一般大气环境下锈蚀结构钢表面特征与随机模型
收稿日期: 2019-05-20
修回日期: 2019-11-16
网络出版日期: 2019-12-10
基金资助
国家自然科学基金项目(51908455);中国博士后科学基金项目(2019M653572);陕西省教育厅科研计划项目(19JS042)
Surface Characteristics and Stochastic Model of Corroded Structural Steel Under General Atmospheric Environment
Received date: 2019-05-20
Revised date: 2019-11-16
Online published: 2019-12-10
Supported by
National Natural Science Foundation of China(51908455);China Postdoctoral Science Foundation(2019M653572);Scientific Research Project of Shaanxi Provincial Department of Education(19JS042)
对处于大气腐蚀环境中的结构钢开展了6批次人工加速腐蚀实验和为期8 a的自然暴露实验,利用表面形貌测试方法和腐蚀表征参数自编分析程序对锈蚀结构钢表面特征参数及演变规律进行研究,明确锈蚀深度、锈坑深度、锈坑径深比分布特征,揭示其均值、方差等统计参数及锈坑形状的变化规律。研究表明,一般大气环境下结构钢锈蚀深度服从正态分布,锈坑深度与径深比服从对数正态分布;随着腐蚀程度的增大,锈蚀深度均值、标准差与功率谱密度峰值以及锈坑深度对数均值均逐渐增大,锈坑径深比对数均值逐渐减小;锈坑形状由圆柱或半球体逐渐向圆锥体转变。最后基于锈蚀深度参数和锈坑参数统计分析结果,考虑各表征参数的变化规律与内在联系,建立了锈蚀深度随机场模型与锈坑随机分布模型,实现了一般大气环境锈蚀钢材表面特征的准确模拟与重建。
王友德 , 徐善华 , 李晗 , 张海江 . 一般大气环境下锈蚀结构钢表面特征与随机模型[J]. 金属学报, 2020 , 56(2) : 148 -160 . DOI: 10.11900/0412.1961.2019.00156
Steel structures exposed to corrosive atmospheres for a long time are highly susceptible to corrosion damage. The safety assessments of existing corroded steel structures rely heavily on the quantification of corrosion itself. In order to study the corrosion characteristics of structural steel in general atmospheric environment, 6 batches of artificial accelerated corrosion experiments and 8 a of natural exposure experiments were carried out. The surface characteristic parameters and evolution rules of corroded structural steel were studied by the surface morphology tests and self-programmed morphology analysis program. The distribution characteristics of corrosion depth, pit depth and aspect ratio were clarified, and the changing laws of statistical parameters (such as mean value and standard deviation) and pitting shapes were revealed. The results indicated that the corrosion depth of structural steel in general atmospheric environment obeyed the normal distribution, and the pit depth and aspect ratio obeyed the lognormal distribution. With the increase of corrosion degree, the mean value and standard deviation of corrosion depth, the peak value of power spectrum density of corrosion depth, and the logarithmic mean value of pit depth gradually increased, and the logarithmic mean value of pit aspect ratio decreased. Meanwhile, the shape of pits was gradually changed from a cylinder or hemisphere to a cone. Finally, based on the statistical analysis results of corrosion depth parameters and pit parameters, and taking the variation laws and internal relationships of characterization parameters into consideration, the stochastic field model of corrosion depth and the random distribution model of corrosion pits were established, which achieved the accurate simulation and reconstruction of surface characteristics of corroded steel under general atmospheric environment.
| [1] | Leech T. The collapse of the Kinzua viaduct: A combination of design oversight and material fatigue left a century-old railroad bridge vulnerable to an F-1 tornado [J]. Am. Sci., 2005, 93: 348 |
| [2] | Witcher T R. From disaster to prevention: The silver bridge [J]. Civ. Eng. Mag. Arch., 2017, 87: 44 |
| [3] | Albrecht P, Hall T T. Atmospheric corrosion resistance of structural steels [J]. J. Mater. Civil. Eng., 2003, 15: 2 |
| [4] | Ye D, Zhao D W, Li J, et al. Study on the effects of air pollution on corrosion of carbon steel [J]. J. Chongqing Architect. Univ., 2005, 27: 80 |
| [4] | (叶 堤, 赵大为, 李 娟等. 大气污染对碳钢的腐蚀影响研究 [J]. 重庆建筑大学学报, 2005, 27: 80) |
| [5] | Ye D, Zhao D W, Chen G C, et al. Study on the effects of air pollution on corrosion of metals in inland area [J]. Equip. Environ. Eng., 2006, 3(1): 37 |
| [5] | (叶 堤, 赵大为, 陈刚才等. 非海洋地区大气污染对金属材料的腐蚀影响研究 [J]. 装备环境工程, 2006, 3(1): 37) |
| [6] | Yang X Z, Yang W. Electrochemical Thermodynamics of Metal Corrosion: Potential-PH Diagram and its Application [M]. Beijing: Chemical Industry Press, 1991: 123 |
| [6] | (杨熙珍, 杨 武. 金属腐蚀电化学热力学: 电位—PH图及其应用 [M]. 北京: 化学工业出版社, 1991: 123) |
| [7] | Wang Y K, Wharton J A, Shenoi R A. Ultimate strength analysis of aged steel-plated structures exposed to marine corrosion damage: A review [J]. Corros. Sci., 2014, 86: 42 |
| [8] | Southwell C R, Bultman J D, Hummer C W. Seawater Corrosion Handbook [M]. New Jersey: Noyes Data Corporation, 1979: 87 |
| [9] | Garbatov Y, Guedes S C, Wang G. Nonlinear time dependent corrosion wastage of deck plates of ballast and cargo tanks of tankers [J]. J. Offshore Mech. Arct. Eng., 2007, 129: 48 |
| [10] | Melchers R E. Corrosion uncertainty modelling for steel structures [J]. J. Constr. Steel. Res., 1999, 52: 3 |
| [11] | Hui Y L, Lin Z S, Li R. Experimental study and analysis on the property of corroded rebar [J]. Ind. Constr., 1997, 27(6): 10 |
| [11] | (惠云玲, 林志伸, 李 荣. 锈蚀钢筋性能试验研究分析 [J]. 工业建筑, 1997, 27(6): 10) |
| [12] | Reiser D B, Alkire R C. The measurement of shape change during early stages of corrosion pit growth [J]. Corros. Sci., 1984, 24: 579 |
| [13] | Pidaparti R M, Patel R R. Correlation between corrosion pits and stresses in Al alloys [J]. Mater. Lett., 2008, 62: 4497 |
| [14] | Luo L H, Huang Y H, Weng S, et al. Mechanism-related modelling of pit evaluation in the CrNiMoV steel in simulated environment of low pressure nuclear steam turbine [J]. Mater. Des., 2016, 105: 240 |
| [15] | Horner D A, Connolly B J, Zhou S, et al. Novel images of the evolution of stress corrosion cracks from corrosion pits [J]. Corros. Sci., 2011, 53: 3466 |
| [16] | Wang Y F, Cheng G X. Quantitative evaluation of pit sizes for high strength steel: Electrochemical noise, 3-D measurement, and image-recognition-based statistical analysis [J]. Mater. Des., 2016, 94: 176 |
| [17] | Tang F J, Lin Z B, Chen G D, et al. Three-dimensional corrosion pit measurement and statistical mechanical degradation analysis of deformed steel bars subjected to accelerated corrosion [J]. Constr. Build. Mater., 2014, 70: 104 |
| [18] | Holme B, Lunder O. Characterisation of pitting corrosion by white light interferometry [J]. Corros. Sci., 2007, 49: 391 |
| [19] | Xu S H, Qiu B. Experimental study on fatigue behavior of corroded steel [J]. Mater. Sci. Eng., 2013, A584: 163 |
| [20] | Xu S H, Wang Y D. Estimating the effects of corrosion pits on the fatigue life of steel plate based on the 3D profile [J]. Int. J. Fatigue, 2015, 72: 27 |
| [21] | Mu X, Wei J, Dong J H, et al. Electrochemical study on corrosion behaviors of mild steel in a simulated tidal zone [J]. Acta Metall. Sin., 2012, 48: 420 |
| [21] | (穆 鑫, 魏 洁, 董俊华等. 低碳钢在模拟海洋潮差区的腐蚀行为的电化学研究 [J]. 金属学报, 2012, 48: 420) |
| [22] | Chen L. Study on the deterioration properties of corroded steel [D]. Xi'an: Xi'an University of Architecture and Technology, 2010 |
| [22] | (陈 露. 腐蚀后钢材材料性能退化研究 [D]. 西安: 西安建筑科技大学, 2010) |
| [23] | Melchers R E. Pitting corrosion of mild steel in marine immersion environment—Part 1: Maximum pit depth [J]. Corrosion, 2004, 60: 824 |
| [24] | Melchers R E. Pitting corrosion of mild steel in marine immersion environment—Part 2: Variability of maximum pit depth [J]. Corrosion, 2004, 60: 937 |
| [25] | Wang Y W. Ultimate strength of ship structures with corrosion wastage [D]. Shanghai: Shanghai Jiao Tong University, 2008 |
| [25] | (王燕舞. 考虑腐蚀影响船舶结构极限强度研究 [D]. 上海: 上海交通大学, 2008) |
| [26] | Wang Y W, Huang X P, Cui W C. Pitting corrosion model of mild and low-alloy steel in marine environment—Part 1: Maximum pit depth [J]. J. Ship Mech., 2007, 11: 577 |
| [26] | (王燕舞, 黄小平, 崔维成. 船舶结构钢海洋环境点蚀模型研究之一: 最大点蚀深度时变模型 [J]. 船舶力学, 2007, 11: 577) |
| [27] | Silva J E, Garbatov Y, Guedes S C. Ultimate strength assessment of rectangular steel plates subjected to a random localized corrosion degradation [J]. Eng. Struct., 2013, 52: 295 |
| [28] | Melchers R E, Ahammed M, Jeffrey R, et al. Statistical characterization of surfaces of corroded steel plates [J]. Mar. Struct., 2010, 23: 274 |
| [29] | Teixeira ? P, Soares C G. Ultimate strength of plates with random fields of corrosion [J]. Struct. Infrastruct. Eng., 2008, 4: 363 |
| [30] | Rahbar-Ranji A. Ultimate strength of corroded steel plates with irregular surfaces under in-plane compression [J]. Ocean Eng., 2012, 54: 261 |
| [31] | Qiu B. The study on surface characteristics and eccentric compressive load-capacity of corroded H-shape steel members at neutral salt fog environment [D]. Xi'an: Xi'an University of Architecture and Technology, 2014 |
| [31] | (邱 斌. 中性盐雾环境下锈蚀H型钢表面特征及偏压承载性能研究 [D]. 西安: 西安建筑科技大学, 2014) |
| [32] | Wang R H, Ajit Shenoi R, Sobey A. Ultimate strength assessment of plated steel structures with random pitting corrosion damage [J]. J. Const. Steel Res., 2018, 143: 331 |
| [33] | Kong Z Y. Study on the degradation of fatigue properties for corrosion steel specimens by test [D]. Xi'an: Xi'an University of Architecture and Technology, 2010 |
| [33] | (孔正义. 腐蚀钢构件疲劳性能退化试验研究 [D]. 西安: 西安建筑科技大学, 2010) |
| [34] | Shang Y. Study on the corrosive environment influences on the characteristics of the steel-structure surface [D]. Xi'an: Xi'an University of Architecture and Technology, 2011 |
| [34] | (商 钰. 腐蚀环境对钢结构表面锈蚀特征影响的研究 [D]. 西安: 西安建筑科技大学, 2011) |
| [35] | Xu S H, Wang Y D, Xue Q F. Evaluation indicators and extraction method for pitting corrosion of structural steel [J]. J. Harbin Inst. Technol., 2015, 22: 15 |
| [36] | Wang Y D, Xu S H, Wang H, et al. Predicting the residual strength and deformability of corroded steel plate based on the corrosion morphology [J]. Constr. Build. Mater., 2017, 152: 777 |
| [37] | Nakai T, Matsushita H, Yamamoto N, et al. Effect of pitting corrosion on local strength of hold frames of bulk carriers (1st report) [J]. Mar. Struct., 2004, 17: 403 |
| [38] | Kainuma S, Jeong Y S, Ahn J H. Investigation on the stress concentration effect at the corroded surface achieved by atmospheric exposure test [J]. Mater. Sci. Eng., 2014, A602: 89 |
| [39] | Li C G. Characterization of 3D surface micro-topography by 2D power spectrum [J]. Acta Metrol. Sin., 2004, 25: 11 |
| [39] | (李成贵. 三维表面微观形貌的二维功率谱表征 [J]. 计量学报, 2004, 25: 11) |
| [40] | Liang S X, Sun W L, Li J. Simulation of multi-dimensional random fields by stochastic harmonic functions [J]. J. Tongji Univ. (Nat. Sci.), 2012, 40: 965 |
| [40] | (梁诗雪, 孙伟玲, 李 杰. 随机场的随机谐和函数表达 [J]. 同济大学学报(自然科学版), 2012, 40: 965) |
| [41] | Zhou X Y, Ke W. The optimal probability distribution function of pits and its evolution under cyclic loading [J]. J. Chin. Soc. Corros. Prot., 1992, 12: 227 |
| [41] | (周向阳, 柯 伟. 点蚀坑参数的最佳分布形式及其在交变载荷下的演化 [J]. 中国腐蚀与防护学报, 1992, 12: 227) |
| [42] | Aziz P M. Application of the statistical theory of extreme values to the analysis of maximum pit depth data for aluminum [J]. Corrosion, 1956, 12: 35 |
| [43] | Shinozuka M, Deodatis G. Simulation of multi-dimensional Gaussian stochastic fields by spectral representation [J]. Appl. Mech. Rev., 1996, 49: 29 |
/
| 〈 |
|
〉 |