金属材料的凝固专刊

非平衡凝固与固态相变的一体化研究

  • 刘峰 ,
  • 张旭 ,
  • 张玉兵
展开
  • 西北工业大学凝固技术国家重点实验室 西安 710072

作者简介 刘 峰,男,1974年生,教授

收稿日期: 2018-03-26

  网络出版日期: 2018-04-02

基金资助

资助项目 国家重点研发计划项目Nos.2017YFB0305100、2017YFB0703001,国家自然科学基金项目Nos.51431008、51790481,中央高校基本科研业务费项目No.3102017jc01002和西北工业大学凝固技术国家重点实验室自主研究课题项目No.117-TZ-2015

Unified Analysis of Non-Equilibrium Solidification and Solid-State Phase Transformations

  • Feng LIU ,
  • Xu ZHANG ,
  • Yubing ZHANG
Expand
  • State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China

Received date: 2018-03-26

  Online published: 2018-04-02

Supported by

Supported by National Key Research and Development Program of China (Nos.2017YFB0305100 and 2017YFB0703001), National Natural Science Foundation of China (Nos.51431008 and 51790481), Fundamental Research Funds for the Central Universities (No.3102017jc01002) and Research Fund of the State Key Laboratory of Solidification Processing of Northwestern Polytechnical University (No.117-TZ-2015)

摘要

无论从相变,还是从材料热加工或材料设计而言,非平衡凝固与固态相变的一体化研究均具有深远的科学意义和极大的工程应用前景。本综述系统阐述了单相固溶体合金、共晶合金、包晶合金、多组元高温合金和铝合金的非平衡凝固及其包晶反应、块体转变、亚稳-稳定相转变、沉淀析出、再结晶和晶粒长大等固态转变行为。进而从非平衡凝固影响后续固态相变、非平衡凝固导致固态相变新机制、非平衡凝固与固态相变的一体化组织调控3个层次,探讨了非平衡凝固与随后固态相变的物理关联,实现了非平衡凝固和固态相变共同作用下的微观组织控制。本综述旨在为非平衡凝固效应的定量表征以及非平衡凝固与固态相变共同作用下的组织预测提供理论支撑。

本文引用格式

刘峰 , 张旭 , 张玉兵 . 非平衡凝固与固态相变的一体化研究[J]. 金属学报, 2018 , 54(5) : 701 -716 . DOI: 10.11900/0412.1961.2018.00112

Abstract

Considering both phase transition and material hot-working or material design, unified analysis of non-equilibrium solidification and solid-state phase transformations has profound significance of science and great prospect of engineering application. Here, non-equilibrium solidification and solid state transformation behavior, correlated with peritectic reaction, massive transformation, metastable-stable transformation, precipitation, recrystallization and grain growth, for single phase solid solution alloy, eutectic alloy, peritectic alloy, multi-component super alloy and aluminum alloy, have been systematically reviewed. Regarding further the influence of non-equilibrium solidification on subsequent solid-state transformations, the new transformation mechanism induced by non-equilibrium solidification and the integrated microstructure regulation, the physical correlation between non-equilibrium solidification and subsequent solid-state transformations were discussed, and eventually, the microstructure control under the joint action of non-equilibrium solidification and solid phase transformations was realized. This review is expected to provide theoretical support for quantitative characterization of non-equilibrium solidification effect and microstructure prediction under the joint action of non-equilibrium solidification and solid-state transformations.

参考文献

[1] Kim Y J, Perepezko J H.The thermodynamics and competitive kinetics of metastable τ phase development in MnAl-base alloys[J]. Mater. Sci. Eng., 1993, A163: 127
[2] Vandyoussefi M, Kerr H W, Kurz W.Directional solidification and δ /γ solid state transformation in Fe-3%Ni alloy[J]. Acta Mater., 1997, 45: 4093
[3] Lima M, Kurz W.Massive transformation and absolute stability[J]. Metall. Mater. Trans., 2002, 33A: 2337
[4] Aziz M J.Model for solute redistribution during rapid solidification[J]. J. Appl. Phys., 1982, 53: 1158
[5] Lu K.Nanocrystalline metals crystallized from amorphous solids: Nanocrystallization, structure, and properties[J]. Mater. Sci. Eng., 1996, R16: 161
[6] Lu K.Synthesis of nanocrystalline materials from amorphous solids[J]. Adv. Mater., 1999, 11: 1127
[7] Liu F, Yang G C.Stress-induced recrystallization mechanism for grain refinement in highly undercooled superalloy[J]. J. Cryst. Growth, 2001, 231: 295
[8] Liu F, Zhao D W, Yang G C.Solidification of undercooled molten Ni-based alloys[J]. Metall. Mater. Trans., 2001, 32B: 449
[9] Yang C L, Yang G C, Liu F, et al.Metastable phase formation in eutectic solidification of highly undercooled Fe83B17 alloy melt[J]. Physica, 2006, 373B: 136
[10] Lu Y P, Yang G C, Liu F, et al.The transition of alpha-Ni phase morphology in highly undercooled eutectic Ni78.6Si21.4 alloy[J]. Europhys. Lett., 2006, 74: 281
[11] Chen Y Z, Yang G C, Liu F, et al.Microstructure evolution in undercooled Fe-7.5at%Ni alloys[J]. J. Cryst. Growth, 2005, 282: 490
[12] Chen Y Z, Yang G C, Liu F, et al.Microstructural transitions of metastable phase in undercooled Fe-7.5%Ni alloy[J]. J. Cryst Growth., 2006, 289: 1
[13] Yang C, Liu F, Yang G, et al.Stability of bulk metastable Fe83B17 eutectic alloy prepared by hypercooling method[J]. Appl. Phys., 2007, 86A: 231
[14] Liu F, Yang G C.Refinement of γ' precipitate with melt undercooling in Nickel-based superalloy[J]. Mater. Trans., 2001, 42: 1135
[15] Liu F, Kirchheim R.Nano-scale grain growth inhibited by reducing grain boundary energy through solute segregation[J]. J. Cryst. Growth, 2004, 264: 385
[16] Liu F, Yang G C, Kirchheim R.Overall effects of initial melt undercooling, solute segregation and grain boundary energy on the grain size of as-solidified Ni-based alloys[J]. J. Cryst. Growth, 2004, 264: 392
[17] Chen Y Z, Liu F, Yang G C, et al.Suppression of peritectic reaction in the undercooled peritectic Fe-Ni melts[J]. Scr. Mater., 2007, 57: 779
[18] Chen Y Z, Liu F, Yang G C, et al.δ /γ transformation in non-equilibrium solidified peritectic Fe-Ni alloy[J]. Sci. China, 2007, 50G: 421
[19] Hillert M.Solidification and Casting of Metals [M]. London: The Metals Society Press, 1979: 81
[20] Dhindaw B K, Antonsson T, Fredriksson H, et al.Characterization of the peritectic reaction in medium-alloy steel through microsegregation and heat-of-transformation studies[J]. Metall. Mater. Trans., 2004, 35A: 2869
[21] ?ad?rl? E.Investigation of the microhardness and the electrical resistivity of undercooled Ni-10 at.% Si alloys[J]. J. Non-Cryst. Solids, 2011, 357: 809
[22] Lu Y P, Liu F, Yang G C, et al.Grain refinement in solidification of highly undercooled eutectic Ni-Si alloy[J]. Mater. Lett., 2007, 61: 987
[23] Fan K, Liu F, Yang G C, et al.Precipitation in as-solidified undercooled Ni-Si hypoeutectic alloy: Effect of non-equilibrium solidification[J]. Mater. Sci. Eng., 2011, A528: 6844
[24] Wang H F, Liu F, Chen Z, et al.Analysis of non-equilibrium dendrite growth in a bulk undercooled alloy melt: Model and application[J]. Acta Mater., 2007, 55: 497
[25] Dang B, Liu C C, Liu F, et al.Effect of as-solidified microstructure on subsequent solution-treatment process for A356 Al alloy[J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 634
[26] Aaron H B, Kotler G R.Second phase dissolution[J]. Metall. Trans., 1971, 2: 393
[27] Dang B, Zhang X, Chen Y Z, et al.Breaking through the strength-ductility trade-off dilemma in an Al-Si-based casting alloy[J]. Sci. Rep., 2016, 6: 30874
[28] Chen Z, Tang Y Y, Chen Q, et al.The interrelated effect of initial melt undercooling, solute trapping and solute drag on the grain growth mechanism of as-solidified Ni-B alloys[J]. J. Alloys Compd., 2014, 610: 561
[29] Furtkamp M, Gottstein G, Molodov D A, et al.Grain boundary migration in Fe-3.5% Si bicrystals with [001] tilt boundaries[J]. Acta Mater., 1998, 46: 4103
[30] Liu F, Yang G C.Rapid solidification of highly undercooled bulk liquid superalloy: Recent developments, future directions[J]. Int. Mater. Rev., 2006, 51: 145
[31] Xu X L, Liu F.Crystal growth due to recrystallization upon annealing rapid solidification microstructures of deeply undercooled single phase alloys quenched before recalescence[J]. Cryst. Growth Des., 2014, 14: 2110
[32] Chien C L, Musser D, Gyorgy E M, et al.Magnetic properties of amorphous FexB100-x (72≤x≤86) and crystalline Fe3B[J]. Phys. Rev., 1979, 20B: 283
[33] Inal O T, Keller L, Yost F G.High-temperature crystallization behaviour of amorphous Fe80B20[J]. J. Mater. Sci., 1980, 15: 1947
[34] Xu J F, Yang W, Liu F, et al.Effect of non-equilibrium solidification on subsequent solid-state transitions[J]. J. Xi'an Technol. Univ., 2009, 29: 41(许军峰, 杨伟, 刘峰等. 非平衡凝固对随后固态转变的影响[J]. 西安工业大学学报, 2009, 29: 41)
[35] Jiang J, Dézsi I, Gonser U, et al.A study of amorphous Fe79B21 alloy powders produced by chemical reduction[J]. J. Non-Cryst. Solids, 1990, 116: 247
[36] Burke J.The Kinetics of Phase Transformations in Metals [M]. Oxford: Pergamon Press, 1965
[37] Zhang H W, Wang J Q, Lu K.Kinetics of crystallization nucleation and growth in Al-rich metallic glass[J]. Acta Metall. Sin., 2002, 38: 609(张宏闻, 王建强, 卢柯. 非晶态铝合金晶化过程的形核与长大行为研究. 金属学报, 2002, 38: 609)
[38] Liu F, Yang G C.Effect of microstructure and γ' precipitate from undercooled DD3 superalloy on mechanical properties[J]. J. Mater. Sci., 2002, 37: 2713
[39] Liu F, Cai Y, Guo X F.Structure evolution in undercooled DD3 single crystal superalloy[J]. Mater. Sci. Eng., 2000, A291: 9
[40] Liu F, Guo X F, Yang G C.Recrystallization mechanism for the grain refinement in undercooled DD3 single-crystal superalloy[J]. J. Cryst. Growth, 2000, 219: 489
[41] Liebmann W K, Miller E A.Preparation, phase-boundary energies, and thermoelectric properties of InSb-Sb eutectic alloys with ordered microstructures[J]. J. Appl. Phys., 1963, 34: 2653
[42] Zhang K, Liu F, Gu B, et al.Recrystallization of as-solidified highly-undercooled Fe40Ni40B20 eutectic alloy: In situ formation of duplex structure[J]. J. Alloys Compd., 2013, 575: 444
[43] Willnecker R, Herlach D M, Feuerbacher B.Evidence of nonequilibrium processes in rapid solidification of undercooled metals[J]. Phys. Rev. Lett., 1989, 62: 2707
[44] Gu B, Liu F.Characterization of structural inhomogeneity in Al88Ce8Co4 metallic glass[J]. Acta Mater., 2016, 112: 94
[45] Song S J, Liu F.Kinetic modeling of solid-state partitioning phase transformation with simultaneous misfit accommodation[J]. Acta Mater., 2016, 108: 85
[46] Song S J, Liu F, Zhang Z H.Analysis of elastic-plastic accommodation due to volume misfit upon solid-state phase transformation[J]. Acta Mater., 2014, 64: 266
[47] Wang K, Shang S L, Wang Y, et al.Martensitic transition in Fe via Bain path at finite temperatures: A comprehensive first-principles study[J]. Acta Mater., 2018, 147: 261
[48] Hong M, Wang K, Chen Y Z, et al.A thermo-kinetic model for martensitic transformation kinetics in low-alloy steels[J]. J. Alloys Compd., 2015, 647: 763
[49] Huang L K, Lin W T, Lin B, et al.Exploring the concurrence of phase transition and grain growth in nanostructured alloy[J]. Acta Mater., 2016, 118: 306
[50] Lin B, Wang K, Liu F, et al.An intrinsic correlation between driving force and energy barrier upon grain boundary migration[J]. J. Mater. Sci. Technol., 2017, DOI: 10.1016/j.jmst.2017.11.002. (in press)
[51] Chen Z, Liu F, Yang X Q, et al.A thermokinetic description of nanoscale grain growth: Analysis of the activation energy effect[J]. Acta Mater., 2012, 60: 4833
[52] Gong M M,Castro R H R, Liu F. Modeling the final sintering stage of doped ceramics: Mutual interaction between grain growth and densification[J]. J. Mater. Sci., 2018, 53: 1680
[53] Liu F, Wang H F, Song S J, et al.Competitions correlated with nucleation and growth in non-equilibrium solidification and solid-state transformation[J]. Prog. Phys., 2012, 32: 57
[54] Kostorz G.Phase Transformations in Materials[M]. Weinheim: Wiley-VCH, 2001: 630
[55] Kelton K F.Crystal nucleation in liquids and glasses[J]. Solid State Phys., 1991, 45: 75
[56] Martyushev L M, Seleznev V D.Maximum entropy production principle in physics, chemistry and biology[J]. Phys. Rep., 2006, 426: 1
文章导航

/