研究论文

Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究

  • 李海勇 ,
  • 李赛毅
展开
  • 1.中南大学 材料科学与工程学院 长沙 410083
    2.中南大学 有色金属材料科学与工程教育部重点实验室 长沙 410012
李海勇,男,1994年生,硕士生

收稿日期: 2020-12-28

  修回日期: 2021-04-02

  网络出版日期: 2021-05-20

基金资助

国家自然科学基金项目(51271204);中南大学高性能计算公共平台项目

Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations

  • Haiyong LI ,
  • Saiyi LI
Expand
  • 1.School of Materials Science and Engineering, Central South University, Changsha 410083, China
    2.Key Laboratory of Nonferrous Metal Materials Science and Engineering, Ministry of Education, Central South University, Changsha 410012, China
LI Saiyi, professor, Tel: (0731)88876621, E-mail: saiyi@csu.edu.cn

Received date: 2020-12-28

  Revised date: 2021-04-02

  Online published: 2021-05-20

Supported by

National Natural Science Foundation of China(51271204);High Performance Computing Center of Central South University

摘要

选取具有不同取向差角的纯Al <111>对称倾斜晶界,采用合成驱动力法模拟晶界在300~800 K温度下的迁移行为,研究温度对迁移行为的影响。结果表明,晶界迁移行为的温度相关性随取向差角而变化,可以归为3类:取向差角为8.61°~21.79°的晶界呈现明显反热激活迁移,38.21°~60°晶界总体上表现为热激活迁移,27.80°~32.20°晶界在低温下为热激活迁移,在较高温度下转变为反热激活迁移。8.61°~21.79°晶界的迁移率总体上远高于其他晶界,但差异随温度升高而减小。结构单元模型能够准确体现不同晶界在各个温度下的结构特点,且结构单元类型相同的晶界表现出相似的迁移行为温度相关性。不同温度区间内同一晶界的迁移行为温度相关性变化可能与结构单元多个变体之间的转变有关。

本文引用格式

李海勇 , 李赛毅 . 纯Al <111>对称倾斜晶界迁移行为温度相关性的分子动力学研究[J]. 金属学报, 2022 , 58(2) : 250 -256 . DOI: 10.11900/0412.1961.2020.00527

Abstract

The migration behavior of <111> symmetric tilt grain boundaries (GBs) having different misorientation angles was simulated using a molecular dynamics synthetic driving force method. The effect of temperature on the migration behavior was investigated in the temperature range of 300-800 K. The results demonstrated that the temperature dependencies of GB migration varied with the misorientation. GBs with a misorientation of 8.61°-21.79° exhibited antithermally activated migration, whereas those with a misorientation of 38.21°-60° exhibited thermally activated migration. For the GBs having a misorientation of 27.80°-32.20°, there was an apparent transition from thermally activated migration at low temperature to antithermally activated migration at high temperature. The mobility of the GBs having a misorientation of 8.61°-21.79° was much higher than that of other GBs, but the differences between them decreased with increasing temperature. The GB structures at different temperatures can be well described using the structural unit model. GBs with structures consisting of similar types of structural units exhibit comparable temperature dependencies in their mobility. The complex temperature dependencies of migration behavior shown by some GBs appear to be related to structural changes featured by the transformation between variants belonging to the same type of structural units.

参考文献

1 Gottstein G , Shvindlerman L S . Grain Boundary Migration in Metals: Thermodynamics, Kinetics, Applications [M]. 2nd Ed., Boca Raton: Taylor & Francis, 2010: 145
2 Winning M , Gottstein G , Shvindlerman L S . Stress induced grain boundary motion [J]. Acta Mater., 2001, 49: 211
3 Winning M , Rollett A D , Gottstein G , et al . Mobility of low-angle grain boundaries in pure metals [J]. Philos. Mag., 2010, 90: 3107
4 Shivindlerman L S , Gottstein G , Molodov D A . Grain boundary motion in pure metals: Effect of interaction between adsorbed atoms at moving boundaries [J]. Phys. Status Solidi, 1997, 160a: 419
5 Molodov D A , Czubayko U , Gottstein G , et al . Mobility of <111> tilt grain boundaries in the vicinity of the special misorientation = 7 in bicrystals of pure aluminium [J]. Scr. Metall. Mater., 1995, 32: 529
6 Upmanyu M , Srolovitz D J , Shvindlerman L S , et al . Misorientation dependence of intrinsic grain boundary mobility: Simulation and experiment [J]. Acta Mater., 1999, 47: 3901
7 Kopetsky C V , Shvindlerman L S , Sursaeva V G . Effect of athermal motion of grain boundaries [J]. Scr. Metall., 1978, 12: 953
8 Rheinheimer W , Hoffmann M J . Non-Arrhenius behavior of grain growth in strontium titanate: New evidence for a structural transition of grain boundaries [J]. Scr. Mater., 2015, 101: 68
9 Homer E R , Holm E A , Foiles S M , et al . Trends in grain boundary mobility: Survey of motion mechanisms [J]. JOM, 2014, 66: 114
10 Priedeman J L , Olmsted D L , Homer E R . The role of crystallography and the mechanisms associated with migration of incoherent twin grain boundaries [J]. Acta Mater., 2017, 131: 553
11 Humberson J , Holm E A . Anti-thermal mobility in the Σ3 [111] 60° {11 8 5} grain boundary in nickel: Mechanism and computational considerations [J]. Scr. Mater., 2017, 130: 1
12 Bair J L , Homer E R . Antithermal mobility in 7 and 9 grain boundaries caused by stick-slip stagnation of ordered atomic motions about coincidence site lattice atoms [J]. Acta Mater., 2019, 162: 10
13 Yu T T , Yang S , Deng C . Survey of grain boundary migration and thermal behavior in Ni at low homologous temperatures [J]. Acta Mater., 2019, 177: 151
14 Han J , Thomas S L , Srolovitz D J . Grain-boundary kinetics: A unified approach [J]. Prog. Mater. Sci., 2018, 98: 386
15 Homer E R , Patala S , Priedeman J L . Grain boundary plane orientation fundamental zones and structure-property relationships [J]. Sci. Rep., 2015, 5: 15476.
16 Olmsted D L , Holm E A , Foiles S M . Survey of computed grain boundary properties in face-centered cubic metals—II: Grain boundary mobility [J]. Acta Mater., 2009, 57: 3704
17 Yang L , Lai C M , Li S Y . A survey of the crystallography-dependency of twist grain boundary mobility in Al based on atomistic simulations [J]. Mater. Lett., 2020, 263: 127293.
18 Yang L , Lai C M , Li S Y . Statistical analysis of grain boundary mobility in Al simulated using a modified synthetic driving force molecular dynamics method [J]. Mater. Lett., 2018, 227: 90
19 Beck P A , Sperry P R , Hu H . The orientation dependence of the rate of grain boundary migration [J]. J. Appl. Phys., 1950, 21: 420
20 Lücke K , Rixen R , Senna M . Formation of recrystallization textures in rolled aluminum single crystals [J]. Acta Metall., 1976, 24: 103
21 Plimpton S . Fast parallel algorithms for short-range molecular dynamics [J]. J. Comput. Phys., 1995, 117: 1
22 Liu X Y , Ercolessi F , Adams J B . Aluminium interatomic potential from density functional theory calculations with improved stacking fault energy [J]. Modell. Simul. Mater. Sci. Eng., 2004, 12: 665
23 Adlakha I , Solanki K N . Structural stability and energetics of grain boundary triple junctions in face centered cubic materials [J]. Sci. Rep., 2015, 5: 8692
24 Men H , Fan Z . Molecular dynamic simulation of the atomic structure of aluminum solid-liquid interfaces [J]. Mater. Res. Express, 2014, 1: 025705
25 Tschopp M A , McDowell D L . Structures and energies of Σ3 asymmetric tilt grain boundaries in copper and aluminium [J]. Philos. Mag., 2007, 87: 3147
26 Janssens K G F , Olmsted D , Holm E A , et al . Computing the mobility of grain boundaries [J]. Nat. Mater., 2006, 5: 124
27 Yang L , Li S Y . A modified synthetic driving force method for molecular dynamics simulation of grain boundary migration [J]. Acta Mater., 2015, 100: 107
28 Stukowski A . Visualization and analysis of atomistic simulation data with OVITO—The Open Visualization Tool [J]. Modell. Simul. Mater. Sci. Eng., 2009, 18: 015012
29 Sutton A P , Vitek V . On the structure of tilt grain boundaries in cubic metals I. Symmetrical tilt boundaries [J]. Philos. Trans. R. Soc. London, 1983, 309A: 1
30 Zhou J , Mohles V . Towards realistic molecular dynamics simulations of grain boundary mobility [J]. Acta Mater., 2011, 59: 5997
31 Holm E A , Foiles S M , Homer E R , et al . Comment on “Toward realistic molecular dynamics simulations of grain boundary mobility” by Zhou and Mohles [J]. Scr. Mater., 2012, 66: 714
文章导航

/