模拟工业-海岸大气中SO2对Q235B钢腐蚀行为的影响*
陈文娟, 女, 1986年生, 博士生
收稿日期: 2013-11-15
修回日期: 2014-03-13
网络出版日期: 2014-07-20
基金资助
* 国家自然科学基金项目 51201170和 51131007资助
EFFECT OF SO2 ON CORROSION EVOLUTION OF Q235B STEEL IN SIMULATED COASTAL- INDUSTRIAL ATMOSPHERE
Received date: 2013-11-15
Revised date: 2014-03-13
Online published: 2014-07-20
Supported by
Supported by National Natural Science Foundation of China (Nos.51201170 and 51131007)
陈文娟 , 郝龙 , 董俊华 , 柯伟 , 文怀梁 . 模拟工业-海岸大气中SO2对Q235B钢腐蚀行为的影响*[J]. 金属学报, 2014 , 50(7) : 802 -810 . DOI: 10.3724/SP.J.1037.2013.00738
采用循环干/湿模拟腐蚀增重实验、动电位极化曲线、电化学阻抗谱和XRD方法, 研究了模拟海岸-工业大气中SO2对Q235B钢腐蚀行为的影响. 结果表明, 在腐蚀初期SO2抑制了Q235B钢的腐蚀; 在腐蚀后期, SO2促进了Q235B钢的腐蚀. 当SO2的浓度较低时, 腐蚀速率随SO2浓度的升高而增大; 当SO2的浓度较高时, 腐蚀速率随SO2浓度的升高而减小. 工业-海岸大气中的SO2组分可以抑制腐蚀产物中g -FeOOH和b -FeOOH的生成, 而促进a -FeOOH生成. 低碳钢腐蚀速率随SO2浓度变化出现的极值现象与SO2导致的锈层相组分变化密切相关.
| [1] | Leygraf C, Graedel T. Atmospheric Corrosion. New York: John Wiley & Sons, 2000: 10 |
| [2] | Singh D D N, Yadav S, Saha J K. Corros Sci, 2008; 50: 93 |
| [3] | Casta?o J G, Botero C A, Restrepo A H, Agudelo E A, Correa E, Echeverría F. Corros Sci, 2010; 52: 216 |
| [4] | Hou W, Liang C. Corrosion, 1999; 55: 65 |
| [5] | Zhang Q C, Wu J S, Wang J J, Zheng W L, Li A B. Mater Chem Phys, 2002; 77: 603 |
| [6] | Mendoza A R, Corvo F. Corros Sci, 1999; 41: 75 |
| [7] | Dawson J L, Ferreira M G S. Corros Sci, 1986; 26: 1009 |
| [8] | Weissenrieder J, Leygraf C. J Electrochem Soc, 2004; 151: B165 |
| [9] | Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2012; 58: 175 |
| [10] | Dong J H. Corros Sci Prot Technol, 2010; 22: 261 |
| [10] | (董俊华. 腐蚀科学与防护技术, 2010; 22: 261) |
| [11] | Hao L, Zhang S X, Dong J H, Ke W. Metall Mater Trans, 2012; 43: 1724 |
| [12] | Wang J H, Wei F I, Chang Y S, Shih H C. Mater Chem Phys, 1997; 47: 1 |
| [13] | Misawa T, Hashimoto K, Shimodaira S. Corros Sci, 1974; 14: 131 |
| [14] | Evans U R, Taylor C A J. Corros Sci, 1972; 12: 227 |
| [15] | Saha J K. Corrosion of Constructional Steels in Marine and Industrial Environment. Heidelberg: Springer, 2013: 13 |
| [16] | Fuente D D L, Díaz I, Simancas J, Chico B, Morcillo M. Corros Sci, 2011; 53: 604 |
| [17] | Chen Y Y, Tzeng H J, Wei L I, Shih H C. Mater Sci Eng, 2005; A398: 47 |
| [18] | Ishikawa T, Katoh R, Yasukawa A, Kandori K, Nakayama T, Yuse F. Corros Sci, 2001; 43: 1727 |
| [19] | Asami K, Kikuchi M. Corros Sci, 2003; 45: 2671 |
| [20] | Shiotani K, Tanimoto W, Maeda C, Kawabata F, Amano K. Corros Eng, 2000; 49: 67 |
| [21] | Allam I M, Arlow J S, Saricimen H. Corros Sci, 1991; 32: 417 |
| [22] | Dong J H, Han E H, Ke W. Sci Technol Adv Mater, 2007; 8: 559 |
| [23] | Melchers R E. Corros Sci, 2008; 50: 3446 |
| [24] | Stramann M, Bohnenkamp K, Engell H J. Corros Sci, 1983; 23: 969 |
| [25] | Vaynman S, Guico R S, Fine M E, Manganello S J. Metall Mater Trans, 1997; 28A: 1274 |
| [26] | Mansfeld F. Corrosion, 1988; 44: 856 |
| [27] | Mansfeld F, Lin S, Chen Y C. J Electrochem Soc, 1988; 135: 906 |
| [28] | Stern M, Geary A L. J Electrochem Soc, 1957; 104: 56 |
| [29] | Revie R W, Uhlig H H. Corrosion and Corrosion Control. 4th Ed., New York: John Wiley & Sons, 2008: 115 |
| [30] | Stratmann M, Streckel H, Kim K T, Crockett S. Corros Sci, 1990; 30: 715 |
| [31] | Zhang S H, Lyon S B. Corros Sci, 1993; 35: 713 |
| [32] | Frankel G S, Stratmann M, Rohwerder M, Michalik A, Maier B, Dora J, Wicinski M. Corros Sci, 2007; 49: 2021 |
/
| 〈 |
|
〉 |