论文

核电站控制棒驱动机构驱动杆用1Cr13厚壁管材成分选择与工艺优化

  • 都祥元 ,
  • 苏国跃
展开
  • 中国科学院金属研究所, 沈阳 110016
都祥元, 男, 1977年生, 博士

收稿日期: 2011-04-06

  修回日期: 2011-06-09

  网络出版日期: 2011-09-11

COMPONENT SELECTION AND TECHNOLOGICAL OPTIMIZATION OF THICK WALL 1Cr13 TUBE USED AS CONTROL POLES IN NUCLEAR POWER STATION DRIVING MACHINES

  • DU Xiang-Yuan ,
  • SU Guo-Ti
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-04-06

  Revised date: 2011-06-09

  Online published: 2011-09-11

摘要

通过优化设计与控制C, Ni, Cr主合金元素和H, O, N气体元素含量, 优化管材冷轧工艺, 有效防止了1Cr13管材加工时的开裂现象, 保证了管材表面质量良好; 通过调整成品热处理工艺, 使试制的管材样件的力学性能完全满足了技术条件要求.

关键词: 1Cr13钢; 管材; 冷轧; 热处理

本文引用格式

都祥元 , 苏国跃 . 核电站控制棒驱动机构驱动杆用1Cr13厚壁管材成分选择与工艺优化[J]. 金属学报, 2011 , 47(9) : 1155 -1158 . DOI: 10.3724/SP.J.1037.2011.00209

Abstract

The control poles for driving machine in the built and building nuclear power station are made of thick wall 1Cr13 tubes which all depend on overseas importation. With the fast development of domestic nuclear power stations and the need with coming export, as one of the key parts of driving machines, the 1Cr13 tubes used as control poles should be finished in our country. By optimizing the contents of C, Ni, Cr, H, O and N etc., and adjusting the technology of cold rolling, the cracking problem of 1Cr13 tube as control poles during machining is avoided and favorable surface quality is also obtained. The mechanical properties of  finished tubes reach the technical request after proper heat--treatment.

参考文献

[1] Lu S Y, Zhang T K, Kang X F, Yang C Q, Wang X. Stainless Steel, Beijing: Atomic Energy Press, 1995: 23

(陆世英, 张廷凯, 康喜范, 杨长强, 王熙. 不锈钢. 北京: 原子能出版社, 1995: 23)

[2] Cui Z Q. Metal and Heat Treatment. Beijing: Mechanical Industry Press, 1988: 285

(崔忠圻. 金属学与热处理. 北京: 机械工业出版社, 1988: 285)

[3] Barid J D. Met Mater, 1971; 4: 1

[4] Bao J. Spec Steel Technol, 2006; 11(2): 20

(鲍进. 特钢技术, 2006; 11(2): 20)

[5] Li H S. Spec Steel Technol, 2006; 12(4): 25

(李海生. 特钢技术, 2006; 12(4): 25)

[6] Zhang Y T. Manual for Heat Treatment Technician. Beijing: Mechanical Industry Press, 2005: 89

(张玉庭. 热处理技师手册. 北京: 机械工业出版社, 2005: 89)

[7] Woodfine B C. J Iron Steel Inst, 1953; 173: 229
文章导航

/

〈 〉