Al19.3Co15Cr15Ni50.7高熵合金的热变形行为
收稿日期: 2020-09-07
修回日期: 2020-10-10
网络出版日期: 2021-03-31
基金资助
国家自然科学基金项目(11674274)
Thermal Deformation Behavior of Al19.3Co15Cr15Ni50.7 High Entropy Alloy
Received date: 2020-09-07
Revised date: 2020-10-10
Online published: 2021-03-31
Supported by
National Natural Science Foundation of China(11674274)
为研究铸态Al19.3Co15Cr15Ni50.7高熵合金的热变形行为,利用Gleeble-3500热模拟试验机对试样进行热压缩实验,获得了在应变速率为0.001~0.1 s-1和变形温度为973~1273 K条件下的真应力-真应变曲线。根据 Arrhenius模型构建该合金应变为0.1~0.7的流变应力下的本构方程,得出不同应变条件下的变形激活能和材料参数,以应变ε为自变量将材料常数进行6次多项式拟合,并对本构方程进行验证。基于动态材料模型的功率耗散理论和失稳判据构建功率耗散图和失稳图,并将2者叠加,得到应变为0.3~0.7的热加工图。结果表明,1273 K时的流变应力曲线呈现明显的动态回复的特征,其他温度下的流变应力曲线呈现动态再结晶的特征,并且流变应力随变形温度的下降或应变速率的提升而提升。建立本构方程并进行验证,判定系数R2 = 0.956,较高的判定系数表明建立的流变应力本构模型能够比较精确地预测合金的流变应力。高温压缩后的SEM结果显示:相比于铸态微观组织,合金经历热变形之后,组织中出现一些空隙与局部塑性流动,长条状的B2相发生了弯折、断裂,且断裂处的长条状B2相被撕裂成连续的片层状。最后基于动态材料模型(DMM)理论计算出热加工图,从而得到优异的热加工区间。
刘庆琦 , 卢晔 , 张翼飞 , 范笑锋 , 李瑞 , 刘兴硕 , 佟雪 , 于鹏飞 , 李工 . Al19.3Co15Cr15Ni50.7高熵合金的热变形行为[J]. 金属学报, 2021 , 57(10) : 1299 -1308 . DOI: 10.11900/0412.1961.2020.00349
Al19.3Co15Cr15Ni50.7 is a eutectic high entropy alloy with a lamellar structure and good high-temperature properties. To study the thermal deformation behavior of the samples (diameter 8 mm, height 10 mm), the samples were hot compressed using the Gleeble-3500 thermal simulation-testing machine. The true stress-true strain curves were obtained for strain rates between 0.001 and 0.1 s-1 and deformation temperatures from 973 K to 1273 K. According to the Arrhenius model, the constitutive equation of the alloy in the strain range of 0.1-0.7 is established, and the deformation activation energy and material parameters under different strain conditions were obtained. With the strain (ε) as the independent variable, the material constants are fitted using the sixth order polynomial, such that the material constant of a certain strain, and the constitutive equation of the strain is obtained. Finally, the constitutive equation is verified. Based on the power dissipation theory and instability criterion of the dynamic material model, the power dissipation and instability diagram are constructed, and the hot working diagram in the strain range of 0.3-0.7 for the Al19.3Co15Cr15Ni50.7 high entropy alloy is established by the superposition of the two diagrams. The results show that the flow stress curve at 1273 K presents dynamic recovery characteristics, while the flow stress curve at other temperatures presents dynamic recrystallization characteristics, and the flow stress increases with a decrease in the deformation temperature or an increase in the strain rate. The constitutive equation was established and verified, and the decision coefficient R2 = 0.956, which was relatively high, indicates that the established flow stress constitutive model could predict the flow stress of the alloy. After high-temperature compression, compared with the as-cast microstructure, the strip-shaped B2 phase has some bending after hot deformation, and even fracture may occur under the condition of a high-strain rate. The original fine lamellar B2 phase grows into coarse lamellar, and based on the dynamic material model (DMM) theory, the stable zone and unstable zone are determined, and the optimal process parameters are determined.
| 1 | Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299 |
| 2 | Murty B S, Yeh J W, Ranganathan S, et al. Alloy design and phase selection rules in high-entropy alloys [A]. High-Entropy Alloys [M]. Amsterdam: Elsevier, 2019: 51 |
| 3 | Shi Y Z, Yang B, Liaw P K. Corrosion-resistant high-entropy alloys: A review [J]. Metals, 2017, 7: 43 |
| 4 | Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys [J]. Sci. Rep., 2014, 4: 6200 |
| 5 | Lu Y P, Gao X Z, Jiang L, et al. Directly cast bulk eutectic and near-eutectic high entropy alloys with balanced strength and ductility in a wide temperature range [J]. Acta Mater., 2017, 124: 143 |
| 6 | Baker L, Wu M, Wang Z W. Eutectic/eutectoid multi-principle component alloys: A review [J]. Mater. Charact., 2019, 147: 545 |
| 7 | Jiang H, Qiao D X, Lu Y P, et al. Direct solidification of bulk ultrafine-microstructure eutectic high-entropy alloys with outstanding thermal stability [J]. Scr. Mater., 2019, 165: 145 |
| 8 | Liu D J, Yu P F, Li G, et al. High-temperature high-entropy alloys AlxCo15Cr15Ni70-x based on the Al-Ni binary system [J]. Mater. Sci. Eng., 2018, A724: 283 |
| 9 | Pollock T M, Tin S. Nickel-based superalloys for advanced turbine engines: Chemistry, microstructure and properties [J]. J. Propul. Power, 2006, 22: 361 |
| 10 | Guo J T, Cui C Y, Chen Y X, et al. Microstructure, interface and mechanical property of the DS NiAl/Cr(Mo, Hf) composite [J]. Intermetallics, 2001, 9: 287 |
| 11 | Gao P F, Fu M W, Zhan M, et al. Deformation behavior and microstructure evolution of titanium alloys with lamellar microstructure in hot working process: A review [J]. J. Mater. Sci. Technol., 2020, 39: 56 |
| 12 | Aghaie-Khafri M, Golarzi N. Dynamic and metadynamic recrystallization of Hastelloy X superalloy [J]. J. Mater. Sci., 2008, 43: 3717 |
| 13 | Lin P, Feng A H, Yuan S J, et al. Microstructure and texture evolution of a near-α titanium alloy during hot deformation [J]. Mater. Sci. Eng., 2013, A563: 16 |
| 14 | Prasad Y V R K. Author's reply: Dynamic materials model: basis and principles [J]. Metall. Mater. Trans., 1996, 27A: 235 |
| 15 | Wang L, Yang G, Lei T, et al. Hot deformation behavior of GH738 for A-USC turbine blades [J]. J. Iron Steel Res. Int., 2015, 22: 1043 |
| 16 | Zhao M M, Qin S, Feng J, et al. Effect of Al and Ni on hot deformation behavior of 1Cr9Al(1~3)Ni(1~7)WVNbB steel [J]. Acta Metall. Sin., 2020, 56: 960 |
| 16 | 赵嫚嫚, 秦 森, 冯 捷等. Al、Ni对1Cr9Al(1~3)Ni(1~7)WVNbB钢热变形行为的影响 [J]. 金属学报, 2020, 56: 960 |
| 17 | Xiao Y H, Guo C. Flow stress model for steel 30Cr during hot deformation [J]. Forg. Stamp. Technol., 2018, 43(1): 176 |
| 17 | 肖艳红, 郭 成. 30Cr钢高温变形流变应力模型 [J]. 锻压技术, 2018, 43(1): 176 |
| 18 | Ning Y Q, Wang T, Fu M W, et al. Competition between work-hardening effect and dynamic-softening behavior for processing as-cast GH4720Li superalloys with original dendrite microstructure during moderate-speed hot compression [J]. Mater. Sci. Eng., 2015, A642: 187 |
| 19 | Huang T Y. Materials Processing Technology [M]. Beijing: Tsinghua University Press, 2009: 20 |
| 19 | 黄天佑. 材料加工工艺 [M]. 北京: 清华大学出版社, 2009: 20 |
| 20 | Lin Y C, Chen M S, Zhong J. Constitutive modeling for elevated temperature flow behavior of 42CrMo steel [J]. Comput. Mater. Sci., 2008, 42: 470 |
| 21 | Bruni C, Forcellese A, Gabrielli F. Hot workability and models for flow stress of NIMONIC 115 Ni-base superalloy [J]. J. Mater. Process. Technol., 2002, 125-126: 242 |
| 22 | Sellars C M, McTegart W J. On the mechanism of hot deformation [J]. Acta Metall., 1966, 14: 1136 |
| 23 | Lin Y C, Wen D X, Deng J, et al. Constitutive models for high-temperature flow behaviors of a Ni-based superalloy [J]. Mater. Des., 2014, 59: 115 |
| 24 | Vo P, Jahazi M, Yue S, et al. Flow stress prediction during hot working of near-α titanium alloys [J]. Mater. Sci. Eng., 2007, A447: 99 |
| 25 | Wang Y, Lin D L, Law C C. A correlation between tensile flow stress and Zener-Hollomon factor in TiAl alloys at high temperatures [J]. J. Mater. Sci. Lett., 2000, 19: 1185 |
| 26 | Lino R, Guadanini L G L, Silva L B, et al. Effect of Nb and Ti addition on activation energy for austenite hot deformation [J]. J. Mater. Res. Technol., 2019, 8: 180 |
| 27 | Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59 |
| 27 | 肖伯律, 黄治冶, 马 凯等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59 |
| 28 | Prasad Y V R K, Seshacharyulu T. Modelling of hot deformation for microstructural control [J]. Int. Mater. Rev., 1998, 43: 243 |
| 29 | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Trans., 1984, 15A: 1883 |
/
| 〈 |
|
〉 |