NaCl溶液腐蚀后304不锈钢的射流空蚀特征
收稿日期: 2020-04-07
修回日期: 2020-05-12
网络出版日期: 2020-07-07
基金资助
国家自然科学基金项目(51775251)
Characteristics of Waterjet Cavitation Erosion of 304 Stainless Steel After Corrosion in NaCl Solution
Received date: 2020-04-07
Revised date: 2020-05-12
Online published: 2020-07-07
Supported by
National Natural Science Foundation of Chin(51775251)
对采用3%NaCl溶液腐蚀后的304不锈钢试样,借助符合ASTM G134标准的射流空蚀实验装置进行空蚀实验,测量表征试样的质量损失、表面微观组织、表面三维形貌和显微硬度,分析304不锈钢试样的空蚀特征,探究腐蚀时间和空蚀时间对空蚀效果的影响。结果表明,腐蚀时间为24 h的试样,空蚀120 min后即进入空蚀衰减阶段。在空蚀前期,空蚀坑的尺寸小且深度较浅;空蚀后期,试样表面的塑性变形加重,大尺寸空蚀坑增多,晶界处的微裂纹沿晶界扩展,最终空蚀坑之间相互连接导致试样表面出现晶界剥落现象。试样的表面粗糙度随着空蚀时间延长而增大;未经3%NaCl溶液腐蚀时的表面粗糙度最大。空蚀时间为120 min时,腐蚀时间为120 h的试样,其表面塑性变形较腐蚀时间为24 h的试样加剧,且晶界处出现微裂纹。3%NaCl溶液的腐蚀起到延缓空蚀的作用,但延缓程度随着腐蚀时间的延长而减小。
刘海霞 , 陈金豪 , 陈杰 , 刘光磊 . NaCl溶液腐蚀后304不锈钢的射流空蚀特征[J]. 金属学报, 2020 , 56(10) : 1377 -1385 . DOI: 10.11900/0412.1961.2020.00107
The 304 stainless steel specimens were corroded in 3%NaCl solution, and then cavitation erosion experiments were performed on these specimens using an experimental rig that conformed to the ASTM G134 standard. The effects of both the corrosion time and erosion time on cavitation erosion were analyzed. The cavitation erosion characteristics were described via the mass loss, surface microstructure, three-dimensional surface morphology and microhardness. The results show that for the specimen corroded for 24 h, the stage of cavitation erosion attenuation commences at the cavitation erosion time of 120 min. In the early stage of cavitation erosion, erosion pits manifest small size and depth. In the later stage of cavitation erosion, the plastic deformation is intensified and large erosion pits are abundant. Microcracks expand along grain boundaries. Eventually, the interconnection between erosion pits incurs peeling-off of grain boundaries. The surface roughness increases with the cavitation erosion time. Compared to the corroded specimens, the non-corroded specimen demonstrates higher surface roughness after cavitation erosion. As the corrosion time increases from 24 h to 120 h and the cavitation erosion time is remained at 120 min, the plastic deformation is strengthened and microcracks emerge at grain boundaries. The 3%NaCl solution helps to suppress cavitation erosion. Nevertheless, as the corrosion time increases, the suppression effect attenuates.
| [1] | Lebon G S B, Tzanakis I, Pericleous K, et al. Experimental and numerical investigation of acoustic pressures in different liquids [J]. Ultrasonics-Sonochem, 2018, 42: 411 |
| [2] | Franc J P, Michel J M. Fundamentals of Cavitation [M]. Holland: Kluwer Academic Publishers, 2004: 269 |
| [3] | Peng K W, Tian S C, Li G S, et al. Mapping cavitation impact field in a submerged cavitating jet [J]. Wear, 2018, 396-397: 22 |
| [4] | Zhou M M, Liu H X, Kang C, et al. Resistance of curved surfaces to the cavitation erosion produced through high-pressure submerged waterjet [J]. Wear, 2019, 440-441: 203091 |
| [5] | Liu H X, Kang C, Zhang W, et al. Flow structures and cavitation in submerged waterjet at high jet pressure [J]. Exp. Thermal Fluid Sci., 2017, 88: 504 |
| [6] | Lehocka D, Klich J, Foldyna J, et al. Copper alloys disintegration using pulsating water jet [J]. Measurement, 2016, 82: 375 |
| [7] | Kang C, Liu H X, Zhang T, et al. Investigation of submerged waterjet cavitation through surface property and flow information in ambient water [J]. Appl. Surf. Sci., 2017, 425: 915 |
| [8] | Wu C Q, Ren R M, Liu P T, et al. Cavitation erosion of 304 stainless steel induced by caviting water jet [J]. Chin. J. Mater. Res., 2016, 30: 473 |
| [8] | (吴从前, 任瑞铭, 刘鹏涛等. 304不锈钢空化水射流表面空蚀损伤研究 [J]. 材料研究学报, 2016, 30: 473) |
| [9] | Liu H, Zhao X J, Liu P T, et al. Cavitation damage on surface of pure copper by cavitating water jet erosion [J]. Mater. Mech. Eng., 2017, 41(5): 68 |
| [9] | (刘 欢, 赵秀娟, 刘鹏涛等. 空化水射流冲蚀纯铜的表面空蚀损伤 [J]. 机械工程材料, 2017, 41(5): 68) |
| [10] | Azhari A, Schindler C, Hilbert K, et al. Influence of waterjet peening and smoothing on the material surface and properties of stainless steel 304 [J]. Surf. Coat. Technol., 2014, 258: 1176 |
| [11] | Zheng Z B, Zheng Y G. Effects of surface treatments on the corrosion and erosion-corrosion of 304 stainless steel in 3.5% NaCl solution [J]. Corros. Sci., 2016, 112: 657 |
| [12] | Zhao Y L, Zhou F, Yao J, et al. Erosion-corrosion behavior and corrosion resistance of AISI 316 stainless steel in flow jet impingement [J]. Wear, 2015, 328-329: 464 |
| [13] | Aribo S, Barker R, Hu X M, et al. Erosion-corrosion behaviour of lean duplex stainless steels in 3.5% NaCl solution [J]. Wear, 2013, 302: 1602 |
| [14] | Kovendhan M, Kang H, Jeong S, et al. Study of stainless steel electrodes after electrochemical analysis in sea water condition [J]. Environ. Res., 2019, 173: 549 |
| [15] | Qiao Y X, Wang S, Liu B, et al. Synergistic effect of corrosion and cavitation erosion of high nitrogen stainless steel [J]. Acta Metall. Sin., 2016, 52: 233 |
| [15] | (乔岩欣, 王 硕, 刘 彬等. 新型高氮钢的腐蚀和空蚀交互作用研究 [J]. 金属学报, 2016, 52: 233) |
| [16] | Yong X Y, Xiao N, Shen H J, et al. Responses of the corroded surface layer of austenitic stainless steel to different corrosive conditions under cavitation [J]. Mater. Sci. Eng., 2016, A671: 118 |
| [17] | Luo Q, Zhang Q, Qin Z B, et al. The synergistic effect of cavitation erosion and corrosion of nickel-aluminum copper surface layer on nickel-aluminum bronze alloy [J]. J. Alloys Compd., 2018, 747: 861 |
| [18] | Niederhofer P, Richrath L, Huth S, et al. Influence of conventional and powder-metallurgical manufacturing on the cavitation erosion and corrosion of high interstitial CrMnCN austenitic stainless steels [J]. Wear, 2016, 360-361: 67 |
| [19] | Basumatary J, Nie M, Wood R J K. The synergistic effects of cavitation erosion-corrosion in ship propeller materials [J]. J. Bio- Tribo-Corros., 2015, 1: 1 |
| [20] | Selvam K, Saini J, Perumal G, et al. Exceptional cavitation erosion-corrosion behavior of dual-phase bimodal structure in austenitic stainless steel [J]. Tribol. Int., 2019, 134: 77 |
| [21] | Basumatary J, Wood R J K. Synergistic effects of cavitation erosion and corrosion for nickel aluminium bronze with oxide film in 3.5% NaCl solution [J]. Wear, 2017, 376-377: 1286 |
| [22] | ASTM. ASTM G134-17 Standard test method for erosion of solid materials by cavitating liquid jet [S]. West Conshohocken, PA: ASTM International, 2017 |
| [23] | Soyama H, Takakuwa O. Enhancing the aggressive strength of a cavitating jet and its practical application [J]. J. Fluid Sci. Technol., 2011, 6: 510 |
| [24] | Qu X H. The corrossion susceptibility study on 304 stainless steel in circulating cooling water containing chloride ion [D]. Beijing: Beijing University of Chemical Technology, 2008 |
| [24] | (曲秀华. 304不锈钢在含氯离子循环冷却水中腐蚀敏感性的影响 [D]. 北京: 北京化工大学, 2008) |
| [25] | Yang L Q, Zhang C, Xiao J S. Effect of NaCl solution concentration on acoustic emission feature during corrosion of 304 stainless steel [J]. Trans. Mater. Heat Treat., 2014, 35(12): 184 |
| [25] | (杨立清, 张 超, 肖俊生. NaCl溶液浓度对304不锈钢腐蚀过程的声发射特征影响 [J]. 材料热处理学报, 2014, 35(12): 184) |
| [26] | Zhuang D D, Chen W B, Ouyang Y D, et al. Comparative investigation of ultrasonic cavitation erosion mechanism for low-carbon and 304 stainless steels [J]. Surf. Technol., 2019, 48(1): 225 |
| [26] | (庄栋栋, 陈文博, 欧阳亚东等. 低碳钢与304不锈钢的超声空蚀机理对比研究 [J]. 表面技术, 2019, 48(1): 225) |
| [27] | Zhang T, Liu H X, Kang C, et al. Ultrasonic cavitation erosion behavior and mechanism of Pb-brass alloy in different liquids [J]. Surf. Technol., 2018, 47(1): 109 |
| [27] | (张 桃, 刘海霞, 康 灿等. 铅黄铜合金在不同溶体介质中的超声空蚀行为及机理 [J]. 表面技术, 2018, 47(1): 109) |
/
| 〈 |
|
〉 |