Mg-5Al-xCa合金的热裂行为
收稿日期: 2016-08-02
网络出版日期: 2016-12-08
基金资助
国家自然科学基金项目Nos.51504153和51571145以及辽宁省自然科学基金项目No.201602548
Hot Cracking Behavior of Mg-5Al-xCa Alloys
Received date: 2016-08-02
Online published: 2016-12-08
Supported by
Supported by National Natural Science Foundation of China (Nos.51504153 and 51571145) and Natural Science Foundation of Liaoning Province (No.201602548)
在浇注温度700 ℃、模具温度200 ℃条件下,通过热裂曲线和凝固曲线测试以及OM、XRD、SEM等手段分析了Ca加入量对Mg-5Al-xCa (x=0.5、1.0、2.0、3.0、4.0、5.0,质量分数,%)合金热裂敏感性的影响。结果表明,当Ca加入量增加到4.0%时,合金的热裂敏感性随着Ca加入量的增加而减小;Mg-5Al-4.0Ca合金的热裂敏感性最小,其热裂敏感性系数仅为0.824;Ca加入量增加到5.0%时,合金的热裂敏感性又出现上升,其热裂敏感性系数上升到0.96。加入适量的Ca会降低Mg-5Al-xCa合金凝固时α-Mg的析出温度,并抑制Mg17Al12相形成,缩小合金凝固温度范围,增加组织中的共晶含量,有利于合金凝固后期的补缩,从而降低合金的热裂敏感性。但加入过多的Ca会增加含Ca脆性相的数量,并使合金组织发生粗化,从而导致合金的热裂敏感性增加。
关键词: Mg-Al-Ca合金; 热裂敏感性; 凝固曲线; 显微组织
王峰 , 董海阔 , 王志 , 毛萍莉 , 刘正 . Mg-5Al-xCa合金的热裂行为[J]. 金属学报, 2017 , 53(2) : 211 -219 . DOI: 10.11900/0412.1961.2016.00353
Mg-Al-Ca base alloys have great potential for application because of its low cost and good high temperature creep properties, but its higher hot cracking susceptibility greatly limits the application of the alloy. The effect of Ca addition on the hot cracking susceptibility of Mg-5Al-xCa (x=0.5, 1.0, 2.0, 3.0, 4.0, 5.0, mass fraction, %) alloys at the pouring temperature 700 ℃ and mold temperature 200 ℃ was studied by using hot cracking curve test, solidification curve test, OM, XRD and SEM. The results showed that the hot cracking susceptibility of alloys decreased with increasing Ca addition until to 4.0%, and the Mg-5Al-4.0Ca alloy had minimal hot cracking susceptibility, which cracking susceptibility coefficient was only 0.824. But when Ca addition increased to 5.0%, the hot cracking susceptibility of the alloy increased, and the cracking susceptibility coefficient increased to 0.96. The appropriate Ca addition can reduce the precipitation temperature of α-Mg in Mg-5Al-xCa alloys, inhibit precipitation of Mg17Al12 phase, narrow solidification temperature range of the alloy and increase eutectic content, which are helpful for the alloy having a stronger ability of compensation at the solidification end to decrease hot cracking susceptibility. But excessive Ca addition will increase the numbers of brittle phases containing Ca and coarsen the microstructure, resulting in the increase of hot cracking susceptibility.
| [1] | Liu Z, Wang Z G, Wang Y, et al.Application and developing tendency of magnesium die casting alloys in automobile industry[J]. Spec. Cast. Nonferrous Alloys, 2002, 22(S1): 300 |
| [1] | (刘正, 王中光, 王越等. 压铸镁合金在汽车工业中的应用和发展趋势[J]. 特种铸造及有色合金, 2002, 22(S1): 300) |
| [2] | Lou Y, Bai X, Li L X.Effect of Sr addition on microstructure of as-cast Mg-Al-Ca alloy[J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 1247 |
| [3] | Suzuki A, Saddock N D, Jones J W, et al.Solidification paths and eutectic intermetallic phases in Mg-Al-Ca ternary alloys[J]. Acta Mater., 2005, 53: 2823 |
| [4] | Zhang J, Feng Y C, Wang Q, et al.Effects of different Ca and Nd addition on corrosion resistance of Mg-6Al alloys[J]. Spec. Cast. Nonferrous Alloys, 2015, 35: 430 |
| [4] | (张靖, 冯义成, 王琴等. 不同Ca和Nd含量对Mg-6Al合金腐蚀性能的影响[J]. 特种铸造及有色合金, 2015, 35: 430) |
| [5] | Bai J, Sun Y S, Xue F, et al.Microstructures and creep properties of Mg-6Al-(Sr, Ca) alloys[J]. Acta Metall. Sin., 2006, 42: 1267 |
| [5] | (白晶, 孙扬善, 薛烽等. Mg-6Al-(Sr, Ca)合金的显微组织和蠕变性能[J]. 金属学报, 2006, 42: 1267) |
| [6] | Li H Y, Bai Y Y, Zhang H T, et al.Effect of Mn on hot cracking tendency of Mg-6.5Zn alloys[J]. Acta Metall. Sin., 2014, 50: 1237 |
| [6] | (李浩宇, 柏媛媛, 张海涛等. Mn对Mg-6.5Zn合金热裂倾向性的影响[J]. 金属学报, 2014, 50: 1237) |
| [7] | Liang W Z, Ji Z S, Zuo F, et al.Present research status and developing tendency of heat resistance Mg alloy[J]. Spec. Cast. Nonferrous Alloys, 2003, 23(2): 39 |
| [7] | (梁维中, 吉泽升, 左锋等. 耐热镁合金的研究现状及发展趋势[J]. 特种铸造及有色合金, 2003, 23(2): 39) |
| [8] | Luo A H, Sachdev A K, Powell B R.Advanced casting technologies for lightweight automotive applications[J]. Foundry, 2011, 60: 113 |
| [8] | (罗爱华, Sachdev A K, Powell B R.汽车轻量化先进铸造技术[J]. 铸造, 2011, 60: 113) |
| [9] | Cao G, Kou S.Hot tearing of ternary Mg-Al-Ca alloy castings[J]. Metall. Mater. Trans., 2006, 37A: 3647 |
| [10] | Cao G, Kou S.Hot cracking of binary Mg-Al alloy castings[J]. Mater. Sci. Eng., 2006, A417: 230 |
| [11] | Qiu K Q, Tao S R, Re Y, et al.Effect of Ca on the hot tearing susceptibility of Mg-7Al-2Si casting alloys[J]. Spec. Cast. Nonferrous Alloys, 2013, 33: 186 |
| [11] | (邱克强, 陶思伟, 热焱等. Ca对Mg-7Al-2Si合金热裂倾向的影响[J]. 特种铸造及有色合金, 2013, 33: 186) |
| [12] | Huang H, Fu P H, Peng L M, et al.Effect of mould temperature and pouring temperature on the hot tearing and fluidity of AZ91D magnesium alloy[J]. Spec. Cast. Nonferrous Alloys, 2012, 32: 81 |
| [12] | (黄皓, 付彭怀, 彭立明等. 模具温度和浇注温度对AZ91D镁合金热裂和流动性能的影响[J]. 特种铸造及有色合金, 2012, 32: 81) |
| [13] | Suzuki A, Saddock N D, Jones J W, et al.Phase equilibria in the Mg-Al-Ca ternary system at 773 and 673 K[J]. Metall. Mater. Trans., 2006, 37A: 975 |
| [14] | Clyne T W, Wolf M, Kurz W.The effect of melt composition on solidification cracking of steel, with particular reference to continuous casting[J]. Metall. Trans., 1982, 13B: 259 |
| [15] | Clyne T W, Davies G J.The influence of composition on solidification cracking susceptibility in binary alloy systems[J]. Brit. Found., 1981, 74: 65 |
| [16] | Hou D H, Liang S M, Chen R S, et al.Solidification behavior and grain size of sand casting Mg-6Al-xZn alloys[J]. Acta Metall. Sin., 2015, 50: 601 |
| [16] | (侯丹辉, 梁松茂, 陈荣石等. 砂型铸造Mg-6Al-xZn合金凝固行为及晶粒尺寸[J]. 金属学报, 2015, 50: 601) |
| [17] | Xu S W, Matsumoto N, Yamamoto K, et al.High temperature tensile properties of as-cast Mg-Al-Ca alloys[J]. Mater. Sci. Eng., 2009, A509: 105 |
| [18] | Yang G Y, Hao Q T, Jie W Q, et al.Effect of Ca addition on the microstructure and mechanical properties of Mg-5Al-0.4Zn casting alloy[J]. Acta Metall. Sin., 2005, 41: 933 |
| [18] | (杨光昱, 郝启堂, 介万奇等. Ca加入量对Mg-5Al-0.4Zn基铸造合金组织与力学性能的影响[J]. 金属学报, 2005, 41: 933) |
| [19] | TerBush J R, Chen O H, Jones J W, et al. The dependence of creep behavior on elemental partitioning in Mg-5Al-3Ca-xSn alloys[J]. Metall. Mater. Trans., 2012, 43A: 3120 |
| [20] | Liang S M, Zhang H W, Xia M X, et al.Microstructure and mechanical properties of melt-conditioned high-pressure die-cast Mg-Al-Ca alloy[J]. Trans. Nonferrous Met. Soc. China, 2010, 20: 1205 |
| [21] | Liu Z, Zhang S B, Mao P L, et al.Effects of Y on hot tearing susceptibility of Mg-Zn-Y-Zr alloys[J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 907 |
| [22] | Zhang D T, Suzuki M, Maruyama K.Study on the texture of a friction stir welded Mg-Al-Ca alloy[J]. Acta Metall. Sin.(Engl. Lett.), 2006, 19: 335 |
| [23] | Wang S Y, Wang Q D, Ding W J, et al.Research development of hot tear mechanism for cast alloys[J]. Spec. Cast. Nonferrous Alloys, 2000, 20(2): 48 |
| [23] | (王业双, 王渠东, 丁文江等. 合金的热裂机理及其研究进展[J]. 特种铸造及有色合金, 2000, 20(2): 48) |
| [24] | Ding H, Fu H Z, Liu Z Y, et al.Compensation of solidification contraction and hot cracking tendency of alloys[J]. Acta Metall. Sin., 1997, 33: 921 |
| [24] | (丁浩, 傅恒志, 刘忠元等. 凝固收缩补偿与合金的热裂倾向[J]. 金属学报, 1997, 33: 921) |
| [25] | Zhang Z M, Lü T, Xu C J, et al.Microstructure of binary Mg-Al eutectic alloy wires produced by the Ohno continuous casting process[J]. Acta Metall. Sin.(Engl. Lett.), 2008, 21: 275 |
/
| 〈 |
|
〉 |