预变形温度对纳米贝氏体相变动力学及组织的影响
作者简介 徐士新,男,1989年生,硕士
收稿日期: 2017-11-30
网络出版日期: 2018-05-15
基金资助
“十二五”国家科技支撑计划项目No.2012BAE03B01
Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure
Received date: 2017-11-30
Online published: 2018-05-15
Supported by
Supported by Key Projects in the National Science & Technology Pillar Program during the 12th Five-Year Plan Period (No.2012BAE03B01)
采用热模拟试验机在300~850 ℃施加20%的压缩预变形后进行300 ℃等温相变实验,研究了预变形温度对中碳纳米贝氏体钢等温相变动力学及组织的影响。结果表明,预变形工艺使贝氏体相变孕育期显著缩短;低温预变形工艺使贝氏体相变在整个等温区间内均得到加速,高温预变形工艺使贝氏体相变仅在等温初期得到加速,等温后期相变速率明显减缓;随预变形温度的降低,贝氏体铁素体板条厚度逐渐增加;预变形工艺增加了贝氏体相变组织小角度晶界的频率,低温预变形试样的小角度晶界频率高于高温预变形试样。利用解析相变模型计算了贝氏体等温相变过程中的相变动力学参数n,并对贝氏体相变过程中的形核长大方式进行了判定,发现预变形工艺改变了贝氏体相变的形核位置,低温预变形试样主要以晶隅形核为主,高温预变形试样主要以晶棱、晶面形核为主。
徐士新 , 余伟 , 李舒笳 , 王坤 , 孙齐松 . 预变形温度对纳米贝氏体相变动力学及组织的影响[J]. 金属学报, 2018 , 54(8) : 1113 -1121 . DOI: 10.11900/0412.1961.2017.00506
As a new steel, nanobainite steel has favourable strength and good plasticity, but the bainite transformation needs a longer time, so as to severely slow production efficiency down. So, the research of acceleration methods of bainite transformation is of significance. In this work, in order to accelerate the bainite transformation rate, the 20% compression pre-deformation at 300~850 ℃ and isothermal transformation at 300 ℃ were conducted on a thermal simulator. The effects of pre-deformation temperature on nanobainite transformation kinetics and microstructure of the medium carbon nanobainite steel were investigated. The results showed that pre-deformation process obviously shortened the incubation time of bainite transformation. Low pre-deformation temperature could accelerate bainite transformation at whole isothermal region, while high pre-deformation temperature accelerated bainite transformation at the initial stage, and hindered bainite transformation at later stage. Bainite ferrite lath thickness was increased with decreasing pre-deformation temperature. The pre-deformation process increased the frequency of small angle grain boundary of bainite transformation microstructure, and the frequency of small angle grain boundary of low pre-deformation temperature was higher than that of high pre-deformation temperature. The kinetic parameters n of bainite transformation was calculated by the analytical model, the model of nucleation and growth were identified, the pre-deformation process changed the nucleation position of bainite transformation. The crystal corner nucleation was mainly obtained through low pre-deformation temperature, and the crystal edge and the crystal face nucleation were mainly obtained through high pre-deformation temperature.
| [1] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 1[J]. Mater. Sci. Technol., 2001, 17: 512 |
| [2] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 2[J]. Mater. Sci. Technol., 2001, 17: 517 |
| [3] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Very strong low temperature bainite[J]. Mater. Sci. Technol., 2002, 18: 279 |
| [4] | Caballero F G, Bhadeshia H K D H. Very strong bainite[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 251 |
| [5] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Mechanical properties of low-temperature bainite [J]. Mater. Sci. Forum, 2005, 500-501: 285 |
| [6] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Development of hard bainite[J]. ISIJ Int., 2003, 43: 1238 |
| [7] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Acceleration of low-temperature bainite[J]. ISIJ Int., 2003, 43: 1821 |
| [8] | Umemoto M, Furuhara T, Tamura I.Effects of austenitizing temperature on the kinetics of bainite reaction at constant austenite grain size in Fe-C and Fe-Ni-C alloys[J]. Acta Metall., 1986, 34: 2235 |
| [9] | Bhadeshia H K D H. Nanostructured bainite[J]. Proc. R. Soc., 2010, 466A: 3 |
| [10] | Yoozbashi M N, Yazdani S, Wang T S.Design of a new nanostructured, high-Si bainitic steel with lower cost production[J]. Mater. Des., 2011, 32: 3248 |
| [11] | Bhadeshia H K D H, David S A, Vitek J M, et al. Stress induced transformation to bainite in Fe-Cr-Mo-C pressure vessel steel[J]. Mater. Sci. Technol., 1991, 7: 686 |
| [12] | Matsuzaki A, Bhadeshia H K D H, Harade H. Stress affected bainitic transformation in a Fe-C-Si-Mn alloy[J]. Acta Metall. Mater., 1994, 42: 1081 |
| [13] | Shipway P H, Bhadeshia H K D H. The effect of small stresses on the kinetics of the bainite transformation[J]. Mater. Sci. Eng., 1995, A201: 143 |
| [14] | Xu Z Y.Effect of stress on bainitic transformation in steel[J]. Acta. Metall. Sin., 2004, 40: 113(徐祖耀. 应力对钢中贝氏体相变的影响[J]. 金属学报, 2004, 40: 113) |
| [15] | Gong W, Tomota Y, Koo M S, et al.Effect of ausforming on nanobainite steel[J]. Scr. Mater., 2010, 63: 819 |
| [16] | Gong W, Tomota Y, Adachi Y, et al.Effects of ausforming temperature on bainite transformation, microstructure and variant selection in nanobainite steel[J]. Acta Mater., 2013, 61: 4142 |
| [17] | Ohtsuka H.Effects of strong magnetic fields on bainitic transformation[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 279 |
| [18] | Bhadeshia H K D H, Edmonds D V. The bainite transformation in a silicon steel[J]. Metall. Trans., 1979, 10A: 895 |
| [19] | Xu Q K.A study of the incomplete phenomenon of bainite transformation in a low carbon Fe-C-Mo alloy[J]. J. Chongqing Univ., 1987, (3): 59(徐启昆. 铁碳钼合金贝氏体转变不完全现象的研究[J]. 重庆大学学报, 1987, (3): 59) |
| [20] | Johnson W A, Mehl R F.Reaction kinetics in process of nucleation and growth[J]. Trans. AIME, 1939, 135: 416 |
| [21] | Avrami M.Kinetics of phase change. I General theory[J]. J. Chem. Phys., 1939, 7: 1103 |
| [22] | Avrami M.Kinetics of phase change. II Transformation-time relations for random distribution of nuclei[J]. J. Chem. Phys., 1940, 8: 212 |
| [23] | Avrami M.Granulation, phase change, and microstructure kinetics of phase change. III[J]. J. Chem. Phys., 1941, 9: 177 |
| [24] | Sidel S M, Santos F A, Gordo V O, et al.Avrami exponent of crystallization in tellurite glasses[J]. J. Therm. Anal. Calorim., 2011, 106: 613 |
| [25] | Quidort D, Bréchet Y J M. The role of carbon on the kinetics of bainite transformation in steels[J]. Scr. Mater., 2002, 47: 151 |
| [26] | Liu F, Sommer F, Mittemeijer E J.An analytical model for isothermal and isochronal transformation kinetics[J]. J. Mater. Sci., 2004, 39: 1621 |
| [27] | Liu F, Sommer F, Bos C, et al.Analysis of solid state phase transformation kinetics: Models and recipes[J]. Int. Mater. Rev., 2007, 54: 193 |
| [28] | Liu F, Sommer F, Mittemeijer E J.Analysis of the kinetics of phase transformations; roles of nucleation index and temperature dependent site saturation, and recipes for the extraction of kinetic parameters[J]. J. Mater. Sci., 2007, 42: 573 |
| [29] | Christian J W.The Theory of Transformations in Metals and Alloys[M]. 3rd Ed., Oxford: Elsevier Ltd., 2002: 546 |
| [30] | Quidort D, Brechet Y J M. A model of isothermal and non isothermal transformation kinetics of bainite in 0.5% C steels[J]. ISIJ Int., 2002, 42: 1010 |
| [31] | Zhang Z M, Cai Q W, Yu W, et al.Continuous cooling transformation behavior and kinetic models of transformations for an ultra-low carbon bainitic steel[J]. J. Iron Steel Res. Int., 2012, 19: 73 |
| [32] | Wang Q C, Yang Z G, Li Z D.A theoretical analysis on effect of deformation above Ae3 to the nucleation of proeutectoid ferrite transformation[J]. Acta. Metall. Sin., 2007, 43: 344(王启超, 杨志刚, 李昭东. Ae3温度以上变形对先共析铁素体相变形核影响的理论分析[J]. 金属学报, 2007, 43: 344) |
| [33] | Bhadeshia H K D H, Honeycombe R W K. Steels: Microstructure and Properties[M]. 3rd Ed., Oxford: Elsevier Ltd., 2006: 129 |
| [34] | Legros M, Dehm G, Arzt E, et al.Observation of giant diffusivity along dislocation cores[J]. Science, 2008, 319: 1646 |
| [35] | Bhadeshia H K D H. Bainite in Steels [M]. 2nd Ed., Cambridge: Cambridge University Press, 2001: 124 |
| [36] | Singh S B, Bhadeshia H K D H. Estimation of bainite plate-thickness in low-alloy steels[J]. Mater. Sci. Eng., 1998, A245: 72 |
| [37] | Hase K, Garcia-Mateo C, Bhadeshia H K D H. Bainite formation influenced by large stress[J]. Mater. Sci. Technol., 2004, 20: 1499 |
/
| 〈 |
|
〉 |