论文

辐照与He协同作用对低活度铁素体/马氏体钢F82H微观结构的影响

  • 杨文 ,
  • 佟振峰
展开
  • 1) 中国原子能科学研究院, 北京 102413
    2) Paul Scherrer Institut, 5232 Villigen PSI, Switzerland
佟振峰, 男, 1977年生, 副研究员

收稿日期: 2011-04-06

  修回日期: 2010-05-03

  网络出版日期: 2011-07-11

基金资助

国家重点基础研究发展计划项目2011CB610503和国家自然科学基金项目10975194资助

EFFECTS OF RADIATION AND He ON MICROSTRUCTURES OF LOW ACTIVE FERRITIC/MARTENSITIC STEEL F82H

  • YANG Wen ,
  • TONG Zhen-Feng
Expand
  • 1) China Insitute of Atomic Energy, Beijing 102413
    2) Paul Scherrer Institut, 5232 Villigen PSI, Switzerland

Received date: 2011-04-06

  Revised date: 2010-05-03

  Online published: 2011-07-11

Supported by

Supported by National Basic Research Program of China (No.2011CB610503) and National Natural Science Foundation of China (No.10975194)

摘要

利用散裂中子源模拟聚变环境辐照F82H铁素铁/马氏体钢, 辐照温度为150-450 ℃, 辐照剂量为6.1-20.2 dpa. 对不同温度和剂量辐照后样品的微观结构进行了TEM观察, 结果表明, 当辐照温度高于208 ℃, 辐照剂量高于9.5 dpa, He浓度高达680×10-6时的样品中存在尺寸约为1.6 nm的高密度 He泡. 分析了辐照剂量、温度以及嬗变He浓度对F82H钢微观结构的影响.

本文引用格式

杨文 , 佟振峰 . 辐照与He协同作用对低活度铁素体/马氏体钢F82H微观结构的影响[J]. 金属学报, 2011 , 47(7) : 965 -970 . DOI: 10.3724/SP.J.1037.2011.00208

Abstract

Low active ferritic/martensitic steel, F82H, has been developed as a candidate material for structural
applications of fusion reactors because it has relatively low shifts in ductile-to-brittle transition temperature
(DBTT) and excellent irradiation swell resistance. More works have been done in recent years on the
microstructure and mechanical properties of F82H steel before and after irradiation, but most of the tested samples were
irradiated at low temperature (<400 ℃). In this work, the microstructure of F82H steel irradiated in the Swiss
spallation neutron source SINQ in a temperature range of 150-450 ℃ and a dose range of 6.1-20.2 dpa was
studied. Defect clusters and He bubble were observed by TEM in the irradiated specimens.
The results showed that there existed high density He bubbles with size of 1.6 nm under irradiation temperature higher than
208℃, irradiation dose higher than 9.5 dpa and He concentration 680×10-6. The effects of
irradiation dose, irradiation temperature and He concentration on microstructure of F82H steel were discussed.

参考文献

[1] Klueh R L, Harries D R. High–Chromium Ferritic and Martensitic Steels for Nuclear Applications. West Conshohocken, PA: ASTM, 2001: 19

[2] Kohyama A, Hishinuma A, Gelles D S, Klueh R L, Dietz W, Ehrlich K. J Nucl Mater, 1996; 233–237: 138

[3] Miwa Y, Wakai E, Shiba K, Hashimoto N, Robertson J P, Rowcli A F, Hishinuma A. J Nucl Mater, 2000; 283–287: 334

[4] Schaublin R, Spatig P, Victoria M. J Nucl Mater, 1998; 258–263: 1178

[5] Sawai T,Wakai E, TomitaT, NaitoA, Jitsukawa S. J Nucl Mater, 2002; 307–311: 312

[6] Spatig P, Schaublin R, Gyger S, Victoria M. J NuclMater, 1998; 258–263: 1345

[7] Shiba K, Suzuki M, Hishinuma A. J Nucl Mater, 1996; 233–237: 309

[8] Jitsukawa S, Tamura M, vander Schaaf B, Klueh R L, Alamo A, Petersen C, Schirra M, Spaetig P, Odette G R, Tavassoli A A, Shiba K, Kohyama A, Kimura A. J Nucl Mater, 2002; 307–311: 179

[9] Stamm U, Schroeder H. J Nucl Mater, 1988; 155–157: 1059

[10] Ullmaier H. Radiat Eff, 1983; 78: 1

[11] Klueh R L, Hashimoto N, Sokolov M A, Shiba K, Jitsukawa S. J Nucl Mater, 2006; 357: 156

[12] Malaplate J, Vincent L, Averty X, Henry J, Marini B. Eng Fract Mech, 2008; 75: 3570

[13] Henry J, Vincent L, Averty X, Marini B, Jung P. J Nucl Mater, 2007; 367–370: 411

[14] Tong Z, Dai Y. J Nucl Mater, 2010; 398: 43

[15] Gupta G, Jiao Z, Ham A N, Busby J T, Was G S. J Nucl Mater, 2006; 351: 162

[16] Dai Y, Foucher Y, James M R, Oliver B M. J Nucl Mater, 2003; 318: 167

[17] Jiao Z, Ham N, Was G S. J Nucl Mater, 2007; 367–370: 440

[18] Trinkaus H, Singh B N. J Nucl Mater, 2003; 323: 229

[19] Jia X, Dai Y. J Nucl Mater, 2006; 356: 105
文章导航

/

〈 〉