羟基亚乙基二膦酸对20SiMn钢在含Cl-混凝土模拟孔隙液中的缓蚀行为

  • 曹凤婷 ,
  • 魏洁 ,
  • 董俊华 ,
  • 柯伟 ,
  • 王铁钢 ,
  • 范其香
展开
  • 1.中国科学院金属研究所沈阳材料科学国家研究中心 沈阳 110016
    2.天津职业技术师范大学机械工程学院天津市高速切削与精密加工重点实验室 天津 300222
曹凤婷,女,1988年生,讲师,博士

收稿日期: 2019-11-11

  修回日期: 2020-01-04

  网络出版日期: 2020-01-22

基金资助

国家自然科学基金项目(U1867216);国家自然科学基金项目(51501201);国家自然科学基金项目(51801219)

Corrosion Inhibition Behavior of 1-Hydroxyethylidene-1, 1-Diphosphonic Acid on 20SiMn Steel in Simulated Concrete Pore Solution Containing Cl-

  • Fengting CAO ,
  • Jie WEI ,
  • Junhua DONG ,
  • Wei KE ,
  • Tiegang WANG ,
  • Qixiang FAN
Expand
  • 1.Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2.Tianjin Key Laboratory of High Speed Cutting and Precision Machining, School of Mechanical Engineering, Tianjin University of Technology and Education, Tianjin 300222, China

Received date: 2019-11-11

  Revised date: 2020-01-04

  Online published: 2020-01-22

Supported by

National Natural Science Foundation of China(U1867216);National Natural Science Foundation of China(51501201);National Natural Science Foundation of China(51801219)

摘要

采用电化学技术(动电位极化曲线、自腐蚀电位、EIS以及Mott-Schottky曲线)和表面分析方法(SEM、XPS)研究了羟基亚乙基二膦酸(HEDP)对空冷20SiMn低合金钢在含Cl-的高碱性混凝土模拟孔隙液中的缓蚀作用及机理。结果表明, HEDP对20SiMn钢在含1 mol/L NaCl饱和Ca(OH)2溶液中的缓蚀效果随HEDP浓度的升高存在极值,最佳浓度为1.441×10-4 mol/L。在此浓度下HEDP将20SiMn钢的钝性保持时间从6 h延长至9 h,缓蚀效率达到46.45%~59.78%。在发生点蚀的情况下,HEDP对点蚀的发展亦有显著的抑制作用,缓蚀效率超过93%。电化学和表面分析结果表明,HEDP优先吸附在钝化膜表面,通过竞争吸附机制屏蔽了侵蚀性Cl-向钝化膜表面的附着,从而对其产生保护作用。

本文引用格式

曹凤婷 , 魏洁 , 董俊华 , 柯伟 , 王铁钢 , 范其香 . 羟基亚乙基二膦酸对20SiMn钢在含Cl-混凝土模拟孔隙液中的缓蚀行为[J]. 金属学报, 2020 , 56(6) : 898 -908 . DOI: 10.11900/0412.1961.2019.00382

Abstract

The corrosion of steel rebar in concrete will be induced once the passive film is destroyed by chlorides or carbonation. Several techniques have been employed to reduce the corrosion so far. Among them, adding inhibitors is effective one because of its advantages, such as high efficiency and easy handling. 1-hydroxyethylidene-1,1-diphosphonic acid (HEDP), a typical organic phosphonic acid, is a low toxic corrosion inhibitor for steel and iron in neutral aerobic environment. This compound was first used as scale inhibitor in water treatment industry, such as cooling water circulation system. The molecule of HEDP has two phosphate groups, making it a powerful chelating ability with metallic ions. However, most of the current studies of HEDP focus on neutral or near-neutral systems, and there are few reports on the corrosion inhibition of steel reinforcement in alkaline environment. Therefore, it is not clear whether HEDP can play the role of corrosion inhibitor by protecting the passive film and resist foreign corrosive Cl-. In this work, the inhibition effect of HEDP towards 20SiMn steel was investigated in simulated concrete pore solution contaminated by Cl- (Sat.Ca(OH)2+1 mol/L NaCl) by electrochemical methods (corrosion potential, potentiodynamic polarization curves, EIS and Mott-Schottcky curves) and surface analysis techniques (SEM, XPS). The results showed that HEDP was a mixed inhibitor and its inhibition efficiency increased first and then decreased with the increase of concentration, the optimal concentration is 1.441×10-4 mol/L . At the optimal concentration, HEDP could obviously enlarge the passive region, prolong the passive period of 20SiMn steel from 6 h to 9 h , and improve the charge-transfer resistance significantly with the inhibition efficiency around 46.45%~59.78%. When pitting corrosion occurs, HEDP could hinder its development with the inhibition efficiency over 93%. The inhibition mechanism was the preferential adsorption of HEDP over Cl- by forming a complete adsorption film outside the passive film of the steel.

参考文献

[1] Biezma M V, San Cristóbal J R. Methodology to study cost of corrosion [J]. Corros. Eng. Sci. Technol., 2005, 40: 344
[2] Page C L, Treadaway K W J. Aspects of the electrochemistry of steel in concrete [J]. Nature, 1982, 297: 109
[3] Jones S, Martys N, Lu Y, et al. Simulation studies of methods to delay corrosion and increase service life for cracked concrete exposed to chlorides [J]. Cem. Concr. Compos., 2015, 58: 59
[4] Cao F T, Wei J, Dong J H, et al. Corrosion behavior of 20SiMn steel rebar in carbonate/bicarnonate solutions with the same pH value [J]. Acta Metall. Sin., 2014, 50: 674
[4] 曹凤婷, 魏 洁, 董俊华等. 20SiMn钢在恒定pH值的碳酸盐溶液中的腐蚀行为 [J]. 金属学报, 2014, 50: 674
[5] Andrade C, Page C L. Pore solution chemistry and corrosion in hydrated cement systems containing chloride salts: A study of cation specific effects [J]. Br. Corros. J., 1986, 21: 49
[6] Pourbaix M. Some applications of potential-pH diagrams to the study of localized corrosion [J]. J. Electrochem. Soc., 1976, 123: C25
[7] Abd El Haleem S M, El Wanees S A, Bahgat A. Environmental factors affecting the corrosion behaviour of reinforcing steel. VI. Benzotriazole and its derivatives as corrosion inhibitors of steel [J]. Corros. Sci., 2014, 87: 321
[8] Zhou X, Yang H Y, Wang F H. Investigation on the inhibition behavior of a pentaerythritol glycoside for carbon steel in 3.5% NaCl saturated Ca(OH)2 solution [J]. Corros. Sci., 2012, 54: 193
[9] Felh?si I, Keresztes Z, Kármán F H, et al. Effects of bivalent cations on corrosion inhibition of steel by 1-hydroxyethane-1,1-diphosphonic acid [J]. J. Electrochem. Soc., 1999, 146: 961
[10] Kármán F H, Felh?si I, Kálman E, et al. The role of oxide layer formation during corrosion inhibition of mild steel in neutral aqueous media [J]. Electrochim. Acta, 1998, 43: 69
[11] Akrout H, Bousselmi L, Maximovitch S, et al. Adsorption of corrosion inhibitors (SA, HEDP) using EQCM: Chloride effect and synergic behavior [J]. J. Mater. Sci., 2012, 47: 8085
[12] Awad H S, Turgoose S. Role of complexes in inhibition of mild steel by zinc-1-hydroxyethylidene-1, 1-diphosphonic acid mixtures [J]. Br. Corros. J., 2002, 37: 147
[13] Kolodyńska D. Cu(II), Zn(II), Ni(II), and Cd(II) complexes with HEDP removal from industrial effluents on different ion exchangers [J]. Ind. Eng. Chem. Res., 2010, 49: 2388
[14] Wang Z L, Yang Y X, Zhang J B, et al. A study on electroplating of zinc nickel alloy with HEDP plating bath [J]. Russ. J. Electrochem., 2006, 42: 22
[15] Lacour S, Daeluchat V, Bollinger J C, et al. Influence of carbonate and calcium ions on the phosphonate complexation with Cu, Zn, Cd and Ni in fresh waters: An evaluation of thermodynamic constants and a chemical model [J]. Environ. Technol., 1999, 20: 249
[16] Pu S M, Chen M Y, Chen Y Q, et al. Zirconium ions integrated in 1-hydroxyethylidene-1,1-diphosphonic acid (HEDP) as a metalorganic-like complex coating on biodegradable magnesium for corrosion control [J]. Corros. Sci., 2018, 144: 277
[17] Sekine I, Hirakawa Y. Effect of 1-hydroxyethylidene-1, 1-diphosphonic acid on the corrosion of SS 41 steel in 0.3% sodium chloride solution [J]. Corrosion, 1986, 42: 272
[18] Mohammedi D, Benmoussa A, Fiaud C, et al. Synergistic or additive corrosion inhibition of mild steel by a mixture of HEDP and metasilicate at pH 7 and 11 [J]. Mater. Corros., 2004, 55: 837
[19] Awad H S. The effect of zinc-to-HEDP molar ratio on the effectiveness of zinc-1, hydroxyethylidene-1, 1 diphosphonic acid in inhibiting corrosion of carbon steel in neutral solutions [J]. Anti-Corros. Method Mater., 2005, 52: 22
[20] Wei J. Research on improving the corrosion resistance of hot-rolled rebar by chemical cooling process [D]. Shenyang: Institute of Metal Research, Chinese Academy of Science, 2009
[20] 魏 洁. 化学冷却工艺提高热轧螺纹钢耐蚀性的研究 [D]. 沈阳: 中国科学院金属研究所, 2009
[21] Burstein G T, Liu C, Souto R M, et al. Origins of pitting corrosion [J]. Corros. Eng. Sci. Technol., 2004, 39: 25
[22] Kimura M, Kihira H, Ohta N, et al. Control of Fe(O,OH)6 nano-network structures of rust for high atmospheric-corrosion resistance [J]. Corros. Sci., 2005, 47: 2499
[23] Olefjord I, Brox B, Jelvestam U. Surface composition of stainless steels during anodic dissolution and passivation studied by ESCA [J]. J. Electrochem. Soc., 1985, 132: 2854
[24] Wang Y, Jiang S L, Zheng Y G, et al. Electrochemical behaviour of Fe-based metallic glasses in acidic and neutral solutions [J]. Corros. Sci., 2012, 63: 159
[25] Lu Y F. Corrosion behavior of 3Ni0.3Cu low alloy steel in simulated deep groundwater environments [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2015
[25] 卢云飞. 3Ni0.3Cu低合金钢在深层地下水模拟溶液中的腐蚀行为 [D]. 沈阳: 中国科学院金属研究所, 2015
[26] Morrison S R. Electrochemistry at Semiconductor and Oxidized Metal Electrodes [M]. New York: Plenum Press, 1980: 316
[27] MacDonald D D, Urquidi‐MacDonald M. Theory of steady‐state passive films [J]. J. Electrochem. Soc., 1990, 137: 2395
[28] Cao F T, Wei J, Dong J H, et al. The corrosion inhibition effect of phytic acid on 20SiMn steel in saturated Ca(OH)2 solution with 1 mol·L-1 NaCl [J]. Corros. Eng. Sci. Technol., 2018, 53: 283
[29] Cui X F, Li Q F, Li Y, et al. Microstructure and corrosion resistance of phytic acid conversion coatings for magnesium alloy [J]. Appl. Surf. Sci., 2008, 255: 2098
[30] Oku M, Hirokawa K. X-ray photoelectron spectroscopy of Co3O4, Fe3O4, Mn3O4, and related compounds [J]. J. Electron. Spectrosc. Relat. Phenom., 1976, 8: 475
[31] Tan B J, Sherwood P M A, Klabunde K J. XPS studies of gold films prepared from nonaqueous gold colloids [J]. Langmuir, 1990, 6: 106
[32] Allen G C, Hallam K R. Characterisation of the spinels MxCo1-xFe2O4 (M=Mn, Fe or Ni) using X-ray photoelectron spectroscopy [J]. Appl. Surf. Sci., 1996, 93: 25
[33] Marcus P, Grimal J M. The anodic dissolution and passivation of Ni-Cr-Fe alloys studied by ESCA [J]. Corros. Sci., 1992, 33: 805
[34] Hanawa T, Ota M. Calcium phosphate naturally formed on titanium in electrolyte solution [J]. Biomaterials, 1991, 12: 767
[35] Pearson R G. Acids and bases [J]. Science, 1966, 151: 172
[36] Dong J H, Song G L, Lin H C, et al. The adsoption of thiourea and its derivatives on iron electrode in acidic solution [J]. Acta Phys. Chim. Sin., 1996, 12: 34
[36] 董俊华, 宋光玲, 林海潮等. 酸性介质中硫脲及衍生物在纯铁上的吸附作用 [J]. 物理化学学报, 1996, 12: 34
文章导航

/