综述

(9~12)%Cr马氏体耐热钢中微量B元素的择优分布行为及其对微观组织与力学性能的影响

  • 杨柯 ,
  • 梁烨 ,
  • 严伟 ,
  • 单以银
展开
  • 1. 中国科学院金属研究所  沈阳 110016
    2. 中国科学技术大学材料科学与工程学院  沈阳 110016
    3. 中国科学院金属研究所中国科学院核用材料与安全评价重点实验室  沈阳 110016
杨 柯,男,1961年生,研究员

收稿日期: 2019-05-06

  修回日期: 2019-07-29

  网络出版日期: 2019-08-27

基金资助

国家重点研发计划项目(2017YFB0305201);国家自然科学基金项目(51971226)

Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels

  • Ke YANG ,
  • Ye LIANG ,
  • Wei YAN ,
  • Yiyin SHAN
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
    3. Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China

Received date: 2019-05-06

  Revised date: 2019-07-29

  Online published: 2019-08-27

Supported by

National Key Research and Development Program of China(2017YFB0305201);National Natural Science Foundation of China(51971226)

摘要

(9~12)%Cr钢中添加微量B元素可显著抑制M23C6碳化物的熟化,从而提高蠕变强度,增加蠕变断裂寿命。钢中B元素的择优分布行为是其充分发挥积极作用的关键,也是深入研究其作用机理的前提,一直是(9~12)%Cr马氏体耐热钢领域的研究热点。本文简述了B元素对钢力学性能的影响,介绍了表征钢中微量B元素分布的常用实验手段。在阐述B元素在钢中的物理冶金学原理以及固溶与扩散机制的基础上,重点讨论了B元素在(9~12)%Cr马氏体耐热钢中的择优分布行为及其影响因素。最后对目前微量B元素抑制马氏体耐热钢中M23C6碳化物熟化的2种机理进行了梳理,系统地阐述了B元素的择优分布行为与其抑制M23C6碳化物熟化、提高蠕变性能的积极作用之间的关系,深化对B元素在(9~12)%Cr马氏体耐热钢中的作用机理的认识。

本文引用格式

杨柯 , 梁烨 , 严伟 , 单以银 . (9~12)%Cr马氏体耐热钢中微量B元素的择优分布行为及其对微观组织与力学性能的影响[J]. 金属学报, 2020 , 56(1) : 53 -65 . DOI: 10.11900/0412.1961.2019.00146

Abstract

Addition of small amount of boron (B) in the (9~12)%Cr martensitic heat resistant steels can obviously prohibit the Ostwald ripening of M23C6 carbides so as to improve creep strength as well as creep rupture life. With the purpose of taking full advantages of B element, it is critical to make B preferentially distribute in (9~12)%Cr martensitic heat resistant steels. The mechanism of B preventing M23C6 carbides from ripening is also on the premise of clearly identifying the preferential distribution of B in the steels. Much concern has been growing over the preferential distribution of B in the research of (9~12)%Cr martensitic heat resistant steels. Therefore, this article gives a review on this aspect. Following a summary of the effect of B on mechanical properties, several commonly used characterizing methods for B segregation in the steels are introduced. Based on the physical metallurgy and the solution, diffusion mechanisms of B element, discussions on the preferential distribution of B element at prior austenite grain boundaries and in the M23C6 carbides as well as the related factors are emphasized. At last, two prevalent mechanisms of B restraining the coarsening of M23C6 carbides in (9~12)%Cr martensitic heat resistant steels are given by an intensive explanation so that the relationship between the preferential distribution of B and its advantage of increasing creep performance by suppressing the ripening M23C6 carbides are systematically elaborated, which gives a deep understanding of the role of B element in (9~12)%Cr martensitic heat resistant steels.

参考文献

[1] Liu Z D, Cheng S C, Bao H S, et al. Localization of boiler steel technology in China used for ultra super critical power plants [J]. Iron Steel, 2009, 44(6): 1
[1] (刘正东, 程世长, 包汉生等. 超超临界火电机组用锅炉钢技术国产化问题 [J]. 钢铁, 2009, 44(6): 1)
[2] Li W W. Research on the mechanism design and evaluation method of power coal supply chain's coordination under uncertainty conditions [D]. Harbin: Harbin Institute of Technology, 2016
[2] (李巍巍. 不确定条件下电煤供应链协调的机制设计及评价方法研究 [D]. 哈尔滨: 哈尔滨工业大学, 2016)
[3] Shu G G, Liu J N, Shi C Z, et al. Microstructure, Mechanical Properties and Engineering Application of T/P91 Heat Resistant Steel for Supercritical Power Plants [M]. Xi'an: Shanxi Science and Technology Press, 2006: 9
[3] (束国刚, 刘江南, 石崇哲等. 超临界锅炉用T/P91钢的组织性能与工程应用 [M]. 西安: 陕西科学技术出版社, 2006: 9)
[4] Msuyama F. History of power plants and progress in heat resistant steels [J]. ISIJ Int., 2001, 41: 612
[5] Maruyama K, Sawada K, Koike J I. Strengthening mechanisms of creep resistant tempered martensitic steel [J]. ISIJ Int., 2001, 41: 641
[6] Abe F. Research and development of heat-resistant materials for advanced USC power plants with steam temperatures of 700 ℃ and above [J]. Engineering, 2015, 1: 211
[7] Yan P, Liu Z D, Bao H S, et al. Effect of normalizing temperature on the strength of 9Cr-3W-3Co martensitic heat resistant steel [J]. Mater. Sci. Eng., 2014, A597: 148
[8] Liu F, Fors D H R, Golpayegani A, et al. Effect of boron on carbide coarsening at 873 K (600 ℃) in 9 to 12 pct chromium steels [J]. Metall. Mater. Trans., 2012, 43A: 4053
[9] Abe F. Behavior of boron in 9Cr heat resistant steel during heat treatment and creep deformation [J]. Key Eng. Mater., 2007, 345-346: 569
[10] Abe F. Precipitate design for creep strengthening of 9%Cr tempered martensitic steel for ultra-supercritical power plants [J]. Sci. Technol. Adv. Mater., 2008, 9: 013002
[11] Abe F. Effect of boron on microstructure and creep strength of advanced ferritic power plant steels [J]. Procedia Eng., 2011, 10: 94
[12] Titova T I, Shulgan N A, Malykhina I Y. Effect of boron microalloying on the structure and hardenability of building steel [J]. Met. Sci. Heat Treat., 2007, 49: 39
[13] Grange R A, Garvey T M. Factors affecting the hardenability of boron-treated steels [J]. Trans. Am. Soc. Met., 1946, 37: 136
[14] Maitrepierre P, Thivellier D, Tricot R. Influence of boron on the decomposition of austenite in low carbon alloyed steels [J]. Metall. Mater. Trans., 1975, 6A: 287
[15] Hwang B, Suh D W, Kim S J. Austenitizing temperature and hardenability of low-carbon boron steels [J]. Scr. Mater., 2011, 64: 1118
[16] Karlsson L, Nordén H, Odelius H. Non-equilibrium grain boundary segregation of boron in austenitic stainless steel—I. Large scale segregation behaviour [J]. Acta Metall., 1988, 36: 1
[17] Asahi H. Effects of Mo addition and austenitizing temperature on hardenability of low alloy B-added steels [J]. ISIJ Int., 2002, 42: 1150
[18] Li X L. The segregations of boron and niobium at grain boundaries in microalloyed steel and high-purity nickel [D]. Beijing: University of Science and Technology Beijing, 2017
[18] (李向龙. 硼、铌元素在微合金钢与高纯镍中的晶界偏聚行为 [D]. 北京: 北京科技大学, 2017)
[19] Kapadia B M. Effect of boron additions on the toughness of heat-treated low-alloy steels [J]. J. Heat Treat., 1987, 5: 41
[20] Ghali S N, El-Faramawy H S, Eissa M M. Influence of boron additions on mechanical properties of carbon steel [J]. J. Miner. Mater. Charact. Eng., 2012, 11: 995
[21] Yan P, Liu Z D, Bao H S, et al. Effect of microstructural evolution on high-temperature strength of 9Cr-3W-3Co martensitic heat resistant steel under different aging conditions [J]. Mater. Sci. Eng., 2013, A588: 22
[22] Shirzadi A, Jackson S. Structural Alloys for Power Plants [M]. Cambridge: Woodhead Publishing, 2014: 250
[23] Golpayegani A, Liu F, Svensson H, et al. Microstructure of a creep-resistant 10 pct chromium steel containing 250 ppm boron [J]. Metall. Mater. Trans., 2011, 42A: 940
[24] H?ttestrand M, Andrén H O. Boron distribution in 9-12% chromium steels [J]. Mater. Sci. Eng., 1999, A270: 33
[25] Mayr P, Martín F M, Albu M, et al. Correlation of creep strength and microstructural evolution of a boron alloyed 9Cr3W3CoVNb steel in as-received and welded condition [J]. Mater. High Temp., 2010, 27: 67
[26] Horiuchi T, Igarashi M, Abe F. Improved utilization of added B in 9Cr heat-resistant steels containing W [J]. ISIJ Int., 2002, 42(Suppl.1) S67
[27] Mayr P, Holzer I, Mendez-Martin F, et al. Experience with 9Cr3W3CoVNbBN base material and crosswelds at 650 ℃ for implementation in USC power plants [A]. 3rd Symposium on Heat Resistant Steels and Alloys for High Efficiency USC Power Plants [C]. Tsukuba, Japan: National Institute for Materials Science, 2009: 1
[28] Albu M, Mayr P, Martín F M, et al. The influence of boron on the microstructure of a 9 wt% Cr ferritic steel [J]. Mater. High Temp., 2011, 28: 120
[29] Lejcek P. Grain Boundary Segregation in Metals [M]. Berlin: Springer-Verlag Berlin and Heidelberg, 2010: 27
[30] Shigesato G, Fujishiro T, Hara T. Grain boundary segregation behavior of boron in low-alloy steel [J]. Metall. Mater. Trans., 2014, 45A: 1876
[31] He X L, Chu Y Y, Zhang X L, et al. The distribution of boron in steel [J]. Acta Metall. Sin., 1979, 13: 235
[31] (贺信莱, 诸幼义, 张秀林等. 硼在钢中的分布 [J]. 金属学报, 1979, 13: 235)
[32] Jahazi M, Jonas J J. The non-equilibrium segregation of boron on original and moving austenite grain boundaries [J]. Mater. Sci. Eng., 2002, A335: 49
[33] Li W Q, Sun J Y, Xu H X, et al. Application of fission track etching method for study carburized boron steels [J]. Iron Steel, 1992, 27(6): 42
[33] (李文卿, 孙继跃, 许洪新等. 显微径迹照相技术在渗碳硼钢研究中的应用 [J]. 钢铁, 1992, 27(6): 42)
[34] Yin H T, Wang J. SIMS analysis technology and the applied research [J]. Chin. J. Spectrosc. Lab., 2008, 25: 180
[34] (尹会听, 王 洁. 二次离子质谱分析技术及应用研究 [J]. 光谱实验室, 2008, 25: 180)
[35] Li Y J, Ponge D, Choi P, et al. Atomic scale investigation of non-equilibrium segregation of boron in a quenched Mo-free martensitic steel [J]. Ultramicroscopy, 2015, 159: 240
[36] Yong Q L. Secondary Phases in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 167
[36] (雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 167)
[37] Li P S, Xiao L J, Xie Z. Thermodynamic analysis of AlN and BN competitive precipitation in low carbon steel [J]. J. Iron Steel Res., 2009, 21(5): 16
[37] (李培松, 肖丽俊, 谢 植. 低碳钢中AlN和BN竞相析出热力学分析 [J]. 钢铁研究学报, 2009, 21(5): 16)
[38] Klimenkov M, Materna-Morris E, M?slang A. Boron effect on the microstructure of 9%Cr ferritic-martensitic steels [J]. J. Nucl. Mater., 2015, 462: 280
[39] Busby P E, Wells C. Diffusion of boron in alpha iron [J]. JOM, 1954, 6(9): 972
[40] Wang W D, Zhang S H, He X L. Diffusion of boron in alloys [J]. Acta Metall. Mater., 1995, 43: 1693
[41] Hayashi Y, Sugeno T. Nature of boron in α-iron [J]. Acta Metall., 1970, 18: 693
[42] Fors D H R, Wahnstr?m G. Nature of boron solution and diffusion in α-iron [J]. Phys. Rev., 2008, 77B: 132102
[43] Bialon A F, Hammerschmidt T, Drautz R. Ab initio study of boron in α-iron: Migration barriers and interaction with point defects [J]. Phys. Rev., 2013, 87B: 104109
[44] McLellan R B, Ko C. The diffusion of boron in f.c.c. iron [J]. J. Phys. Chem. Solids, 1993, 54: 465
[45] Busby P E, Warga M E, Wells C. Diffusion and solubility of boron in iron and steel [J]. JOM, 1953, 5(11): 1463
[46] Zhang X, Li X L, Wu P, et al. First principles calculation of boron diffusion in fcc-Fe [J]. Curr. Appl. Phys., 2018, 18: 1108
[47] Takahashi J, Ishikawa K, Kawakami K, et al. Atomic-scale study on segregation behavior at austenite grain boundaries in boron- and molybdenum-added steels [J]. Acta Mater., 2017, 133: 41
[48] Hondros E D, Seah M R, Hofmann S, et al. Physical Metallurgy [M]. 4th Ed., Amsterdam: North-Holland, 1996: 1201
[49] Williams T M, Stoneham A M, Harries D R. The segregation of boron to grain boundaries in solution-treated Type 316 austenitic stainless steel [J]. Met. Sci., 1976, 10: 14
[50] Xu T D, Cheng B Y. Kinetics of non-equilibrium grain-boundary segregation [J]. Prog. Mater. Sci., 2004, 49: 109
[51] Li Y J, Ponge D, Choi P, et al. Segregation of boron at prior austenite grain boundaries in a quenched martensitic steel studied by atom probe tomography [J]. Scr. Mater., 2015, 96: 13
[52] Mun D J, Shin E J, Cho K C, et al. Cooling rate dependence of boron distribution in low carbon steel [J]. Metall. Mater. Trans., 2012, 43A: 1639
[53] Miyamoto G, Goto A, Takayama N, et al. Three-dimensional atom probe analysis of boron segregation at austenite grain boundary in a low carbon steel—Effects of boundary misorientation and quenching temperature [J]. Scr. Mater., 2018, 154: 168
[54] Zhu H Y, Sun J, Wang W, et al. Experimental investigation on segregation and remelting behaviors of boron-containing steel with low carbon [J]. Results Phys., 2019, 12: 67
[55] Chu Y Y, He X L, Tang L, et al. Two kinds of boron segregation at austenite grain boundaries [J]. Acta Metall. Sin., 1987, 23: 169
[55] (褚幼义, 贺信莱, 唐 立等. 硼在奥氏体晶界的两类偏聚 [J]. 金属学报, 1987, 23: 169)
[56] Aust K T, Hanneman R E, Niessen P, et al. Solute induced hardening near grain boundaries in zone refined metals [J]. Acta Metall., 1968, 16: 291
[57] Zhang S H, He X L, Chu Y Y, et al. Behaviour of boron segregation to grain boundaries in bcc Fe-3%Si alloy [J]. Acta Metall. Sin., 1993, 29(6): 1
[57] (章三红, 贺信莱, 褚幼义等. 硼在体心立方Fe-3%Si合金中的晶界偏聚行为 [J]. 金属学报, 1993, 29(6): 1)
[58] Brailsford A D, Bullough R. The rate theory of swelling due to void growth in irradiated metals [J]. J. Nucl. Mater., 1972, 44: 121
[59] Simpson C J, Aust K T, Winegard W C. The formation of Pb2Au precipitates at high velocity grain boundaries after quenching [J]. Metall. Mater. Trans., 1970, 1B: 1482
[60] Watanabe S, Ohtani H, Kunitake T. The Influence of hot rolling and heat treatments on the distribution of boron in steel [J]. Trans. Iron Steel Ins. Jpn., 1983, 23: 31
[61] Gay A S, Fraczkiewicz A, Biscondi M. Mechanisms of the intergranular segregation of boron in (B2) FeAl alloys [J]. Mater. Sci. Forum, 1999, 294-296: 453
[62] Xu T D. Non-equilibrium grain-boundary segregation kinetics [J]. J. Mater. Sci., 1987, 22: 337
[63] Wang H, Yan W, van Zwaag S, et al. On the 650 ℃ thermostability of 9-12Cr heat resistant steels containing different precipitates [J]. Acta Mater., 2017, 134: 143
[64] Hald J. Microstructure and long-term creep properties of 9-12% Cr steels [J]. Int J. Pressure Vessels Piping, 2008, 85: 30
[65] Umantsev A, Olson G B. Ostwald ripening in multicomponent alloys [J]. Scr. Metall. Mater., 1993, 29: 1135
[66] Abe F. Coarsening behavior of lath and its effect on creep rates in tempered martensitic 9Cr-W steels [J]. Mater. Sci. Eng., 2004, A387-389: 565
[67] Takahashi N, Fujita T, Yamada T. Effect of boron on long period creep rupture strength of 12%Cr heat resisting steel [J]. Tetsu Hagané, 1975, 61: 2263
[67] (高橋 紀雄, 藤田 利夫, 山田 武海. 12%Cr耐熱鋼の長時間クリープ破断強度におよぼすBの影響 [J]. 鉄と鋼, 1975, 61: 2263)
[68] H?ttestrand M, Schwind M, Andrén H O. Microanalysis of two creep resistant 9-12% chromium steels [J]. Mater. Sci. Eng., 1998, A250: 27
[69] Lundin L, F?llman S, Andrén H O. Microstructure and mechanical properties of a 10% chromium steel with improved creep resistance at 600 ℃ [J]. Mater. Sci. Technol., 1997, 13: 233
文章导航

/