Inconel 625熔敷金属中δ相的形核与粗化机理*

  • 邸新杰 ,
  • 邢希学 ,
  • 王宝森
展开
  • 1 天津大学天津市现代连接技术重点实验室, 天津 300072
    2 天津大学材料科学与工程学院,天津300072
    3 宝山钢铁股份有限公司宝钢研究院, 上海 201900
null

邸新杰, 男, 1973年生, 副教授, 博士

收稿日期: 2013-07-08

  修回日期: 2013-08-09

  网络出版日期: 2014-03-20

基金资助

*天津市自然科学基金项目 11JCYBJC06000 和天津市科技支撑重点项目 11ZCGYSF00100资助

NUCLEATION AND COARSENING MECHANISM OF δ PHASE IN INCONEL 625 DEPOSITED METAL

  • Xinjie DI ,
  • Xixue XING ,
  • Baosen WANG
Expand
  • 1 Tianjin Key Laboratory of Advanced Joining Technology, Tianjin University, Tianjin 300072
    2 School of Materials Science and Engineering, Tianjin University, Tianjin 300072
    3 Baosteel Research Institute, Baoshan Iron & Steel Co., Ltd., Shanghai 201900

Received date: 2013-07-08

  Revised date: 2013-08-09

  Online published: 2014-03-20

Supported by

Supported by Tianjin Natural Science Foundation (No.11JCYBJC06000) and Key Project of Tianjin Municipal Science and Technology Support Program (No.11ZCGYSF00100)

摘要

利用扫描电镜(SEM)和透射电镜(TEM)研究了Inconel 625熔敷金属中δ相的形成机理, 并揭示了焊后热处理(PWHT)过程中δ相粗化的内在规律. 结果表明, 经850 ℃焊后热处理的Inconel 625熔敷金属中大量析出的针条状δ相呈网格状分布在基体γ相中, 且其附近出现了贫γ"相区域. δ相的形成是一个类贝氏体转变的固态相变过程, 其晶核是在γ"相密排面的层错上通过切变方式形成的. 同时, δ相的粗化行为是扩散控制的长大过程. 保温时间较短时, 实际δ相颗粒的平均尺寸符合LSW理论, 随着保温时间的延长, δ相的高密度、不同向析出特征使得其实际尺寸偏离了经典LSW理论的预测值.

本文引用格式

邸新杰 , 邢希学 , 王宝森 . Inconel 625熔敷金属中δ相的形核与粗化机理*[J]. 金属学报, 2014 , 50(3) : 323 -328 . DOI: 10.3724/SP.J.1037.2013.00383

Abstract

Using Inconel 625 wire to weld high yield strength steels or stainless steels that commonly used in nuclear power plant components and gas turbines can significantly improve high temperature mechanical properties and corrosion resistance of weld structure. However, toughness, fatigue strength and creep rupture strength of weld would decline obviously because of the precipitation of δ phase during service at elevated temperatures for a long time. This work aims to investigate nucleation mechanism of δ phase in Inconel 625 deposited metal by means of SEM and TEM. Meanwhile, coarsening inherent law of δ phase during post-weld heat treatment (PWHT) at 850 ℃ for 2, 4 and 8 h respectively was revealed. The results indicate that a large number of needle-like δ phase precipitates in Inconel 625 deposited metal after PWHT at 850 ℃. These δ phases appear a grid-like distribution in γ-matrix, and there are some poor γ" phase regions appearing near δ phase. Formation process of δ phase is a solid phase transformation process which is like bainite transformation in steels. Crystal nucleus of δ phase form in the close-packed plane of γ" phase by shear mode, and coarsening behavior of δ phase is a diffusion-controlled growth process. When PWHT holding time is shorter, actual average size of δ phase is in line with LSW theory. With PWHT holding time extending, its actual average size deviates from the predicted value of classical LSW theory, because of the high-density and non-directional precipitation characteristics of δ phase.

参考文献

[1] Special Metals Corporation Products. INCONEL? alloy 625, www.specialmetals.com/products
[2] Murr L E, Martinez E, Gaytan S M.Metall Mater Trans, 2011; 42A: 3491
[3] Xu Y L, Ran Q X, Li J, Peng J C, Xiao X S, Cao X L, Jia G Q.Mater Sci Eng, 2013; A569: 27
[4] Paul C P, Ganesh P, Mishra S K, Bhargava P, Negi J, Nath A K.Opt Laser Technol, 2007; 39: 800
[5] Evans N D, Maziase P J, Shingledecker J P, Yamamoto Y.Mater Sci Eng, 2008; A498: 412
[6] Dupont J N, Lippold J C, Kiser S D. Welding Metallurgy and Weldability of Nickel-base Alloys. New Jersey: John Wiley & Sons, 2009: 47
[7] Shankar V, Bhanu Sankara Rao K, Mannan S L.J Nucl Mater, 2001; 288: 222
[8] Smith G D, Tillack D J, Patel S J. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale PA: The Minerals Metals & Materials Society, 2001: 35
[9] Janaki Ram D J, Venugopal Reddy A, Prasad Rao K, Madhusudhan Reddy G.J Mater Proc Technol, 2005; 167: 73
[10] Shoemaker L E. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Warrendale PA: The Minerals Metals & Materials Society, 2005: 409
[11] Cortial F, Corrieu J M, Vernot-Loier C.Metall Mater Trans, 1995; 26A: 1273
[12] Mathew M D, Bhanu Sankara Rao K, Mannan S L.Mater Sci Eng, 2004; A372: 327
[13] Mathew M D, Parameswaran P, Bhanu Sankara Rao K.Mater Charact, 2008; 59: 508
[14] Sundararaman M, Mukhopadhyay P, Banerjee S.Metall Trans, 1988; A19: 453
[15] Huang Y, Langdon T G. J Mater Sci, 2007; 42: 421
[16] Zhang H Y, Zhang S H, Cheng M, Li Z X.Mater Charact, 2010; 61: 49
[17] Yeh A C, Lu K W, Kuo C M, Bor H Y, Wei C N.Mater Sci Eng, 2011; A530: 525
[18] Kuo C M, Yang Y T, Bor H Y, Wei C N, Tai C C. Mater Sci Eng, 2009; A510-511: 289
[19] Dong J X, Xie X S, Wang M.Ordnance Mater Sci Eng, 1993; 16: 51
[20] Xie X S, Dong J X, Fu S H, Zhang M C.Acta Metall Sin, 2010; 46: 1289
[20] (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
[21] Footner P K, Richards B P.J Mater Sci, 1982; 17: 2141
[22] Smokingermain R E,translated by Zhang R J. Modern Physical Metallurgy. Beijing: Metallurgical Industry Press, 1980: 176
[22] (Smokingermain R E著,张人洁译. 现代物理冶金学. 北京: 冶金工业出版社, 1980: 176)
[23] Cahn J W.Acta Metall, 1966; 14: 83
[24] Orian R A.Acta Metall, 1964; 12: 1399
[25] Burke M G, Miller M K.Precipitationin Alloy 718. Pennsylvania: TMS, 1991: 3377
文章导航

/

〈 〉