坩埚尺寸和电磁频率对半固态A356铝合金浆料流动的影响
作者简介 刘 政,男,1958年生,教授,博士
收稿日期: 2017-06-26
网络出版日期: 2017-11-09
基金资助
资助项目 国家自然科学基金项目Nos.51144009和51361012,江西省自然科学基金项目No.20142bab206012以及江西省教育厅科技项目No.GJJ14407
Effects of Crucible Size and Electromagnetic Frequency on Flow During Fabrication of Semisolid A356 Al Alloy Slurry
Received date: 2017-06-26
Online published: 2017-11-09
Supported by
Supported by National Natural Science Foundation of China (Nos.51144009 and 51361012), Natural Science Foundation of Jiangxi Province (No.20142bab206012) and Science and Technology Program of the Education Department of Jiangxi Province (No.GJJ14407)
采用数值模拟方法,通过改变坩埚长短轴比例R和电磁搅拌频率研究半固态A356铝合金浆料的流动规律,以及R对半固态A356铝合金浆料初生相组织的影响。结果表明:随着R增大,半固态A356铝合金在短轴上所受的最大电磁力和最大流速呈先增大后减小的趋势,在长轴上所受的最大电磁力和最大流速呈先增大后减小再增大的现象;频率越高,短轴和长轴上所受的电磁力差和流速差越明显,因而可使熔体流动时出现“加速-减速-加速”的循环运动现象。当电磁频率和R分别为30 Hz和1.1时,坩埚长轴和短轴上的最大流速分别为153.6和143.2 mm/s,流速差最小,此时可制备出较优的半固态A356铝合金浆料。
刘政 , 陈志平 , 陈涛 . 坩埚尺寸和电磁频率对半固态A356铝合金浆料流动的影响[J]. 金属学报, 2018 , 54(3) : 435 -442 . DOI: 10.11900/0412.1961.2017.00251
A356 aluminum alloy has been widely used in semisolid processing because of its wide range of liquidus and solidus temperatures. The flow of the melt during solidification has a certain influence on the composition, solute distribution, phase morphology and crystal defects of the alloy in the solidification structure. The flow of melt is an important factor that influences the overall performance of the solidification process. The researchers use various external fields to act on the melt to induce the melt flow. Electromagnetic stirring has the characteristics of no contact, no pollution, light oxidation, less gas content and easy to control stirring parameters. It is the most popular method to fabricate semisolid alloy slurry. The electromagnetic force of the electromagnetic field can be used to study the flow phenomena of the melt. Numerical simulation combined with experimental research can get better results. The effects of crucible size and electromagnetic frequency on flow during fabrication of semisolid A356 aluminum alloy slurry under electromagnetic stirring through numerical simulation as well as the influence of crucible size on the primary phase of semisolid A356 aluminum alloy slurry induced by electromagnetic field were investigated. The results show that with the increasing of the major and minor axial ratio of crucible (R), the maximum electromagnetic force and maximum flow rate of the semisolid A356 aluminum alloy at the minor axis firstly increase and then decrease, and the maximum electromagnetic force and maximum flow rate of the semisolid A356 aluminum alloy at the major axis increase first, then decrease and then increase. The higher the electromagnetic frequency, the electromagnetic force difference and the flow rate difference of the semisolid A356 aluminum alloy at the minor axis and the major axis are apparent, so that occurs the phenomenon of "acceleration-deceleration-acceleration" in the melt flow. When the electromagnetic frequency and R are 30 Hz and 1.1 respectively, the maximum flow rate at the major axis and the minor axis of the crucible are 153.6 and 143.2 mm/s respectively, and the flow rate difference is the smallest, better semisolid A356 aluminum alloy slurry can be fabricated at this condition.
| [1] | Kang C G, Bae J W, Kim B M. The grain size control of A356 aluminum alloy by horizontal electromagnetic stirring for rheology forging [J]. J. Mater. Process. Technol., 2007, 187-188: 344 |
| [2] | Chung I G, Bolouri A, Kang C G.A study on semisolid processing of A356 aluminum alloy through vacuum-assisted electromagnetic stirring[J]. Int. J. Adv. Manuf. Technol., 2012, 58: 237 |
| [3] | Liu Z, Mao W M, Zhao Z D.Effect of pouring temperature on semi-solid slurry of A356 Al alloy prepared by weak electromagnetic stirring[J]. Trans. Nonferrous Met. Soc. China, 2006, 16: 71 |
| [4] | Barman N, Kumar P, Dutta P.Studies on transport phenomena during solidification of an aluminum alloy in the presence of linear electromagnetic stirring[J]. J. Mater. Process. Technol., 2009, 209: 5912 |
| [5] | Dao V L, Zhao S D, Lin W J.Numerical and experimental study on effect of process parameters on preparation of A356 aluminum alloy semi-solid slurry by electromagnetic stirring[J]. Int. J. Appl. Electrom., 2013, 41: 153 |
| [6] | Zhang Z F, Chen X R, Xu J, et al.Numerical simulation on electromagnetic field, flow field and temperature field in semisolid slurry preparation by A-EMS[J]. Rare Met., 2010, 29: 635 |
| [7] | Liu Z, Zhang J Y.Research on morphology evolution of different rare-earth elements on primary phase in semisolid aluminum alloy under chaotic advection[J]. J. Mech. Eng., 2016, 52(16): 77(刘政, 张嘉艺. 混沌对流中不同稀土元素对半固态铝合金初生相形貌研究 [J]. 机械工程学报, 2016, 52(16): 77) |
| [8] | Xu J F, Wei B B.Liquid phase flow and microstructure formation during rapid solidification[J]. Acta. Phys. Sin., 2004, 53: 1909(徐锦锋, 魏炳波. 急冷快速凝固过程中液相流动与组织形成的相关规律 [J]. 物理学报, 2004, 53: 1909) |
| [9] | Wang J, Zhou Y, Lan S, et al.Numerical simulation and chaotic analysis of an aluminum holding furnace[J]. Metall. Mater. Trans., 2014, 45B: 2194 |
| [10] | Liu Z, Liu X M, Hu C H, et al.Research on fractal characteristics of primary phase morphology in semi-solid A356 alloy[J]. Acta Metall. Sin.(Engl. Lett.), 2009, 22: 421 |
| [11] | Hu Z H, Wu G H, Zhang P, et al.Primary phase evolution of rheo-processed ADC12 aluminum alloy[J]. Trans. Nonferrous Met. Soc. China, 2016, 26: 19 |
| [12] | Nikrityuk P A, Eckert K, Grundmann R.A numerical study of unidirectional solidification of a binary metal alloy under influence of a rotating magnetic field[J]. Int. J. Heat Mass Transfer, 2006, 49: 1501 |
| [13] | Dadzis K, Lukin G, Meier D, et al.Directional melting and solidification of gallium in a traveling magnetic field as a model experiment for silicon processes[J]. J. Cryst. Growth, 2016, 445: 90 |
| [14] | Zhao J Z, Li H L, Zhao L.Effects of convections and motions of minority phase droplets on solidification of monotectic alloys[J]. Acta Metall. Sin., 2009, 45: 1435(赵九洲, 李海丽, 赵雷. 对流和弥散相液滴运动对偏晶合金凝固的影响 [J]. 金属学报, 2009, 45: 1435) |
| [15] | Wang J, Fautrelle Y, Nguyen-Thi H, et al.Thermoelectric magnetohydrodynamic flows and their induced change of solid-liquid interface shape in static magnetic field-assisted directional solidification[J]. Metall. Mater. Trans., 2016, 47A: 1169 |
| [16] | Wang B, Wang X D, Etay J, et al.Flow driven by an archimedean helical permanent magnetic field. Part I: Flow patterns and their transitions[J]. Metall. Mater. Trans., 2016, 47B: 1369 |
| [17] | Chowdhury J, Ganguly S, Chakraborty S.Numerical simulation of transport phenomena in electromagnetically stirred semi-solid materials processing[J]. J. Phys., 2005, 38D: 2869 |
| [18] | Chen X R, Zhang Z F, Xu J, et al.Numerical simulation of electromagnetic field, flow field and temperature field in semi-solid slurry preparation by electromagnetic stirring[J]. Chin. J. Nonferrous Met., 2010, 20: 937(陈兴润, 张志峰, 徐骏等. 电磁搅拌法制备半固态浆料过程电磁场、流场和温度场的数值模拟 [J]. 中国有色金属学报, 2010, 20: 937) |
| [19] | Tao W Y, Zhao S D, Lin W J.Numerical simulation on A356 aluminum alloy semi-solid slurry preparation with electromagnetic stirring[J]. J. Mech. Eng., 2012, 48(14): 50(陶文琉, 赵升吨, 林文捷. A356铝合金半固态浆料电磁搅拌法制备过程的数值模拟 [J]. 机械工程学报, 2012, 48(14): 50) |
| [20] | Liu Z, Zhang J Y, Yu Z F.Simulation and analysis on chaotic characteristic of flow in Al alloy melt under electromagnetic field[J]. Chin. J. Nonferrous Met., 2015, 25: 3026(刘政, 张嘉艺, 余昭福. 电磁场作用下中铝合金熔体流动的混沌特征的仿真与分析 [J]. 中国有色金属学报, 2015, 25: 3026) |
| [21] | Liu Z, Liu X M, Zhu T, et al.Effects of electromagnetic stirring with low current frequency on RE distribution in semisolid aluminum alloy[J]. Acta Metall. Sin., 2015, 51: 272(刘政, 刘小梅, 朱涛等. 低频电磁搅拌对半固态铝合金中稀土分布的影响 [J]. 金属学报, 2015, 51: 272) |
| [22] | Liu Z, Zhang J Y, Luo H L, et al.Research on morphology evolution of primary phase in semisolid A356 alloy under chaotic advection[J]. Acta Metall. Sin., 2016, 52: 177(刘政, 张嘉艺, 罗浩林等. 混沌对流下的半固态A356铝合金初生相形貌演变研究 [J]. 金属学报, 2016, 52: 177) |
| [23] | Yin J F, You Y X, Li W, et al.Numerical analysis for the characteristics of flow control around a circular cylinder with a turbulent boundary layer separation using the electromagnetic force[J]. Acta Phys. Sin., 2014, 63: 206(尹纪富, 尤云祥, 李巍等. 电磁力控制湍流边界层分离圆柱绕流场特性数值分析 [J]. 物理学报, 2014, 63: 206) |
| [24] | Bai X W, Zhang H O, Zhou X M, et al.Electromagneto-fluid coupling simulation of arc rapid prototyping process with external high-frequency magnetic field[J]. J. Mech. Eng., 2016, 52(4): 60(柏兴旺, 张海鸥, 周祥曼等. 外加高频磁场下电弧快速成形过程的电磁-流体耦合数值模拟 [J]. 机械工程学报, 2016, 52(4): 60) |
| [25] | Wang C Z, Liu F G, Zhang Y T, et al.Numerical simulation on electromagnetic, thermal and fluid fields in preparing process of semi-solid slurry[J]. J. Shenyang Univ. Technol., 2010, 32: 279(王承志, 刘凤国, 张玉妥等. 半固态浆料制备过程的电磁热流体数值模拟 [J]. 沈阳工业大学学报, 2010, 32: 279) |
| [26] | Liu H P, Xu M G, Qiu S T, et al.Numerical simulation of fluid flow in a round bloom mold with in-mold rotary electromagnetic stirring[J]. Metall. Mater. Trans., 2012, 43B: 1657 |
| [27] | Zhao Q, Zhang X G, Zhang H Y, et al.Numerical simulation of spiral magnetic field of electromgnetic stirring[J]. Chin. J. Nonferrous Met., 2014, 24: 1041(赵倩, 张兴国, 张环月等. 螺旋磁场电磁搅拌的数值模拟 [J]. 中国有色金属学报, 2014, 24: 1041) |
| [28] | Zhang J, Wang E G, Deng A Y, et al.Effects of mold EMS parameters on distributions of magnetic induction and electromagnetic force during continuous casting[J]. J. Northeastern Univ.(Nat. Sci.), 2010, 31: 1432(张 静, 王恩刚, 邓安元等. 连铸结晶器电磁搅拌参数对磁场分布的影响 [J]. 东北大学学报(自然科学版), 2010, 31: 1432) |
| [29] | Li N, Zhang R, Zhang L M, et al.Study on grain refinement mechanism of hypoeutectic Al-7%Si alloy under low voltage alternating current pulse[J]. Acta Metall. Sin., 2017, 53: 192(李宁, 张蓉, 张利民等. 低压交流电脉冲下Al-7%Si合金晶粒细化机理研究 [J]. 金属学报, 2017, 53: 192) |
/
| 〈 |
|
〉 |