钝化处理对316L不锈钢血液相容性的影响

  • 史永娟 ,
  • 任伊宾 ,
  • 杨柯 ,
  • 张炳春
展开
  • 1. 中国科学院金属研究所, 沈阳 110016
    2. 中国科学院研究生院, 北京 100049
史永娟, 女, 1987年生, 硕士生

收稿日期: 2011-08-10

  修回日期: 2011-10-15

  网络出版日期: 2011-12-11

基金资助

国家自然科学基金项目31000428和中科院知识创新工程重要方向性项目KGCX2-YW-207资助

THE EFFECT OF PASSIVATION ON THE HAEMOCOMPATIBILITY OF 316L STAINLESS STEEL

  • SHI Yong-Juan ,
  • REN Yi-Bin ,
  • YANG Ke ,
  • ZHANG Bing-Chun
Expand
  • 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2. Graduate School of Chinese Academy of Sciences, Beijing 100049

Received date: 2011-08-10

  Revised date: 2011-10-15

  Online published: 2011-12-11

Supported by

Supported by National Natural Science Foundation of China (No.31000428) and Main Direction Program of Knowledge Innovation of Chinese Academy of Sciences (No.KGCX2–YW–207)

摘要

通过血小板黏附和蛋白吸附研究了硝酸钝化(NT)和柠檬酸钝化(CT)对316L不锈钢血液相容性的影响, 并通过XPS分析、接触角和表面电荷测量,研究了经两种方法钝化的316L不锈钢表面钝化层成分、表面张力及表面电荷等表面性能对血小板黏附和蛋白吸附的影响. 研究结果表明, 柠檬酸钝化后的316L不锈钢表现出相对较好的血液相容性, 这与316L不锈钢经柠檬酸钝化后较高的表面张力和相对较低的表面正电荷等表面性能有关. 同时研究表明,316L不锈钢表面白蛋白的吸附量与表面张力的极性分量成线性关系,而纤维蛋白原吸附量与表面电荷密度呈线性关系.

本文引用格式

史永娟 , 任伊宾 , 杨柯 , 张炳春 . 钝化处理对316L不锈钢血液相容性的影响[J]. 金属学报, 2011 , 47(12) : 1575 -1580 . DOI: 10.3724/SP.J.1037.2011.00520

Abstract

The difference of haemocompatibility of medical 316L stainless steel passivated by nitric acid (NT) and citric acid (CT) was studied. Platelet adhesion and protein adsorption were studied to evaluate the haemocompatibility of the 316L stainless steel passivated by the two different methods. XPS analysis, water contact angle and surface charge measurement were used to analyze the surface properties of the steel such as chemical composition and depth distribution of the main elements in passivated films, surface energy and surface charge. The results showed that the 316L steel passivated by citric acid displayed better haemocompatibility, which could be related to the higher surface energy and relatively lower surface charge. The results also showed that the polar component of surface energy was of linear relation with the albumin adsorption on 316L stainless steel while the surface charge had the same relation with fibrinogen adsorption.

参考文献

[1] Shahryari A,Azari F, Vali H, Omanovic S. Acta Biomater, 2010; 6: 695

[2] Shih C C, Shih C M, Su Y Y, Su L H J, Chang M S, Lin S J. Corros Sci, 2004; 46: 427

[3] Shahryari A, Omanovic S, Szpunar J A. Mater Sci Eng, 2008; C28: 94

[4] Barbosa M A. Corros Sci, 1983; 23: 1293

[5] Noh J S, Laycock N J, Gao W, Wells D B. Corros Sci, 2000; 42: 2069

[6] Hong T, Ogushi T, Nagumo M. Corros Sci, 1996; 38: 881

[7] Ma L Y, Ding Y, Ma L Q, Yao C R, Shen W D. Surf Technol, 2007; 36: 39

(马李洋, 丁毅, 马立群, 姚春荣, 沈卫东. 表面技术, 2007; 36: 39)

[8] Rodrigues S N, Gon¸calves I C, Martins M C L, Barbosa M A, Ratner B D. Biomaterials, 2006; 27: 5357

[9] Mitsakakis K, Lousinian S, Logothetidis S. Biomol Eng, 2007; 24: 119.

[10] Huang Y, Xiaoying L, Qian W, Tang Z, Zhong Y. Acta Biomater, 2010; 6: 2083.

[11] Gray J J. Curr Opin Struct Biol, 2004; 14: 110

[12] Anselme K. Biomaterials, 2000; 21: 667

[13] MacDonald D E, Rapuano B E, Deo N, Stranick M, Somasundaran P, Boskey A L. Biomaterials, 2004; 25: 3135

[14] Cacciafesta P, Humphris A D L, Jandt K D, Miles M J. Langmuir, 2000; 16: 8167

[15] Gon¸calves I C, Martins M C L, Barbosa M A, Ratner B D. Biomaterials, 2005; 26: 3891

[16] Dion I, Baquey C, Candelon B, Monties J. Int J Artif Organs, 1992; 15: 617

[17] Yuan Y, Liu C, Yin M. J Mater Sci: Mater Med, 2008; 19: 2187

[18] Kaelble D H, Moacanin J. Polymer, 1977; 18: 475

[19] Michiardi A, Aparicio C, Ratner B D, Planell J A, Gil J. Biomaterials, 2007; 28: 586

[20] Nyilas E, Ward Jr R. J Biomed Mater Res, 1977; 11: 69

[21] Depalma V, Baier R, Ford J, Gott V, Furuse A. J Biomed Mater Res, 1972; 6: 37
文章导航

/

〈 〉