Ti-6Al-4V合金熔模铸造过程中的固态相变微观组织演变的数值模拟
作者简介 邵珩,男,1989年生,博士
收稿日期: 2016-12-28
网络出版日期: 2017-06-08
基金资助
中欧航空科技合作项目,欧盟地平线2020——研究与创新框架方案, 国家重点基础研究发展计划项目No.2011CB706801, 国家自然科学基金项目Nos.51171089和51374137,国家重大科技计划项目No.2012ZX04012011及国家高技术研究发展计划项目 No.2007AA04Z141
Numerical Simulation of Microstructure Evolution During the Solid Phase Transformation of Ti-6Al-4V Alloy in Investment Casting
Received date: 2016-12-28
Online published: 2017-06-08
Supported by
Supported by China-EU (European Union) Science & Technology Cooperation in Aviation, Horizon 2020 Framework Programme for Research and Innovation (2014-2020) of EU, National Basic Research Program of China (No.2011CB706801), National Natural Science Foundation of China (Nos.51171089 and 51374137), National Science and Technology Major Project (No.2012ZX04012011) and High Technology Research and Development Program of China (No.2007AA04Z141)
针对Ti-6Al-4V合金熔模铸造固态相变过程中的微观组织演变,对α相片层的生长,采用了多组元Zener-Hillert模型计算片层边缘生长速率,根据溶质守恒,建立片层宽面的生长速率多元溶质扩散生长模型,模拟得到了多个α相集束竞争生长的微观组织。模拟结果表明,Ti-6Al-4V合金熔模铸造固态相变过程中,α相片层边缘生长受杂质元素影响较小,而在宽面上,杂质元素含量引起的过冷度占总过冷度的比例约为0.45;Ti-6Al-4V合金熔模铸造固态相变潜热约为70 kJ/kg,与JMatPro软件中的数据吻合较好。模拟得到的组织形态结果与金相组织吻合较好,模拟得到的生长速率与实验估测的速率相当。
邵珩 , 李岩 , 南海 , 许庆彦 . Ti-6Al-4V合金熔模铸造过程中的固态相变微观组织演变的数值模拟[J]. 金属学报, 2017 , 53(9) : 1140 -1152 . DOI: 10.11900/0412.1961.2016.00579
Investment casting is widely used in producting complex thin-wall titanium alloy components. In this process, the β→α phase transformation decides the final microstructures of these components. However most of present studies on phase transformation of titanium alloys focus on the microstructure evolution in heat treatment process or after deformation rather than in casting process now. It is a main reason only this work aims at the solid phase transformation of Ti-6Al-4V alloy in investment casting. In this work, the growth model of edge of α phase plates based on multi component Zener-Hiller model, and the growth model of broad face of α phase plates based on diffusion and conservation of multi components were established. The growth competition of different colonies, which consist of α phase plates in same orientation, was simulated and the microstructures and their evolution with temperature were obtained. The comparison between simulated microstructures and their evolution with temperature and experimental data indicated that the proportion of undercooling degree caused by impurities in the alloy is about 45% of the total undercooling degree in broad face of α phase plates and a much smaller portion in edge of α phase plates. The comparison also showed that the enthalpy change of solid phase transformation of titanium alloy is about 70 kJ/kg. The simulated and experimental morphologies look like similar and the simulated growth rate is also in good accordance with experiment inferred growth rate.
Key words: titanium alloy; solid phase transformation; numerical simulation
| [1] | Cui C X, Hu B M, Zhao L C, et al.Titanium alloy production technology, market prospects and industry development[J]. Mater. Des., 2011, 32: 1684 |
| [2] | Li Y H, Sun Z Q, Li X L, et al.Recent progress of biomedical porous titanium for bone implants[J]. J. Optoelect. Adv. Mater., 2014, 16: 513 |
| [3] | Zhou L.Review of titanium industry progress in America, Japan and China[J]. Rare Met. Mater. Eng., 2003, 32: 577(周廉. 美国、日本和中国钛工业发展评述[J]. 稀有金属材料与工程, 2003, 32: 577) |
| [4] | Williams J C, Starke E A Jr. Progress in structural materials for aerospace systems[J]. Acta Mater., 2003, 51: 5775 |
| [5] | Filip R, Kubiak K, Ziaja W, et al.The effect of microstructure on the mechanical properties of two-phase titanium alloys[J]. J. Mater. Process. Technol., 2003, 133: 84 |
| [6] | Jovanovi? M T, Tadi? S, Zec S, et al.The effect of annealing temperatures and cooling rates on microstructure and mechanical properties of investment cast Ti-6Al-4V alloy[J]. Mater. Des., 2006, 27: 192 |
| [7] | Sui Y W, Li B S, Liu A H, et al.Microstructures and hardness of Ti-6Al-4V alloy staging castings under centrifugal field[J]. Trans. Nonferrous Met. Soc. China, 2008, 18: 291 |
| [8] | Ahmed T, Rack H J.Phase transformations during cooling in α+β titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 206 |
| [9] | Lütjering G.Influence of processing on microstructure and mecha-nical properties of (α+β) titanium alloys[J]. Mater. Sci. Eng., 1998, A243: 32 |
| [10] | Bhattacharyya D, Viswanathan G B, Denkenberger R, et al.The role of crystallographic and geometrical relationships between α and β phases in an α/β titanium alloy[J]. Acta Mater., 2003, 51: 4679 |
| [11] | Bhattacharyya D, Viswanathan G B, Fraser H L.Crystallographic and morphological relationships between β phase and the Widmanst?tten and allotriomorphic α phase at special β grain boundaries in an α/β titanium alloy[J]. Acta Mater., 2007, 55: 6765 |
| [12] | Whittaker R, Fox K, Walker A.Texture variations in titanium alloys for aeroengine applications[J]. Mater. Sci. Technol., 2010, 26: 676 |
| [13] | He D, Zhu J C, Zaefferer S, et al.Influences of deformation strain, strain rate and cooling rate on the Burgers orientation relationship and variants morphology during β→α phase transformation in a near α titanium alloy[J]. Mater. Sci. Eng., 2012, A549: 20 |
| [14] | Katzarov I, Malinov S, Sha W.Finite element modeling of the morphology of β to α phase transformation in Ti-6Al-4V alloy[J]. Metall. Mater. Trans., 2002, 33A: 1027 |
| [15] | Yang M, Wang G, Teng C Y, et al.3D phase field simulation of effect of interfacial energy anisotropy on sideplate growth in Ti-6Al-4V[J]. Acta Metall. Sin., 2012, 48: 148(杨梅, 王刚, 滕春禹等. Ti-6Al-4V中界面能对α相片层生长的影响三维相场模拟[J]. 金属学报, 2012, 48: 148) |
| [16] | Shi R, Zhou N, Niezgoda S R, et al.Microstructure and transformation texture evolution during α precipitation in polycrystalline α/β titanium alloys——A simulation study[J]. Acta Mater., 2015, 94: 224 |
| [17] | Song K J, Wei Y H, Dong Z B, et al.Numerical simulation of β to α phase transformation in heat affected zone during welding of TA15 alloy[J]. Comp. Mater. Sci., 2013, 72: 93 |
| [18] | Jacot A, Rappaz M.A pseudo-front tracking technique for the modelling of solidification microstructures in multi-component alloys[J]. Acta Mater., 2002, 50: 1909 |
| [19] | Shi R, Ma N, Wang Y.Predicting equilibrium shape of precipitates as function of coherency state[J]. Acta Mater., 2012, 60: 4172 |
| [20] | Carman A, Zhang L C, Ivasishin O M, et al.Role of alloying elements in microstructure evolution and alloying elements behaviour during sintering of a near-β titanium alloy[J]. Mater. Sci. Eng., 2011, A528: 1686 |
| [21] | Lutjering G, Williams J C.Titanium[M]. Berlin: Springer-Verlag, 2003: 44 |
| [22] | Hillert M, H?glund L, ?gren J.Diffusion-controlled lengthening of Widmanst?tten plates[J]. Acta Mater., 2003, 51: 2089 |
| [23] | Nastac L.Numerical modeling of solidification morphologies and segregation patterns in cast dendritic alloys[J]. Acta Mater., 1999, 47: 4253 |
| [24] | Shao H, Li Y, Nan H, et al.Research on the interfacial heat transfer coeffecient between casting and ceramic shell in investment casting process of Ti6Al4V alloy[J]. Acta Metall. Sin., 2015, 51: 976(邵珩, 李岩, 南海等. 熔模铸造条件下Ti6Al4V合金铸件与陶瓷型壳间界面换热系数研究[J]. 金属学报, 2015, 51: 976) |
| [25] | Liu Z, Welsch G.Literature survey on diffusivities of oxygen, aluminum, and vanadium in alpha titanium, beta titanium, and in rutile[J]. Metall. Trans., 1988, 19A: 1121 |
| [26] | Mills K C.Recommended Values of Thermophysical Properties for Selected Commercial Alloys [M]. Cambridge: Woodhead Publishing Ltd., 2002: 211 |
/
| 〈 |
|
〉 |