MODELING OF ISOTHERMAL AUSTENITE TO FERRITE TRANSFORMATION IN A Fe-CALLOY BY PHASE-FIELD METHOD

  • Jun ZHANG ,
  • Chengwu ZHENG ,
  • Dianzhong LI
Expand
  • 1 School of Chemistry and Materials Science, University of Science and Technology of China, Hefei 230026, China
    2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China;

Received date: 2015-12-17

  Online published: 2016-06-01

Supported by

Supported by National Natural Science Foundation of China (Nos.51371169 and 51401214)

摘要

运用相场法研究了Fe-C合金在临界区等温过程中发生的奥氏体-铁素体相变过程. 通过分析铁素体生长过程中C的扩散行为, 发现奥氏体-铁素体相变表现为混合控制生长的特征, 奥氏体/铁素体相界面处于非平衡状态. 进一步研究了不同等温温度(1010, 1048和 1087 K)下奥氏体-铁素体相变的微观组织和C浓度场的演化情况. 结果表明, 随着等温温度的降低, 铁素体形核率增加, 铁素体相变平衡体积分数增加, 但奥氏体内部C浓度分布的不均匀程度加剧, 1010 K等温时的微观组织呈现为不规则细小铁素体晶粒围绕分散分布的残余奥氏体的两相结构. 随着等温温度的降低, 奥氏体-铁素体相变过程表现出由扩散控制生长模式向界面控制生长模式转化的趋势.

本文引用格式

张军 , 郑成武 , 李殿中 . 相场法模拟Fe-C合金中奥氏体-铁素体等温相变过程*[J]. 金属学报, 2016 , 52(11) : 1449 -1458 . DOI: 10.11900/0412.1961.2015.00651

Abstract

Austenite-to-ferrite transformation in modern steels is a key metallurgical phenomenon as it can be exploited to produce microstructures that are closely associated with significant improvement of their properties. Both experimental and theoretical studies of this transformation have received much attention. In particular, in recent years, considerable efforts have been directed to the development of numerical models for adequate quantitative descriptions of the nucleation and growth of ferrite grains as well as the overall transformation kinetics. In this work, a modified multi-phase field model has been developed to simulate the isothermal γ-α transformation in a Fe-C alloy. This model takes both the effect of a finite interface mobility and a finite diffusivity into account, which hence enables a clear description of the mixed-mode nature of the transformation. In contrast to the diffusion-controlled phase transformation model, the carbon concentration in front of the moving γ-α interface is found to be non-equilibrium under this circumstance. In order to study the microstructural behavior and kinetics over the entire temperature range of the phase transformation, three different isothermal transformation processes have been imulated. The simulation results indicate that the nucleation density of ferrite increases with decreasing the temperature, which thus leads to a larger volume fraction of ferrite. However, the heterogeneous distribution of carbon in the untransformed austenite is intensified. The final microstructural product of the transformation at low temperature of 1010 K consists of fine residual austenite islands surrounded by fine polygonal ferrite. The simulation results also indicate that the transformation mode from austenite to ferrite varies from essentially diffusion-controlled at high temperature towards interface-controlled at low temperature.

参考文献

[1] Offerman S E, van Dijk N H, Sietsma J, Lauridsen E M, Margulies L, Grigull S, Poulsen H F, van der Zwaag S.Acta Mater, 2004; 52: 4757
[2] Zener C. J Appl Phys, 1949; 20: 950
[3] Christian J W.The Theory of Transformations in Metals and Alloys. 3rd Ed., Oxford: Elsevier Science, 2002: 1
[4] Sietsma J, van der Zwaag S.Acta Mater, 2004; 52: 4143
[5] Kumar M, Sasikumar R, Nair P K.Acta Mater, 1998; 46: 6291
[6] Zhang L, Zhang C B, Wang Y M, Wang S Q, Ye H Q.Acta Mater, 2003; 51: 5519
[7] Lan Y J, Li D Z, Li Y Y.Acta Mater, 2004; 52: 1721
[8] Tong M M, Li D Z, Li Y Y.Acta Mater, 2005; 53: 1485
[9] Steinbach I, Pezzolla F, Nestler B, See?elberg M, Prieler R, Schmitz G J, Rezende J L L.Physica, 1996; 94D: 135
[10] Chen L Q.Annu Rev Mater Res, 2002; 32: 113
[11] Warren J A, Kobayashi R, Lobovsky A E, Carter W C.Acta Mater, 2003; 51: 6035
[12] Boettger B, Apel M, Eiken J, Schaffnit P, Steinbach I.Steel Res Int, 2008; 79: 608
[13] Gao Y J, Luo Z R, Hu X Y, Huang C G.Acta Metall Sin, 2010; 46: 1161
[13] (高英俊, 罗志荣, 胡项英, 黄创高. 金属学报, 2010; 46: 1161)
[14] Zhao Y, Zhang H Y, Wei H, Zheng Q, Jin T, Sun X F.Acta Metall Sin, 2013; 49: 981
[14] (赵彦, 张宏宇, 韦华, 郑启, 金涛, 孙晓峰. 金属学报, 2013; 49: 981)
[15] Ke C B, Ma X, Zhang X P.Acta Metall Sin, 2010; 46: 84
[15] (柯常波, 马骁, 张新平. 金属学报, 2010; 46: 84)
[16] Zhou G Z, Wang Y X, Chen Z.Acta Metall Sin, 2012; 48: 485
[16] (周广钊, 王永欣, 陈铮. 金属学报, 2012; 48: 485)
[17] Loginova I, ?gren J, Amberg G.Acta Mater, 2004; 52: 4055
[18] Mecozzi M G, Sietsma J, van der Zwaag S, Apel M, Schaffnit P, Steinbach I.Metall Mater Trans, 2005; 36A: 2327
[19] Huang C J, Browne D J, McFadden S.Acta Mater, 2006; 54: 11
[20] Moelans N.Acta Mater, 2011; 59: 1077
[21] Moelans N, Blanpain B, Wollants P.Phys Rev, 2008; 78B: 1098
[22] Eiken J, B?ttger B, Steinbach I.Phys Rev, 2006; 73E: 066122
[23] Gustafson P.Metall Trans, 1987; 18A: 175
[24] Umemoto M, Hiramatsu A, Moriya A, Watanabe T, Nanba S, Nakajima N, Anan G, Higo Y.ISIJ Int, 1992; 32: 306
[25] Zheng C W, Xiao N M, Hao L H, Li D Z, Li Y Y.Acta Mater, 2009; 57: 2956
[26] Du Q, Faber V, Gunzburger M.SIAM Rev, 1999; 41: 637
[27] Chandra R, Dagum L, Kohr D, Maydan D, McDonald J, Menon R. Parallel Programming in Open MP. San Mateo: Morgan Kaufmann Publishers, 2000: 1
[28] Chen H, van der Zwaag S.Acta Mater, 2014; 72: 1
[29] van Leeuwen Y, Sietsma J, van der Zwaag S.ISIJ Int, 2003; 43: 767
[30] van Bohemen S M C, Bos C, Sietsma J.Metall Mater Trans, 2011; 42A: 2609
文章导航

/

〈 〉