W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算
收稿日期: 2020-10-26
修回日期: 2020-12-17
网络出版日期: 2020-12-25
A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties
Received date: 2020-10-26
Revised date: 2020-12-17
Online published: 2020-12-25
利用基于密度泛函理论的第一性原理方法结合声子谱计算和价键作用分析,研究了Ir含量对W1 - x Ir x (x = 0~12.96,原子分数,%)合金几何结构、相稳定性、力学性能以及热力学稳定性的影响,构建了Ir的添加量与W-Ir合金的相稳定性、力学以及热力学性能的变化关系。发现W-Ir合金的相稳定性随着Ir含量的增加而逐渐降低,这与W—Ir价键中部分反键态占据Fermi能级以下区域有关;Ir在W中的添加量小于7.4%时,W-Ir合金满足基态相稳定性要求;随着温度的升高以及Ir含量的增加,W-Ir合金的热力学稳定性得到提升,表明Ir适合添加到高温条件下应用的W中;Ir的加入能降低剪切模量,改善钨合金韧性,与实验观察一致,但Ir也能提升平面抗剪切变形能力。本征脆性的Ir对W的强韧化作用与W—Ir原子键合时轨道电子的转移和重叠方式有关。
皇甫顥 , 王子龙 , 刘永利 , 孟凡顺 , 宋久鹏 , 祁阳 . W1 - x Ir x 固溶合金几何结构、电子结构、力学和热力学性能的第一性原理计算[J]. 金属学报, 2022 , 58(2) : 231 -240 . DOI: 10.11900/0412.1961.2020.00418
Tungsten (W) possess comprehensive physical and chemical properties that are suitable for aerospace and space nuclear power applications, including the highest melting temperature (3410oC) among metals, high elastic modulus, thermal shock resistance, and high temperature strength. However, its poor ductility at room temperatures significantly hinders its fabricability and potential use in the above-mentioned fields. Accordingly, to improve the ductility of W, solid solution strengthening is the primary method considered besides grain refining and deformation strengthening. Experimental studies have shown that Ir is a brittle metal with an fcc structure, but it can greatly improve the ductility of W; however, the corresponding mechanism is still unclear. Thus, using the first principles method based on density functional theory together with phonon spectrum calculations, the effect of the addition of different contents of Ir on the structure, phase stability, mechanical properties, and thermodynamic properties of W were studied. The relation between the addition of different contents of Ir and above-mentioned properties of W-Ir alloys were theoretically investigated. It was found that Ir can induce instability in the W-Ir alloy in the ground state due to the occupation of its antibonding electrons below the Fermi level. When content of Ir added is less than 7.4%, the formation of the W-Ir alloy becomes stable in the ground state. With an increase in temperature and the content of Ir, the thermodynamic stability is improved, implying that Ir is suitable for incorporation with W for application at high temperature. The addition of Ir helps to improve the toughness of the W alloy, which is consistent with the experimental observation. Besides, Ir can simultaneously improve the planar shear resistance. Furthermore, the pCOHP analysis revealed that the inherent mechanism of the ductile effect of brittle Ir in W is attributed to their different modes of electron transition and overlapping. For Ir, electrons transfer from its higher energy orbital of
Key words: W; Ir; elastic property; thermodynamic property; ground state stability; electronic structure
| 1 | Yin W H , Tang H P . Refractory Metal Materials and Engineering Applications [M]. Beijing: Metallurgical Industry Press, 2012: 9 |
| 1 | 殷为宏, 汤慧萍 . 难熔金属材料与工程应用 [M]. 北京: 冶金工业出版社, 2012: 9 |
| 2 | Mu K Q , Xu K D , Wei A B , et al . Burn-off and erosion resistance of several high temperature materials to solid propellant [J]. J. Iron Steel Res., 1995, (5): 89 |
| 2 | 牟科强, 徐克玷, 韦昂邦 等 . 几种高温材料抗燃气烧蚀性能的研究 [J]. 钢铁研究学报, 1995, (5): 89 |
| 3 | Fahrenholtz W G , Wuchina E J , Lee W E , et al . Ultra-high Temperature Ceramics: Materials for Extreme Environment Applications [M]. Hoboken, New Jersey: Wiley, 2014: 37 |
| 4 | Wang L G , He D S . Interstellar navigation plasma rocket engine [J]. Astronavigation, 1964, 10: 1 |
| 4 | 王礼国, 何德胜 . 星际航行等离子火箭发动机 [J]. 宇宙航行, 1964, 10: 1 |
| 5 | Leichtfried G , Schneibel J H , Heilmaier M . Ductility and impact resistance of powder-metallurgical molybdenum-rhenium alloys [J]. Metall. Mater. Trans., 2006, 37A: 2955 |
| 6 | Leonhardt T . Properties of tungsten-rhenium and tungsten-rhenium with hafnium carbide [J]. JOM, 2009, 61:(7) 68 |
| 7 | Geach G A , Hughes J E . The alloys of rhenium with molybdenum or with tungsten and having good high-temperature properties [A]. Proceedings of the 2nd Plansee Seminar [C]. New York: Pergamon Press Ltd., 1956: 245 |
| 8 | Luo A H , Shin K S , Jacobson D L . Ultrahigh temperature tensile properties of arc-melted tungsten and tungsten-iridium alloys [J]. Scr. Metall. Mater., 1991, 25: 2411 |
| 9 | Luo A H , Jacobson D L , Shin K S . Solution softening mechanism of iridium and rhenium in tungsten at room temperature [J]. Int. J. Refract. Met. Hard Mater., 1991, 10: 107 |
| 10 | McKamey C G , Lee E H , Cohron J W , et al . Grain growth behaviour and high strain rate tensile properties of gas tungsten arc welds in iridium alloy DOP-26 [J]. Sci. Technol. Weld. Joining, 2000, 5: 297 |
| 11 | Wei Y , Chen L , Cai H Z , et al . Study on high temperature oxidation performance of iridium and iridium-rhodium alloy [J]. Precious Met., 2018, 39(1): 16 |
| 11 | 魏 燕, 陈 力, 蔡宏中 等 . 铱及铱铑合金的高温氧化性能研究 [J]. 贵金属, 2018, 39(1): 16 |
| 12 | Dai S L , Hu Z H . Preparation and application of ductile iridium [J]. Precious Met., 1999, 20(3): 13 |
| 12 | 戴松林, 胡志海 . 塑性铱的研究及其应用 [J]. 贵金属, 1999, 20(3): 13 |
| 13 | Gornostyrev Y N , Katsnelson M I , Medvedeva N I , et al . Peculiarities of defect structure and mechanical properties of iridium: Results of ab initio electronic structure calculations [J]. Phys. Rev., 2000, 62B: 7802 |
| 14 | Kontsevoi O Y , Gornostyrev Y N , Freeman A J . Modeling the dislocation properties and mechanical behavior of Ir, Rh, and their refractory alloys [J]. JOM, 2005, 57(3): 43 |
| 15 | Wolverton C . Crystal structure and stability of complex precipitate phases in Al-Cu-Mg-(Si) and Al-Zn-Mg alloys [J]. Acta mater., 2001, 49: 3129 |
| 16 | Yu R , Zhu J , Ye H Q . Calculations of single-crystal elastic constants made simple [J]. Comput. Phys. Commun., 2010, 181: 671 |
| 17 | Press W H , Flannery B P , Teukolsky S A , et al . Numerical Recipes: The Art of Scientific Computing [M]. Cambridge: Cambridge University Press, 2007: 26 |
| 18 | Pokluda J , ?erny M , ?ob M , et al . Ab initio calculations of mechanical properties: Methods and applications [J]. Prog. Mater. Sci., 2015, 73: 127 |
| 19 | Verma J K D , Nag B D . On the elastic moduli of a crystal and voigt and reuss relations [J]. J. Phys. Soc. Jpn., 1965, 20: 635 |
| 20 | Hill R . The elastic behaviour of a crystalline aggregate [J]. Proc. Phys. Soc., 1952, 65A: 349 |
| 21 | Pugh S F . XCII. Relations between the elastic moduli and the plastic properties of polycrystalline pure metals [J]. Philos. Mag., 1954, 45: 823 |
| 22 | Togo A , Oba F , Tanaka I . First-principles calculations of the ferroelastic transition between rutile-type and CaCl2-type SiO2 at high pressures [J]. Phys. Rev., 2008, 78B: 134106 |
| 23 | Mei Z G , Wang Y , Shang S L , et al . First-principles study of lattice dynamics and thermodynamics of TiO2 polymorphs [J]. Inorg. Chem., 2011, 50: 6996 |
| 24 | Deringer V L , Tchougréeff A L , Dronskowski R . Crystal orbital Hamilton population (COHP) analysis as projected from plane-wave basis sets [J]. J. Phys. Chem., 2011, 115A: 5461 |
| 25 | Hughbanks T , Hoffmann R . Chains of trans-edge-sharing molybdenum octahedra: Metal-metal bonding in extended systems [J]. J. Am. Chem. Soc., 1983, 105: 3528 |
| 26 | Dronskowski R , Bl?echl P E . Crystal orbital Hamilton populations (COHP): Energy-resolved visualization of chemical bonding in solids based on density-functional calculations [J]. J. Phys. Chem., 1993, 97: 8617 |
| 27 | Maintz S , Deringer V L , Tchougréeff A L , et al . LOBSTER: A tool to extract chemical bonding from plane-wave based DFT [J]. J. Comput. Chem., 2016, 37: 1030 |
| 28 | Kresse G , Furthmüller J . Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set [J]. Comput. Mater. Sci., 1996, 6: 15 |
| 29 | Kresse G , Furthmüller J . Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169 |
| 30 | Perdew J P , Burke K , Ernzerhof M . Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865 |
| 31 | Bl?chl P E . Projector augmented-wave method [J]. Phys. Rev., 1994, 50B: 17953 |
| 32 | Monkhorst H J , Pack J D . Special points for Brillouin-zone integrations [J]. Phys. Rev., 1976, 13B: 5188 |
| 33 | Parrish W . Results of the IUCr precision lattice-parameter project [J]. Acta Cryst., 1960, 13: 838 |
| 34 | Dewaele A , Loubeyre P , Mezouar M . Equations of state of six metals above 94 GPa [J]. Phys. Rev., 2004, 70B: 094112 |
| 35 | Featherston F H , Neighbours J R . Elastic constants of tantalum, tungsten, and molybdenum [J]. Phys. Rev., 1963, 130: 1324 |
| 36 | Stathis J H , Bolef D I . Elastic constants of tungsten between 4.2 and 77 K [J]. J. Appl. Phys., 1980, 51: 4770 |
| 37 | S?derlind P , Eriksson O , Wills J M , et al . Theory of elastic constants of cubic transition metals and alloys [J]. Phys. Rev., 1993, 48B: 5844 |
| 38 | Bercegeay C , Bernard S . First-principles equations of state and elastic properties of seven metals [J]. Phys. Rev., 2005, 72B: 214101 |
| 39 | Ko?i L , Ma Y , Oganov A R , et al . Elasticity of the superconducting metals V, Nb, Ta, Mo, and W at high pressure [J]. Phys. Rev., 2008, 77B: 214101 |
| 40 | Guo Z C , Luo F , Zhang X L , et al . First-principles calculations of elastic, phonon and thermodynamic properties of W [J]. Mol. Phys., 2016, 114: 3430 |
| 41 | Bolef D I , De Klerk J . Elastic constants of single‐crystal Mo and W between 77° and 500°K [J]. J. Appl. Phys., 1962, 33: 2311 |
| 42 | Yamabe-Mitarai Y , Ro Y , Harada H , et al . Ir-base refractory superalloys for ultra-high temperatures [J]. Metall. Mater. Trans., 1998, 29A: 537 |
| 43 | Simmons G , Wang H . Single Crystal Elastic Constants and Calculated Aggregate Properties: A Handbook [M]. 2nd Ed., Cambridge: MIT Press, 1971: 35 |
| 44 | Martienssen M , Warlimont H . Springer Handbook of Condensed Matter and Materials Dada [M]. Berlin: Springer Verlag, 2005: 386 |
| 45 | Yan H Y , Zhang M G , Zheng B B , et al . Modeling the elastic anisotropies and mechanical strengths of Ir3 X intermetallics [J]. J. Alloys Compd., 2017, 696: 611 |
| 46 | Pan Y , Wen M , Wang L , et al . Iridium concentration driving the mechanical properties of iridium-aluminum compounds [J]. J. Alloys Compd., 2015, 648: 771 |
| 47 | Mehl M J , Papaconstantopoulos D A . Applications of a tight-binding total-energy method for transition and noble metals: Elastic constants, vacancies, and surfaces of monatomic metals [J]. Phys. Rev., 1996, 54B: 4519 |
| 48 | Kamran S , Chen K Y , Chen L . Ab initio examination of ductility features of fcc metals [J]. Phys. Rev., 2009, 79B: 024106 |
| 49 | Wang Z L , Gao W J , Liu Y L , et al . A first principles investigation of W1 - x Mo x (x = 0-68.75 at.%) alloys: Structural, electronic, mechanical and thermal properties [J]. J. Alloys Compd., 2020, 829: 154480 |
| 50 | Hoffmann R . Solids and Surfaces: A Chemist's View of Bonding in Extended Structures [M]. New York: VCH Publishers, 1988: 106 |
/
| 〈 |
|
〉 |