选区激光熔化316L不锈钢的拉伸性能
收稿日期: 2019-08-19
修回日期: 2019-09-04
网络出版日期: 2019-09-25
基金资助
国家磁约束核聚变能发展研究专项项目(2014GB117000)
Tensile Properties of Selective Laser Melted 316L Stainless Steel
Received date: 2019-08-19
Revised date: 2019-09-04
Online published: 2019-09-25
Supported by
National Magnetic Confinement Fusion Science Program of China(2014GB117000)
对选区激光熔化(selective laser melting,SLM) 316L不锈钢的拉伸性能及断裂机制进行了研究,并对拉伸断裂后的试样进行显微组织表征与分析,探究了拉伸变形过程中微观组织的演化规律。结果表明:采用选区激光熔化技术制备的316L不锈钢具有较好的强塑性匹配,其中晶粒内部纳米尺度胞状结构有助于强度的提升;其拉伸性能明显优于传统手段制备的316L不锈钢。选区激光熔化316L不锈钢在拉伸过程中奥氏体晶粒内部产生形变孪晶,并且形变孪晶的出现存在取向相关,在取向接近<001>的晶粒中不易出现,而在取向接近<110>-<111>的晶粒中较易出现。
余晨帆 , 赵聪聪 , 张哲峰 , 刘伟 . 选区激光熔化316L不锈钢的拉伸性能[J]. 金属学报, 2020 , 56(5) : 683 -692 . DOI: 10.11900/0412.1961.2019.00278
Selective laser melting (SLM), as the most common additive manufacturing (AM) method, is capable of manufacturing metallic components with complex shape layer by layer. Compared with conventional manufacturing technologies such as casting or forging, the SLM technology has the advantages of high degree accuracy, high material utilization rate and environmentally friendly, and has attracted great attention in the fields of aerospace, nuclear power and medicine. The 316L austenitic stainless steel is widely used in the industrial field because of the excellent corrosion resistance and plasticity. It is also one of the commonly used material systems for SLM. In this work, the tensile properties and fracture mechanism of 316L stainless steel fabricated via SLM technology were investigated. The microstructure of the SLMed 316L specimens after tensile fracture was characterized and analyzed. The results show that the SLMed 316L stainless steel has a relatively desirable combination of strength and ductility, and its tensile performance is obviously better than that of 316L stainless steel prepared by traditional methods. The nanometer-scale cell structure inside the grain contributes to the improvement of strength. Deformation twins were observed in the SLMed 316L stainless steel after tensile test. The appearance of twins is oriented-dependent, and it is easy to occur in the grain with the direction near <110>-<111>.
| 1 | Xu W, Lui E W, Pateras A, et al. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance [J]. Acta Mater., 2017, 125: 390 |
| 2 | Gao P, Wei K W, Yu H C, et al. Influence of layer thickness on microstructure and mechanical properties of selective laser melted Ti-5Al-2.5Sn alloy [J]. Acta Metall. Sin., 2018, 54: 999 |
| 2 | 高 飘, 魏恺文, 喻寒琛等. 分层厚度对选区激光熔化成形Ti-5Al-2.5Sn合金组织与性能的影响规律 [J]. 金属学报, 2018, 54: 999 |
| 3 | Zhang W Q, Zhu H H, Hu Z H, et al. Study on the selective laser melting of AlSi10Mg [J]. Acta Metall. Sin., 2017, 53: 918 |
| 3 | 张文奇, 朱海红, 胡志恒等. AlSi10Mg的激光选区熔化成形研究 [J]. 金属学报, 2017, 53: 918 |
| 4 | Tomus D, Rometsch P A, Heilmaier M, et al. Effect of minor alloying elements on crack-formation characteristics of Hastelloy-X manufactured by selective laser melting [J]. Addit. Manuf., 2017, 16: 65 |
| 5 | Zhang Y J, Wang H B, Song X Y, et al. Preparation and performance of spherical Ni powder for SLM processing [J]. Acta Metall. Sin., 2018, 54: 1833 |
| 5 | 张亚娟, 王海滨, 宋晓艳等. SLM球形Ni粉的制备与打印工艺性能 [J]. 金属学报, 2018, 54: 1833 |
| 6 | Zhou X, Li K L, Zhang D D, et al. Textures formed in a CoCrMo alloy by selective laser melting [J]. J. Alloys Compd., 2015, 631: 153 |
| 7 | Wang D Z, Yu C F, Ma J, et al. Densification and crack suppression in selective laser melting of pure molybdenum [J]. Mater. Des., 2017, 129: 44 |
| 8 | Zhou X, Liu X H, Zhang D D, et al. Balling phenomena in selective laser melted tungsten [J]. J. Mater. Process. Technol., 2015, 222: 33 |
| 9 | Krakhmalev P, Yadroitsava I, Fredriksson G, et al. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels [J]. Mater. Des., 2015, 87: 380 |
| 10 | Sun Y, Hebert R J, Aindow M. Non-metallic inclusions in 17-4PH stainless steel parts produced by selective laser melting [J]. Mater. Des., 2018, 140: 153 |
| 11 | Lai C L, Tsay L W, Chen C. Effect of microstructure on hydrogen embrittlement of various stainless steels [J]. Mater. Sci. Eng., 2013, A584: 14 |
| 12 | Guo S, Han E H, Wang H T, et al. Life prediction for stress corrosion behavior of 316L stainless steel elbow of nuclear power plant [J]. Acta Metall. Sin., 2017, 53: 455 |
| 12 | 郭 舒, 韩恩厚, 王海涛等. 核电站316L不锈钢弯头应力腐蚀行为的寿命预测 [J]. 金属学报, 2017, 53: 455 |
| 13 | Casati R, Lemke J, Vedani M. Microstructure and fracture behavior of 316L austenitic stainless steel produced by selective laser melting [J]. J. Mater. Sci. Technol., 2016, 32: 738 |
| 14 | Kong D C, Dong C F, Ni X Q, et al. Mechanical properties and corrosion behavior of selective laser melted 316L stainless steel after different heat treatment processes [J]. J. Mater. Sci. Technol., 2019, 35: 1499 |
| 15 | Scipioni Bertoli U, MacDonald B E, Schoenung J M. Stability of cellular microstructure in laser powder bed fusion of 316L stainless steel [J]. Mater. Sci. Eng., 2019, A739: 109 |
| 16 | Shamsujjoha M, Agnew S R, Fitz-Gerald J M, et al. High strength and ductility of additively manufactured 316L stainless steel explained [J]. Metall. Mater. Trans., 2018, 49A: 3011 |
| 17 | Suryawanshi J, Prashanth K G, Ramamurty U. Mechanical behavior of selective laser melted 316L stainless steel [J]. Mater. Sci. Eng., 2017, A696: 113 |
| 18 | Salman O O, Gammer C, Chaubey A K, et al. Effect of heat treatment on microstructure and mechanical properties of 316L steel synthesized by selective laser melting [J]. Mater. Sci. Eng., 2019, A748: 205 |
| 19 | Niendorf T, Leuders S, Riemer A, et al. Highly anisotropic steel processed by selective laser melting [J]. Metall. Mater. Trans., 2013, 44B: 794 |
| 20 | Liu L F, Ding Q Q, Zhong Y, et al. Dislocation network in additive manufactured steel breaks strength-ductility trade-off [J]. Mater. Today, 2018, 21: 354 |
| 21 | Mullins W W, Sekerka R F. Stability of a planar interface during solidification of a dilute binary alloy [J]. J. Appl. Phys., 1964, 35: 444 |
| 22 | Yao T Z, Xu T H, Wang D H. Effects of yield ratio rising on use security of pipeline steel [J]. Mater. Mech. Eng., 2012, 36(8): 62 |
| 22 | 姚婷珍, 许天旱. 王党会. 屈强比升高对管线钢使用安全性的影响 [J]. 机械工程材料, 2012, 36(8): 62 |
| 23 | Lu L, Li Z B, Bi Z Y, et al. Relationship between tension toughness and fracture toughness of low alloy steel [J]. J. Iron Steel Res., 2014, 26(6): 67 |
| 23 | 芦 琳, 李周波, 毕宗岳等. 低碳低合金钢的静力韧度与断裂韧度 [J]. 钢铁研究学报, 2014, 26(6): 67 |
| 24 | Gu D D, Chen H Y. Selective laser melting of high strength and toughness stainless steel parts: The roles of laser hatch style and part placement strategy [J]. Mater. Sci. Eng., 2018, A725: 419 |
| 25 | Roland T, Retraint D, Lu K, et al. Enhanced mechanical behavior of a nanocrystallised stainless steel and its thermal stability [J]. Mater. Sci. Eng., 2007, A445-446: 281 |
| 26 | Brass A M, Chêne J. Hydrogen uptake in 316L stainless steel: Consequences on the tensile properties [J]. Corros. Sci., 2006, 48: 3222 |
| 27 | Chen X H, Lu J, Lu L, et al. Tensile properties of a nanocrystalline 316L austenitic stainless steel [J]. Scr. Mater., 2005, 52: 1039 |
| 28 | Hong S G, Lee S B. The tensile and low-cycle fatigue behavior of cold worked 316L stainless steel: Influence of dynamic strain aging [J]. Int. J. Fatigue, 2004, 26: 899 |
| 29 | Maloy S A, James M R, Willcutt G, et al. The mechanical properties of 316L/304L stainless steels, Alloy 718 and Mod 9Cr-1Mo after irradiation in a spallation environment [J]. J. Nucl. Mater., 2001, 296: 119 |
| 30 | Panda S S, Singh V, Upadhyaya A, et al. Sintering response of austenitic (316L) and ferritic (434L) stainless steel consolidated in conventional and microwave furnaces [J]. Scr. Mater., 2006, 54: 2179 |
| 31 | Stinville J C, Cormier J, Templier C, et al. Monotonic mechanical properties of plasma nitrided 316L polycrystalline austenitic stainless steel: Mechanical behaviour of the nitrided layer and impact of nitriding residual stresses [J]. Mater. Sci. Eng., 2014, A605: 51 |
| 32 | Zhang M, Sun C N, Zhang X, et al. Fatigue and fracture behaviour of laser powder bed fusion stainless steel 316L: Influence of processing parameters [J]. Mater. Sci. Eng., 2017, A703: 251 |
| 33 | Matthews M J, Guss G, Khairallah S A, et al. Denudation of metal powder layers in laser powder bed fusion processes [J]. Acta Mater., 2016, 114: 33 |
| 34 | Khairallah S A, Anderson A T, Rubenchik A, et al. Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones [J]. Acta Mater., 2016, 108: 36 |
| 35 | Qiu C L, Panwisawas C, Ward M, et al. On the role of melt flow into the surface structure and porosity development during selective laser melting [J]. Acta Mater., 2015, 96: 72 |
| 36 | Gutierrez-Urrutia I, Zaefferer S, Raabe D. The effect of grain size and grain orientation on deformation twinning in a Fe-22 wt.% Mn-0.6 wt.% C TWIP steel [J]. Mater. Sci. Eng., 2010, A527: 3552 |
| 37 | Sun S J, Tian Y Z, Lin H R, et al. Transition of twinning behavior in CoCrFeMnNi high entropy alloy with grain refinement [J]. Mater. Sci. Eng., 2018, A712: 603 |
| 38 | Li D D, Qian L H, Liu S, et al. Effect of manganese content on tensile deformation behavior of Fe-Mn-C TWIP steels [J]. Acta Metall. Sin., 2018, 54: 1777 |
| 38 | 李冬冬, 钱立和, 刘 帅等. Mn含量对Fe-Mn-C孪生诱发塑性钢拉伸变形行为的影响 [J]. 金属学报, 2018, 54: 1777 |
| 39 | de Campos M F, Loureiro S A, Rodrigues D, et al. Estimative of the stacking fault energy for a FeNi(50/50) alloy and a 316L stainless steel [J]. Mater. Sci. Forum, 2008, 591-593: 3 |
| 40 | Wang Y M, Voisin T, McKeown J T, et al. Additively manufactured hierarchical stainless steels with high strength and ductility [J]. Nat. Mater., 2018, 17: 63 |
/
| 〈 |
|
〉 |