连续加热条件下过共析钢奥氏体化研究

  • 李俊杰 ,
  • Godfrey Andrew ,
  • 刘伟 ,
  • 张弛
展开
  • 清华大学材料学院先进材料教育部重点实验室, 北京 100084
null

李俊杰, 男, 1987年生, 博士生

修回日期: 2014-02-19

  网络出版日期: 2014-10-25

INVESTIGATION OF AUSTENITIZATION DURING CONTINUOUS HEATING PROCESS IN HYPEREUTECTOID STEELS

  • Junjie LI ,
  • Andrew Godfrey ,
  • Wei LIU ,
  • Chi ZHANG
Expand
  • Key Laboratory of Advanced Materials, Ministry of Education, School of Materials Science and Engineering, Tsinghua University, Beijing 100084

Revised date: 2014-02-19

  Online published: 2014-10-25

摘要

采用热膨胀仪和差示扫描量热仪(DSC)研究了过共析钢在连续加热条件下奥氏体化过程, 测定了不同阶段的临界温度点, 通过Thermo-Calc与Dictra软件进行了理论计算, 并且研究了加热速率、初始组织以及含C量对其的影响. 结果表明, 整个连续加热过程可以分为5个阶段, 临界温度点的实验结果与计算结果基本吻合. 提高加热速率可以提高逆共析转变的起始和终了温度, 增大逆共析转变温度区间, 残余渗碳体溶解终了温度不变, 奥氏体均匀化终了温度升高. 粗大的珠光体初始组织使得逆共析转变起始和终了温度提高, 增大了逆共析转变的温度区间, 残余渗碳体溶解和奥氏体均匀化阶段的终了温度也有所提高. 增大含C量对逆共析转变几乎没有影响, 但是会明显提高残余渗碳体和奥氏体均匀化阶段终了的温度.

本文引用格式

李俊杰 , Godfrey Andrew , 刘伟 , 张弛 . 连续加热条件下过共析钢奥氏体化研究[J]. 金属学报, 2014 , 50(10) : 1179 -1188 . DOI: 10.11900/0412.1961.2014.00078

Abstract

Cold-drawn pearlitic steel wires exhibit ultrahigh strength and have important applications where high strength and wear resistance are required. The hypereutectoid compositions present a promising potential for increasing the mechanical properties, especially the strength. The austenitization process strongly influences the following pearlitic microstructure and thus the mechanical properties. Continuous heating is always used in the industrial processing. However, the austenitization of pearlite in hypereutectoid steels during continuous heating has not been investigated systematically. In this work, the dilatometer and DSC were employed to investigate the austenitization kinetics of hypereutectoid steels during continuous heating. Microstructure evolution was observed with SEM and EBSD. The dilatometer and DSC curves were analyzed with derivative method. The whole austenitization can be divided into five stages: initial microstructure, reverse eutectoid transformation, retained cementite dissolution, homogenization and homogeneous austenite. Tangent method was used for measuring the critical temperatures of different stages. Experimental determination of transformed fraction was obtained through the lever method. Calculation with Thermo-Calc and Dictra software was carried out for the austenitization and considered to be a reasonable result by comparing with the experimental data. There is a turning point for the reduction rate of cementite and formation of austenite at the finishing temperature of reverse eutectoid transformation, which is similar with the austenitization in low carbon steel and spheroidal pearlite of hypereutectoid steel. Effects of heating rates, initial microstructure and carbon content were studied by varying the relevant parameters. Higher heating rate increases the starting and finishing temperatures of reverse eutectoid transformation and widens the temperature range, has no effect on the finishing temperature of retained cementite dissolution, increases the finishing temperature of homogenization. Coarser initial pearlitic microstructure increases the starting and finishing temperatures, widens the temperature range for reverse eutectoid transformation, increases the finishing temperature for retained cementite dissolution and homogenization. Enhancement of carbon content has little effect on the reverse eutectoid transformation, but increases the finishing temperature for retained cementite dissolution and homogenization. The effects mentioned above on the austenitization kinetics were discussed for mechanism analysis and compared with the observations of relevant systems provided by other research.

参考文献

[1] Li Y J, Choi P, Goto S, Borchers C, Raabe D, Kirchheim R. Acta Mater, 2012; 60: 4005
[2] Tashiro H. Nipp Steel Technol Rep, 1999; 80: 6
[3] Choi H C, Park K T. Scr Mater, 1996; 34: 857
[4] Taleff E M, Sridhar G B, Pourladian B. Wire J Int, 2003; 36: 73
[5] Bae C M, Nam W J, Lee C S. Metall Mater Trans, 2000; 31A: 2665
[6] Li J J, Godfrey A, Liu W. Acta Metall Sin, 2013; 49: 583
[6] (李俊杰, Godfrey Andrew, 刘 伟. 金属学报, 2013; 49: 583)
[7] Lee S J, Park J S, Lee Y K. Scr Mater, 2008; 59: 87
[8] Chae J Y, Jang J H, Zhang G, Kim K H, Lee J S, Bhadeshia H, Suh D W. Scr Mater, 2011; 65: 245
[9] San Martin D, Rivera-Diaz-Del-Castillo P E J, Garcia-De-Andres C. Scr Mater, 2008; 58: 926
[10] Shtansky D V, Nakai K, Ohmori Y. Acta Mater, 1999; 47: 2619
[11] Karmazin L, Krejci J. Mater Sci Eng, 1994; A185: 5
[12] De Andres C , Caballero F G, Capdevila C, Alvarez L F. Mater Charact, 2002; 48: 101
[13] Gupta C, Dey G K, Chakravartty J K, Srivastav D, Banerjee S. Scr Mater, 2005; 53: 559
[14] Xu G, Wan L, Yu S F, Liu L, Luo F. Mater Lett, 2008; 62: 3978
[15] Li Z D, Miyamoto G, Yang Z G, Furuhara T. Metall Mater Trans, 2011; 42A: 1586
[16] Yang Z N, Yang Z G, Xia Y, Zhang C. Acta Metall Sin, 2013; 49: 890
[16] (杨泽南, 杨志刚, 夏 苑, 张 弛. 金属学报, 2013; 49: 890)
[17] Xia Y, Enomoto M, Yang Z G, Li Z D, Zhang C. Philos Mag, 2013; 93: 1095
[18] Han K, Mottishaw T D, Smith G, Edmonds D V, Stacey A G. Mater Sci Eng, 1995; A190: 207
[19] Zhang Y D, Esling C, Gong M L, Vincent G, Zhao X, Zuo L. Scr Mater, 2006; 54: 1897
[20] Walentek A, Seefeldt M, Verlinden B, Aernoudt E, Van Houtte P. J Microsc, 2006; 224: 256
[21] Farahat A. J Mater Process Technol, 2008; 204: 365
[22] Liu Y C, Sommer F, Mittemeijer E J. Acta Mater, 2006; 54: 3383
[23] Liu Y C, Sommer F, Mittemeijer E J. Acta Mater, 2003; 51: 507
[24] Oliveira F L G, Andrade M S, Cota A B. Mater Charact, 2007; 58: 256
[25] Scheil E. Arch Eisenhutten, 1935; 8: 565
[26] Li Z D, Miyamoto G, Yang Z G, Furuhara T. Scr Mater, 2009; 60: 485
[27] Caballero F G, Capdevila C, de Andres C G. Mater Sci Technol, 2001; 17: 686
[28] Caballero F G, Capdevila C, de Andres C . Metall Mater Trans, 2001; 32A: 1283
文章导航

/

〈 〉