GH4169合金与S31042钢线性摩擦焊接头组织及力学性能
收稿日期: 2020-07-21
修回日期: 2020-10-30
网络出版日期: 2020-11-19
基金资助
国家自然科学基金项目(U1660201)
Microstructure and Mechanical Properties of Linear Friction Welding Joint of GH4169 Alloy/S31042 Steel
Received date: 2020-07-21
Revised date: 2020-10-30
Online published: 2020-11-19
Supported by
National Natural Science Foundation of China(U1660201)
使用25 Hz振动频率、2 mm振幅、100 MPa摩擦压力和150 MPa顶锻压力的工艺参数对GH4169合金和S31042钢进行线性摩擦焊连接,通过OM、SEM和TEM分析异质接头的组织特征,并进行拉伸、硬度和蠕变实验测试异质接头在室温和高温环境下的力学性能。结果表明,GH4169合金与S31042钢的连接界面在线性摩擦焊过程中发生动态再结晶,形成无孔无裂纹的冶金结合,同时焊缝区在高温和应力作用下形成大量弥散分布的强化相颗粒。通过细晶强化和析出强化的综合作用,异质接头的抗拉强度高于S31042钢,焊缝区的硬度明显高于2种母材。
李彦默 , 郭小辉 , 陈斌 , 李培跃 , 郭倩颖 , 丁然 , 余黎明 , 苏宇 , 李文亚 . GH4169合金与S31042钢线性摩擦焊接头组织及力学性能[J]. 金属学报, 2021 , 57(3) : 363 -374 . DOI: 10.11900/0412.1961.2020.00271
S31042 steel is a typical 25Cr-20Ni type austenitic heat-resistant steel with excellent resistance to oxidation and creep rupture strength near 600oC. This austenitic steel is widely used as a super-heater or re-heater in ultra-super critical plants with steam specifications as high as 600oC and 25 MPa. To reduce CO2 emissions and improve power generation, the application of advanced ultra-super critical plants (steam parameters 700oC and 30 MPa) can be promoted. Owing to its excellent mechanical properties as well as good corrosion resistance at elevated temperature above 650oC, GH4169 alloys have the potential to be used in advanced ultra-super critical plants. Practically, it is meaningful to investigate the welding process of GH4169/S31042 dissimilar materials. In this work, the joint between dissimilar materials (S31042/GH4169) was studied by linear friction welding, and the microstructures and mechanical properties of the joint were investigated by OM, SEM, TEM, hardness testing, tensile testing, and creep testing at 700oC. Good metallurgic bonding was obtained under the optimized welding process parameters of 25 Hz (frequency), 2 mm (amplitude), 100 MPa of frictional pressure, and 150 MPa of forging pressure. Dynamic recrystallization occurred and the secondary phase particles precipitated within the weld zone. The microhardness of the welded joint was higher than that of the base metal, and the tensile properties of the joint were higher than S31042 steel, which is attributed to both fine grain and dispersion strengthening.
| 1 | Du H, Cheng Y, Hou L, et al. Evolution of intergranular corrosion resistance for HR3C heat-resistant austenitic stainless steel at elevated temperature [J]. Corros. Eng. Sci. Technol., 2017, 52: 343 |
| 2 | Wang J, Qiao Y F, Dong N, et al. The Influence of temperature on the oxidation mechanism in air of HR3C and aluminum-containing 22Cr-25Ni austenitic stainless steels [J]. Oxid. Met., 2018, 89: 713 |
| 3 | Fang Y Y, Zhao J, Li X N. Precipitates in HR3C steel aged at high temperature [J]. Acta Metall. Sin., 2010, 46: 844 |
| 3 | 方圆圆, 赵 杰, 李晓娜. HR3C钢高温时效过程中的析出相 [J]. 金属学报, 2010, 46: 844 |
| 4 | Li Y M, Liu Y C, Liu C X, et al. Mechanism for the formation of Z-phase in 25Cr-20Ni-Nb-N austenitic stainless steel [J]. Mater. Lett., 2018, 233: 16 |
| 5 | Hu G D, Wang P, Li D Z, et al. Precipitate evolution in a modified 25Cr-20Ni austenitic heat resistant stainless steel during creep rupture test at 750oC [J]. Acta Metall. Sin., 2018, 54: 1705 |
| 5 | 胡国栋, 王 培, 李殿中等. 新型25Cr-20Ni奥氏体耐热不锈钢750℃持久实验过程中析出相演变 [J]. 金属学报, 2018, 54: 1705 |
| 6 | Yang Y H, Zhu L H, Wang Q J, et al. Microstructural evolution and the effect on hardness and plasticity of S31042 heat-resistant steel during creep [J]. Mater. Sci. Eng., 2014, A608: 164 |
| 7 | Wang J Z, Liu Z D, Bao H S, et al. Evolution of precipitates of S31042 heat resistant steel during 700oC aging [J]. J. Iron Steel Res. Int., 2013, 20: 113 |
| 8 | Peng Z F, Ren W, Yang C, et al. Relationship between the evolution of phase parameters of grain boundary M23C6 and embrittlement of HR3C super-heater tubes in service [J]. Acta Metall. Sin., 2015, 51: 1325 |
| 8 | 彭志方, 任 文, 杨 超等. HR3C钢运行过热器管的脆化与晶界M23C6相参量演化的关系 [J]. 金属学报, 2015, 51: 1325 |
| 9 | Wang B, Liu Z C, Cheng S C, et al. Microstructure evolution and mechanical properties of HR3C steel during long-term aging at high temperature [J]. J. Iron. Steel Res. Int., 2014, 21: 765 |
| 10 | Hu Z F, Zhang Z. Investigation the effect of precipitating characteristics on the creep behavior of HR3C austenitic steel at 650oC [J]. Mater. Sci. Eng., 2019, A742: 451 |
| 11 | Hari P R, Arivazhagan N, Rao M N, et al. Hot corrosion studies on alloy 617 OCC in the context of its use in advanced ultra-supercritical (A-USC) power plants [J]. Trans. Indian Inst. Met., 2017, 70: 775 |
| 12 | Aung N N, Liu X B. Effect of temperature on coal ash hot corrosion resistance of Inconel 740 superalloy [J]. Corros. Sci., 2014, 82: 227 |
| 13 | Zhang H J, Li C, Liu Y C, et al. Effect of hot deformation on γ″ and δ phase precipitation of Inconel 718 alloy during deformation & isothermal treatment [J]. J. Alloys Compd., 2017, 716: 65 |
| 14 | Zhang H J, Li C, Guo Q Y, et al. Hot tensile behavior of cold-rolled Inconel 718 alloy at 650oC: The role of δ phase [J]. Mater. Sci. Eng., 2018, A722: 136 |
| 15 | Zhang X, Li H W, Zhan M, et al. Electron force-induced dislocations annihilation and regeneration of a superalloy through electrical in-situ transmission electron microscopy observations [J]. J. Mater. Sci. Technol., 2020, 36: 79 |
| 16 | Zhang H J, Li C, Guo Q Y, et al. Deformation mechanism of L12-γ′ phase in bimodal γ″-γ′ precipitation hardened Inconel 718 superalloy [J]. Adv. Eng. Mater., 2018, 20: 1800652 |
| 17 | Zhang H J, Li C, Liu Y C, et al. Precipitation behavior during high-temperature isothermal compressive deformation of Inconel 718 alloy [J]. Mater. Sci. Eng., 2016, A677: 515 |
| 18 | Liu Y C, Zhang H J, Guo Q Y, et al. Microstructure evolution of Inconel 718 superalloy during hot working and its recent development tendency [J]. Acta Metall. Sin., 2018, 54: 1653 |
| 18 | 刘永长, 张宏军, 郭倩颖等. Inconel 718变形高温合金热加工组织演变与发展趋势 [J]. 金属学报, 2018, 54: 1653 |
| 19 | Li W Y, Vairis A, Preuss M, et al. Linear and rotary friction welding review [J]. Int. Mater. Rev., 2016, 61: 71 |
| 20 | Shao Y, Li Y M, Liu C X, et al. Annealing process optimization of high frequency longitudinal resistance welded low-carbon ferritic stainless steel pipe [J]. Acta Metall. Sin., 2019, 55: 1367 |
| 20 | 邵 毅, 李彦默, 刘晨曦等. 低碳铁素体不锈钢高频直缝电阻焊管退火工艺优化 [J]. 金属学报, 2019, 55: 1367 |
| 21 | Ji Y J, Zhang T C, Zhang L F, et al. Structure and mechanical property of TC17 linear friction welding joint [J]. Trans. China Weld. Inst., 2019, 40(9): 156 |
| 21 | 季亚娟, 张田仓, 张连锋等. TC17钛合金线性摩擦焊接头组织及性能 [J]. 焊接学报, 2019, 40(9): 156 |
| 22 | Chang C C, Zhang T C, Li J, et al. Microstructure and properties of linear friction welded joint of hyperoxia TC4/TC17 dissimilar titanium alloys [J]. Trans. China Weld. Inst., 2019, 40(12): 109 |
| 22 | 常川川, 张田仓, 李 菊等. 高氧TC4/TC17钛合金线性摩擦焊接头组织特征及力学性能 [J]. 焊接学报, 2019, 40(12): 109 |
| 23 | Zhang C C, Zhang T C, Jin J L. Microstructure and mechanical properties of linear friction welding joint of TC21/TC4-DT [J]. Trans. China Weld. Inst., 2019, 40(12): 133 |
| 23 | 张传臣, 张田仓, 金俊龙. TC21+TC4-DT线性摩擦焊接头组织与力学性能试验 [J]. 焊接学报, 2019, 40(12): 133 |
| 24 | Chang C C, Zhang T C, Li J. Study on microstructure and microhardness of linear friction welded joints of Ti-22Al-27Nb alloy [J]. Trans. China Weld. Inst., 2019, 40(3): 140 |
| 24 | 常川川, 张田仓, 李 菊. Ti-22Al-27Nb合金线性摩擦焊接头组织与显微硬度分析 [J]. 焊接学报, 2019, 40(3): 140 |
| 25 | Ma T J, Chen T, Li W Y, et al. Formation mechanism of linear friction welded Ti-6Al-4V alloy joint based on microstructure observation [J]. Mater. Charact., 2011, 62: 130 |
| 26 | Ma T J, Li W Y, Xu Q Z, et al. Microstructure evolution and mechanical properties of linear friction welded 45 steel joint [J]. Adv. Eng. Mater., 2007, 9: 703 |
| 27 | Yang X W, Li W Y, Li J L, et al. Finite element modeling of the linear friction welding of GH4169 superalloy [J]. Mater. Des., 2015, 87: 215 |
| 28 | Ma T J, Xiao Y, Li W Y, et al. Investigation on microstructure and texture evolution of linear friction welded IN718 superalloy joints [J]. Trans. China Weld. Inst., 2016, 37(11): 119 |
| 28 | 马铁军, 肖 遥, 李文亚等. 线性摩擦焊IN718接头微观组织与织构演变 [J]. 焊接学报, 2016, 37(11): 119 |
| 29 | Duan L J, Liu Y C. Relationships between elastic constants and EAM/FS potential functions for cubic crystals [J]. Acta Metall. Sin., 2020, 56: 112 |
| 29 | 段灵杰, 刘永长. 立方晶体弹性常数和EAM/FS势函数的关系 [J]. 金属学报, 2020, 56: 112 |
| 30 | Ma T J, Yan M, Yang X W, et al. Microstructure evolution in a single crystal nickel-based superalloy joint by linear friction welding [J]. Mater. Des., 2015, 85: 613 |
| 31 | Chen X, Xie F Q, Ma T J, et al. Effects of post-weld heat treatment on microstructure and mechanical properties of linear friction welded Ti2AlNb alloy [J]. Mater. Des., 2016, 94: 45 |
| 32 | He J C, Zhang T C, Li J. Effect of heat treatment on microstructure and hardness of Ti2AlNb linear friction welding joint [J]. Trans. China Weld. Inst., 2019, 40(4): 119 |
| 32 | 贺建超, 张田仓, 李 菊. 热处理对Ti2AlNb线性摩擦焊接头组织与硬度的影响 [J]. 焊接学报, 2019, 40(4): 119 |
| 33 | Li J, Zhang T C, Guo D L. Influence of heat treatment on microstructure and mechanical properties of TC17(α+β)/TC17(β) linear friction welding joint [J]. Trans. China Weld. Inst., 2018, 39(5): 97 |
| 33 | 李 菊, 张田仓, 郭德伦. 热处理对TC17(α+β)/TC17(β)线性摩擦焊接头组织及力学性能的影响 [J]. 焊接学报, 2018, 39(5): 97 |
| 34 | Li Y M, Liu C X, Yu L M, et al. Effect of high-temperature ageing on microstructure and mechanical properties of linear friction welded S31042 steel joint [J]. Acta Metall. Sin., 2018, 54: 981 |
| 34 | 李彦默, 刘晨曦, 余黎明等. 高温时效对S31042钢线性摩擦焊接头组织和力学性能的影响 [J]. 金属学报, 2018, 54: 981 |
/
| 〈 |
|
〉 |