SiZr液相烧结法制备SiC-ZrC涂层对C/SiC复合材料抗氧化性能的影响
收稿日期: 2020-09-09
修回日期: 2020-11-04
网络出版日期: 2021-01-14
Effect of SiC-ZrC Coating Prepared by SiZr Liquid Phase Sintering on the Oxidation Resistance of C/SiC Composites
Received date: 2020-09-09
Revised date: 2020-11-04
Online published: 2021-01-14
皮慧龙 , 石小磊 , 徐兴祥 . SiZr液相烧结法制备SiC-ZrC涂层对C/SiC复合材料抗氧化性能的影响[J]. 金属学报, 2021 , 57(6) : 791 -796 . DOI: 10.11900/0412.1961.2020.00357
Owing to their low density and good mechanical properties at high temperatures, C/SiC composites are increasingly used in the aerospace industry. They are also being proposed as thermal-structural materials in the hypersonic field; however, C/SiC composites are easily oxidized in high-temperature air environments. In this study, a C/SiC composite was coated with a SiC-ZrC oxidation-resistant layer by a two-step sintering method using Si-25%Zr (mass fraction) alloy, and the phase evolution of the coating was studied during the sintering. The oxidation resistance of the material was then tested at 1400oC in an air environment. The microstructural changes of the coating before and after oxidation and the effect of oxidation on the bending properties of C/SiC were analyzed. After the reaction with carbon, Si and ZrSi2 disappear in the coating, leaving only pure ZrC and SiC. The ZrC phase refined the structure of the reactive SiC layer. The grain size of the sintered SiC was 2 μm, versus 5-20 μm for SiC sintered from pure Si. The refined grains created a dense and continuous SiO2 film during the oxidation process. As the oxidation time was increased at 1400oC, the C/SiC composite with the SiC-ZrC coating began losing weight at 200 s, but began gaining weight at 500 s as a dense SiO2 film was formed. After 1000 s of oxidation, the flexural strength of the C/SiC composites was 335 MPa, only 5% lower than that of the initial C/SiC composite. According to this result, the sintered SiC-ZrC oxidation-resistant film effectively protected the mechanical properties of the C/SiC composite during the oxidation process.
Key words: oxidation resistant coating; SiC-ZrC; liquid-phase sintering
| 1 | Nie T, Liu W Q. Application of C/SiC composites in thermal protection system of nose-cone [J]. Comput. Simul., 2013, 30(9): 109 |
| 1 | 聂 涛, 刘伟强. C/SiC复合材料在鼻锥热防护系统中的应用研究 [J]. 计算机仿真, 2013, 30(9): 109 |
| 2 | Xiao P, Xiong X, Zhang H B, et al. Progress and application of C/C-SiC ceramic braking materials [J]. Chin. J. Nonferrous Met., 2005, 15: 667 |
| 2 | 肖 鹏, 熊 翔, 张红波等. C/C-SiC陶瓷制动材料的研究现状与应用 [J]. 中国有色金属学报, 2005, 15: 667 |
| 3 | Ma Q S, Liu H T, Pan Y, et al. Research progress on the application of C/SiC composites in scramjet [J]. J. Inorg. Mater., 2013, 28: 247 |
| 3 | 马青松, 刘海韬, 潘 余等. C/SiC复合材料在超燃冲压发动机中的应用研究进展 [J]. 无机材料学报, 2013, 28: 247 |
| 4 | Zhu X J, Xia Y W. Application of C/SiC composites in space optical system abroad [J]. Aerosp. Mater. Technol., 2013, 43(4): 20 |
| 4 | 朱晓娟, 夏英伟. C/SiC材料在国外空间光学系统上的应用 [J]. 宇航材料工艺, 2013, 43(4): 20 |
| 5 | Zhang Y, Feng D, Chen X C. Development of properties and process on continuous fiber reinforced SiC composite [J]. Mater. Rev., 2005, 19(3): 63 |
| 5 | 张 勇, 冯 涤, 陈希春. 连续纤维增强SiC复合材料制备工艺与性能研究进展 [J]. 材料导报, 2005, 19(3): 63 |
| 6 | Xie W J, Qiu H P, Chen M W, et al. Influence of carbon fiber treatment on flexural properties of C/SiC composites [J]. Solid State Phenom., 2018, 281: 408 |
| 7 | Li J S, Zhang C R, Li B. Advances in boron nitride interphases in ceramic matrix composites [J]. Mater. Rev., 2011, 25(17): 14 |
| 7 | 李俊生, 张长瑞, 李 斌. 陶瓷基复合材料中氮化硼界面相研究进展 [J]. 材料导报, 2011, 25(17): 14 |
| 8 | Li C G. Effects of elevated temperature on the structures and tensile properties of PAN-based carbon fibers [D]. Harbin: Harbin Institute of Technology, 2014 |
| 8 | 李承高. 高温处理对PAN基碳纤维结构与拉伸性能的影响 [D]. 哈尔滨: 哈尔滨工业大学, 2014 |
| 9 | Wen H M, Dong S M, Ding Y S, et al. SiC/Yb2SiO5 multilayer coatings for oxidation protection of Cf/SiC composites [J]. Rare Met. Mater. Eng., 2009, 38: 1580 |
| 9 | 温海明, 董绍明, 丁玉生等. Cf/SiC复合材料SiC/Yb2SiO5抗氧化复合涂层研究 [J]. 稀有金属材料与工程, 2009, 38: 1580 |
| 10 | Ma Q S, Cai L H. Fabrication of Y2Si2O7 coating and its oxidation protection for C/SiC composites [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 390 |
| 11 | Ma Q S, Cai L H. Fabrication and oxidation resistance of mullite/yttrium silicate multilayer coatings on C/SiC composites [J]. J. Adv. Ceram., 2017, 6: 360 |
| 12 | Zhang W H, Cheng L F, Zhang L T, et al. Preparation and anti-oxidation behavior of Si-C-B self-healing coating on C/SiC composite [J]. J. Inorg. Mater., 2008, 23: 774 |
| 12 | 张伟华, 成来飞, 张立同等. C/SiC复合材料表面Si-C-B自愈合涂层的制备与抗氧化行为 [J]. 无机材料学报, 2008, 23: 774 |
| 13 | Yan Z Q, Xiong X, Xiao P, et al. Preparation of SiC coatings on surface of C/SiC composites by the chemical vapor deposition and their oxidation resistance behavior [J]. J. Chin. Ceram. Soc., 2008, 36: 1098 |
| 13 | 闫志巧, 熊 翔, 肖 鹏等. C/SiC复合材料表面化学气相沉积涂覆SiC涂层及其抗氧化性能 [J]. 硅酸盐学报, 2008, 36: 1098 |
| 14 | Cheng L F, Xu Y D, Zhang L T, et al. Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites [J]. Carbon, 2002, 40: 2229 |
| 15 | Wu S J, Cheng L F, Zhang L T, et al. Oxidation behavior of 2D C/SiC with a multi-layer CVD SiC coating [J]. Surf. Coat. Technol., 2006, 200: 4489 |
| 16 | Hwang K J, Bae S Y, Kim K H, et al. Controlled infiltration profile of SiC coating layer on graphite by Si vapor deposition reaction [J]. J. Ceram. Process. Res., 2019, 20: 169 |
| 17 | Kang P C, Chen G Q, Zhang B, et al. Oxidation protection of carbon fibers by a reaction sintered nanostructured SiC coating [J]. Surf. Coat. Technol., 2011, 206: 305 |
| 18 | Zhao Y W, Sun W T, Li J P, et al. Preparation and microstructure of C/C-SiC composites by reactive melt infiltration [J]. Aerosp. Mater. Technol., 2013, (2): 64 |
| 18 | 赵彦伟, 孙文婷, 李军平等. C/C-SiC复合材料的反应熔渗法制备与微观组织 [J]. 宇航材料工艺, 2013, (2): 64 |
| 19 | Yan Z Q, Xiong X, Xiao P, et al. Oxidation kinetics and mechanism of C/SiC composites fabricated by MSI process [J]. J. Inorg. Mater., 2007, 22: 1151 |
| 19 | 闫志巧, 熊 翔, 肖 鹏等. MSI工艺制备C/SiC复合材料的氧化动力学和机理 [J]. 无机材料学报, 2007, 22: 1151 |
| 20 | Wang J P, Jin Z H, Qian J M, et al. Research progress on mechanism and kinetics of C/C-SiC composites prepared by reactive melt infiltration [J]. J. Chin. Ceram. Soc., 2005, 33: 1120 |
| 20 | 王继平, 金志浩, 钱军民等. 反应熔渗法制备C/C-SiC复合材料及其反应机理和动力学的研究进展 [J]. 硅酸盐学报, 2005, 33: 1120 |
| 21 | Pampuch R, Walasek E, Bialoskórski J. Reaction mechanism in carbon-liquid silicon systems at elevated temperatures [J]. Ceram. Int., 1986, 12: 99 |
| 22 | Sawyer G R, Page T F. Microstructural characterization of “REFEL” (reaction-bonded) silicon carbides [J]. J. Mater. Sci., 1978, 13: 885 |
| 23 | Ness J N, Page T F. Microstructural evolution in reaction-bonded silicon carbide [J]. J. Mater. Sci., 1986, 21: 1377 |
| 24 | He Z J, Sun L B, Li C, et al. Wetting and brazing of Cf /C composites with Si-Zr eutectic alloy: The formation of nano- and coarse-SiC reaction layers [J]. Carbon, 2020, 167: 92 |
| 25 | Yin X G. Study on mechanic and high-temperature properties of C/SiC ceramic based composites [D]. Beijing: Tsinghua University, 2011 |
| 25 | 殷晓光. C/SiC陶瓷基复合材料的力学及高温性能研究 [D]. 北京: 清华大学, 2011 |
/
| 〈 |
|
〉 |