核电站DMWJ中材料拘束的影响与优化

  • 杨杰 ,
  • 王雷
展开
  • 上海理工大学能源与动力工程学院上海市动力工程多相流动与传热重点实验室 上海 200093
杨 杰,男,1987年生,副教授,博士

收稿日期: 2019-09-10

  修回日期: 2020-03-02

  网络出版日期: 2020-03-13

基金资助

国家自然科学基金项目(51975378);国家自然科学基金项目(51605292)

Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants

  • Jie YANG ,
  • Lei WANG
Expand
  • Shanghai Key Laboratory of Multiphase Flow and Heat Transfer in Power Engineering, School of Energy and Power Engineering, University of Shanghai for Science and Technology, Shanghai 200093, China

Received date: 2019-09-10

  Revised date: 2020-03-02

  Online published: 2020-03-13

Supported by

National Natural Science Foundation of China(51975378);National Natural Science Foundation of China(51605292)

摘要

选用新一代核电安全端52M镍基合金异种金属焊接接头(DMWJ)为研究对象,以热影响区中危险位置为初始裂纹所在位置,系统研究了热影响区(HAZ)、熔合区(FZ)和近界面区(NIZ)材料拘束对DMWJ断裂行为的影响,并在此基础上对DMWJ各区域的材料拘束进行优化设计。结果表明,对于热影响区裂纹,当单独改变裂纹所在HAZ区域的强度时,J-R阻力曲线随着HAZ区域材料拘束失配系数(Ms)的增加而单调增加;当单独改变裂纹周边FZ或NIZ区域的强度时,J-R阻力曲线随着FZ或NIZ区域Ms的增加先增加后降低再不变。材料拘束优化后,DMWJ的J-R阻力曲线均明显高于实际DMWJ的J-R阻力曲线,同时改变3个区域的材料拘束失配系数,当Ms (HAZ):Ms (FZ):Ms (NIZ)=2:1.4:0.84时,得到了几倍于目前DMWJ的J-R阻力曲线。

本文引用格式

杨杰 , 王雷 . 核电站DMWJ中材料拘束的影响与优化[J]. 金属学报, 2020 , 56(6) : 840 -848 . DOI: 10.11900/0412.1961.2019.00298

Abstract

The material constraint is an important factor affecting the fracture behavior of dissimilar metal welded joint (DMWJ). For accurately design, manufacture and structure integrity assessment, is necessary to clarify the influence of material constraint on the DMWJ. However, there is still a lack of a systematic research on the influence of material constraint on the fracture behavior of the DMWJ in the current nuclear power plants, and how to improve the fracture resistance of the DMWJ by the optimal design of the material constraint should be considered. In this work, a 52M nickel-based alloy DMWJ in nuclear power plants was selected, the initial crack which located in the heat affected zone (HAZ) was manufactured, and the fracture behaviors of the DMWJ under different material constraints of HAZ, fusion zone (FZ) and near interface zone (NIZ) were studied. In addition, the optimal design of the material constraint was investigated. The results show that for the HAZ crack, the J-resistance curves increase monotonously with increasing the strength of HAZ where the crack is located in. And the J-resistance curves increase firstly, then decrease and remain steady with increasing the strength of FZ and NIZ where the crack is nearby. The optimized DMWJs have higher J-resistance curves, and when Ms (HAZ): Ms (FZ):Ms (NIZ)=2:1.4:0.84, the optimized DMWJ has the highest J-resistance curve which is several times of the current J-resistance curve.

参考文献

[1] Li J, Wu X Q, Han E H, et al. A review of corrosion failure of welded structural metallic materials for light water reactor plant [J]. Corros. Sci. Prot. Technol., 2014, 26: 1
[1] 李 江, 吴欣强, 韩恩厚等. 核电焊接结构材料腐蚀失效研究现状与进展 [J]. 腐蚀科学与防护技术, 2014, 26: 1
[2] Celin R, Tehovnik F. Degradation of a Ni-Cr-Fe alloy in a pressurised-water nuclear power plant [J]. Mater. Technol., 2011, 45: 151
[3] Ogawa T, Itatani M, Saito T, et al. Fracture assessment for a dissimilar metal weld of low alloy steel and Ni-base alloy [J]. Int. J. Press. Vessels Pip., 2012, 90-91: 61
[4] Ming H L, Zhang Z M, Wang J Q, et al. Microstructure of a domestically fabricated dissimilar metal weld joint (SA508-52M-309L-CF8A) in nuclear power plant [J]. Mater. Charact., 2019, 148: 100
[5] Ming H L, Zhang Z M, Wang J Q, et al. Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW [J]. Mater. Charact., 2017, 123: 233
[6] Ming H L, Zhu R L, Zhang Z M, et al. Microstructure, local mechanical properties and stress corrosion cracking susceptibility of an SA508-52M-316LN safe-end dissimilar metal weld joint by GTAW [J]. Mater. Sci. Eng., 2016, A669: 279
[7] Ming H L, Zhang Z M, Wang J Q, et al. Microstructure and local properties of a domestic safe-end dissimilar metal weld joint by using hot-wire GTAW [J]. Acta Metall. Sin., 2017, 53: 57
[7] 明洪亮, 张志明, 王俭秋等. 国产核电安全端异种金属焊接件的微观结构及局部性能研究 [J]. 金属学报, 2017, 53: 57
[8] Dong L J, Peng Q J, Han E H, et al. Microstructure and intergranular stress corrosion cracking susceptibility of a SA508-52M-316L dissimilar metal weld joint in primary water [J]. J. Mater. Sci. Technol., 2018, 34: 1281
[9] Dong L J, Peng Q J, Xue H, et al. Correlation of microstructure and stress corrosion cracking initiation behaviour of the fusion boundary region in a SA508 Cl. 3-Alloy 52M dissimilar weld joint in primary pressurized water reactor environment [J]. Corros. Sci., 2018, 132: 9
[10] Wang H T, Wang G Z, Xuan F Z, et al. Local mechanical properties of a dissimilar metal welded joint in nuclear power systems [J]. Mater. Sci. Eng., 2013, A568: 108
[11] Wang H T, Wang G Z, Xuan F Z, et al. Fracture mechanism of a dissimilar metal welded joint in nuclear power plant [J]. Eng. Fail. Anal., 2013, 28: 134
[12] Blouin A, Chapuliot S, Marie S, et al. Brittle fracture analysis of dissimilar metal welds [J]. Eng. Fract. Mech., 2014, 131: 58
[13] Chen Z R, Lu Y H. TEM observation of martensite layer at the weld interface of an A508III to inconel 82 dissimilar metal weld joint [J]. Metall. Mater. Trans., 2015, 46A: 5494
[14] Chen Z R, Lu Y H, Ding X F, et al. Microstructural and hardness investigations on a dissimilar metal weld between low alloy steel and Alloy 82 weld metal [J]. Mater. Charact., 2016, 121: 166
[15] Jahanzeb N, Shin J H, Singh J, et al. Effect of microstructure on the hardness heterogeneity of dissimilar metal joints between 316L stainless steel and SS400 steel [J]. Mater. Sci. Eng., 2017, A700: 338
[16] Wang H T, Wang G Z, Xuan F Z, et al. An experimental investigation of local fracture resistance and crack growth paths in a dissimilar metal welded joint [J]. Mater. Des., 2013, 44: 179
[17] Samal M K, Seidenfuss M, Roos E, et al. Investigation of failure behavior of ferritic-austenitic type of dissimilar steel welded joints [J]. Eng. Fail. Anal., 2011, 18: 999
[18] Fan K, Wang G Z, Xuan F Z, et al. Local fracture resistance behavior of interface regions in a dissimilar metal welded joint [J]. Eng. Fract. Mech., 2015, 136: 279
[19] Chhibber R, Arora N, Gupta S R, et al. Use of bimetallic welds in nuclear reactors: Associated problems and structural integrity assessment issues [J]. Proc. Inst. Mech. Eng., 2006, 220C: 1121
[20] Laukkanen A, Nevasmaa P, Ehrnstén U, et al. Characteristics relevant to ductile failure of bimetallic welds and evaluation of transferability of fracture properties [J]. Nucl. Eng. Des., 2007, 237: 1
[21] Shang Y B, Shi H J, Wang Z X, et al. In-situ SEM study of short fatigue crack propagation behavior in a dissimilar metal welded joint of nuclear power plant [J]. Mater. Des., 2015, 88: 598
[22] Kim Y J, Kim J S, Cho S M, et al. 3-D constraint effects on J testing and crack tip constraint in M(T), SE(B), SE(T) and C(T) specimens: Numerical study [J]. Eng. Fract. Mech., 2004, 71: 1203
[23] ?stby E, Thaulow C, Zhang Z L. Numerical simulations of specimen size and mismatch effects in ductile crack growth-Part I: Tearing resistance and crack growth paths [J]. Eng. Fract. Mech., 2007, 74: 1770
[24] ?stby E, Thaulow C, Zhang Z L. Numerical simulations of specimen size and mismatch effects in ductile crack growth-Part II: Near-tip stress fields [J]. Eng. Fract. Mech., 2007, 74: 1793
[25] Yang J, Wang G Z, Xuan F Z, et al. An experimental investigation of in-plane constraint effect on local fracture resistance of a dissimilar metal welded joint [J]. Mater. Des., 2014, 53: 611
[26] Yang J, Wang G Z, Xuan F Z, et al. Out-of-plane constraint effect on local fracture resistance of a dissimilar metal welded joint [J]. Mater. Des., 2014, 55: 542
[27] Yang J, Wang L. Fracture mechanism of cracks in the weakest location of dissimilar metal welded joint under the interaction effect of in-plane and out-of-plane constraints [J]. Eng. Fract. Mech., 2018, 192: 12
[28] Zhang Z L, Hauge M, Thaulow C. Two-parameter characterization of the near-tip stress fields for a bi-material elastic-plastic interface crack [J]. Int. J. Fract., 1996, 79: 65
[29] Betegón C, Pe?uelas I. A constraint based parameter for quantifying the crack tip stress fields in welded joints [J]. Eng. Fract. Mech., 2006, 73: 1865
[30] Xue H, Sun J W. Study on micro region of crack tip of welded joints under different matches of yield stress [J]. Hot Work. Technol., 2016, 45(21): 239
[30] 薛 河, 孙剑伟. 不同屈服强度匹配下焊接接头裂纹尖端微观区域的研究 [J]. 热加工工艺, 2016, 45(21): 239
[31] Rakin M, Medjo B, Gubeljak N, et al. Micromechanical assessment of mismatch effects on fracture of high-strength low alloyed steel welded joints [J]. Eng. Fract. Mech., 2013, 109: 221
[32] Yang J, Wang G Z, Xuan F Z, et al. Unified correlation of in-plane and out-of-plane constraint with fracture resistance of a dissimilar metal welded joint [J]. Eng. Fract. Mech., 2014, 115: 296
[33] Yang J, Wang L. Effect range of the material constraint-I. Center crack [J]. Materials (Basel), 2019, 12(1): E67
[34] Dai Y, Yang J, Wang L. Effect range of the material constraint-II. Interface crack [J]. Metals (Basel), 2019, 9: 696
[35] Wang H T, Wang G Z, Xuan F Z, et al. Local mechanical properties and Microstructures of Alloy52M dissimilar metal welded joint between A508 ferritic steel and 316L stainless steel [J]. Adv. Mater. Res., 2012, 509: 103
[36] Yang J. Micromechanical analysis of in-plane constraint effect on local fracture behavior of cracks in the weakest locations of dissimilar metal welded joint [J]. Acta Metall. Sin. (Engl. Lett., 2017, 30: 840
[37] Linder C, Armero F. Finite elements with embedded branching [J]. Finite Elem. Anal. Des., 2009, 45: 280
[38] Lloberas-Valls O, Huespe A E, Oliver J, et al. Strain injection techniques in dynamic fracture modeling [J]. Comput. Meth. Appl. Mech. Eng., 2016, 308: 499
文章导航

/