温度对Cr26Mo1超纯高铬铁素体不锈钢在3.5%NaCl溶液中耐点蚀性能的影响

  • 董俊华 ,
  • 魏欣 ,
  • 佟健 ,
  • 郑志 ,
  • 柯伟
展开
  • 1. 中国科学院金属研究所, 沈阳 110016
    2. 大连理工大学材料科学与工程学院, 大连 116024
魏欣, 男, 1982年生, 博士生

收稿日期: 2011-07-27

  修回日期: 2012-03-16

  网络出版日期: 2012-04-11

基金资助

国家自然科学基金资助项目 51071160

INFLUENCE OF TEMPERATURE ON PITTING CORROSION RESISTANCE OF Cr26Mo1 ULTRA PURE HIGH CHROMIUM FERRITE STAINLESS STEEL IN 3.5%NaCl SOLUTION

  • DONG Jun-Hua ,
  • WEI Xin ,
  • TONG Jian ,
  • ZHENG Zhi ,
  • KE Wei
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2. College of Materials Science and Engineering, Dalian University ofTechnology, Dalian 116024

Received date: 2011-07-27

  Revised date: 2012-03-16

  Online published: 2012-04-11

摘要

通过循环极化曲线、Mott--Schottky曲线以及电化学阻抗谱等方法研究了温度对 Cr26Mo1超纯高铬铁素体不锈钢在3.5%NaCl溶液中耐点蚀性能的影响. 结果表明: 随着温度升高, Cr26Mo1超纯高铬铁素体不锈钢的自腐蚀电位降低, 腐蚀电流密度增大, 点蚀电位下降, 钝化膜阻抗降低. Cr26Mo1不锈钢钝化膜的半导体类型和性质在不同温度下发生改变. Cr26Mo1不锈钢发生点蚀的孕育期随着温度的升高而缩短, 点蚀敏感性增加, 已发生点蚀的试样不能够自修复.

本文引用格式

董俊华 , 魏欣 , 佟健 , 郑志 , 柯伟 . 温度对Cr26Mo1超纯高铬铁素体不锈钢在3.5%NaCl溶液中耐点蚀性能的影响[J]. 金属学报, 2012 , 48(4) : 502 -507 . DOI: 10.3724/SP.J.1037.2011.00489

Abstract

The remarkable uniform corrosion resistance of ultra pure high chromium ferrite stainless steel in various rigorous corrosive environments is based on the formation of a passive film on its surface. However, it is suspected that this stainless steel was easy to suffer from pitting corrosion. In this work, the influences of temperature on the pitting corrosion resistance of Cr26Mo1 ultra pure high chromium ferrite stainless steel were studied by electrochemical methods such as cyclic polarization curves, Mott-Schottky curves and electrochemical impedance spectroscopy in 3.5%NaCl solution. The results showed that with the increase of the temperature, open-circuit corrosion potential and pitting corrosion potential decreased, corrosion current density increased, the impedance of passive film decreased. The semi-conductive styles and properties of passive film changed at different temperatures. Also, the pregnancy time of pitting shortened and the sensitivity of pitting increased remarkably as the temperature increased. In addition, the cyclic polarization curves indicated that the repassivation of existing pits was more difficult when the potential was swept toward the negative direction.

参考文献

[1] Ilevbare G O, Burstein G T.  Corros Sci, 2003; 45: 1545

[2] Sekine I, Okano C, Yuasa M.  Corros Sci, 1990; 30: 351

[3] Hiraide N.  World Iron Steel, 2004; 6: 33

[4] You X M, Jiang Z H, Li H B, Shen M H, Cao Y.  China Metall,2006; 16(11): 16

    (游香米, 姜周华, 李花兵, 申明辉, 曹阳. 中国冶金, 2006; 16(11): 16 )

[5] Latanision R M, Kloppers M J, Bellucci F.  Corrosion, 1992; 48: 229

[6] Kaneko M, Isaaca H S.  Corros Sci, 2002; 44: 1825

[7] Shan Y T, Luo X H, Hu X Q, Liu S.  J Mater Sci Technol, 2011; 27: 352

[8] Ernst P, Newman R C.  Corros Sci, 2007; 49: 3705

[9] Rosenfeld I L, Danilov I S, Oranskaya R N.  J Electrochem Soc,1978; 125: 1728

[10] Stockert L, Hunkeler F, Bohni H.  Corrosion, 1985; 41: 676

[11] Carmezim M J, Simoes A M, Montemor M F, Da C B M.  Corros Sci,2005; 47: 581

[12] Ferreira M G S, Hakiki N E, Goodlet G, Faty S, Simoes A M P, Da C B M. Electrochim Acta, 2001; 46: 3767

[13] McCafferty E.  Corros Sci, 2003; 45: 301

[14] Jin B, Zheng M S, Zhu J W.  Corros Sci Prot Technol, 2006; 18: 348

     (金波, 郑茂盛, 朱杰武. 腐蚀科学与防护技术, 2006; 18: 348)

[15] Lin Y H, Du R G, Hu R G, Lin C J.  Acta Phys Chim Sin, 2005; 21: 740

     (林玉华, 杜荣归, 胡融刚, 林昌健. 物理化学学报, 2005; 21: 740)

[16] Li W S, Luo J L.  Electrochem Commun, 1999; 1: 349

[17] Paola A P, Shukla D, Stimming U.  Electrochim Acta, 1991; 36: 345

[18] Sunseri C, Piazza S, Di Quarto F.  J Electrochem Soc,1990; 137: 2411

[19] Montemor M F, Ferreira M G S, Hakiki N E, Da C B M.  Corros Sci,2000; 42: 1635

[20] Macdonald D D, Urquidi-Macdonald M.  J Electrochem Soc,1990; 137: 2395

[21] Eghbali F, Moayed M H, Davoodi A, Ebrahimi N.  Corros Sci,2011; 53: 513

[22] Moayed M H, Newman R C.  Corros Sci, 2006; 48: 1004

[23] Cao C N.  Principles of Electrochemistry of Corrosion.Beijing: Chemical Industry Press, 2008: 248

     (曹楚南, 腐蚀电化学原理, 北京: 化学工业出版社, 2008: 248)

[24] Eghbali F, Moayed M H, Davoodi A, Ebrahimi N.  Corros Sci,2011; 53: 513

[25] Ningshen S, Mudali U K, Mittal V K, Khatak H S.  Corros Sci,2007; 49: 481
 
文章导航

/