高熵合金中的晶格畸变
收稿日期: 2020-09-09
修回日期: 2020-12-13
网络出版日期: 2020-12-29
基金资助
香港研究资助局项目(CityU11200719)
Lattice Distortion in High-Entropy Alloys
Received date: 2020-09-09
Revised date: 2020-12-13
Online published: 2020-12-29
Supported by
Research Grants Council, RGC(CityU11200719)
杨勇 , 赫全锋 . 高熵合金中的晶格畸变[J]. 金属学报, 2021 , 57(4) : 385 -392 . DOI: 10.11900/0412.1961.2020.00359
Lattice distortion has been deemed as one of the most distinctive structural features of high-entropy alloys. However, despite its fundamental importance, the notion of lattice distortion and its characterization is still an issue under debate. In this work, based on the recent work on theoretical modeling, atomistic simulations and experiments, the physical origin of lattice distortion in high-entropy alloys and its resultant intrinsic residual stresses or strains are discussed.
| 1 | Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299 |
| 2 | Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213 |
| 3 | Ye Y F, Wang Q, Lu J, et al. High-entropy alloy: Challenges and prospects [J]. Mater. Today, 2016, 19: 349 |
| 4 | Zhang Y, Zuo T T, Tang Z, et al. Microstructures and properties of high-entropy alloys [J]. Prog. Mater. Sci., 2014, 61: 1 |
| 5 | Zhang W R, Liaw P K, Zhang Y. Science and technology in high-entropy alloys [J]. Sci. China Mater., 2018, 61: 2 |
| 6 | He Q F, Ding Z Y, Ye Y F, et al. Design of high-entropy alloy: A perspective from nonideal mixing [J]. JOM, 2017, 69: 2092 |
| 7 | Li Z M, Pradeep K G, Deng Y, et al. Metastable high-entropy dual-phase alloys overcome the strength-ductility trade-off [J]. Nature, 2016, 534: 227 |
| 8 | Lei Z F, Liu X J, Wu Y, et al. Enhanced strength and ductility in a high-entropy alloy via ordered oxygen complexes [J]. Nature, 2018, 563: 546 |
| 9 | Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153 |
| 10 | Schuh B, Mendez-Martin F, V?lker B, et al. Mechanical properties, microstructure and thermal stability of a nanocrystalline CoCrFeMnNi high-entropy alloy after severe plastic deformation [J]. Acta Mater., 2015, 96: 258 |
| 11 | Chuang M H, Tsai M H, Wang W R, et al. Microstructure and wear behavior of AlxCo1.5CrFeNi1.5Tiy high-entropy alloys [J]. Acta Mater., 2011, 59: 6308 |
| 12 | Chuang M H, Tsai M H, Tsai C W, et al. Intrinsic surface hardening and precipitation kinetics of Al0.3CrFe1.5MnNi0.5 multi-component alloy [J]. J. Alloys Compd., 2013, 551: 12 |
| 13 | Shuang S, Ding Z Y, Chung D, et al. Corrosion resistant nanostructured eutectic high entropy alloy [J]. Corros. Sci., 2020, 164: 108315 |
| 14 | Yeh J W. Alloy design strategies and future trends in high-entropy alloys [J]. JOM, 2013, 65: 1759 |
| 15 | Pickering E J, Jones N G. High-entropy alloys: A critical assessment of their founding principles and future prospects [J]. Int. Mater. Rev., 2016, 61: 183 |
| 16 | Miracle D B, Senkov O N. A critical review of high entropy alloys and related concepts [J]. Acta Mater., 2017, 122: 448 |
| 17 | Antillon E, Woodward C, Rao S I, et al. Chemical short range order strengthening in a model FCC high entropy alloy [J]. Acta Mater., 2020, 190: 29 |
| 18 | He Q F, Yang Y. On lattice distortion in high entropy alloys [J]. Front. Mater., 2018, 5: 42 |
| 19 | Ye Y F, Liu C T, Yang Y. A geometric model for intrinsic residual strain and phase stability in high entropy alloys [J]. Acta Mater., 2015, 94: 152 |
| 20 | Ye Y F, Zhang Y H, He Q F, et al. Atomic-scale distorted lattice in chemically disordered equimolar complex alloys [J]. Acta Mater., 2018, 150: 182 |
| 21 | Lee C, Song G, Gao M C, et al. Lattice distortion in a strong and ductile refractory high-entropy alloy [J]. Acta Mater., 2018, 160: 158 |
| 22 | Mizutani U. Hume-Rothery Rules for Structurally Complex Alloy Phases [M]. Boca Raton, FL: CRC Press, 2011: 1 |
| 23 | Song H Q, Tian F Y, Hu Q M, et al. Local lattice distortion in high-entropy alloys [J]. Phys. Rev. Mater., 2017, 1: 023404 |
| 24 | Owen L R, Jones N G. Lattice distortions in high-entropy alloys [J]. J. Mater. Res., 2018, 33: 2954 |
| 25 | Zhang Y, Zhou Y J, Lin J P, et al. Solid-solution phase formation rules for multi-component alloys [J]. Adv. Eng. Mater., 2008, 10: 534 |
| 26 | Wang Z J, Huang Y H, Yang Y, et al. Atomic-size effect and solid solubility of multicomponent alloys [J]. Scr. Mater., 2015, 94: 28 |
| 27 | Ge H J, Tian F Y. A review of ab initio calculation on lattice distortion in high-entropy alloys [J]. JOM, 2019, 71: 4225 |
| 28 | Owen L R, Pickering E J, Playford H Y, et al. An assessment of the lattice strain in the CrMnFeCoNi high-entropy alloy [J]. Acta Mater., 2017, 122: 11 |
| 29 | Shao Y T, Yuan R L, Hu Y, et al. The paracrystalline nature of lattice distortion in a high entropy alloy [Z]. arXiv preprint arXiv:1903.04082, 2019 |
| 30 | Huang K. Solid State Physics [M]. Beijing: People Education Press, 1979: 1 |
| 30 | 黄 昆. 固体物理学 [M]. 北京: 人民教育出版社, 1979: 1 |
| 31 | Patterson J D, Bailey B C. Solid-State Physics: Introduction to the Theory [M]. Berlin, Heidelberg: Springer, 2007: 1 |
| 32 | Finney J L. Random packings and the structure of simple liquids. I. The geometry of random close packing [J]. Proc. Roy. Soc. London, 1970, 319A: 479 |
| 33 | Yang X, Zhang Y. Prediction of high-entropy stabilized solid-solution in multi-component alloys [J]. Mater. Chem. Phys., 2012, 132: 233 |
| 34 | King H W. Quantitative size-factors for metallic solid solutions [J]. J. Mater. Sci., 1966, 1: 79 |
| 35 | Eshelby J D. The continuum theory of lattice defects [A]. |
| 35 | Seitz F, Turnbull D. Solid State Physics [M]. New York: Academic Press, 1956: 79 |
| 36 | Yeh J W, Lin S J, Chin T S, et al. Formation of simple crystal structures in Cu-Co-Ni-Cr-Al-Fe-Ti-V alloys with multiprincipal metallic elements [J]. Metall. Mater. Trans., 2004, 35A: 2533 |
| 37 | Yeh J W, Chang S Y, Hong Y D, et al. Anomalous decrease in X-ray diffraction intensities of Cu-Ni-Al-Co-Cr-Fe-Si alloy systems with multi-principal elements [J]. Mater. Chem. Phys., 2007, 103: 41 |
| 38 | Zhang F X, Tong Y, Jin K, et al. Lattice distortion and phase stability of Pd-doped NiCoFeCr solid-solution alloys [J]. Entropy, 2018, 20: 900 |
/
| 〈 |
|
〉 |