论文

快速凝固制备Laves相增强NiAl基复合材料的微观组织及力学性能

  • 盛立远 ,
  • 章炜 ,
  • 赖琛 ,
  • 郭建亭 ,
  • 奚廷斐 ,
  • 叶恒强
展开
  • 1) 北京大学深圳研究院人体组织再生与修复深圳重点实验室, 深圳 518057
    2) 中国科学院金属研究所, 沈阳 110016
盛立远, 男, 1979年生, 副研究员

收稿日期: 2013-07-16

  修回日期: 2013-08-24

  网络出版日期: 2013-11-11

基金资助

国家重点基础研究发展计划项目2012CB933600, 中国博士后基金项目2012M510271,国家自然科学基金项目31370956, 深圳战略新兴产业发展专项资金项目JCYJ20130402172114948和JCYJ20130402164725011资助

MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LAVES PHASE STRENGTHENING NiAl BASE COMPOSITE FABRICATED BY RAPID SOLIDIFICATION

  • SHENG Liyuan ,
  • ZHANG Wei ,
  • LAI Chen ,
  • GUO Jianting ,
  • XI Tingfei ,
  • YE Hengqiang
Expand
  • 1) Shenzhen Key Laboratory of Human Tissue Regeneration and Repair, Shenzhen Institute, Peking University, Shenzhen 518057
    2) Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-07-16

  Revised date: 2013-08-24

  Online published: 2013-11-11

摘要

利用水冷Cu模喷铸快速凝固技术制备Laves相(Cr2Nb)增强NiAl基复合材料,并对比研究了普通铸造和快速凝固工艺制备的NiAl/Laves相材料的微观组织和力学性能.结果显示, 普通铸造合金中的Laves相相对粗大, 呈不连续状分布于NiAl相周围,NiAl相中析出了棒状的Laves相, 由于Ni和Al元素在Laves相中的存在,合金中Laves相在室温下拥有C14的晶体结构.快速凝固工艺有效地细化了NiAl和Laves相,并使NiAl相界的Laves相形成NiAl/Laves共晶层片, 呈胞状结构包覆NiAl相. 但是,快速凝固工艺仍然无法完全抑制细长针状Laves相在NiAl中的析出, 但抑制了α-Cr相的析出.压缩性能显示, 相对普通铸造工艺, 快速凝固工艺制备的胞状Laves相增强NiAl基复合材料具有更佳的室温和高温性能,其性能的改善应归因于胞状Laves的结构以及胞状Laves相在高温变形过程中的纳米化.

本文引用格式

盛立远 , 章炜 , 赖琛 , 郭建亭 , 奚廷斐 , 叶恒强 . 快速凝固制备Laves相增强NiAl基复合材料的微观组织及力学性能[J]. 金属学报, 2013 , 49(11) : 1318 -1324 . DOI: 10.3724/SP.J.1037.2013.00413

Abstract

The Laves phase strengthening NiAl base composite was fabricated by conventionally casting and rapid solidification, and their microstructure and mechanical properties were investigated together. The results exhibit that the Laves phase in the conventional cast alloy is relative coarse and distributes along the NiAl phase boundary. Moreover, small stick-like Laves phase precipitates in the NiAl phase. Due to the segregation of Ni and Al in Laves phase, it still keeps the C14 crystal structure. The rapid solidification refines the NiAl and Laves phase greatly and promotes the formation of NiAl/Laves phase eutectic structure, which surrounds the NiAl phase and forms the cell-like structure. However, the rapid solidification can not handicap the precipitation of needle-like Laves phase in the NiAl phase. But, the rapid solidification restrains the formation ofα-Cr phase. The compression tests show that the cell-like Laves phase strengthening NiAl base composite has better mechanical properties at ambient and elevated temperature, compared with the conventional cast alloy. The improvement of mechanical properties should be attributed to the cell-like Laves phase and the nanocrystallization of the cell-like Laves phase during high-temperature deformation.

参考文献

[1] Miracle D B.  Acta Metall Mater, 1993; 41: 649

[2] Guo J T.  Ordered Intermetallic Compound NiAl Alloy. Beijing: Science Press, 2003: 104
(郭建亭. 有序金属间化合物镍铝合金. 北京: 科学出版社, 2003: 104)
[3] Sheng L Y, Yang F, Xi T F, Guo J T, Ye H Q.  Mater Sci Eng, 2012; A555: 131
[4] Sheng L Y, Xie Y, Xi T F, Guo J T, Zheng Y F, Ye H Q.  Mater Sci Eng, 2011; A528: 8324
[5] Cline H E, Walter J L.  Metall Trans, 1970; 1: 2907
[6] Sheng L Y, Guo J T, Zhang W, Xie Y, Zhou L Z, Ye H Q.  Acta Metall Sin, 2009; 45: 1025
(盛立远, 郭建亭, 章炜, 谢亿, 周兰章, 叶恒强. 金属学报, 2009; 45: 1025)
[7] Chen X F, Johnson D R, Noebe R D, Olliver B F.  J Mater Res, 1995; 10: 1159
[8] Zeumer B, Sauthoff G.  Intermetallics, 1997; 5: 641
[9] Johnson D R, Chen X F, Oliver B F, Noebe R D, Whittenberger J D.Intermetallics, 1995; 3: 141
[10] Sheng L Y, Guo J T, Ye H Q.  Mater Des, 2009; 30: 964
[11] Sheng L Y, Wang L J, Xi T F, Zheng Y F, Ye H Q.  Mater Des, 2011; 32: 4810
[12] Sheng L Y, Guo J T, Ren W L, Zhang Z X, Ren Z M, Ye H Q.  Intermetallics, 2011; 19: 143
[13] Sheng L Y, Yang F, Xi T F, Zheng Y F, Guo J T.  Trans Nonferrous Met Soc China, 2013; 23: 983
[14] Kazantzis A V, Aindow M, Jones I P.  Mater Sci Eng, 1997; A233: 44
[15] Bewlay B P, Sutliff J A, Jackson M R, Lipsitt H A.  Acta Metall Mater, 1994; 42: 2869
[16] Sheng L Y, Yang F, Xi T F, Zheng Y F, Guo J T.  Intermetallics, 2012; 27: 14
[17] Sheng L Y, Zhang W, Guo J T, Zhou L Z, Ye H Q.  Intermetallics, 2009; 17: 1115
[18] Sheng L Y, Guo J T, Xi T F, Zhang B C, Ye H Q.  Prog Nat Sci: Mater Int, 2012; 22: 231
[19] Sheng L Y, Zhang W, Guo J T, Ye H Q.  Mater Charact, 2009; 60: 1311
[20] Takeyama M, Liu C T.  Mater Sci Eng, 1991; A132: 61
[21] Lu K, Lu L, Suresh S.  Science, 2009; 324: 349
[22] Sheng L Y, Zhang W, Guo J T, Yang F, Liang Y C, Ye H Q.  Intermetallics, 2010; 18: 740
[23] Sheng L Y, Yang F, Xi T F, Guo J T.  J Alloys Compd, 2013; 554: 182
[24] Sheng L Y, Yang F, Guo J T, Xi T F, Ye H Q.  Composites, 2013; 45B: 785
[25] Zhang J H, Leng Z, Liu S J, Li J Q, Zhang M L, Wu R Z.  J Alloys Compd, 2011; 509: 7717
[26] Sheng L Y, Zhang W, Guo J T, Wang Z S, Ye H Q.  Mater Des, 2009; 30: 2752
[27] Roland J C, Reis D, Vian B, Roy S.  Biol Cell, 1989; 67: 209
文章导航

/