受冲击时裂纹易在界面处产生,且裂纹尖端应力集中导致界面处材料易脱黏等问题。本文针对陶瓷-金属叠层复合材料的界面结构及结合强度的问题,从界面结构的制备和观察、界面断裂的相场模拟、界面抗冲击性的有限元模拟和界面强度的第一原理计算等方面进行了综述,并对未来发展方向提出建议。
关键词: 陶瓷-金属叠层复合材料; 界面结合; 相场法模拟; 第一原理计算; 有限元仿真
赵宇宏 , 景舰辉 , 陈利文 , 徐芳泓 , 侯华 . 装甲防护陶瓷-金属叠层复合材料界面研究进展[J]. 金属学报, 2021 , 57(9) : 1107 -1125 . DOI: 10.11900/0412.1961.2021.00051
A composite material with a laminated structure can be fabricated through layer-by-layer stacking of ceramic and metal in a certain order. It has characteristics of high strength, high hardness, low density of ceramics, and strong ductility of metals; thus, it can be used for bulletproof armor materials. During bullet antipenetration, the ceramic panel is responsible for decelerating and breaking the projectile, and the metal backplate absorbs the kinetic energy of the bullet through plastic deformation, thereby forming a complete bulletproof armor system. However, there are some problems associated with laminated materials, such as the significant difference between the properties of ceramic and metal, weak interface bonding strength, and easy occurrence of tip cracks due to the increase in the internal stress of the impacted material. The ceramic-metal interface easily leads to a sudden change in material properties, and crack propagation and migration affect the properties. After being impacted, cracks first appear in the interlayer, where the interface bonding strength is still unideal, easily leading to a drop between the ceramic panel and metal backplate. In this study, the preparation and observation of interface structure, phase-field simulation of interface fracture, finite element simulation of interface impact resistance, meshless smoothed-particle hydrodynamic method for high-velocity impact and large deformation, and first-principles calculations of interface strength were reviewed. Finally, some suggestions are presented for future development: (1) Strengthening the research of ceramic toughening to enhance the matching degree between the ceramic panel and metal backplate, reducing the sudden change of ceramic to metal performance, and making the performance of ceramic-metal laminated materials more uniform is crucial. In addition, studying metal strengthening is necessary. On the premise of not damaging metal ductility, nano-phases can be added to prepare metal matrix composites for metal strengthening; (2) More multiscale research methods, such as phase-field method, finite element analysis, and first-principles calculations are needed, especially focusing on how to organically and effectively combine these methods. The complementary coupling of multiscale experimental research and computational simulation methods is a powerful tool for the interface design of ceramic-metal laminated materials in the future.
| 1 | Lee M, Yoo Y H. Analysis of ceramic/metal armour systems [J]. Int. J. Impact Eng., 2001, 25: 819 |
| 2 | Zaera R, Sánchez-Gálvez V. Analytical modelling of normal and oblique ballistic impact on ceramic/metal lightweight armours [J]. Int. J. Impact Eng., 1998, 21: 133 |
| 3 | Rowe R G, Skelly D W, Larsen M, et al. Microlaminated high temperature intermetallic composites [J]. Scr. Metall. Mater., 1994, 31: 1487 |
| 4 | Wang D C. Preparation and characterization of laminated Al/A2O3 composites with nacre-inspired hierarchical complexity [D]. Harbin: Harbin Institute of Technology, 2017 |
| 4 | 王道畅. 仿贝壳珍珠层结构叠层Al/Al2O3复合材料制备及性能测试 [D]. 哈尔滨: 哈尔滨工业大学, 2017 |
| 5 | Song H C, Liang Z Y, Zhang Z G. Gunship with ceramic/composite armor [J]. Aviat. Maint. Eng., 1994, (9): 9 |
| 5 | 宋焕成, 梁志勇, 张佐光. 武装直升机与陶瓷/复合材料装甲 [J]. 航空制造工程, 1994, (9): 9 |
| 6 | Hu Y L, Jiang F. Development and current status of armor ceramics [J]. Ordn. Mater. Sci. Eng., 1996, 19(5): 37 |
| 6 | 胡玉龙, 蒋 凡. 装甲陶瓷的发展现状和趋势 [J]. 兵器材料科学与工程, 1996, 19(5): 37 |
| 7 | Rashad M, Pan F S, Tang A T, et al. Effect of graphene nanoplatelets addition on mechanical properties of pure aluminum using a semi-powder method [J]. Prog. Nat. Sci.: Mater. Int., 2014, 24: 101 |
| 8 | Rashad M, Pan F S, Tang A T, et al. Development of magnesium-graphene nanoplatelets composite [J]. J. Compos. Mater., 2015, 49: 285 |
| 9 | Cao Z, Wang X D, Li J L, et al. Reinforcement with graphene nanoflakes in titanium matrix composites [J]. J. Alloys Compd., 2017, 696: 498 |
| 10 | Jiao F F, Liu M Y, Jiang F C, et al. Continuous carbon fiber reinforced Ti/Al3Ti metal-intermetallic laminate (MIL) composites fabricated using ultrasonic consolidation assisted hot pressing sintering [J]. Mater. Sci. Eng., 2019, A765: 138255 |
| 11 | Tasdemirci A, Tunusoglu G, Güden M. The effect of the interlayer on the ballistic performance of ceramic/composite armors: Experimental and numerical study [J]. Int. J. Impact Eng., 2012, 44: 1 |
| 12 | Gama B A, Bogetti T A, Fink B K, et al. Aluminum foam integral armor: A new dimension in armor design [J]. Compos. Struct., 2001, 52: 381 |
| 13 | Shen Z Y, Huang G H, He L M, et al. Preparation and mechanical properties of large-side TiAl/Ti3Al microlaminated thin sheets [J]. J. Mater. Eng., 2018, 46(5): 72 |
| 13 | 申造宇, 黄光宏, 何利民等. 大尺寸TiAl/Ti3Al微叠层超薄板制备和力学性能 [J]. 材料工程, 2018, 46(5): 72 |
| 14 | Wadley H N G, O'masta M R, Dharmasena K P, et al. Effect of core topology on projectile penetration in hybrid aluminum/alumina sandwich structures [J]. Int. J. Impact Eng., 2013, 62: 99 |
| 15 | Sadanandan S, Hetherington J G. Characterisation of ceramic/steel and ceramic/aluminium armours subjected to oblique impact [J]. Int. J. Impact Eng., 1997, 19: 811 |
| 16 | Yungwirth C J, O'connor J, Zakraysek A, et al. Explorations of hybrid sandwich panel concepts for projectile impact mitigation [J]. J. Am. Ceram. Soc., 2011, 94: s62 |
| 17 | übeyli M, Y?ld?r?m R O, ?gel B. Investigation on the ballistic behavior of Al2O3/Al2024 laminated composites [J]. J. Mater. Process. Technol., 2008, 196: 356 |
| 18 | Shirvanimoghaddam K, Khayyam H, Abdizadeh H, et al. Effect of B4C, TiB2 and ZrSiO4 ceramic particles on mechanical properties of aluminium matrix composites: Experimental investigation and predictive modelling [J]. Ceram. Int., 2016, 42: 6206 |
| 19 | Prakash A, Rajasankar J, Anandavalli N, et al. Influence of adhesive thickness on high velocity impact performance of ceramic/metal composite targets [J]. Int. J. Adhes. Adhes., 2013, 41: 186 |
| 20 | Medvedovski E. Ballistic performance of armour ceramics: Influence of design and structure. Part 1 [J]. Ceram. Int., 2010, 36: 2103 |
| 21 | Medvedovski E. Ballistic performance of armour ceramics: Influence of design and structure. Part 2 [J]. Ceram. Int., 2010, 36: 2117 |
| 22 | Li Y. Research progress on gradient metallic materials [J]. Mater. China, 2016, 35: 658 |
| 22 | 李 毅. 梯度结构金属材料研究进展 [J]. 中国材料进展, 2016, 35: 658 |
| 23 | Li W K, Han B H, Zhao Z M. Research progress in ceramics armor materials [J]. Spec. Cast. Nonferrous Alloys, 2018, 38: 259 |
| 23 | 李维锴, 韩保红, 赵忠民. 装甲防护陶瓷材料的研究进展 [J]. 特种铸造及有色合金, 2018, 38: 259 |
| 24 | Jiao L J, Li J. Application of ceramics-metal function gradient composite material in armor [J]. J. Sichuan Ordn., 2006, 27(4): 22 |
| 24 | 焦丽娟, 李 军. 陶瓷-金属功能梯度复合材料在装甲防护中的应用 [J]. 四川兵工学报, 2006, 27(4): 22 |
| 25 | Chao Z L, Jiang L T, Chen G Q, et al. The microstructure and ballistic performance of B4C/AA2024 functionally graded composites with wide range B4C volume fraction [J]. Composites, 2019, 161B: 627 |
| 26 | Yu H. Experimental study on penetration resistance of functionally graded materials [D]. Xi'an: Northwestern Polytechnical University, 2004 |
| 26 | 于 洪. 功能梯度材料抗侵彻性能试验研究 [D]. 西安: 西北工业大学, 2004 |
| 27 | Medvedovski E. Lightweight ceramic composite armour system [J]. Adv. Appl. Ceram., 2006, 105: 241 |
| 28 | Gao Y B, Zhang W, Yi C H, et al. Effects of adhesive layer on anti-penetration performance of ceramic/metal composite armour [J]. J. Vibrat. Shock, 2019, 38(13): 95 |
| 28 | 高玉波, 张 伟, 宜晨虹等. 黏结层对陶瓷/金属复合装甲抗弹性能的影响研究 [J]. 振动与冲击, 2019, 38(13): 95 |
| 29 | Li Y, Zhao J P, Zeng G, et al. Ni/Ni3Al microlaminate composite produced by EB-PVD and the mechanical properties [J]. Mater. Lett., 2004, 58: 1629 |
| 30 | Gao Y B, Zhang W, Xu P, et al. Influence of epoxy adhesive layer on impact performance of TiB2-B4C composites armor backed by aluminum plate [J]. Int. J. Impact Eng., 2018, 122: 60 |
| 31 | Wu Y, Wang X D, Liu D, et al. Development and application analysis of ceramic composites armor for helicopter [J]. J. Aeron. Mater., 2019, 39(5): 34 |
| 31 | 武 岳, 王旭东, 刘 迪等. 直升机陶瓷复合装甲发展现状及新型材料应用前景 [J]. 航空材料学报, 2019, 39(5): 34 |
| 32 | Fang L H, Zheng X Y, Ma L, et al. Armor protection development of tank & armored vehicle [J]. J. Sichuan Ordn., 2014, 35(2): 23 |
| 32 | 房凌晖, 郑翔玉, 马 丽等. 坦克装甲车辆装甲防护发展研究 [J]. 四川兵工学报, 2014, 35(2): 23 |
| 33 | Signetti S, Pugno N M. Evidence of optimal interfaces in bio-inspired ceramic-composite panels for superior ballistic protection [J]. J. Eur. Ceram. Soc., 2014, 34: 2823 |
| 34 | Wu C D, Shi R Y, Zhang J, et al. Synthesis of functionally graded AA7075-B4C composite with multi-level gradient structure [J]. Ceram. Int., 2019, 45: 7761 |
| 35 | Wang Y. The fabrication of iron and nickel-based metal-intermetallic-laminate composites and study on microstructure and properties of intermetallic layer [D]. Dalian: Dalian University of Technology, 2016 |
| 35 | 王 宇. 铁基及镍基金属/金属间化合物微叠层复合材料制备与化合物层组织性能研究 [D]. 大连: 大连理工大学, 2016 |
| 36 | Saravanan R A, Surappa M K. Fabrication and characterisation of pure magnesium-30 vol.% SiCP particle composite [J]. Mater. Sci. Eng., 2000, A276: 108 |
| 37 | Wu C, Li Y K, Wang Z. Evolution and mechanism of crack propagation method of interface in laminated Ti/Al2O3 composite [J]. J. Alloys Compd., 2016, 665: 37 |
| 38 | Li Y W, Xiao L R, Zhao X J, et al. Preparation, microstructure and properties of (SiCp/Cu)-copper foil laminated composites [J]. Acta Mater. Compos. Sin., 2018, 35: 896 |
| 38 | 李雨蔚, 肖来荣, 赵小军等. (SiCp/Cu)-铜箔叠层复合材料的制备与组织性能 [J]. 复合材料学报, 2018, 35: 896 |
| 39 | Jin Q, Ren X P, Li S X, et al. Effect of SiC fiber reinforcement on structure properties of laminated composite [J]. J. Plast. Eng., 2019, 26(5): 166 |
| 39 | 金 旗, 任学平, 李殊霞等. SiC纤维增强体对叠层复合材料结构性能的影响 [J]. 塑性工程学报, 2019, 26(5): 166 |
| 40 | Han Y Q, Lin C F, Han X X, et al. Fabrication, interfacial characterization and mechanical properties of continuous Al2O3 ceramic fiber reinforced Ti/Al3Ti metal-intermetallic laminated (CCFR-MIL) composite [J]. Mater. Sci. Eng., 2017, A688: 338 |
| 41 | Chen S, Zhang Z M, Zhang L. Review on dynamic fracture of ceramics materials in armor applications [J]. Spec. Cast. Nonferrous Alloys, 2016, 36: 401 |
| 41 | 陈 硕, 赵忠民, 张 龙. 陶瓷装甲材料动态力学研究进展 [J]. 特种铸造及有色合金, 2016, 36: 401 |
| 42 | de Oliveira Braga F, Lopes P H L M, Oliveira M S, et al. Thickness assessment and statistical optimization of a 3-layered armor system with ceramic front and curaua fabric composite/aluminum alloy backing [J]. Composites, 2019, 166B: 48 |
| 43 | Li L, Zhu Z C, Zhou D J. Application of finite element analysis in development of metal clad materials [J]. Southern Met., 2015, (6): 1 |
| 43 | 李 龙, 祝志超, 周德敬. 有限元分析在金属层状复合材料开发中的应用 [J]. 南方金属, 2015, (6): 1 |
| 44 | Zhang R, Han B, Li L, et al. Influence of prestress on ballistic performance of bi-layer ceramic composite armors: Experiments and simulations [J]. Compos. Struct., 2019, 227: 111258 |
| 45 | Zhang Z, Zhou J, Zhou J, et al. Research progress on preparation technology and failure mechanism of metal/ceramic laminated composites [J]. J. Aeron. Mater., 2020, 40(6): 33 |
| 45 | 张 振, 周 玖, 周 婕等. 金属陶瓷层状复合材料制备工艺与失效机制研究进展 [J]. 航空材料学报, 2020, 40(6): 33 |
| 46 | Heuzeroth F, Fritzsche J, Peuker U A. Wetting and its influence on the filtration ability of ceramic foam filters [J]. Particuology, 2015, 18: 50 |
| 47 | Bao S, Syvertsen M, Kvithyld A, et al. Wetting behavior of aluminium and filtration with Al2O3 and SiC ceramic foam filters [J]. Trans. Nonferrous Met Soc. China, 2014, 24: 3922 |
| 48 | Chaklader A C D, Armstrong A M, Misra S K. Interface reactions between metals and ceramics: IV, Wetting of sapphire by liquid copper-oxygen alloys [J]. J. Am. Ceram. Soc., 1968, 51: 630 |
| 49 | Mihailovic M, Volkov-Husovi? T, Raic K. Micro-and nano-scale wetting of reactive metal at metal/ceramic interface [J]. Adv. Sci. Technol., 2006, 45: 1526 |
| 50 | Zhao J Z, Gao J Q, Jin Z H. Preparation of three- dimensional structure silicon carbide reinforced aluminum matrix composites [J]. Ordn. Mater. Sci. Eng., 2004, 27(6): 11 |
| 50 | 赵敬忠, 高积强, 金志浩. 三维碳化硅结构增强铝基复合材料的制备 [J]. 兵器材料科学与工程, 2004, 27(6): 11 |
| 51 | Liu L X. Wettability of molten Ni-(Cr, W) alloys on alumina ceramic substrate [D]. Chongqing: Chongqing University of Technology, 2009 |
| 51 | 刘兰霄. 熔融Ni-(Cr, W)合金与Al2O3陶瓷的润湿性研究 [D]. 重庆: 重庆理工大学, 2009 |
| 52 | Wang W X. Study on interfacial wettability and mechanical properties of Al2O3/Cu composites [D]. Xi'an: Xi'anUniversity of Technology, 2019 |
| 52 | 王文祥. Al2O3/Cu复合材料的界面润湿性及其力学性能研究 [D]. 西安: 西安理工大学, 2019 |
| 53 | Chen S, Zhao Z M, Huang X G, et al. Interfacial microstructure and mechanical properties of laminated composites of TiB2-based ceramic and 42CrMo alloy steel [J]. Mater. Sci. Eng., 2016, A674: 335 |
| 54 | Cui X P, Fan G H, Geng L, et al. Influence of raw material selection and fabrication parameters on microstructure and properties of micro-laminated TiB2-TiAl composite sheets [J]. Mater. Sci. Eng., 2014, A589: 83 |
| 55 | Monazzah A H, Pouraliakbar H, Jandaghi M R, et al. Influence of interfacial adhesion on the damage tolerance of Al6061/SiCp laminated composites [J]. Ceram. Int., 2017, 43: 2632 |
| 56 | Zhang H, Yu J D, Pei X Y, et al. An overview of phase field approach to fracture [J]. Chin. J. High. Pressure Phys., 2019, 33(3): 030109 |
| 56 | 张 豪, 于继东, 裴晓阳等. 相场断裂方法发展概况 [J]. 高压物理学报, 2019, 33(3): 030109 |
| 57 | Hansen-D?rr A C, de Borst R, Hennig P, et al. Phase-field modelling of interface failure in brittle materials [J]. Comput. Methods Appl. Mech. Eng., 2019, 346: 25 |
| 58 | Roy S, Butz B, Wanner A. Damage evolution and domain-level anisotropy in metal/ceramic composites exhibiting lamellar microstructures [J]. Acta Mater., 2010, 58: 2300 |
| 59 | Bai Y H, Zhang B X, Du H L, et al. Efficient multiscale strategy for toughening HfB2 ceramics: A heterogeneous ceramic-metal layered architecture [J]. J. Am. Ceram. Soc., 2021, 104: 1841 |
| 60 | Hu Z J, Shen P, Jiang Q C. Developing high-performance laminated Cu/TiC composites through melt infiltration of Ni-doped freeze-cast preforms [J]. Ceram. Int., 2019, 45: 11686 |
| 61 | Guo H J, Zhao Y H, Sun Y Y, et al. Phase field crystal study of grain boundary structure and annihilation mechanism in low-angle grain boundary [J]. Superlattices Microstruct., 2019, 129: 163 |
| 62 | Zhao Y H, Zhang B, Hou H, et al. Phase-field simulation for the evolution of solid/liquid interface front in directional solidification process [J]. J. Mater. Sci. Technol., 2019, 35: 1044 |
| 63 | Sun Y Y, Zhao Y H, Zhao B J, et al. Multi-component phase-field simulation of microstructural evolution and elemental distribution in Fe-Cu-Mn-Ni-Al alloy [J]. Calphad, 2020, 69: 101759 |
| 64 | Yang Y B, Zhao Y H, Tian X L, et al. Microscopic phase-field simulation for precipitation process of Ni60Al20V20 medium entropy alloy [J]. Acta Phys. Sin., 2020, 69(14): 140201 |
| 64 | 杨一波, 赵宇宏, 田晓林等. Ni60Al20V20中熵合金沉淀过程微扩散相场法模拟 [J]. 物理学报, 2020, 69(14): 140201 |
| 65 | Griffith A A. The phenomena of rupture and flow in solids [J]. Philos. Trans. R. Soc., 1921, 221A: 163 |
| 66 | Francfort G A, Marigo J J. Revisiting brittle fracture as an energy minimization problem [J]. J. Mech. Phys. Solids, 1998, 46: 1319 |
| 67 | Bourdin B, Francfort G A, Marigo J J. Numerical experiments in revisited brittle fracture [J]. J. Mech. Phys. Solids, 2000, 48: 797 |
| 68 | Wilson Z A, Borden M J, Landis C M. A phase-field model for fracture in piezoelectric ceramics [J]. Int. J. Fract., 2013, 183: 135 |
| 69 | Ziaei-Rad V, Shen L, Jiang J H, et al. Identifying the crack path for the phase field approach to fracture with non-maximum suppression [J]. Comput. Methods Appl. Mech. Eng., 2016, 312: 304 |
| 70 | Kuhn C, Müller R. A continuum phase field model for fracture [J]. Eng. Fract. Mech., 2010, 77: 3625 |
| 71 | Duda F P, Ciarbonetti A, Sánchez P J, et al. A phase-field/gradient damage model for brittle fracture in elastic-plastic solids [J]. Int. J. Plast., 2015, 65: 269 |
| 72 | Ambati M, Gerasimov T, De Lorenzis L. Phase-field modeling of ductile fracture [J]. Comput. Mech., 2015, 55: 1017 |
| 73 | Liu Y Y C, Weng K X, Shen Y X. A manifold learning approach to accelerate phase field fracture simulations in the representative volume element [J]. SN Appl. Sci., 2020, 2: 1682 |
| 74 | Russ J, Slesarenko V, Rudykh S, et al. Rupture of 3D-printed hyperelastic composites: Experiments and phase field fracture modeling [J]. J. Mech. Phys. Solids, 2020, 140: 103941 |
| 75 | Li P F, Yvonnet J, Combescure C. An extension of the phase field method to model interactions between interfacial damage and brittle fracture in elastoplastic composites [J]. Int. J. Mech. Sci., 2020, 179: 105633 |
| 76 | Dean A, Reinoso J, Jha N K, et al. A phase field approach for ductile fracture of short fibre reinforced composites [J]. Theor. Appl. Fract. Mech., 2020, 106: 102495 |
| 77 | Hirshikesh, Pramod A L N, Annabattula R K, et al. Adaptive phase-field modeling of brittle fracture using the scaled boundary finite element method [J]. Comput. Methods Appl. Mech. Eng., 2019, 355: 284 |
| 78 | Wu J, McAuliffe C, Waisman H, et al. Stochastic analysis of polymer composites rupture at large deformations modeled by a phase field method [J]. Comput. Methods Appl. Mech. Eng., 2016, 312: 596 |
| 79 | Van Do T, Doan D H, Duc N D, et al. Phase-field thermal buckling analysis for cracked functionally graded composite plates considering neutral surface [J]. Compos. Struct., 2017, 182: 542 |
| 80 | Carlsson J, Isaksson P. Dynamic crack propagation in wood fibre composites analysed by high speed photography and a dynamic phase field model [J]. Int. J. Solids Struct., 2018, 144-145: 78 |
| 81 | Khaderi S N, Murali P, Ahluwalia R. Failure and toughness of bio-inspired composites: Insights from phase field modelling [J]. Comput. Mater. Sci., 2014, 95: 1 |
| 82 | Paggi M, Reinoso J. Revisiting the problem of a crack impinging on an interface: A modeling framework for the interaction between the phase field approach for brittle fracture and the interface cohesive zone model [J]. Comput. Methods Appl. Mech. Eng., 2017, 321: 145 |
| 83 | Zhang Z, Suo Z G. Split singularities and the competition between crack penetration and debond at a bimaterial interface [J]. Int. J. Solids Struct., 2007, 44: 4559 |
| 84 | Zhou Y S, Liang S, Wang D P, et al. Study on bulletpro of performance of ceramic/UHMWPE laminate/damping material composite target [J]. Compos. Sci. Eng., 2021, (4): 66 |
| 84 | 周越松, 梁 森, 王得盼等. 陶瓷/UHMWPE层合板/阻尼材料复合靶板防弹性能研究 [J]. 复合材料科学与工程, 2021, (4): 66 |
| 85 | Zhang L. Interface and high strain rate deformation behavior of layered B4C/Al composites [D]. Jinan: University of Jinan, 2020 |
| 85 | 张 柳. 层状B4C/Al复合材料的界面研究与高应变速率变形行为 [D]. 济南: 济南大学, 2020 |
| 86 | Liu Y Y. The design and toughing mechanism research of heterogeneous modulus laminated boron carbide composites [D]. Harbin: Harbin Engineering University, 2012 |
| 86 | 刘莹莹. 异质模量层状碳化硼复合材料的设计及韧化机制研究 [D]. 哈尔滨: 哈尔滨工程大学, 2012 |
| 87 | Yamamoto S, Sato K, Koseki H. A study on lateral impact of Timoshenko beam [J]. Comput. Mech., 1990, 6: 101 |
| 88 | Liu B X, Huang L J, Geng L, et al. Microstructure and tensile behavior of novel laminated Ti-TiBw/Ti composites by reaction hot pressing [J]. Mater. Sci. Eng., 2013, A583: 182 |
| 89 | Maiti D K, Sinha P K. Bending, free vibration and impact response of thick laminated composite plates [J]. Comput. Struct., 1996, 59: 115 |
| 90 | Singh B N, Yadav D, Iyengar N G R. Natural frequencies of composite plates with random material properties using higher-order shear deformation theory [J]. Int. J. Mech. Sci., 2001, 43: 2193 |
| 91 | Messina A, Soldatos K P. A general vibration model of angle-ply laminated plates that accounts for the continuity of interlaminar stresses [J]. Int. J. Solids Struct., 2002, 39: 617 |
| 92 | Zeng D, Fang D N. Numerical analysis of fracture behavior of laminated ceramic in three-point bending [J]. J. Basic Sci. Eng., 2000, 8: 398 |
| 92 | 曾 东, 方岱宁. 用界面元分析层状陶瓷的三点弯曲断裂性能 [J]. 应用基础与工程科学学报, 2000, 8: 398 |
| 93 | Huang Y, Wang C A. Multiphase Composite Ceramics with High Performance [M]. Beijing: Tsinghua University Press, 2008: 1 |
| 93 | 黄 勇, 汪长安. 高性能多相复合陶瓷 [M]. 北京: 清华大学出版社, 2008: 1 |
| 94 | Yu Y H, Wang Y B, Tan H N, et al. Elastic modulus, Poisson ratio of ZA35/TiC and dynamic performance of lts structural parts [J]. Mater. Heat Treat., 2012, 41(16): 40 |
| 94 | 于英华, 王益博, 谈海南等. ZA35/TiC合金弹性模量、泊松比及其结构件动态性能研究 [J]. 热加工工艺, 2012, 41(16): 40 |
| 95 | Luo D J, Wang Y W, Wang F C, et al. The influence of metal cover plates on ballistic performance of silicon carbide subjected to large-scale tungsten projectile [J]. Mater. Des., 2020, 191: 108659 |
| 96 | Pang Z J. Study of efficient meshfree methods for large deformation analysis [D]. Dalian: Dalian University of Technology, 2018 |
| 96 | 庞志佳. 大变形分析的高效无网格法研究 [D]. 大连: 大连理工大学, 2018 |
| 97 | Pang M H, Wang Z K, Jiao H W. The contrastand analysis of SPH method and FEM method [J]. Mach. Des. Manuf., 2008, (2): 32 |
| 97 | 逄明华, 王占奎, 焦红伟. 无网格法中SPH方法和有限元方法的对比分析 [J]. 机械设计与制造, 2008, (2): 32 |
| 98 | Seo H D, Park H J, Kim J I, et al. The particle-attached element interpolation for density correction in smoothed particle hydrodynamics [J]. Adv. Eng. Soft., 2021, 154: 102972 |
| 99 | Lucy L B. A numerical approach to the testing of the fission hypothesis [J]. Astron. J., 1977, 8: 1013 |
| 100 | Belytschko T, Lu Y Y, Gu L. Element-free Galerkin methods [J]. Int. J. Numer. Methods Eng., 1994, 37: 229 |
| 101 | Atluri S N, Zhu T. A new Meshless Local Petrov-Galerkin (MLPG) approach in computational mechanics [J]. Comput. Mech., 1998, 22: 117 |
| 102 | Atluri S N, Kim H G, Cho J Y. A critical assessment of the truly Meshless Local Petrov-Galerkin (MLPG), and Local Boundary Integral Equation (LBIE) methods [J]. Comput. Mech., 1999, 24: 348 |
| 103 | Wendland H. Meshless Galerkin methods using radial basis functions [J]. Math. Comp., 1999, 68: 1521 |
| 104 | Hao S, Park H S, Liu W K. Moving particle finite element method [J]. Int. J. Numer. Methods Eng., 2002, 53: 1937 |
| 105 | Liu W K, Han W M, Lu H S, et al. Reproducing kernel element method. Part I: Theoretical formulation [J]. Comput. Methods Appl. Mech. Eng., 2004, 193: 933 |
| 106 | Sigalotti L D G, Rendón O, Klapp J, et al. A new insight into the consistency of the SPH interpolation formula [J]. Appl. Math. Comput., 2019, 356: 50 |
| 107 | Li B, Habbal F, Ortiz M. Optimal transportation meshfree approximation schemes for fluid and plastic flows [J]. Int. J. Numer. Methods Eng., 2010, 83: 1541 |
| 108 | Ma T B, Su X, Hao L. Numerical simulation of hypervelocity impact based on the optimal transportation meshfree method [J]. Trans. Beijing Inst. Technol., 2020, 40: 617 |
| 108 | 马天宝, 粟 鑫, 郝 莉. 基于OTM方法的超高速碰撞问题数值模拟 [J]. 北京理工大学学报, 2020, 40: 617 |
| 109 | Zhang T L, Ma T B, Hao L. Parallel research on numerical simulation of hypervelocity impact based on pOTM method [J]. J. Ordn. Equip. Eng., 2021, 42(1): 144 |
| 109 | 张天龙, 马天宝, 郝 莉. 基于pOTM方法的超高速碰撞并行数值模拟研究 [J]. 兵器装备工程学报, 2021, 42(1): 144 |
| 110 | Zhu M L. A comparative study of three mesh-free methods: Smoothed particle hydrodynamics, dissipative particle dynamics and smoothed dissipative particle dynamics [D]. Jilin: University of Jilin, 2020 |
| 110 | 朱曼琳. 三种无网格法的对比研究——光滑粒子动力学、耗散粒子动力学和光滑耗散粒子动力学 [D]. 吉林: 吉林大学, 2020 |
| 111 | Li G A. Deformation behaviors and microstructure change of several metals under high velocity impact conditions [D]. Harbin: Harbin Institute of Technology, 2005 |
| 111 | 李国爱. 高速撞击条件下几种金属材料的变形及组织演变行为 [D]. 哈尔滨: 哈尔滨工业大学, 2005 |
| 112 | Yang Y, Li X J, Zhu D M, et al. Research development of materials damage effect under hypervelocity impact [J]. Ordn. Mater. Sci. Eng., 2014, 37(5): 133 |
| 112 | 杨 益, 李晓军, 朱大明等. 超高速碰撞材料毁伤效应研究进展 [J]. 兵器材料科学与工程, 2014, 37(5): 133 |
| 113 | Dong H P, Guo F, Huang W J, et al. Shear banding behavior of AA2099 Al-Li alloy in asymmetrical rolling and its effect on recrystallization in subsequent annealing [J]. Mater. Charac., 2021, 177: 111155 |
| 114 | Dong E T. A first-principles study of metal-ceramic interfacial bonding [D]. Jilin: Jilin University, 2013 |
| 114 | 董二婷. 金属-陶瓷界面结合的第一原理研究 [D]. 吉林: 吉林大学, 2013 |
| 115 | Fan R. A first-principles investigation on the interfacial bonding properties of ceramic/metal composites [D]. Shanghai: Shanghai Jiaotong University, 2019 |
| 115 | 范 睿. 陶瓷/金属复合材料界面结合性能的第一性原理研究 [D]. 上海: 上海交通大学, 2019 |
| 116 | Freeman A J, Li C, Fu C L. Energetics, bonding mechanism and electronic structure of metal/ceramic interfaces [A]. Metal-Ceramic Interfaces [M]. Oxford: Pergamon, 1990: 2 |
| 117 | Rao F Y, Wu R Q, Freeman A J. Structure and bonding at metal-ceramic interfaces: Ag/CdO(001) [J]. Phys. Rev., 1995, 51B: 10052 |
| 118 | Li C, Freeman A J. Giant monolayer magnetization of Fe on MgO: A nearly ideal two-dimensional magnetic system [J]. Phys. Rev., 1991, 43B: 780 |
| 119 | Wu R Q, Freeman A J. Predicted c(2 × 2) buckling reconstruction of monolayer Mn on Fe(001) and its importance to the interfacial magnetic ordering [J]. Phys. Rev., 1995, 51B: 17131 |
| 120 | Smith J R, Hong T, Srolovitz D J. Metal-ceramic adhesion and the harris functional [J]. Phys. Rev. Lett., 1994, 72: 4021 |
| 121 | Hong T, Smith J R, Srolovitz D J. Metal/ceramic adhesion: A first principles study of MgO/Al and MgO/Ag [J]. J. Adhes. Sci. Technol., 1994, 8: 837 |
| 122 | Hong T, Smith J R, Srolovitz D J. Theory of metal—Ceramic adhesion [J]. Acta Metall. Mater., 1995, 43: 2721 |
| 123 | Hong T, Smith J R, Srolovitz D J. Impurity effects on adhesion: Nb, C, O, B, and S at a Mo/MoSi2 interface [J]. Phys. Rev., 1993, 47B: 13615 |
| 124 | Hong T, Smith J R, Srolovitz D J. Impurity effects on adhesion [J]. Phys. Rev. Lett., 1993, 70: 615 |
| 125 | Zhukovskii Y F, Kotomin E A, Jacobs P W M, et al. Ab initio modeling of metal adhesion on oxide surfaces with defects [J]. Phys. Rev. Lett., 2000, 84: 1256 |
| 126 | Matsunaka D, Shibutani Y. Effects of oxygen vacancy on adhesion of incoherent metal/oxide interface by first-principles calculations [J]. Surf. Sci., 2010, 604: 196 |
| 127 | Benedek R, Alavi A, Seidman D N, et al. First principles simulation of a ceramic/metal interface with misfit [J]. Phys. Rev. Lett., 2000, 84: 3362 |
| 128 | Long Y, Chen N X, Zhang W Q. Pair potentials for a metal-ceramic interface by inversion of adhesive energy [J]. J. Phys.: Condens. Matter, 2005, 17: 2045 |
| 129 | Liu L M, Wang S Q, Ye H Q. Adhesion and bonding of the Al/TiC interface [J]. Surf. Sci., 2004, 550: 46 |
| 130 | Dudiy S V, Lundqvist B I. Wetting of TiC and TiN by metals [J]. Phys. Rev., 2004, 69B: 125421 |
| 131 | Deng C, Xu B, Wu P, et al. Stability of the Al/TiB2 interface and doping effects of Mg/Si [J]. Appl. Surf. Sci., 2017, 425: 639 |
| 132 | Rao L X, Liu H, Liu S, et al. Interface relationship between TiN and Ti substrate by first-principles calculation [J]. Comput. Mater. Sci., 2018, 155: 36 |
| 133 | Liu L M, Wang S Q, Ye H Q. Adhesion of metal-carbide/nitride interfaces: Al/TiC and Al/TiN [J]. J. Phys.: Condens. Matter, 2003, 15: 8103 |
| 134 | Li H T, Chen L F, Yuan X, et al. Interfacial stoichiometry and adhesion at metal/α-Al2O3 interfaces [J]. J. Am. Ceram. Soc., 2011, 94: s154 |
| 135 | Yang J, Ye Z, Huang J H, et al. First-principles calculations on wetting interface between Ag-Cu-Ti filler metal and SiC ceramic: Ag (111)/SiC (111) interface and Ag (111)/TiC (111) interface [J]. Appl. Surf. Sci., 2018, 462: 55 |
| 136 | Liu B B, Yang J F. Mg on adhesion of Al(111)/3C-SiC(111) interfaces from first principles study [J]. J. Alloys Compd., 2019, 791: 530 |
| 137 | Guo X Y, Zhang Y, Jung Y G, et al. Ideal tensile strength and shear strength of ZrO2(111)/Ni(111) ceramic-metal Interface: A first principle study [J]. Mater. Des., 2016, 112: 254 |
/
| 〈 |
|
〉 |