GH4169合金圆盘时效过程残余应力的演化规律研究
收稿日期: 2018-09-07
修回日期: 2019-04-08
网络出版日期: 2019-04-08
基金资助
国家重点研发计划项目((No.2017YFB0702901));国家自然科学基金项目((No.U1708253))
Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk
Received date: 2018-09-07
Revised date: 2019-04-08
Online published: 2019-04-08
Supported by
Supported by National Key Research and Development Program of China((No.2017YFB0702901));National Natural Science Foundation of China((No.U1708253))
以固溶水淬后的GH4169合金圆盘为研究对象,采用原位中子衍射法研究了时效热处理中的升温、保温和空冷3个阶段残余应力的演化行为,分析了残余应力的演化规律和松弛机制。考虑到工件内部残余应力对γ″相析出行为的影响,采用了2种无应力标样作为分析应力的基准。结果表明,淬火后圆盘中心的旋向和径向存在340.62 MPa的拉应力,轴向存在-33.34 MPa的压应力。升温阶段,材料屈服强度随温度的升高而降低,部分残余应力通过塑性变形进行释放,圆盘中心旋向/径向残余应力从340.62 MPa降至227.67 MPa。保温阶段,残余应力通过蠕变变形进行释放,随着γ″相逐渐析出,蠕变抗力增大,保温阶段的残余应力松弛主要集中在保温的早期。空冷阶段残余应力基本保持不变。
秦海龙 , 张瑞尧 , 毕中南 , 杜洪标 , 张金辉 . GH4169合金圆盘时效过程残余应力的演化规律研究[J]. 金属学报, 2019 , 55(8) : 997 -1007 . DOI: 10.11900/0412.1961.2018.00428
GH4169 alloy, a precipitation-strengthened nickel-iron base superalloy, has been widely used in aerospace and energy industries due to its excellent high-temperature strength which derived from the coherent phases (γ″ and γ'). To form these precipitates, the manufacturing process of GH4169 usually involves solid solution heat treatment followed by rapid cooling and double ageing heat treatment. Significant residual stresses are induced during rapid cooling and then partially relieved during the subsequent ageing treatment. However, the reduced residual stress after ageing are still large enough to affect the final machining operations, resulting in the component exceeding the dimensional tolerances if they are not well considered. Furthermore, residual stresses in the final components may lead to further distortion beyond estimation during service, which could deteriorate the engine performances. In the present study, the evolution of residual stresses at heating, isothermal ageing, and air-cooling stages of ageing heat treatment in a GH4169 alloy disk was characterized by in situ neutron diffraction. Considering the effect of residual stresses on the precipitation behavior of γ″, two different types of stress-free samples were used as the basis for the stress analysis. The results show that significant residual stresses were induced during water quenching, which were found to be 340.62 MPa tensile in hoop/radial directions and 33.34 MPa compressive in axial direction in the center of the disk. Subsequently, an in situ ageing heat treatment was undertaken at 720 ℃ for 8 h. During the heating stage, the yield strength of the material decreases with increasing temperature, leading to residual stress relaxation through plastic deformation from 340.62 MPa to 227.67 MPa in hoop/radial direction in the disk center. At the isothermal ageing stage, residual stresses relieved apparently by about 40 MPa during the first 100 min, later on a slower linear relaxation remained for the rest of the ageing heat treatment. The strength of the alloy increased and the creep rate decreased due to the formation of γ″ and γ′ strengthening phases, indicating that most of stress relaxation occurred as a result of creep deformation at the early stage of isothermal ageing. The magnitude of residual stress was almost invariable in the subsequent air-cooling stage.
Key words: superalloy; ageing treatment; residual stress; in situ neutron diffraction
| [1] | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2008: 217 |
| [2] | Zhuang J Y, Du J H, Deng Q, et al. Wrought Superalloy GH4169 [M]. Beijing: Metallurgical Industry Press, 2006: 1 |
| [2] | (庄景云, 杜金辉, 邓 群等. 变形高温合金GH4169 [M]. 北京: 冶金工业出版社, 2006: 1) |
| [3] | Lu X D, Du J H, Deng Q. High temperature structure stability of GH4169 superalloy [J]. Mater. Sci. Eng., 2013, A559: 623 |
| [4] | Du J H, Lu X D, Deng Q, et al. High-temperature structure stability and mechanical properties of novel 718 superalloy [J]. Mater. Sci. Eng., 2007, A452-453: 584 |
| [5] | Xie X S, Dong J X, Fu S H, et al. Research and development of γ″ and γ′ strengthened Ni-Fe base superalloy GH4169 [J]. Acta Metall. Sin., 2010, 46: 1289 |
| [5] | (谢锡善, 董建新, 付书红等. γ″和γ′相强化的Ni-Fe基高温合金GH4169的研究与发展 [J]. 金属学报, 2010, 46: 1289) |
| [6] | Geng L, Na Y S, Park N K. Continuous cooling transformation behavior of Alloy 718 [J]. Mater. Lett., 1997, 30: 401 |
| [7] | Dye D, Conlon K T, Reed R C. Characterization and modeling of quenching-induced residual stresses in the nickel-based superalloy IN718 [J]. Metall. Mater. Trans., 2004, 35A: 1703 |
| [8] | Rist M A, James J A, Tin S, et al. Residual stresses in a quenched superalloy turbine disc: Measurements and modeling [J]. Metall. Mater. Trans., 2006, 37A: 459 |
| [9] | Withers P J, Bhadeshia H K D K. Residual stress Part 2—Nature and origins [J]. Mater. Sci. Technol., 2001, 17: 366 |
| [10] | Aba-Perea P E, Pirling T, Preuss M. In-situ residual stress analysis during annealing treatments using neutron diffraction in combination with a novel furnace design [J]. Mater. Des., 2016, 110: 925 |
| [11] | Rolph J, Evans A, Paradowska A, et al. Stress relaxation through ageing heat treatment—A comparison between in situ and ex situ neutron diffraction techniques [J]. C. R. Phys., 2012, 13: 307 |
| [12] | Xu P G, Tomota Y. Progress in materials characterization technique based on in situ neutron diffraction [J]. Acta Metall. Sin., 2006, 42: 681 |
| [12] | (徐平光, 友田阳. 基于原位中子衍射表征技术的进展 [J]. 金属学报, 2006, 42: 681) |
| [13] | Dong P, Wang H, Li J, et al. Residual stress in welded Beryllium ring by neutron diffraction and finite element modeling [J]. At. Energy Sci. Technol., 2015, 49: 2255 |
| [13] | (董 平, 王 虹, 李 建等. 铍环焊接残余应力的中子衍射测试与有限元分析 [J]. 原子能科学技术, 2015, 49: 2255) |
| [14] | Collins D M, D' Souza N, Panwisawas C. In-situ neutron diffraction during stress relaxation of a single crystal nickel-base superalloy [J]. Scr. Mater., 2017, 131: 103 |
| [15] | Allen A J, Hutchings M T, Windsor C G, et al. Neutron diffraction methods for the study of residual stress fields [J]. Adv. Phys., 1985, 34: 445 |
| [16] | Wagner J N, Hofmann M, Wimpory R, et al. Microstructure and temperature dependence of intergranular strains on diffractometric macroscopic residual stress analysis [J]. Mater. Sci. Eng., 2014, A618: 271 |
| [17] | Eto T, Sato A, Mori T. Stress-oriented precipitation of G. P. Zones and θ' in an Al-Cu alloy [J]. Acta Metall., 1978, 26: 499 |
| [18] | Li D Y, Chen L Q. Computer simulation of stress-oriented nucleation and growth of θ′ precipitates in Al-Cu alloys [J]. Acta Mater., 1998, 46: 2573 |
| [19] | Cheng K Y, Jo C Y, Jin T, et al. Influence of applied stress on the γ′ directional coarsening in a single crystal superalloy [J]. Mater. Des., 2010, 31: 968 |
| [20] | Gao M, Harlow D G, Wei R P, et al. Preferential coarsening of γ″ precipitates in Inconel 718 during creep [J]. Metall. Mater. Trans., 1996, 27A: 3391 |
| [21] | Qin H L, Bi Z N, Yu H Y, et al. Influence of stress on γ″ precipitation behavior in Inconel 718 during aging [J]. J. Alloys Compd., 2018, 740: 997 |
| [22] | Qin H L, Bi Z N, Yu H Y, et al. Assessment of the stress-oriented precipitation hardening designed by interior residual stress during ageing in IN718 superalloy [J]. Mater. Sci. Eng., 2018, A728: 183 |
| [23] | Santisteban J R, Daymond M R, James J A, et al. ENGIN-X: A third-generation neutron strain scanner [J]. J. Appl. Cryst., 2006, 39: 812 |
| [24] | Pawley G S. Unit-cell refinement from powder diffraction scans [J]. J. Appl. Crystallogr., 1981, 14: 357 |
| [25] | Denis S, Sj?str?m S, Simon A. Coupled temperature, stress, phase transformation calculation [J]. Metall. Trans., 1987, 18A: 1203 |
| [26] | Aba-Perea P E, Pirlinga T, Withers P J, et al. Determination of the high temperature elastic properties and diffraction elastic constants of Ni-base superalloys [J]. Mater. Des., 2016, 89: 856 |
| [27] | Oradei-Basile A, Radavich J F. A current TTT diagram for wrought alloy 718 [A]. Superalloys 718, 625 and Various Derivatives [C]. Pittsburgh: Springer, 1991: 325 |
| [28] | Wang Y Z, Dong J X, Zhang M C, et al. Stress relaxation behavior and mechanism of AEREX 350 and Waspaloy superalloys [J]. Mater. Sci. Eng., 2016, A678: 10 |
| [29] | Hong S J, Chen W P, Wang T W. A diffraction study of the γ″ phase in INCONEL 718 superalloy [J]. Metall. Mater. Trans., 2001, 32A: 1887 |
| [30] | Kulawik K, Buffat P A, Kruk A, et al. Imaging and characterization of γ′ and γ″ nanoparticles in Inconel 718 by EDX elemental mapping and FIB—SEM tomography [J]. Mater. Charact., 2015, 100: 74 |
| [31] | Liu Y, Qin S W, Zuo X W, et al. Finite element simulation and experimental verification of quenching stress in fully through-hardened cylinders [J]. Acta Metall. Sin., 2017, 53: 733 |
| [31] | (刘 玉, 秦盛伟, 左训伟等. 全淬透圆柱件淬火应力的有限元模拟及实验验证 [J]. 金属学报, 2017, 53: 733) |
| [32] | Foss B J, Gray S, Hardy M C, et al. Analysis of shot-peening and residual stress relaxation in the nickel-based superalloy RR1000 [J]. Acta Mater., 2013, 61: 2548 |
| [33] | Zhang F, Cao W S, Zhang C, et al. Simulation of co-precipitation kinetics of γ′ and γ″ in superalloy 718 [A]. Proceedings of the 9th International Symposium on Superalloy 718 & Derivatives: Energy, Aerospace, and Industrial Applications [C]. Pittsburgh: Springer, 2018: 147 |
| [34] | Fisk M, Ion J C, Lindgren L E. Flow stress model for IN718 accounting for evolution of strengthening precipitates during thermal treatment [J]. Comput. Mater. Sci., 2104, 82: 531 |
| [35] | Oblak J M, Paulonis D F, Duvall D S. Coherency strengthening in Ni base alloys hardened by D022γ′ precipitates [J]. Metall. Trans., 1974, 5: 143 |
| [36] | Han Y F, Chaturvedi M C. A study of back stress during creep deformation of a superalloy inconel 718 [J]. Mater. Sci. Eng., 1987, 85: 59 |
| [37] | Chaturvedi M C, Han Y F. Effect of particle size on the creep rate of superalloy Inconel 718 [J]. Mater. Sci. Eng., 1987, 89: L7 |
| [38] | Kuo C M, Yang Y T, Bor H Y, et al. Aging effects on the microstructure and creep behavior of Inconel 718 superalloy [J]. Mater. Sci. Eng., 2009, A510-511: 289 |
/
| 〈 |
|
〉 |