研究了Gd含量(3.0%、4.5%、6.0%,质量分数)对定向凝固Mg-xGd-0.5Y合金微观组织及室温力学性能的影响,并利用EBSD技术分析其室温拉伸形变行为。结果表明,在抽拉速率为3 mm/min条件下,Mg-xGd-0.5Y合金获得了纵向晶界与热流方向平行、主要沿(
孙衡 , 林小娉 , 周兵 , 赵圣诗 , 唐琴 , 董允 . 定向凝固Mg-xGd-0.5Y合金的微观组织及拉伸变形行为[J]. 金属学报, 2020 , 56(3) : 340 -350 . DOI: 10.11900/0412.1961.2019.00229
The poor plastic deformation ability of magnesium alloy, resulted from its close-packed hexagonal structure and only two independent basal <a> slip systems at room temperature that cannot meet the von Mises criterion, has extremely restricted its application. As the α-Mg dendrites grow along with the heat flow in directional solidification, the uniform columnar crystal structures obtained in Mg can effectively improve its mechanical properties. And the mechanical properties of the anisotropic magnesium alloys were heavily affected by the orientation controlled by the directional solidification parameters. In this work, the effects of Gd content (3.0%, 4.5%, 6.0%, mass fraction) on the microstructure and mechanical properties of directionally solidified Mg-xGd-0.5Y alloy were investigated. The tensile deformation behavior at room temperature was analyzed by EBSD technique. The results showed that the Mg-xGd-0.5Y alloys have a longitudinal grain boundary parallel to the heat flow direction and a preferential growth along the normal direction of the (
| [1] | Liu C M, Ji R F, Zhou H T, et al. Research and development progress of damping capacity of magnesium and magnesium alloys [J]. Chin. J. Nonferrous Met., 2005, 15: 1319 |
| [1] | 刘楚明, 纪仁峰, 周海涛等. 镁及镁合金阻尼特性的研究进展 [J]. 中国有色金属学报, 2005, 15: 1319 |
| [2] | Wan D Q, Wang J C, Yang G C. A study of the effect of Y on the mechanical properties, damping properties of high damping Mg-0.6%Zr based alloys [J]. Mater. Sci. Eng., 2009, A517: 114 |
| [3] | Wang J F, Gao S, Pan F S, et al. Influence of process technology on mechanical and damping properties of ZK60 magnesium alloys [J]. Chin. J. Nonferrous Met., 2009, 19: 821 |
| [3] | 王敬丰, 高 珊, 潘复生等. 加工工艺对ZK60镁合金力学性能和阻尼性能的影响 [J]. 中国有色金属学报, 2009, 19: 821 |
| [4] | Kocks U F, Chandra H. Slip geometry in partially constrained deformation [J]. Acta Metall., 1982, 30: 695 |
| [5] | Hu Y K, Li Q S, Li J W, et al. Research on structure of Mg-3Zn-Y alloy and mechanical property under directional solidification [J]. Heavy Cast. Forg., 2017, (6): 6 |
| [5] | 胡延昆, 李秋书, 李建文等. 定向凝固下Mg-3Zn-Y合金组织和力学性能研究 [J]. 大型铸锻件, 2017, (6): 6 |
| [6] | Mabuchi M, Kobata M, Chino Y, et al. Tensile properties of directionally solidified AZ91 Mg alloy [J]. Mater. Trans., 2003, 44: 436 |
| [7] | Liu S J, Yang G Y, Jie W Q. Microstructure, microsegregation, and mechanical properties of directional solidified Mg-3.0Nd-1.5Gd alloy [J]. Acta Metall. Sin. (Engl. Lett)., 2014, 27: 1134 |
| [8] | Lin X P, Zhao T B, Dong Y, et al. Room-temperature tensile properties of a directionally solidified magnesium alloy and its deformation mechanism dominated by contraction twin and double twin [J]. Mater. Sci. Eng., 2017, A700: 681 |
| [9] | Molodov K D, Al-Samman T, Molodov D A, et al. On the ductility of magnesium single crystals at ambient temperature [J]. Metall. Mater. Trans., 2014, 45A:3275 |
| [10] | Yang H. Mechanical property and twinning behavior of Mg and Mg-Sn alloy single crystal in directional solidification [D]. Chongqing: Chongqing University, 2016 |
| [10] | 杨 鸿. 定向凝固下镁及镁锡合金单晶的力学性能和孪生行为研究 [D]. 重庆: 重庆大学, 2016 |
| [11] | Pettersen K, Lohne O, Ryum N. Dendritic solidification of magnesium alloy AZ91 [J]. Metall. Trans., 1990, 21A: 221 |
| [12] | Du J L, Guo Z P, Zhang A, et al. Correlation between crystallographic anisotropy and dendritic orientation selection of binary magnesium alloys [J]. Sci. Rep., 2017, 7: 13600 |
| [13] | Shuai S S, Guo E Y, Wang M Y, et al. Anomalous α-Mg dendrite growth during directional solidification of a Mg-Zn alloy [J]. Metall. Mater. Trans., 2016, 47A: 4368 |
| [14] | Yang M, Xiong S M, Guo Z. Effect of different solute additions on dendrite morphology and orientation selection in cast binary magnesium alloys [J]. Acta Mater., 2016, 112: 261 |
| [15] | Wang M Y, Xu Y J, Jing T, et al. Growth orientations and morphologies of α-Mg dendrites in Mg-Zn alloys [J]. Scr. Mater., 2012, 67: 629 |
| [16] | Li J L, Wu D, Chen R S, et al. Anomalous effects of strain rate on the room-temperature ductility of a cast Mg-Gd-Y-Zr alloy [J]. Acta Mater., 2018, 159: 31 |
| [17] | Zhang G S, Zhang Z M, Li X B, et al. Effects of repetitive upsetting-extrusion parameters on microstructure and texture evolution of Mg-Gd-Y-Zn-Zr alloy [J]. J. Alloys Compd., 2019, 790: 48 |
| [18] | Liu S J. Researches on the solidification characteristic and mechanical properties of Mg-Zn-Gd-based magnesium alloy [D]. Xi'an: Northwestern Polytechnical University, 2016 |
| [18] | 刘少军. Mg-Zn-Gd系镁合金的凝固特性及其力学性能研究 [D]. 西安: 西北工业大学, 2016 |
| [19] | Zheng W, Wang G C, Wu T. Establishment of constitutive equation of material in region affected by grain boundary and numerical simulation of micro-bulk-forming [J]. J. Mech. Eng., 2011, 47(22): 31 |
| [19] | 郑 伟, 王广春, 吴 涛. 微体积成形晶界影响区域材料本构方程的构建及有限元模拟 [J]. 机械工程学报, 2011, 47(22): 31 |
| [20] | He J J, Mao Y, Lu S L, et al. Texture optimization on Mg sheets by preparing soft orientations of extension twinning for rolling [J]. Mater. Sci. Eng., 2019, A760: 174 |
| [21] | Wang Y C. Study on the anisotropy of mechanical behavior and deformation mechanisms of AZ31 Mg alloys by numerical simulation [D]. Shenyang: Northeastern University, 2014 |
| [21] | 王运程. AZ31镁合金各向异性力学行为及微观形变机制的模拟研究 [D]. 沈阳: 东北大学, 2014 |
| [22] | Cao X H. Monte carlo method of simulation grain growth [D]. Shanghai: East China University of Science and Technology, 2014 |
| [22] | 曹小虎. 晶粒生长的蒙特卡洛模拟方法研究 [D]. 上海: 华东理工大学, 2014 |
| [23] | Yu H H. Research on the relationship between boundary character and strengthening in Mg alloys [D]. Chongqing: Chongqing University, 2018 |
| [23] | 余辉辉. 镁合金中界面特征与细晶强化的关系研究 [D]. 重庆: 重庆大学, 2018 |
| [24] | Wang J, Beyerlein I J, Tomé C N. An atomic and probabilistic perspective on twin nucleation in Mg [J]. Scr. Mater., 2010, 63: 741 |
| [25] | Wang Z Q, Chapuis A, Liu Q. Simulation of mechanical behavior of AZ31 magnesium alloy during twin-dominated large plastic deformation [J]. Trans. Nonferrous Met. Soc. China, 2015, 25: 3595 |
/
| 〈 |
|
〉 |