Effect of Nb on the Continuous Cooling Transformation Rule and Microstructure, Mechanical Properties of Ti-Mo Bearing Microalloyed Steel

  • Xianling HE ,
  • Gengwei YANG ,
  • Xinping MAO ,
  • Chibin YU ,
  • Chuanli DA ,
  • Xiaolong GAN
Expand
  • 1 State Key Laboratory of Refractories and Metallurgy, Wuhan University of Science and Technology, Wuhan 430081, China
    2 Research and Development Institute, Wuhan Iron and Steel (Group) Co., Ltd., Wuhan 430083, China

Received date: 2016-10-05

  Online published: 2017-04-05

Supported by

Supported by China Postdoctoral Science Foundation (No.2014M562072)

摘要

利用热模拟试验机、SEM、HRTEM及EDS研究了Ti-Mo和Ti-Mo-Nb低碳微合金钢的连续冷却转变规律,探讨了Nb对Ti-Mo微合金钢组织及性能的影响。结果表明:Nb元素能够提高钢的Ac1Ac3温度,降低冷却过程中奥氏体的分解温度,缩小铁素体-珠光体相区,使贝氏体相区向左下方移动。此外,Nb的添加能够细化Ti-Mo-Nb微合金钢中的组织,提高硬度。利用HRTEM对冷速为50 ℃/s的样品进行分析,发现:Ti-Mo和Ti-Mo-Nb微合金钢中均存在少量应变诱导析出的碳化物,分别为(Ti, Mo)C和 (Ti, Nb, Mo)C粒子,呈随机分布。2种析出物均为NaCl型结构,其晶格常数分别为0.432和0.436 nm,平均粒径分别为12.11和8.69 nm。Ti-Mo-Nb微合金钢中析出相体积分数更多,尺寸更小,是其组织细化、硬度提高的主要原因。

本文引用格式

何仙灵 , 杨庚蔚 , 毛新平 , 余驰斌 , 达传李 , 甘晓龙 . Nb对Ti-Mo微合金钢连续冷却相变规律及组织性能的影响[J]. 金属学报, 2017 , 53(6) : 648 -656 . DOI: 10.11900/0412.1961.2016.00437

Abstract

In recent years, with the fast development of automotive industry, more and more attention has been focused on developing high strength automobile steels with excellent formability. The microalloying elements, such as Nb, Ti, Mo, which can facilitate grain refinement and precipitation hardening, were added into steels to achieve high strength and good formability. The Ti-Mo and Ti-Mo-Nb microalloyed high strength ferritic steel were developed. In this work, the continuous cooling transformation curves (CCT) of Ti-Mo and Ti-Mo-Nb steels were obtained. And the effect of Nb on the microstructure and mechanical properties of Ti-Mo low carbon microalloyed steel was investigated by means of SEM, HRTEM and EDS. The results showed that Nb could raise the Ac1 and Ac3 temperatures, and restrain the ferrite-pearlite and bainite transformation. Moreover, Nb could also refine the microstructure and harden the matrix of steel which attributed to the strain-induced precipitation of nano-sized (Ti, Nb, Mo)C particles identified by HRTEM and EDS. It was also found that the strain-induced precipitation of (Ti, Mo)C was existed in the Ti-Mo steel. And both of (Ti, Mo)C and (Ti, Nb, Mo)C particles were NaCl type structure. The lattice constants/the average particle sizes of (Ti, Mo)C and (Ti, Nb, Mo)C were 0.432 nm and 0.436 nm / 12.11 nm and 8.69 nm, respectively.

参考文献

[1] Shimizu T, Funakawa Y, Kaneko S.High strength steel sheets for automobile suspension and chassis use-high strength hot-rolled steel sheets with excellent press formability and durability for critical safety parts[J]. JFE Tech. Rep., 2004, 4: 25
[2] Jha G, Das S, Sinha S, et al.Design and development of precipitate strengthened advanced high strength steel for automotive application[J]. Mater. Sci. Eng., 2013, A561: 394
[3] Funakawa Y. Mechanical properties of ultra fine particle dispersion strengthened ferritic steel [J]. Mater. Sci. Forum. Trans. Tech. Publications, 2012, 706-709: 2096
[4] Wang W, Shan Y Y, Yang K.Effect of acicular ferrite microstructure composition on strength of X65 pipeline steel[J]. Acta Metall. Sin., 2007, 43: 578
[4] (王伟, 单以银, 杨柯. 超低碳微合金管线钢中针状铁素体的组成对强度的影响[J]. 金属学报, 2007, 43: 578)
[5] Mao X P, Chen Q L, Sun X J.Metallurgical interpretation on grain refinement and synergistic effect of Mn and Ti in Ti-microalloyed strip produced by TSCR[J]. J. Iron Steel Res. Int., 2014, 21: 30
[6] Zhang K, Sun X J, Yong Q L, et al.Effect of tempering time on microstructure and mechanical properties of high Ti microalloyed quenched martensitic steel[J]. Acta Metall. Sin., 2015, 51: 553
[6] (张可, 孙新军, 雍岐龙等. 回火时间对高Ti微合金化淬火马氏体钢组织及力学性能的影响[J]. 金属学报, 2015, 51: 553)
[7] Chen J, Lü M Y, Tang S, et al.Microstructure, mechanical properties and interphase precipitation behaviors in V-Ti microalloyed steel[J]. Acta Metall. Sin., 2014, 50: 524
[7] (陈俊, 吕梦阳, 唐帅等. V-Ti微合金钢的组织性能及相间析出行为[J]. 金属学报, 2014, 50: 524)
[8] Kestenbach H J, Campos S S, Morales E V.Role of interphase precipitation in microalloyed hot strip steels[J]. Mater. Sci. Technol., 2006, 22: 615
[9] Yang G W, Sun X J, Yong Q L, et al.Austenite grain refinement and isothermal growth behavior in a low carbon vanadium microalloyed steel[J]. J. Iron Steel Res. Int., 2014, 21: 757
[10] Li X L, Wang Z D.Interphase precipitation behaviors of nanometer-sized carbides in a Nb-Ti-bearing low-carbon microalloyed steel[J]. Acta Metall. Sin., 2015, 51: 417
[10] (李小琳, 王昭东. 含Nb-Ti低碳微合金钢中纳米碳化物的相间析出行为[J]. 金属学报, 2015, 51: 417)
[11] Funakawa Y, Shiozaki T, Tomita K, et al.Development of high strength hot-rolled sheet steel consisting of ferrite and nanometer-sized carbides[J]. ISIJ Int., 2004, 44: 1945
[12] Zhang Z Y, Sun X J, Li Z D, et al.Effect of nanometer-sized carbides and grain boundary density on performance of Fe-C-Mo-M(M=Nb, V or Ti) fire resistant steels[J]. Chin. J. Mater. Res., 2015, 29: 269
[12] (张正延, 孙新军, 李昭东等. 纳米级碳化物及小角界面密度对Fe-C-Mo-M (M=Nb、V或Ti)系钢耐火性的影响[J]. 材料研究学报, 2015, 29: 269)
[13] Jang J H, Heo Y U, Lee C H, et al.Interphase precipitation in Ti-Nb and Ti-Nb-Mo bearing steel[J]. Mater. Sci. Technol., 2013, 29: 309
[14] Bu F Z, Wang X M, Chen L, et al.Performance of nanosized carbides precipitation and microstructure evolution in tempering process of Ti-Nb-Mo microalloyed steel[J]. Trans. Mater. Heat Treat., 2015, 36(8): 96
[14] (卜凡征, 王学敏, 陈琳等. Ti-Nb-Mo微合金钢回火过程中纳米碳化物的析出行为及组织演变[J]. 材料热处理学报, 2015, 36(8): 96)
[15] Zhang N.Effect of Nb on microstructure of CFB/M multiphase steel [D]. Beijing: North China Electric Power University (Beijing), 2009
[15] (张楠. Nb对CFB/M复相钢组织的影响[D]. 北京: 华北电力大学(北京), 2009)
[16] Weng Y Q.Microstructure Refinement Theory and Control Technology of Ultrafine Grained Steel [M]. Beijing: Metallurgical Industry Press, 2003: 57
[16] (翁宇庆. 超细晶钢——钢的组织细化理论与控制技术 [M]. 北京: 冶金工业出版社, 2003: 57)
[17] Mecozzi M G, Sietsma J, van der Zwaag S. Analysis of γ→α transformation in a Nb micro-alloyed C-Mn steel by phase field modelling[J]. Acta Mater., 2006, 54: 1431
[18] Liu X F, Jia T, Zhu B Q.Modeling the effect of Nb on austenite→ferrite phase transformation kinetics[J]. J. Northeastern Univ.(Nat. Sci.), 2016, 37: 642
[18] (刘雪峰, 贾涛, 朱本强. Nb对奥氏体→铁素体相变动力学影响的模型[J]. 东北大学学报(自然科学版), 2016, 37: 642)
[19] Bradley J R, Aaronson H I.Growth kinetics of grain boundary ferrite allotriomorphs in Fe-C-X alloys[J]. Metall. Trans., 1981, 12A: 1729
[20] Fossaert C, Rees G, Maurickx T, et al.The effect of niobium on the hardenability of microalloyed austenite[J]. Metall. Mater. Trans., 1995, 26A: 21
[21] Yuan X Q, Liu Z Y, Jiao S H, et al.The onset temperatures of γ to α-phase transformation in hot deformed and non-deformed Nb micro-alloyed steels[J]. ISIJ Int., 2006, 46: 579
[22] Chen C Y, Yen H W, Kao F H, et al.Precipitation hardening of high-strength low-alloy steels by nanometer-sized carbides[J]. Mater. Sci. Eng., 2009, A499: 162
[23] Duan X G, Cai Q W, Wu H B.Ti-Mo ferrite matrix micro-alloy steel with nanometer-sized precipitates[J]. Acta Metall. Sin., 2011, 47: 251
[23] (段修刚, 蔡庆伍, 武会宾. Ti-Mo全铁素体基微合金高强钢纳米尺度析出相[J]. 金属学报, 2011, 47: 251)
[24] Yong Q L.Secondary Phases in Steels [M]. Beijing: Metallurgical Industry Press, 2006: 27
[24] (雍岐龙. 钢铁材料中的第二相 [M]. 北京: 冶金工业出版社, 2006: 27)
[25] Irvine K J, Pickering F B, Gladman T R.Grain-refined C-Mn steels[J]. J. Iron Steel Inst., 1967, 205: 161
[26] Nordberg H, Aromsson B.Solubility of niobium carbide in austenite[J]. J. Iron Steel Inst., 1968, 206: 1263
[27] Pavlina E J, Speer J G, van Tyne C J. Equilibrium solubility products of molybdenum carbide and tungsten carbide in iron[J]. Scr. Mater., 2012, 66: 243
[28] Xu Y, Sun M X, Zhou Y L, et al.Precipitation behavior of (Nb, Ti)C in coiling process and its effect on micro-mechanical characteristics of ferrite[J]. Acta Metall. Sin., 2015, 51: 31
[28] (徐洋, 孙明雪, 周砚磊等. (Nb, Ti)C在轧后卷取中的析出及对铁素体相微观力学特征的影响[J]. 金属学报, 2015, 51: 31)
[29] Wu J B, Liu G Q, Wang H.Effect of Nb, Ti and V on the hot deformation behavior of low carbon Nb microalloyed steels[J]. Acta Metall. Sin., 2010, 46: 838
[29] (吴晋彬, 刘国权, 王浩. Nb, Ti和V对含Nb微合金钢热变形行为的影响[J]. 金属学报, 2010, 46: 838)
文章导航

/