激光沉积薄壁结构热力演化的尺寸效应
收稿日期: 2019-09-25
修回日期: 2019-11-26
网络出版日期: 2019-12-19
基金资助
国家自然科学基金项目(51975387);国家重点研发计划项目(2016YFB1100504);沈阳航空航天大学航空制造工艺数字化国防重点学科实验室开放基金项目(SHSYS2015006)
Dimensional Effect on Thermo-Mechanical Evolution of Laser Depositing Thin-Walled Structure
Received date: 2019-09-25
Revised date: 2019-11-26
Online published: 2019-12-19
Supported by
National Natural Science Foundation of China(51975387);National Key Research and Development Program of China(2016YFB1100504);Open Foundation of Key Lab of Fundamental Science for National Defense of Aeronautical Digital Manufacturing Process of Shenyang Aerospace University(SHSYS2015006)
为研究激光沉积TC4单道薄壁结构热力演化的尺寸效应,采用有限元仿真和实验相结合的方法,分析了薄壁结构长度对温度、应力和基板变形的影响,并通过热电偶测温、基板残余变形验证了模型的可靠性。结果表明,熔池温度随层数循环递增,停光瞬间,试件最高温度急速下降,最低温度以抛物线形式持续上升。长度增加,对熔池极值温度影响不大,但会导致冷却曲线曲率变小,稳定降温速率加快,温度梯度变大。沉积过程中首层应力最大,随层数增加,应力递减,冷却过程中又逐步回升。长度增加,导致首层应力增大,沉积过程中低应力区和冷却过程中高应力区均围绕在薄壁结构附近,其范围扩大,但数值未见增大。沉积过程中基板会产生方向和大小不断变化的纵向翘曲变形,冷却后固定为朝向光源。长度增加,翘曲会更加明显。冷却过程中,基板变形比温度和应力更早达到平衡。
王霞 , 王维 , 杨光 , 王超 , 任宇航 . 激光沉积薄壁结构热力演化的尺寸效应[J]. 金属学报, 2020 , 56(5) : 745 -752 . DOI: 10.11900/0412.1961.2019.00317
To accurately predict and effectively control temperatures, stresses and distortions are key problems existing in laser deposition manufacturing technology. The mechanism of thermo-mechanical evolution during the metal depositing process is not yet clear. In order to study the dimensional effect on thermo-mechanical evolution when TC4 single-pass and thin-walled structures are manufactured by laser deposition, finite element simulations and experiments are combined to explore the influence of the structures' length on temperature, stress and distortion of the substrates. The model reliability is validated by thermocouple temperatures and the residual deformations of substrates. The results show that the temperatures of molten pools increase periodically according to the depositing layers. As soon as the laser is terminated, the maximum temperatures of builds decline at high speed, but the minimum temperatures continue to rise in the form of parabola. When the lengths of thin-walled structures increase, the thermal extremes of molten pools are not affected, but the curvatures of cooling curves diminish, the steady cooling rates accelerate, meanwhile the temperature gradients increase. The initial stresses when depositing the first layer are maximum during manufacturing, the stresses decline progressively with the increasing layer numbers, but recover during cooling. While the lengths expand, stresses of the first layer increase. At the same time both low stress regions during depositing and high stress areas during cooling are enlarged which are around the depositing structures, but the lengths of thin-walled structures appear to have a minimal impact on the stress magnitudes. During deposition, the out-of-plane distortions of the substrates oscillate up and down, after cooling the directions of deformations are fixed towards the light source. The out-of-plane distortions are more obvious as the lengths increase. During cooling the substrates' deformations reach equilibrium earlier than temperatures and stresses.
| 1 | Lu X F, Lin X, Chiumenti M, et al. Finite element analysis and experimental validation of the thermomechanical behavior in laser solid forming of Ti-6Al-4V [J]. Addit. Manuf., 2018, 21: 30 |
| 2 | Heigel J C, Michaleris P, Reutzel E W. Thermo-mechanical model development and validation of directed energy deposition additive manufacturing of Ti-6Al-4V [J]. Addit. Manuf., 2015, 5: 9 |
| 3 | Denlinger E R, Heigel J C, Michaleris P, et al. Effect of inter-layer dwell time on distortion and residual stress in additive manufacturing of titanium and nickel alloys [J]. J. Mater. Process. Technol., 2015, 215: 123 |
| 4 | Chiumenti M, Lin X, Cervera M, et al. Numerical simulation and experimental calibration of additive manufacturing by blown powder technology. Part I: Thermal analysis [J]. Rapid Prototyp. J., 2017, 23: 448 |
| 5 | Lindgren L E, Lundb?ck A. Approaches in computational welding mechanics applied to additive manufacturing: Review and outlook [J]. Compt. Rend. Méc., 2018, 346: 1033 |
| 6 | Fallah V, Alimardani M, Corbin S F, et al. Temporal development of melt-pool morphology and clad geometry in laser powder deposition [J]. Comput. Mater. Sci., 2011, 50: 2124 |
| 7 | Parry L, Ashcroft I A, Wildman R D. Understanding the effect of laser scan strategy on residual stress in selective laser melting through thermo-mechanical simulation [J]. Addit. Manuf., 2016, 12: 1 |
| 8 | ?zcan A, Kollmannsberger S, Jomo J, et al. Residual stresses in metal deposition modeling: Discretizations of higher order [J]. Comput. Math. Appl., 2019, 78: 2247 |
| 9 | Mukherjee T, Zhang W, DebRoy T. An improved prediction of residual stresses and distortion in additive manufacturing [J]. Comput. Mater. Sci., 2017, 126: 360 |
| 10 | Shi L K, Gao S Y, Xi M Z, et al. Finite element simulation for laser direct depositing processes of metallic vertical thin wall Parts I. The simulation for temperature field during depositing processes [J]. Acta Metall. Sin., 2006, 42: 449 |
| 10 | 石力开, 高士友, 席明哲等. 金属直薄壁件激光直接沉积过程的有限元模拟 I. 沉积过程中温度场的模拟 [J]. 金属学报, 2006, 42: 449 |
| 11 | Shi L K, Gao S Y, Xi M Z, et al. Finite element simulation for laser direct depositing processes of metallic vertical thin wall Parts II. The simulation for thermal stress field during depositing processes [J]. Acta Metall. Sin., 2006, 42: 454 |
| 11 | 石力开, 高士友, 席明哲等. 金属直薄壁件激光直接沉积过程的有限元模拟 Ⅱ. 沉积过程中热应力场的模拟 [J]. 金属学报, 2006, 42: 454 |
| 12 | Shi L K, Gao S Y, Xi M Z, et al. Finite element simulation for laser direct depositing processes of metallic vertical thin wall Parts III. The analysis for distortion during depositing processes [J]. Acta Metall. Sin., 2006, 42: 459 |
| 12 | 石力开, 高士友, 席明哲等. 金属直薄壁件激光直接沉积过程的有限元模拟 III. 沉积过程中变形的分析 [J]. 金属学报, 2006, 42: 459 |
| 13 | Gao S Y, Xian S Y, Ji H Z, et al. The analysis on the distortion of subatrate during laser direct depositing processes [J]. J. Plast. Eng., 2007, 14(5): 57 |
| 13 | 高士友, 咸士玉, 纪宏志等. 激光直接沉积过程中基板变形分析 [J]. 塑性工程学报, 2007, 14(5): 57 |
| 14 | Ma L, Huang W D, Yu J, et al. Parametric finite element model of temperature/stress field evolution by metal laser solid forming [J]. Chin. J. Lasers, 2009, 36: 3226 |
| 14 | 马 良, 黄卫东, 于 君等. 金属激光立体成形热应力场参数化有限元模型 [J]. 中国激光, 2009, 36: 3226 |
| 15 | Thompson S M, Bian L K, Shamsaei N, et al. An overview of direct laser deposition for additive manufacturing; Part I: Transport phenomena, modeling and diagnostics [J]. Addit. Manuf., 2015, 8: 36 |
| 16 | Shamsaei N, Yadollahi A, Bian L K, et al. An overview of direct laser deposition for additive manufacturing; Part II: Mechanical behavior, process parameter optimization and control [J]. Addit. Manuf., 2015, 8: 12 |
| 17 | Yang Q C, Zhang P, Cheng L, et al. Finite element modeling and validation of thermomechanical behavior of Ti-6Al-4V in directed energy deposition additive manufacturing [J]. Addit. Manuf., 2016, 12: 169 |
| 18 | Zhang Y, Zhang J. Finite element simulation and experimental validation of distortion and cracking failure phenomena in direct metal laser sintering fabricated component [J]. Addit. Manuf., 2017, 16: 49 |
| 19 | Lu X F, Lin X, Chiumenti M, et al. In situ measurements and thermo-mechanical simulation of Ti-6Al-4V laser solid forming processes [J]. Int. J. Mech. Sci., 2019, 153-154: 119 |
| 20 | Lu X F, Lin X, Chiumenti M, et al. Residual stress and distortion of rectangular and S-shaped Ti-6Al-4V parts by directed energy deposition: Modelling and experimental calibration [J]. Addit. Manuf., 2019, 26: 166 |
| 21 | Ren K, Chew Y, Fuh J Y H, et al. Thermo-mechanical analyses for optimized path planning in laser aided additive manufacturing processes [J]. Mater. Des., 2019, 162: 80 |
| 22 | Ahn J, He E, Chen L, et al. Prediction and measurement of residual stresses and distortions in fibre laser welded Ti-6Al-4V considering phase transformation [J]. Mater. Des., 2017, 115: 441 |
| 23 | Song J, Chew Y X, Bi G J, et al. Numerical and experimental study of laser aided additive manufacturing for melt-pool profile and grain orientation analysis [J]. Mater. Des., 2018, 137: 286 |
| 24 | Bartlett J L, Croom B P, Burdick J, et al. Revealing mechanisms of residual stress development in additive manufacturing via digital image correlation [J]. Addit. Manuf., 2018, 22: 1 |
| 25 | Chen Z, Ye H, Xu H Y. Distortion control in a wire-fed electron-beam thin-walled Ti-6Al-4V freeform [J]. J. Mater. Process. Technol., 2018, 258: 286 |
/
| 〈 |
|
〉 |