Si和Y掺杂对(Ti, Al)N涂层结构和性能的影响

  • 范永中 ,
  • 张淑娟 ,
  • 涂金伟 ,
  • 孙霞 ,
  • 刘芳 ,
  • 李明升
展开
  • 江西科技师范学院江西省材料表面工程重点实验室, 南昌 330013
范永中, 男, 1984年生, 硕士生

收稿日期: 2011-05-09

  修回日期: 2011-12-01

  网络出版日期: 2012-01-11

基金资助

江西省教育厅科学技术基金资助项目GJJ12586

INFLUENCE OF DOPING WITH Si AND Y ON STRUCTURE AND PROPERTIES OF (Ti, Al)N COATING

  • FAN Yong-Zhong ,
  • ZHANG Shu-Juan ,
  • CHU Jin-Wei ,
  • XUN Xia ,
  • LIU Fang ,
  • LI Meng-Sheng
Expand
  • Jiangxi Key Laboratory of Surface Engineering, Jiangxi Science and Technology Normal University, Nanchang 330013

Received date: 2011-05-09

  Revised date: 2011-12-01

  Online published: 2012-01-11

Supported by

Supported by Scientific Research Fund of Jiangxi Provincial Education Department (No.GJJ12586)

摘要

分别在未施加偏压和施加-100 V偏压条件下, 利用磁控溅射技术在压气机叶片用 1Cr11Ni2W2MoV热强不锈钢基体上沉积了Ti0.3Al0.7N和Ti0.39Al0.55Si0.05Y0.01N硬质涂层. 实验结果表明, 施加偏压及Si和Y掺杂明显改变了涂层的相结构, 提高了涂层致密度, 施加-100 V偏压且添加Si和Y的涂层为非晶结构, 表面更加均匀致密. 950 ℃氧化实验表明: Ti0.39Al0.55Si0.05Y0.01NN涂层表面形成极薄且致密的 Al2O3保护性氧化膜, 大大降低了氧化速率. 施加-100 V偏压的(Ti, Al)N和(Ti, Al, Si, Y)N沉积态涂层与未施加偏压的相应涂层相比, 硬度均降低, 尤其是(Ti, Al, Si, Y)N涂层变化显著. 经950 ℃热处理, 施加偏压的(Ti, Al, Si, Y)N涂层硬度略有降低, 这是由于形成了硬度较低的B4相, 而未施加偏压的(Ti, Al, Si, Y)N涂层硬度显著提高, 这归因于B1相固溶体的分解. 划痕测试结果表明, 在实验载荷(50 N)下, 所有涂层均未出现连续性的剥落.

本文引用格式

范永中 , 张淑娟 , 涂金伟 , 孙霞 , 刘芳 , 李明升 . Si和Y掺杂对(Ti, Al)N涂层结构和性能的影响[J]. 金属学报, 2012 , 48(1) : 99 -106 . DOI: 10.3724/SP.J.1037.2011.00292

Abstract

Composite metastable Ti0.3Al0.7N and Ti0.39Al0.55Si0.05Y0.01NN hard coatings were deposited on a wrought martensite steel 1Cr11Ni2W2MoV for aero-engine compressor blades by the magnetron sputtering system with the bias voltage of 0 and -100 V respectively. Detailed microstructure, chemical composition, crystal structure, hardness and adhesion were examined by means of FESEM, EDS, XRD, Micro hardness tester and scratch tester. The influence of doping with Si and Y and bias on structure, oxidation-resistance and mechanical properties of (Ti, Al)N coatings were investigated. Pulsed bias and the doping with Si and Y gave rise to the change of phase structure and improvement of density. Doping with small amounts of Si and Y into (Ti, Al)N significantly improved the oxidation resistance at 950 ℃. The oxidation-resistance of (Ti, Al, Si, Y)N is based on the formation of dense protective Al2O3 layer. The application of negative pulse led to decreased hardness for (Ti, Al)N while remarkable decrease of hardness for (Ti, Al, Si, Y)N. For (Ti, Al, Si, Y)N prepared under -100 V\linebreak bias, annealing 10 h at 950 ℃ slightly decreased it's hardness because of the formation of B4 structure. And for which deposited at 0 V bias, heat-treatment of 950 ℃ for 10 h improved the hardness from 26 GPa to 35 GPa. The hardness change of the coating may be ascribed the transition of B1 phase structure. Scratch tests show that the continuous spall is not occurred for all the coatings under the critical load of 50 N.

参考文献

[1] Paldey S, Deevi S C. Mater Sci Eng, 2003; A3: 58

[2] Mayrhofer P H, Mitterer C, Hultman L, Clemens H. Prog Mater Sci, 2006; 51: 1032

[3] Ma S L, Jie W Q, Xu K W. Chin J Vac Sci Technol, 2002; 22: 438

(马胜利, 介万奇, 徐可为. 真空科学与技术学报, 2002; 22: 438)

[4] Inoue S, Uchida H, Yoshinaga Y, Koterazawa K. Thin Solid Films, 1997; 300: 171

[5] Li M S, Wang F H, Wang T G, Gong J, Sun C, Wen L S. Acta Metall Sin, 2003; 39: 55

(李明升, 王福会, 王铁钢, 宫俊, 孙超, 闻立时. 金属学报, 2003; 39: 55)

[6] Makino Y. Surf Coat Technol, 2005; 193: 185

[7] Pilloud D, Pierson J F, Marco de Lucas M C, Cavaleiro A. Surf Coat Technol, 2008; 202: 2413

[8] Veprek S, Reiprich S, Shizi L. Appl Phys Lett, 1995; 66: 2640

[9] Vaz F, Rebouta L, Andritschky M, Silva M, Soares J C. Surf Coat Technol, 1998; 98: 912

[10] Pfeiler M, Zechner J, Penoy M, Michotte C, Mitterer C, Kathrein M. Surf Coat Technol, 2009; 203: 3104

[11] Lembke M I, Lewis D B, M¨unz W D, Titchmarsh J M. Surf Eng, 2001; 17: 153

[12] Li M S, Feng C J, Wang F H. Funct Mater (suppl), 2007; (38): 2615

(李明升, 冯长杰, 王福会. 功能材料(增刊), 2007; (38): 2615)

[13] Mao Y F, Tang W G, Liu J L, Han P G. Tool Eng, 2006; 40: 20

(毛延发, 唐为国, 刘金良, 韩培刚. 工具技术, 2006; 40: 20)

[14] Jung H G, Kim K Y. Oxid Met, 1998; 49: 403

[15] Flink A, Andersson J M, Alling B, Daniel R, Sjolen J, Karlsson L, Hultman L. Thin Solid Films, 2008; 517: 714

[16] Carvalho S, Rebouta L, Ribeiro E, Vaz F, Tavares C J, Alves E, Barradas N P, Riviere J P. Vacuum, 2009; 83: 1206

[17] Vennemann A, Stock H R, Kohlscheen J, Rambadt S, Erkens G. Surf Coat Technol, 2003; 174–175: 408

[18] Wang F Z, Ma W C. Vapor Deposition Applications Technology. Beijing: China Machine Press, 2006: 291

(王福贞, 马文存. 气相沉积应用技术. 北京: 机械工业出版社, 2006: 291)

[19] Makino Y. Mater Sci Eng, 1995; 2: 67

[20] Vaz F, Rebouta L, Andritschky M, Silva M, Soares J C. J Eur Ceram Soc, 1997; 17: 1971

[21] Banakh O, Schmid P E, Sanjines R, Levy F. Surf Coat Technol, 2003; 163: 57

[22] Chang Y Y, Hsiao C Y. Surf Coat Technol, 2009; 204: 992

[23] M¨unz W D. Werkst Korros, 1990; 41: 753

[24] Veprek S, Sarott F A, Iqbal Z. Phys Rev, 1987; B36: 3344

[25] Veprek S, Maritza G J, Veprek H, Karvankova P, Prochazka J. Thin Solid Films, 2005; 476: 1

[26] Raveh A, Zukerman I, Shneck R, Avni R, Fried I. Surf Coat Technol, 2007; 201: 6136

[27] Tanaka Y, Ichimiya N, Onishi Y, Yamada Y. Surf Coat Technol, 2001; 146–147: 215

[28] Carvalho S, Rebouta L, Cavaleiro A, Rocha L A, Gomes J, Alves E. Thin Solid Films, 2001; 398–399: 391
文章导航

/

〈 〉