双相钛合金高温变形协调性的CPFEM研究

  • 李学雄 ,
  • 徐东生 ,
  • 杨锐
展开
  • 1. 中国科学院金属研究所 沈阳 110016
    2. 中国科学院大学 北京 100049
李学雄,男,1987年生,博士生

收稿日期: 2018-08-17

  修回日期: 2019-03-11

  网络出版日期: 2019-04-25

基金资助

国家重点研发计划项目(No.2016YFB0701304);中国科学院信息化专项课题项目(No.XXH13506-3040);中国科学院战略先导科技专项项目(No.XDC01040100)

Crystal Plasticity Finite Element Method Investigation of the High Temperature Deformation Consistency in Dual-Phase Titanium Alloy

  • Xuexiong LI ,
  • Dongsheng XU ,
  • Rui YANG
Expand
  • 1. Institute of Metal Research, Chinese Academy of Science, Shenyang 110016, China
    2. University of Chinese Academy of Sciences, Beijing 100049, China

Received date: 2018-08-17

  Revised date: 2019-03-11

  Online published: 2019-04-25

Supported by

National Key Research and Development Program of China(No.2016YFB0701304);Informatization Program of the Chinese Academy of Sciences(No.XXH13506-3040);Strategic Priority Research Program of the Chinese Academy of Sciences(No.XDC01040100)

摘要

基于率相关滑移为主的晶体塑性本构模型,结合Voronoi方法创建双相多晶体集合,研究不同组织特征的Ti-6Al-4V合金的高温变形行为,重点关注双相组织中应力、应变空间分布特征及其演化,应力、应变相间分配,并提出一种变形协调性定量评估方法。结果表明,多晶变形过程中,晶界及其附近是变形的优先响应区域;β晶粒与α晶粒之间存在包围结构特征可加剧局域应变的差异分配;晶粒长短轴比越大,周围异相界面越多,则其局域变形协调性越低。αβ相应力频率统计呈双峰形态,α相中平均应变较高,而β相中应力较高。随α相体积分数增加,拉伸屈服强度和应力协调系数降低,而应变协调系数先降低后升高。随α基面织构体积分数增加,拉伸屈服强度和加工硬化率升高,且应力协调系数升高,而应变协调系数先降低后升高。

本文引用格式

李学雄 , 徐东生 , 杨锐 . 双相钛合金高温变形协调性的CPFEM研究[J]. 金属学报, 2019 , 55(7) : 928 -938 . DOI: 10.11900/0412.1961.2018.00380

Abstract

Based on the rate-dependent crystal plasticity constitutive model considering all slip systems, a series of dual-phase polycrystalline models were established using 3D Voronoi tessellation to investigate the high temperature plastic deformation of Ti-6Al-4V alloy with different microstructure features. The spatial distributions and evolution of stress and strain in various grains and phases were calculated in detail, and a new method was proposed to evaluate quantitatively the deformation consistency in the alloy with two phases. Simulations show that grain boundary region responds preferentially in the early stage of deformation. The encircling structure formed between β and α grains can enhance the differences in the local strain distribution. Increasing the aspect ratio of grains and the fractions of heterogeneous phase interface can reduce the local compatibility of deformation. The stress frequency statistics of both α and β phases show a double peak form, with α phase higher in average strain, and β phase higher in stress distribution. Increasing of the volume fractions of α phase may reduce the tensile yield strength, and cause the stress consistency coefficient to decrease, while the strain consistency coefficient decreases first and then increases. As initial α-basal texture intensity increases, both tensile yield strength and stress consistency coefficient increase, while the strain consistency coefficient decreases first and then increases.

参考文献

[1] Lütjering G, Williams J C. Titanium [M]. 2nd Ed. New York: Springer, 2007: 251
[2] Huang B Y, Li C G, Shi L K, et al. Dictionary for Material [M]. Beijing: Chemical Industry Press, 2006: 585
[2] (黄伯云, 李成功, 石力开等. 中国材料工程大典 [M]. 北京: 化学工业出版社, 2006: 585)
[3] Warwick J L W. Texture, microstructure and deformation mechanism in titanium alloys [D]. London: Imperial College London, 2013
[4] Britton T B, Liang H, Dunne F P E, et al. The effect of crystal orientation on the indentation response of commercially pure titanium: Experiments and simulations [J]. Proc. Roy. Soc., 2010, 466A: 695
[5] Wilkinson A J, Clarke E E, Britton T B, et al. High-resolution electron backscatter diffraction: An emerging tool for studying local deformation [J]. J. Strain Anal. Eng. Des., 2010, 45: 365
[6] Tamura I, Tomota Y, Yamaoka Y, et al. The Strength and ductility of two-phase iron alloys [J]. Tetsu Hagané, 1973, 59: 454
[6] (田村 今男, 友田 陽, 山岡 幸男等. 二相混合組織をもつ鉄合金の強度と延性について [J]. 鉄と鋼, 1973, 59: 454
[7] Fan X G, Yang H. Internal-state-variable based self-consistent constitutive modeling for hot working of two-phase titanium alloys coupling microstructure evolution [J]. Int. J. Plast., 2011, 27: 1833
[8] Katani S, Madadi F, Atapour M, et al. Micromechanical modelling of damage behaviour of Ti-6Al-4V [J]. Mater. Des., 2013, 49: 1016
[9] Neti S, Vijayshankar M N, Ankem S. Finite element method modeling of deformation behavior of two-phase materials part I: Stress-strain relations [J]. Mater. Sci. Eng., 1991, A145: 47
[10] Zang X L, Zhao X Q, Joongkeun P, et al. Numerical simulation on distribution of micro stress-strain in dual-phase titanium alloys [J]. Rare Met. Mater. Eng., 2009, 38: 1058
[10] (臧新良, 赵希庆, Joongkeun P等. 双相钛合金微观应力-应变分布的数值模拟 [J]. 稀有金属材料与工程, 2009, 38: 1058)
[11] Kuang S, Kang Y L, Yu H, et al. Stress-strain partitioning analysis of constituent phases in dual phase steel based on the modified law of mixture [J]. Int. J. Miner. Metall. Mater., 2009, 16: 393
[12] Roters F, Eisenlohr P, Hantcherli L, et al. Overview of constitutive laws, kinematics, homogenization and multiscale methods in crystal plasticity finite-element modeling: Theory, experiments, applications [J]. Acta Mater., 2010, 58: 1152
[13] Tang B, Xie S, Liu Y, et al. Crystal plasticity finite element study of incompatible deformation behavior in two phase microstructure in near β titanium alloy [J]. Rare Met. Mater. Eng., 2015, 44: 532
[14] Asaro R J, Needleman A. Overview no.42 Texture development and strain hardening in rate dependent polycrystals [J]. Acta Metall., 1985, 33: 923
[15] Peirce D, Asaro R J, Needleman A. An analysis of nonuniform and localized deformation in ductile single crystals [J]. Acta Metall., 1982, 30: 1087
[16] Hill R. Generalized constitutive relations for incremental deformation of metal crystals by multislip [J]. J. Mech. Phys. Solids, 1966, 14: 95
[17] Hill R, Rice J R. Constitutive analysis of elastic-plastic crystals at arbitrary strain [J]. J. Mech. Phys. Solids, 1972, 20: 401
[18] Hutchinson J W. Bounds and self-consistent estimates for creep of polycrystalline materials [J]. Proc. Roy. Soc., 1976, 348A: 101
[19] Bassani J L, Wu T Y. Latent hardening in single crystals. II. Analytical characterization and predictions [J]. Proc. Roy. Soc., 1991, 435A: 21
[20] Peirce D, Asaro R J, Needleman A. Material rate dependence and localized deformation in crystalline solids [J]. Acta Metall., 1983, 31: 1951
[21] Salkind N J. Encyclopedia of Research Design [M]. Thousand Oaks, Calif: SAGE, 2010: 170
[22] Quey R, Dawson P R, Barbe F. Large-scale 3D random polycrystals for the finite element method: Generation, meshing and remeshing [J]. Comput. Methods Appl. Mech. Eng., 2011, 200: 1729
[23] Si L Y, Deng G Y, Lv C, et al. Polycrystal geometry modeling of crystal plasticity finite element method with Voronoi diagram [J]. J. Mater. Metall., 2009, 8: 193
[23] (司良英, 邓关宇, 吕 程等. 基于Voronoi图的晶体塑性有限元多晶几何建模 [J]. 材料与冶金学报, 2009, 8: 193)
[24] Balasubramanian S, Anand L. Plasticity of initially textured hexagonal polycrystals at high homologous temperatures: Application to titanium [J]. Acta Mater., 2002, 50: 133
[25] Simmons G, Wang H. Single Crystal Elastic Constants and Calculated Aggregate Properties [M]. 2nd Ed., Cambridge: The MIT Press, 1971: 199
[26] Ogi H, Kai S, Ledbetter H, et al. Titanium's high-temperature elastic constants through the hcp-bcc phase transformation [J]. Acta Mater., 2004, 52: 2075
[27] Duan Y P. Research on mesoscopic research and simulation on hot deformation microstructure in TB8 alloy [D]. Hefei: Hefei University of Technology, 2009
[27] (段园培. TB8合金热变形组织介观尺度研究与模拟 [D]. 合肥: 合肥工业大学, 2009)
[28] Ma Y J, Li J W, Lei J F, et al. Influences of microstructure on fatigue crack propagating path and crack growth rates in TC4ELI alloy [J]. Acta Metall. Sin., 2010, 46: 1086
[28] (马英杰, 李晋炜, 雷家峰等. 显微组织对TC4ELI合金疲劳裂纹扩展路径及扩展速率的影响 [J]. 金属学报, 2010, 46: 1086)
[29] Song M, Ma Y J, Wu J, et al. Effect of cooling rate on microstructure and properties of Ti-5.8Al-3Mo-1Cr-2Sn-2Zr-1V-0.15Si alloy [J]. Chin. J. Nonferrous Met., 2010, 20(Spec.1): s588
[29] (宋 淼, 马英杰, 邬 军等. 冷却速率对Ti-5.8Al-3Mo-1Cr-2Sn-2Zr-1V-0.15Si合金组织及性能的影响 [J]. 中国有色金属学报, 2010, 20(专辑1): s588)
[30] Gu X Y, Xu D S, Wang H, et al. Lattice weakening by edge dislocation core under tension [J]. Modell. Simul. Mater. Sci. Eng., 2010, 18: 065004
[31] Wu H N, Xu D S, Wang H, et al. Molecular dynamics simulation of tensile deformation and fracture of γ-TiAl with and without surface defects [J]. J. Mater. Sci. Technol., 2016, 32: 1033
[32] Wang H, Xu D S, Yang R. Defect clustering upon dislocation annihilation in α-titanium and α-zirconium with hexagonal close-packed structure [J]. Modell. Simul. Mater. Sci. Eng., 2014, 22: 085004
[33] Peters M, Gysler A, Lütjering G. Influence of texture on fatigue properties of Ti-6Al-4V [J]. Metall. Mater. Trans., 1984, 15A: 1597
[34] Peters M, Luetjering G. Control of microstructure and texture in Ti-6Al-4V alloy [A]. Titanium'80, Science and Technology: Proceedings of the Fourth International Conference on Titanium [C]. Warrendale, PA: TMS, 1980: 925
[35] Bache M R, Evans W J. Impact of texture on mechanical properties in an advanced titanium alloy [J]. Mater. Sci. Eng., 2001, A319: 409
[36] Paton N E, Backofen W A. Plastic deformation of Titanium at elevated temperatures [J]. Metall. Trans., 1970, 1: 2839
文章导航

/