综述

块体非晶合金的3D打印成形研究进展

  • 李宁 ,
  • 黄信
展开
  • 华中科技大学 材料科学与工程学院 武汉 430074

收稿日期: 2020-11-09

  修回日期: 2021-01-24

  网络出版日期: 2021-03-01

基金资助

国家自然科学基金项目(51971097)

Recent Advances on 3D Printed Bulk Metallic Glasses

  • Ning LI ,
  • Xin HUANG
Expand
  • School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China
LI Ning, professor, Tel: (027)87559606, E-mail: hslining@hust.edu.cn

Received date: 2020-11-09

  Revised date: 2021-01-24

  Online published: 2021-03-01

Supported by

National Natural Science Foundation of China(51971097)

摘要

当前,块体非晶合金作为结构材料,其应用不仅面临室温脆性挑战,而且遭遇成形制造瓶颈。解决上述难题已成为近年来材料领域的研究热点与难点之一。近年来发展起来的3D打印技术,已逐渐成为解决块体非晶合金现存困境,实现工程应用的有效途径之一。然而,由于非晶合金具有与晶态材料完全不同的原子结构,3D打印成形中的微观组织演变、缺陷形成与抑制、性能调控等方面的基础理论不同于常规晶态材料,深入剖析上述科学问题对促进块体非晶合金3D打印成形技术的发展具有重要意义。本文依据近年来的国内外研究动态,针对上述问题进行综合分析,并对其发展趋势进行展望。

本文引用格式

李宁 , 黄信 . 块体非晶合金的3D打印成形研究进展[J]. 金属学报, 2021 , 57(4) : 529 -541 . DOI: 10.11900/0412.1961.2020.00450

Abstract

The application of bulk metallic glasses (BMGs) as structural materials not only involves the challenge of room temperature brittleness but also bottlenecks related to formation and manufacturing. Solving these issues has become one of the research hotspots and difficulties in the material field recently. The recently developed 3D printing technology has gradually become one of the key methods to solve the existing difficulties of BMGs to realize their engineering applications. However, because BMGs have a completely different atomic structure than crystalline materials, the basic theories of material microstructure evolution, defect formation and suppression, and performance adjustment in 3D printing are completely different. The in-depth analysis of the abovementioned scientific issues is very important for the development of BMG 3D printing technology. This article is mainly focused on the research trends at home and abroad with a comprehensive analysis of the above problems and looks forward to the development trends of 3D printing technology.

参考文献

1 Klement W, Willens R H, Duwez P. Non-crystalline structure in solidified gold-silicon alloys [J]. Nature, 1960, 187: 869
2 Nieh T G, Wadsworth J. Homogeneous deformation of bulk metallic glasses [J]. Scr. Mater., 2006, 54: 387
3 Tian L, Cheng Y Q, Shan Z W, et al. Approaching the ideal elastic limit of metallic glasses [J]. Nat. Commun., 2012, 3: 609
4 Wang J F, Li R, Hua N B, et al. Co-based ternary bulk metallic glasses with ultrahigh strength and plasticity [J]. J. Mater. Res., 2011, 26: 2072
5 Cao L F. Research on the preparation of Fe84(NbV)7B9 nanocrystalline soft magnetic materials and related fundamental theory [D]. Changsha: Central South University, 2006
5 曹玲飞. Fe84(NbV)7B9纳米晶软磁材料的制备及其相关基础问题的研究 [D]. 长沙: 中南大学, 2006
6 Pan J, Zhang M, Chen Q, et al. Study of anticorrosion ability of Fe43.7Co7.3Cr14.7Mo12.6C15.5B4.3Y1.9 bulk metallic glass in strong acid solutions [J]. Rare Met. Mater Eng., 2008, 37(suppl.4): 805
6 潘 杰, 张 猛, 谌 祺等. FeCoCrMoCBY块体非晶合金在强酸介质中的耐蚀性能 [J]. 稀有金属材料与工程, 2008, 37(): 805
7 Suryanarayana C, Inoue A. Bulk Metallic Glass [M]. Boca Raton: CRC Press, 2011: 1
8 Schroers J. Processing of bulk metallic glass [J]. Adv. Mater., 2010, 22: 1566
9 Schroers J, Paton N. Amorphous metal alloys form like plastics [J]. Adv. Mater. Process., 2006, 164: 61
10 Saotome Y, Miwa S, Zhang T, et al. The micro-formability of Zr-based amorphous alloys in the supercooled liquid state and their application to micro-dies [J]. J. Mater. Process. Technol., 2001, 113: 64
11 Gu D D, Hagedorn Y C, Meiners W, et al. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium [J]. Acta Mater., 2012, 60: 3849
12 Pauly S, L?ber L, Petters R, et al. Processing metallic glasses by selective laser melting [J]. Mater. Today, 2013, 16: 37
13 Katakam S, Hwang J Y, Paital S, et al. In situ laser synthesis of Fe-based amorphous matrix composite coating on structural steel [J]. Metall. Mater. Trans., 2012, 43A: 4957
14 Zheng B, Zhou Y, Smugeresky J E, et al. Processing and behavior of Fe-based metallic glass components via laser-engineered net shaping [J]. Metall. Mater. Trans., 2009, 40A: 1235
15 Laser engineered net shaping, LENS [EB/OL].
16 Gibson M A, Mykulowycz N M, Shim J, et al. 3D printing metals like thermoplastics: Fused filament fabrication of metallic glasses [J]. Mater. Today, 2018, 21: 697
17 Zhang C, Wang W, Li Y C, et al. 3D printing of Fe-based bulk metallic glasses and composites with large dimensions and enhanced toughness by thermal spraying [J]. J. Mater. Chem., 2018, 6A: 6800
18 Gorodesky N, Sedghani‐Cohen S, Altman M, et al. Concurrent formation of metallic glass during laser forward transfer 3D printing [J]. Adv. Funct. Mater., 2020, 30: 2001260
19 Visser C W, Pohl R, Sun C, et al. Toward 3D printing of pure metals by laser-induced forward transfer [J]. Adv. Mater., 2015, 27: 4087
20 Duoss E. Direct ink writing of bulk metallic glasses [R/OL]. , 2017
21 Li X P, Kang C W, Huang H, et al. Selective laser melting of an Al86Ni6Y4.5Co2La1.5 metallic glass: Processing, microstructure evolution and mechanical properties [J]. Mater. Sci. Eng., 2014, A606: 370
22 Ouyang D, Li N, Xing W, et al. 3D printing of crack-free high strength Zr-based bulk metallic glass composite by selective laser melting [J]. Intermetallics, 2017, 90: 128
23 Deng L, Wang S H, Wang P, et al. Selective laser melting of a Ti-based bulk metallic glass [J]. Mater. Lett., 2018, 212: 346
24 Ouyang D, Xing W, Li N, et al. Structural evolutions in 3D-printed Fe-based metallic glass fabricated by selective laser melting [J]. Addit. Manuf., 2018, 23: 246
25 Bordeenithikasem P, Stolpe M, Elsen A, et al. Glass forming ability, flexural strength, and wear properties of additively manufactured Zr-based bulk metallic glasses produced through laser powder bed fusion [J]. Addit. Manuf., 2018, 21: 312
26 Li N, Zhang J J, Xing W, et al. 3D printing of Fe-based bulk metallic glass composites with combined high strength and fracture toughness [J]. Mater. Des., 2018, 143: 285
27 Mahbooba Z, Thorsson L, Unosson M, et al. Additive manufacturing of an iron-based bulk metallic glass larger than the critical casting thickness [J]. Appl. Mater. Today, 2018, 11: 264
28 Hofmann D C, Bordeenithikasem P, Pate A, et al. Developing processing parameters and characterizing microstructure and properties of an additively manufactured FeCrMoBC metallic glass forming alloy [J]. Adv. Eng. Mater., 2018, 20: 1800433
29 Jung H Y, Choi S J, Prashanth K G, et al. Fabrication of Fe-based bulk metallic glass by selective laser melting: A parameter study [J]. Mater. Des., 2015, 86: 703
30 Wang L, Wang H, Liu Y K, et al. Selective laser melting helps fabricate record-large bulk metallic glass: Experiments, simulation and demonstrative part [J]. J. Alloys Compd., 2019, 808: 151731
31 Zhang C, Li X M, Liu S Q, et al. 3D printing of Zr-based bulk metallic glasses and components for potential biomedical applications [J]. J. Alloys Compd., 2019, 790: 963
32 Xing W, Ouyang D, Chen Z, et al. Effect of energy density on defect evolution in 3D printed Zr-based metallic glasses by selective laser melting [J]. Sci. China Phys. Mech. Astron., 2019, 63: 226111
33 Li X P, Roberts M P, O'Keeffe S, et al. Selective laser melting of Zr-based bulk metallic glasses: Processing, microstructure and mechanical properties [J]. Mater. Des., 2016, 112: 217
34 Shen Y Y, Li Y Q, Chen C, et al. 3D printing of large, complex metallic glass structures [J]. Mater. Des., 2017, 117: 213
35 Sun H, Flores K M. Laser deposition of a Cu-based metallic glass powder on a Zr-based glass substrate [J]. J. Mater. Res., 2011, 23: 2692
36 ??rodowski, Wysocki B, Wróblewski R, et al. New approach to amorphization of alloys with low glass forming ability via selective laser melting [J]. J. Alloys Compd., 2019, 771: 769
37 Yang C, Zhang C, Xing W, et al. 3D printing of Zr-based bulk metallic glasses with complex geometries and enhanced catalytic properties [J]. Intermetallics, 2018, 94: 22
38 Luo Y, Xing L L, Jiang Y D, et al. Additive manufactured large Zr-based bulk metallic glass composites with desired deformation ability and corrosion resistance [J]. Materials (Basel), 2020, 13: 597
39 Pacheco V, Karlsson D, Marattukalam J J, et al. Thermal stability and crystallization of a Zr-based metallic glass produced by suction casting and selective laser melting [J]. J. Alloys Compd., 2020, 825: 153995
40 Marattukalam J J, Pacheco V, Karlsson D, et al. Development of process parameters for selective laser melting of a Zr-based bulk metallic glass [J]. Addit. Manuf., 2020, 33: 101124
41 Lu X Y, Nursulton M, Du Y L, et al. Structural and mechanical characteristics of Cu50Zr43Al7 bulk metallic glass fabricated by selective laser melting [J]. Materials (Basel), 2019, 12: 75
42 Gao X D, Liu Z L, Li J H, et al. Selective laser melting of CuZr-based metallic glass composites [J]. Mater. Lett., 2020, 259: 126724
43 Pauly S, Schricker C, Scudino S, et al. Processing a glass-forming Zr-based alloy by selective laser melting [J]. Mater. Des., 2017, 135: 133
44 Zhai L L, Lu Y Z, Wang L, et al. Quantitative evaluation of hidden hierarchical pores in laser additive manufactured bulk metallic glasses via computed tomography [J]. Mater. Lett., 2020, 265: 127376
45 Zhai L L, Lu Y Z, Zhao X Y, et al. High-throughput screening of laser additive manufactured metallic glass via ultrasonic wave [J]. Sci. Rep., 2019, 9: 17660
46 Xu H D, Lu Y Z, Liu Z H, et al. Laser 3D printing of Zr-based bulk metallic glass [J]. J. Manuf. Process., 2019, 39: 102
47 Lin X, Zhang Y Y, Yang G L, et al. Microstructure and compressive/tensile characteristic of large size Zr-based bulk metallic glass prepared by laser solid forming [J]. J. Mater. Sci. Technol., 2019, 35: 328
48 Yang G L, Lin X, Liu F C, et al. Laser solid forming Zr-based bulk metallic glass [J]. Intermetallics, 2012, 22: 110
49 Su S, Lu Y Z. Laser directed energy deposition of Zr-based bulk metallic glass composite with tensile strength [J]. Mater. Lett., 2019, 247: 79
50 Liang S X, Wang X Q, Zhang W C, et al. Selective laser melting manufactured porous Fe-based metallic glass matrix composite with remarkable catalytic activity and reusability [J]. Appl. Mater. Today, 2020, 19: 100543
51 Zhang P C, Ouyang D, Liu L. Enhanced mechanical properties of 3D printed Zr-based BMG composite reinforced with Ta precipitates [J]. J. Alloys Compd., 2019, 803: 476
52 Zhu Q J, Qu S Y, Wang X H, et al. Synthesis of Fe-based amorphous composite coatings with low purity materials by laser cladding [J]. Appl. Surf. Sci., 2007, 253: 7060
53 Nong X D, Zhou X L, Ren Y X. Fabrication and characterization of Fe-based metallic glasses by Selective Laser Melting [J]. Opt. Laser Technol., 2019, 109: 20
54 Li X P, Kang C W, Huang H, et al. The role of a low-energy-density re-scan in fabricating crack-free Al85Ni5Y6Co2Fe2 bulk metallic glass composites via selective laser melting [J]. Mater. Des., 2014, 63: 407
55 Xie F, Chen Q J, Gao J W. Brittle-ductile transition in laser 3D printing of Fe-based bulk metallic glass composites [J]. Metals, 2019, 9: 78
56 Zhang Y, Liu H S, Mo J Y, et al. Atomic-level crystallization in selective laser melting fabricated Zr-based metallic glasses [J]. Phys. Chem. Chem. Phys., 2019, 21: 12406
57 Zhang Y, Liu H S, Mo J Y, et al. Atomic-scale structural evolution in selective laser melting of Cu50Zr50 metallic glass [J]. Comput. Mater. Sci., 2018, 150: 62
58 Guo S, Wang M, Lin X, et al. Research on the crystallization behavior occurred in the process of preparing bulk metallic glass with selective laser melting [J]. Mater. Res. Express, 2019, 6: 066582
59 Simchi A, Pohl H. Effects of laser sintering processing parameters on the microstructure and densification of iron powder [J]. Mater. Sci. Eng., 2003, A359: 119
60 Zhang Y Y, Lin X, Wei L, et al. Influence of powder size on the crystallization behavior during laser solid forming Zr55Cu30Al10Ni5 bulk amorphous alloy [J]. Intermetallics, 2016, 76: 1
61 Zhang B, Li Y T, Bai Q. Defect formation mechanisms in selective laser melting: A review [J]. Chin. J. Mech. Eng., 2017, 30: 515
62 Qiu C L, Panwisawas C, Ward M, et al. On the role of melt flow into the surface structure and porosity development during selective laser melting [J]. Acta Mater., 2015, 96: 72
63 Ouyang D. Fabrication, structure and properties of 3D printed amorphous alloys by selective laser melting [D]. Wuhan: Huazhong University of Science and Technology, 2019
63 欧阳迪. 激光选区熔化3D打印非晶合金的制备、结构与性能研究 [D]. 武汉: 华中科技大学, 2019
64 Best J P, Ostergaard H E, Li B S, et al. Fracture and fatigue behaviour of a laser additive manufactured Zr-based bulk metallic glass [J]. Addit. Manuf., 2020, 36: 101416
文章导航

/