U65Fe30Al5非晶合金的纳米压痕蠕变行为研究

  • 徐宏扬 ,
  • 柯海波 ,
  • 黄火根 ,
  • 张培 ,
  • 张鹏国 ,
  • 刘天伟
展开
  • 中国工程物理研究院材料研究所 江油 621907

收稿日期: 2016-07-21

  网络出版日期: 2017-04-25

基金资助

国家自然科学基金项目No.51501169,国防基础科研计划项目No.B1520133007,中国工程物理研究院科技发展基金项目Nos.2013A0301015和2014B0302047

Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy

  • Hongyang XU ,
  • Haibo KE ,
  • Huogen HUANG ,
  • Pei ZHANG ,
  • Pengguo ZHANG ,
  • Tianwei LIU
Expand
  • Institute of Materials, China Academy of Engineering Physics, Jiangyou 621907, China

Received date: 2016-07-21

  Online published: 2017-04-25

Supported by

Supported by National Natural Science Foundation of China (No.51501169), National Defense Basic Scientific Research (No.B1520133007) and Scientific and Technological Development Foundation of China Academy of Engineering Physics (Nos.2013A0301015 and 2014B0302047)

摘要

在室温下利用纳米压痕测试技术研究了峰值载荷和加载速率对U65Fe30Al5新型非晶合金蠕变行为的影响规律。结果表明,随着峰值载荷和加载速率的增加,在相同蠕变时间内,蠕变位移呈增大趋势,但当加载速率高于特定阈值时,蠕变位移不再增大。通过蠕变经验公式拟合发现,蠕变过程的应力指数随峰值载荷的增加不断变大,但随加载速率的增加先减小后基本恒定。与常规晶态合金相比,U65Fe30Al5非晶合金具有更大的应力指数,这反映出后者内部结构中富含自由体积。

本文引用格式

徐宏扬 , 柯海波 , 黄火根 , 张培 , 张鹏国 , 刘天伟 . U65Fe30Al5非晶合金的纳米压痕蠕变行为研究[J]. 金属学报, 2017 , 53(7) : 817 -823 . DOI: 10.11900/0412.1961.2016.00322

Abstract

Uranium is a valuable nuclear fuel material, but this application is unavoidably handicapped by the easy creep behavior of the metal caused by the combination of stress and irradiation in nuclear reactor. Uranium-based amorphous alloys, as a kind of potential new materials in the nuclear industry, would be challenged by this issue when used in such situation. However, creep properties of these materials have not been reported in the previous studies. In order to preliminarily investigate the creep phenomenon derived from stress function, this work is performed to study the ambient creep behavior of a new amorphous alloy U65Fe30Al5. This alloy was tested by using a nanoindentation technique under different peak loads and loading rates. The results indicate that the creep displacement gradually increases with either the peak load or the loading rate in equal creeping time, but this tendency vanishes when exceeding a critical loading rate. The fitting based on an empirical creep equation reveals that the stress exponent of the alloy ascends when raising the peak load, and firstly declines with the loading rate and then keeps constant above the critical rate. Compared with conventional crystalline alloys, the U-Co-Al alloy shows a larger stress exponent, reflecting the possible existence of rich free volume in the amorphous alloy.

参考文献

[1] Mu X Y.Creep Mechanics [M]. Xi'an: Xi'an Jiaotong University Press, 1990: 67
[1] (穆霞英. 蠕变力学[M]. 西安: 西安交通大学出版社, 1990: 67)
[2] ?adek J.Creep in Metallic Materials[M]. Amsterdam: Elsevier Science Ltd., 1988: 85
[3] Nabarro F R N, de Villiers H L. The Physics of Creep[M]. London: Taylor and Francis, 1995: 113
[4] Li W B, Henshall J L, Hooper R M, et al.The mechanisms of indentation creep[J]. Acta Metall. Mater., 1991, 39: 3099
[5] Ranaivomanana N, Multon S, Turatsinze A.Basic creep of concrete under compression, tension and bending[J]. Constr. Build. Mater., 2013, 38: 173
[6] Mahmudi R, Roumina R, Raeisinia B.Nvestigation of stress exponent in the power-law creep of Pb-Sb alloys[J]. Mater. Sci. Eng., 2004, A382: 15
[7] Gao Y, Wen S P, Wang X H, et al.Investigation on indentation creep by depth sensing indentation[J]. J. Aeronaut. Mater., 2006, 26(3): 148
[7] (高阳, 文胜平, 王晓慧等. 纳米压痕法测试压痕蠕变的应用研究[J]. 航空材料学报, 2006, 26(3): 148)
[8] Elmustafa A A, Stone D S.Strain rate sensitivity in nanoindentation creep of hard materials[J]. J. Mater. Res., 2007, 22: 2912
[9] Lucas B N, Oliver W C.Indentation power-law creep of high-purity indium[J]. Metall. Mater. Trans., 1999, 30A: 601
[10] Wang W H.The nature and properties of amorphous matter[J]. Prog. Phys., 2013, 33: 177
[10] (汪卫华. 非晶态物质的本质和特性[J]. 物理学进展, 2013, 33: 177)
[11] Huang H G, Wang Y M, Chen L, et al.Study on formation and corrosion resistance of amorphous alloy in U-Co system[J]. Acta Metall. Sin., 2015, 51: 623
[11] (黄火根, 王英敏, 陈亮等. U-Co系非晶合金的形成与耐蚀性研究[J]. 金属学报, 2015, 51: 623)
[12] Huang H G, Ke H B, Wang Y M, et al.Stable U-based metallic glasses[J]. J. Alloys Compd., 2016, 684: 75
[13] Bleiberg M L, Jones L J, Lustman B.Phase changes in pile-irradiated uranium-base alloys[J]. J. Appl. Phys., 1956, 27: 1270
[14] Elliott R O, Giessen B C.On the formation of metallic glasses based on U, Np or Pu[J]. Acta Metall., 1982, 30: 785
[15] Huang H G, Ke H B, Zhang P, et al.Effect of minor alloying on the glass formation of U-based alloys[J]. J. Alloys Compd., 2016, 688: 599
[16] Yang Y, Zeng J F, Ye J C, et al.Structural inhomogeneity and anelastic deformation in metallic glasses revealed by spherical nanoindentation[J]. Appl. Phys. Lett., 2010, 97: 261905
[17] Ma Y, Peng G J, Feng Y H, et al.Nanoindentation investigation on the creep mechanism in metallic glassy films[J]. Mater. Sci. Eng., 2016, A651: 548
[18] Huang Y J, Chiu Y L, Shen J, et al.Indentation creep of a Ti-based metallic glass[J]. J. Mater. Res., 2009, 24: 993
[19] Pang J J, Tan M J, Liew K M, et al.Nanoindentation study of size effect and loading rate effect on mechanical properties of a thin film metallic glass Cu49.3Zr50.7 [J]. Physics, 2012, 407B: 340
[20] Li H, Ngan A H W. Size effects of nanoindentation creep[J]. J. Mater. Res., 2004, 19: 513
[21] Schuh C A, Lund A C, Nieh T G.New regime of homogeneous flow in the deformation map of metallic glasses: elevated temperature nanoindentation experiments and mechanistic modeling[J]. Acta Mater., 2004, 52: 5879
[22] Spaepen F.A microscopic mechanism for steady state inhomogeneous flow in metallic glasses[J]. Acta Metall., 1977, 25: 407
[23] Argon A S.Plastic deformation in metallic glasses[J]. Acta Metall., 1979, 27: 47
[24] Cao Z H, Li P Y, Meng X K.Nanoindentation creep behaviors of amorphous, tetragonal, and bcc Ta films[J]. Mater. Sci. Eng., 2009, A516: 253
[25] Zhang H W, Jing X N, Subhash G, et al.Investigation of shear band evolution in amorphous alloys beneath a Vickers indentation[J]. Acta Mater., 2005, 53: 3849
[26] Machaka R, Derry T E, Sigalas L.Room temperature nanoindentation creep of hot-pressed B6O[J]. Mater. Sci. Eng., 2014, A607: 521
文章导航

/