Q&P钢热处理过程有限元法数值模拟模型研究
收稿日期: 2019-03-26
修回日期: 2019-09-16
网络出版日期: 2019-10-23
基金资助
国家科技支撑计划项目(No.2011BAE13B05);国家自然科学基金项目(No.51075031)
Modelling of Q&P Steel Heat Treatment Process Based on Finite Element Method
Received date: 2019-03-26
Revised date: 2019-09-16
Online published: 2019-10-23
Supported by
National Science and Technology Support Project(No.2011BAE13B05);National Natural Science Foundation of China(No.51075031)
以国内典型淬火-分配(Q&P)高强钢——QP980钢为例,进行热处理全过程物理模拟研究,提出一种耦合温度及时间影响的类蠕变应变方程用以描述材料在Q&P热处理分配过程的体积变化,建立考虑淬火温度影响的Q&P热处理两次淬火过程相变动力学方程、相变应变及相变塑性方程,获得了Q&P钢各相的热膨胀系数。根据温度场、组织场、应力场三场耦合原理,基于物理模拟得到的弹塑性增量本构模型,对商业有限元软件ABAQUS用户子程序进行二次开发,建立了针对Q&P热处理全过程的三场耦合数值仿真模型;通过Gleeble热-力模拟试验机上的Q&P热处理实验对模型进行了实验验证,实验结果与数值模拟结果吻合良好。
张清东 , 林潇 , 刘吉阳 , 胡树山 . Q&P钢热处理过程有限元法数值模拟模型研究[J]. 金属学报, 2019 , 55(12) : 1569 -1580 . DOI: 10.11900/0412.1961.2019.00082
Quenching and partitioning (Q&P) steel is a kind of high strength and toughness steels which has a majority of martensite at room temperature and a certain amount of retained austenite through the quenching and carbon distribution heat treatment process of cold-rolled carbon-silicon-manganese steel. In this work, the typical Q&P high-strength steel, QP980 steel, is taken as an example to carry out the physical simulation study of the whole process of heat treatment. A creep-like strain equation coupled with temperature and time is proposed to describe the volume change of materials during Q&P heat treatment. The phase transformation kinetics equation, phase transformation strain and phase transformation plasticity equation of Q&P heat treatment with the influence of quenching temperature were established, and the thermal expansion coefficient of each phase of Q&P steel was obtained. According to the coupling principles of temperature, microstructure and stress-strain field, a numerical simulation model for the whole process of Q&P heat treatment was developed. In this model, the physical simulation of QP980 steel thermal-elastoplastic incremental constitutive equations are implemented to commercial finite element software ABAQUS as the user subroutines. The model was validated by Q&P heat treatment experiment on Gleeble thermal-mechanical simulator. The calculated values of the models are both in good agreement with the experimental values.
Key words: Q&P steel; heat treatment; numerical simulation; experimental research
| [1] | Speer J G, Edmonds D V, Rizzo F C, et al. Partitioning of carbon from supersaturated plates of ferrite, with application to steel processing and fundamentals of the bainite transformation [J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 219 |
| [2] | Speer J G, Assun??o F C R, Matlock D K, et al. The "quenching and partitioning" process: Background and recent progress [J]. Mater. Res., 2005, 8: 417 |
| [3] | Xu Z Y. New Processes for Steel Heat Treatment [J]. Heat Treatment, 2007(01): 1 |
| [3] | (徐祖耀.钢热处理的新工艺 [J]. 热处理, 2007(01): 1) |
| [4] | Khan S A, Bhadeshia H K D. Kinetics of Martensitic transformation in partially bainitic 300M steel [J]. Mater. Sci. Eng., 1990, A129: 257 |
| [5] | Bhadeshia H K D H. Carbon content of retained austenite in quenched steels [J]. Met. Sci., 1983, 17: 151 |
| [6] | Yamanaka S, Sakanoue T, Yoshii T, et al. Influence of transformation plasticity on the distortion of carburized quenching process of Cr-Mo steel ring [J]. J. Soc. Mater. Sci. Jpn., 1999, 48: 733 |
| [7] | Ju D Y, Narazaki M. Simulation and experimental verification of residual stress and distortion during quenching of steel [A]. Proceeding of the 20th ASM Heat Treating Society Conference [C]. St. Louis, MO, USA: ASM International, 2000: 441 |
| [8] | Arimoto K, Horino T, Ikuta F, et al. Explanation of the origin of distortion and residual stress in water quenched cylinders using computer simulation [J]. J. ASTM Int., 2006, 3: 253 |
| [9] | Inoue T, Yamaguchi T, Wang Z G. Stresses and phase transformations occurring in quenching of carburized steel gear wheel [J]. Mater. Sci. Technol., 1984, 1: 872 |
| [10] | Mukai R, Ju D Y. Simulation of carburizing-quenching of a gear. Effect of carbon content on residual stresses and distortion [J]. J. Phys. IV France, 2004, 120: 489 |
| [11] | Imatani S, Okuno Y, Inoue T. Experiment and simulation for thick-plate bending by high frequency inductor [J]. Acta Metall. Sin. (Engl. Lett.), 1998, 11: 449 |
| [12] | Inoue T, Arimoto K, Ju D Y. Development of heat treatment simulation program "HEARTS"—Theory, strategy, function and some examples [A]. Residual Stresses III: Science and Technology [C], London and New York: Elsevier Applied Science,1992, 1: 226 |
| [13] | Inoue T, Arimoto K. Development and implementation of CAE system “HEARTS” for heat treatment simulation based on metallo-thermo-mechanics [J]. J. Mater. Eng. Perform, 1997, 6: 51 |
| [14] | Ju D Y, Inoue T. On the material process simulation code COSMAP-simulated examples and its experimental verification for heat treatment process [J]. Key Eng. Mater., 2007, 345-346: 955 |
| [15] | Inoue T, Tanaka T, Ju D Y, et al. Transformation plasticity and the effect on quenching process simulation [J]. Key Eng. Mater., 2007, 345-346: 915 |
| [16] | Inoue T. On phenomenological mechanism of transformation plasticity and inelastic behavior of a steel subjected to varying temperature and stress- application of unified transformation-thermo plasticity theory [J]. J. Soc. Mater. Sci. Jpn., 2008, 57: 225 |
| [17] | Inoue T. Phenomenological mechanism of transformation plasticity and the constitutive law coupled with thermo-mechanical plasticity [J]. Adv. Mater. Res., 2008, 33-37: 1351 |
| [18] | Inoue T. Transformation plasticity-the mechanism and some applications [J]. Mater. Sci. Forum, 2009, 614: 11 |
| [19] | Inoue T. Mechanism of transformation plasticity and the unified constitutive equation for transformation-thermo-mechanical plasticity with some applications [J]. Int. J. Microstruct. Mater. Prop., 2010, 5: 319 |
| [20] | Inoue T. Mechanics and characteristics of transformation plasticity and metallo-thermo-mechanical process simulation [J]. Proc. Eng., 2011, 10: 3793 |
| [21] | Inoue T. Macro-, meso-, and nanoscopic metallo thermo mechanics [J]. J. Phys. IV France, 2004, 120: 3 |
| [22] | Denis S. Considering stress-phase transformation interactions in the calculation of heat treatment residual stresses [J]. J. Phys. IV France, 1996, 6: C1-159 |
| [23] | Denis S, Archambault P, Aubry C, et al. Modelling of phase transformation kinetics in steels and coupling with heat treatment residual stress predictions [J]. J. Phys. IV France, 1999, 9: Pr9-323 |
| [24] | Lee S J, Lee Y K. Finite element simulation of quench distortion in a low-alloy steel incorporating transformation kinetics [J]. Acta Mater., 2008, 56: 1482 |
| [25] | Leblond J B, Devaux J, Devaux J C. Mathematical modelling of transformation plasticity in steels I: Case of ideal-plastic phases [J]. Int. J. Plast., 1989, 5: 551 |
| [26] | Leblond J B, Devaux J. A new kinetic model for anisothermal metallurgical transformations in steels including effect of austenite grain size [J]. Acta Metall., 1984, 32: 137 |
| [27] | Liu Y, Qin S W, Hao Q G, et al. Finite element simulation and experimental verification of internal stress of quenched AISI 4140 cylinders [J]. Metall. Mater. Trans., 2017, 48A: 1 |
| [28] | De Oliveira W P, Savi M A, Pacheco P M C L. Finite element method applied to the quenching of steel cylinders using a multi-phase constitutive model [J]. Arch. Appl. Mech., 2013, 83: 1013 |
| [29] | De Oliveira W P, Savi M A, Pacheco P M C L, et al. Thermomechanical analysis of steel cylinders quenching using a constitutive model with diffusional and non-diffusional phase transformations [J]. Mech. Mater., 2010, 42: 31 |
| [30] | Carlone P, Palazzo G S, Pasquino R. Finite element analysis of the steel quenching process: Temperature field and solid-solid phase change [J]. Comput. Math. Appl., 2010, 59: 585 |
| [31] | Smoljan B. Prediction of mechanical properties and microstructure distribution of quenched and tempered steel shaft [J]. J. Mater. Process. Technol., 2006, 175: 393 |
| [32] | Bok H H, Choi J W, Suh D W, et al. Stress development and shape change during press-hardening process using phase-transformation-based finite element analysis [J]. Int. J. Plast., 2015, 73: 142 |
| [33] | Song G S, Liu X H, Wang G D, et al. Numerical Simulation on Carburizing and Quenching of Gear Ring [J]. J. Iron Steel Res., 2007, 14: 47 |
| [34] | Chen B, Peng X H, Nong S N, et al. An incremental constitutive relationship incorporating phase transformation with the application to stress analysis for the quenching process [J]. J. Mater. Process. Technol., 2002, 122: 208 |
| [35] | Han Q L, Liu G Q, Dong L, et al. FEM simulation of quenching process for dissimilar material welded using steel and titanium alloy [J]. Trans. Mater. Heat Treat., 2007, 28(4): 139 |
| [35] | (韩庆礼, 刘国权, 董 雷等. 异种材料淬火过程的有限元模拟 [J]. 材料热处理学报, 2007, 28(4): 139) |
| [36] | Ginzburg V B, translated by Jiang M D, Wang G Z. High-Quality Steel Rolling [M]. Beijing: Metallurgical Industry Press, 2000: 1 |
| [36] | (金兹伯格 V B著, 姜明东, 王国栋译. 高精度板带材轧制理论与实践 [M]. 北京: 冶金工业出版社, 2000: 1) |
| [37] | Coret M, Combescure A. A mesomodel for the numerical simulation of the multiphasic behavior of materials under anisothermal loading (application to two low-carbon steels) [J]. Int. J. Mech. Sci., 2002, 44: 1947 |
| [38] | Jiang Y, Zeng P, Lou L L. Numerical simulation of quenching process of steel 26Cr2Ni4MoV with thermo-mechano-metallurgical coupling [J]. J. Harbin Inst. Technol., 2002, 34: 302 |
| [38] | (蒋 昱, 曾 攀, 娄路亮. 26Cr2Ni4MoV钢淬火过程的三场耦合数值模拟 [J]. 哈尔滨工业大学学报, 2002, 34: 302) |
| [39] | Koistinen D P, Marburger R E. A general equation prescribing the extent of the austenite-martensite transformation in pure iron-carbon alloys and plain carbon steels [J]. Acta Metall., 1959, 7: 59 |
| [40] | Videau J C, Cailletaud G, Pineau A. Experimental study of the transformation-induced plasticity in a Cr-Ni-Mo-Al-Ti steel [J]. J. Phys. IV France, 1996, 6: C1-465 |
| [41] | Coret M, Calloch S, Combescure A. Experimental study of the phase transformation plasticity of 16MND5 low carbon steel induced by proportional and nonproportional biaxial loading paths [J]. Eur. J. Mech., 2004, 23: 823 |
| [42] | Greenwood G W, Johnson R H. The deformation of metals under small stresses during phase transformations [J]. Proc. Royal Soc. London, 1965, 283A: 403 |
| [43] | Atkins E. Elements of X-ray Diffraction [J]. Phys. Today, 1978, 10: 50 |
| [44] | Sun C Y, Zeng P, Lei L P, et al. Experimental extract of transformation plastic strain during phase transformation [J]. J. Plast. Eng., 2007, 14(6): 161 |
| [44] | (孙朝阳, 曾 攀, 雷丽萍等. 基于物理模拟的相变塑性应变分离方法 [J]. 塑性工程学报, 2007, 14(6): 161) |
| [45] | Liu Z. Numerical simulation of heat treatment process [M]. Beijing: Science Press, 1996: 119 |
| [45] | (刘 庄. 热处理过程的数值模拟 [M]. 北京: 科学出版社, 1996: 119) |
| [46] | Xu X J, Chen G X, Liu C C, et al. Numerical simulation of the stresses evolution during tempering of steel [J]. Heat Treat.Met., 1997, (3): 12 |
| [46] | (许学军, 陈国学, 刘春成等. 钢的回火过程中应力演化的数值模拟 [J]. 金属热处理, 1997, (3): 12) |
| [47] | Wang M M. Study on tempering of Mn-Mo-Ni steel for large forgings of nuclear power [D]. Shanghai: Shanghai Jiao Tong University, 2013 |
| [47] | (王明敏. 核电大锻件用Mn-Mo-Ni钢的回火研究 [D]. 上海: 上海交通大学, 2013) |
| [48] | Liu G Y, Li M W, Zhang S J. Thermal numerical simulation and experiment in quenching process of medium and heavy plate [J]. J. Iron Steel Res., 2007, 19(8): 51 |
| [48] | (刘国勇, 李谋渭, 张少军. 中厚板淬火过程的热力学数值模拟及实验 [J]. 钢铁研究学报, 2007, 19(8): 51) |
| [49] | Fang G, Zeng P. Finite element simulation of metal quenching [J]. Tsinghua Sci. Technol., 2004, 9: 555 |
/
| 〈 |
|
〉 |