Optimization and Simulation of Deformation Parameters of SiC/2009Al Composites

  • Kai MA ,
  • Xingxing ZHANG ,
  • Dong WANG ,
  • Quanzhao WANG ,
  • Zhenyu LIU ,
  • Bolv XIAO ,
  • Zongyi MA
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China

Received date: 2019-01-24

  Revised date: 2019-03-14

  Online published: 2019-04-10

Supported by

Supported by National Key Research and Development Program of China(2017YFB0703104);National Natural Science Foundation of China(51871214);National Natural Science Foundation of China(U1508216)

摘要

对粉末冶金法制备的15%SiC (体积分数)/2009Al复合材料热变形参数的仿真优化方法进行了探讨。通过热压缩实验获得复合材料的动态真应力-真应变曲线,由此建立了最大应变量下应变速率敏感指数(m)分布图。在不同m值对应的变形参数下,对复合材料的热压缩过程进行有限元模拟,分析了热压缩样品的流变应力、应变、危险系数分布等,结合微观组织验证了以m作为评价复合材料加工参数依据的可靠性,并由此确定15%SiC/2009Al复合材料的最佳热变形参数所对应的变形温度和应变速率分别为500 ℃和0.01 s-1

本文引用格式

马凯 , 张星星 , 王东 , 王全兆 , 刘振宇 , 肖伯律 , 马宗义 . SiC/2009Al复合材料的变形加工参数的优化仿真研究[J]. 金属学报, 2019 , 55(10) : 1329 -1337 . DOI: 10.11900/0412.1961.2019.00020

Abstract

Particle reinforced aluminum matrix composites (PRAMCs) have the advantages of high specific strength and high specific modulus, and are important engineering materials for aerospace field. However, due to the huge difference in the mechanical properties between the reinforcements and the aluminum matrixes, the plastic forming of PRAMCs is quite difficult, which restricts their wide engineering applications. In order to improve the quality of plastic processing, it is necessary to optimize deformation parameters of PRAMCs. In this study, the hot deformation parameters of a 15%SiC/2009Al composite fabricated by powder metallurgy were optimized using a simulation method. Firstly, true stress-strain curves of the SiC/2009Al composite were obtained through hot compression tests, and then the strain rate sensitivity index (m) map at the ultimate strain was established. Under the deformation parameters corresponding to various m values, the finite element simulation of the hot compression process was carried out. The flow stress, strain and damage coefficient distribution of the hot-compressed samples were analyzed. The results show that it is reliable to use the m value as the basis for optimizing the processing parameters, which were further verified by the microstructural observations. The deformation temperature and strain rate corresponding to the optimum parameters of the composite were determined to be 500 ℃ and 0.01 s-1, respectively.

参考文献

[1] Lloyd D J. Particle reinforced aluminium and magnesium matrix composites [J]. Int. Mater. Rev., 1994, 39(1): 1
[2] Tjong S C. Novel nanoparticle-reinforced metal matrix composites with enhanced mechanical properties [J]. Adv. Eng. Mater., 2007, 9: 639
[3] Ramnath B V, Elanchezhian C, Annamalai R M ,et al. Aluminium metal matrix composites—A review [J]. Rev. Adv. Mater. Sci., 2014, 38: 55
[4] Tham L M, Gupta M, Cheng L. Effect of reinforcement volume fraction on the evolution of reinforcement size during the extrusion of Al-SiC composites [J]. Mater. Sci. Eng., 2002, A326: 355
[5] Li H Z, Wang H J, Zeng M ,et al. Forming behavior and workability of 6061/B4CP composite during hot deformation [J]. Compos. Sci. Technol., 2011, 71: 925
[6] Liu Z Y, Wang Q Z, Xiao B L, et al. Effects of double extrusion on the microstructure and tensile property of the PM processed SiCp/2009Al composites [J]. Acta Metall. Sin., 2010, 46: 1121
[6] (刘振宇, 王全兆, 肖伯律等. 二次挤压对SiCp/2009Al复合材料微观结构和力学性能的影响 [J]. 金属学报, 2010, 46: 1121)
[7] Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59
[7] (肖伯律, 黄治冶, 马 凯等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59)
[8] Kim H Y, Hong S H. High temperature deformation behavior of 20vol.% SiCw2024Al metal matrix composite [J]. Scr. Metall. Mater., 1994, 30: 297
[9] Huang H Y, Fan G L, Tan Z Q ,et al. Superplastic behavior of carbon nanotube reinforced aluminum composites fabricated by flake powder metallurgy [J]. Mater. Sci. Eng., 2017, A699: 55
[10] Mabuchi M, Higashi K, Inoue K ,et al. Experimental investigation of superplastic behavior in a 20vol% Si3N4p5052 aluminum composite [J]. Scr. Mater., 1992, 26: 1839
[11] Huang Z Y, Zhang X X, Xiao B, et al. Hot deformation mechanisms and microstructure evolution of SiCp/2014Al composite [J]. J. Alloys Compd., 2017, 722: 145
[12] Shao J C, Xiao B L, Wang Q Z ,et al. Constitutive flow behavior and hot workability of powder metallurgy processed 20vol.%SiCP/2024Al composite [J]. Mater. Sci. Eng., 2010, A527: 7865
[13] Mokdad F, Chen D L, Liu Z Y ,et al. Three-dimensional processing maps and microstructural evolution of a CNT-reinforced Al-Cu-Mg nanocomposite [J]. Mater. Sci. Eng., 2017, A702: 425
[14] Kai X Z, Zhao Y T, Wang A D ,et al. Hot deformation behavior of in situ nano ZrB2 reinforced 2024Al matrix composite [J]. Compos. Sci. Technol., 2015, 116: 1
[15] Kim W J. The size effect of SiC particulates on activation energy for superplastic flow in a 2124 Al metal matrix composite [J]. Scr. Mater., 1999, 41: 1131
[16] Shi C J, Chen X G. Evolution of activation energies for hot deformation of 7150 aluminum alloys with various Zr and V additions [J]. Mater. Sci. Eng., 2016, A650: 197
[17] Huang Z Y, Zhang X X, Yang C, et al. Abnormal deformation behavior and particle distribution during hot compression of fine-grained 14vol% SiCp/2014Al composite [J]. J. Alloys Compd., 2018, 743: 87
[18] Zhang Z J, Dai G Z, Wu S N ,et al. Simulation of 42CrMo steel billet upsetting and its defects analyses during forming process based on the software DEFORM-3D [J]. Mater. Sci. Eng., 2009, A499: 49
[19] Sornin D, Karch A, Nunes D. Finite element method simulation of the hot extrusion of a powder metallurgy stainless steel grade [J]. Int. J. Mater. Forming, 2015, 8: 145
[20] Chen J F, Yan M F, Wang X R. 3D FEM simulation of hot extrusion process of AerMet100 steel [J]. Trans. Mater. Heat Treat., 2007, 28(S1): 367
[20] (陈俊锋, 闫牧夫, 汪向荣. AerMet100钢热挤压变形过程数值模拟 [J]. 材料热处理学报, 2007, 28(S1): 367)
[21] Zhou L, Huang Z Y, Wang C Z ,et al. Constitutive flow behaviour and finite element simulation of hot rolling of SiCp/2009Al composite [J]. Mech. Mater., 2016, 93: 32
[22] Zhou L, Wang C Z, Zhang X X ,et al. Finite element simulation of hot rolling process for SiCp/Al composites [J]. Acta Metall. Sin., 2015, 51: 889
[22] (周 丽, 王唱舟, 张星星等. SiCp/Al复合材料热轧过程的有限元模拟 [J]. 金属学报, 2015, 51: 889)
[23] Liu Y, Shao J C, Ding L ,et al. Finite element simulation and analysis of 12 vol%SiCP/2024Al matrix composites for hot extrusion process [J]. Acta. Mater. Compos. Sin., 2009, 26(5): 167
[23] (刘 越, 邵军超, 丁 莉等. 12vol%SiCP/2024Al基复合材料热挤压过程有限元模拟与分析 [J]. 复合材料学报, 2009, 26(5): 167)
[24] Zhang J F, Zhang X X, Wang Q Z, et al. Simulations of deformation and damage processes of SiCp/Al composites during tension [J]. J. Mater. Sci. Technol., 2018, 34: 627
[25] McQueen H J, Blum W. Dynamic recovery: Sufficient mechanism in the hot deformation of Al (<99.99) [J]. Mater. Sci. Eng., 2000, A290: 95
[26] Sun Y L, Xie J P, Hao S M ,et al. Dynamic recrystallization model of 30%SiCp/Al composite [J]. J. Alloys Compd., 2015, 649: 865
[27] Yang Q Y, Deng Z H, Zhang Z Q, et al. Effects of strain rate on flow stress behavior and dynamic recrystallization mechanism of Al-Zn-Mg-Cu aluminum alloy during hot deformation [J]. Mater. Sci. Eng., 2016, A662: 204
[28] Kim W J, Hong S H. High-strain-rate superplastic deformation behavior of a powder metallurgy-processed 2124 Al alloy [J]. J. Mater. Sci., 2000, 35: 2779
[29] Du N N, Bower A F, Krajewski P E, et al. The influence of a threshold stress for grain boundary sliding on constitutive response of polycrystalline Al during high temperature deformation [J]. Mater. Sci. Eng., 2008, A494: 86
[30] Lagneborg R, Bergman B. The stress/creep rate behaviour of precipitation-hardened alloys [J]. Met. Sci., 1976, 10: 20
[31] Kaibyshev R, Kazyhanov V, Musin F. Hot plastic deformation of aluminium alloy 2009-15%SiCw composite [J]. Mater. Sci. Technol., 2002, 18: 777
[32] Mishra R S, Bieler T R, Mukherjee A K. Mechanism of high strain rate superplasticity in aluminium alloy composites [J]. Acta Mater., 1997, 45: 561
[33] Wierzbicki T, Bao Y B, Lee Y W, et al. Calibration and evaluation of seven fracture models [J]. Int. J. Mech. Sci., 2005, 47: 719
文章导航

/