论文

铝合金挤压铸造过程微观孔洞形成的建模与仿真

  • 韩志强 ,
  • 杨文 ,
  • 柳百成
展开
  • 1) 清华大学机械工程系, 先进成形制造教育部重点实验室, 北京 100084
    2) 华南理工大学机械与汽车工程学院, 广州 510640 
    3) 清华大学汽车工程系, 汽车安全与节能国家重点实验室, 北京 100084
韩志强, 男, 1968年生, 副教授, 博士

收稿日期: 2010-06-30

  修回日期: 2010-10-26

  网络出版日期: 2011-01-11

基金资助

国家自然科学基金项目50675113和50875143资助

MODELING AND SIMULATION ON MICROPOROSITY FORMED DURING SQUEEZE CASTING OF ALUMINUM ALLOY

  • HAN Zhi-Jiang ,
  • YANG Wen ,
  • LIU Bai-Cheng
Expand
  • 1) Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Department of Mechanical Engineering, Tsinghua University, Beijing 100084
    2) School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640 
    3) State Key Laboratory of Automotive Safety and Energy, Department of Automotive Engineering, Tsinghua University,  Beijing 100084

Received date: 2010-06-30

  Revised date: 2010-10-26

  Online published: 2011-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50675113 and 50875143)

摘要

基于挤压铸造过程微观孔洞的形成机理, 建立了模拟铝合金挤压铸造过程微观孔洞的数学模型. 该模型考虑了传热、凝固收缩、补缩流动、压力传递、氢(H)的再分配等因素, 通过计算凝固收缩导致的补缩流动与压力降低, 以及挤压过程的压力传递, 获得挤压铸造过程糊状区的压力分布, 结合微观孔洞形成条件及H的守恒方程, 计算微观孔洞的体积分数. 对不同工艺条件下铝合金挤压铸造微观孔洞进行了模拟计算, 计算结果与实验结果基本吻合. 计算结果还表明, 适当提高模具温度和挤压压力有利于减少微观孔洞缺陷.

本文引用格式

韩志强 , 杨文 , 柳百成 . 铝合金挤压铸造过程微观孔洞形成的建模与仿真[J]. 金属学报, 2011 , 47(1) : 7 -16 . DOI: 10.3724/SP.J.1037.2010.00313

Abstract

A mathematical model for simulating the microporosity in squeeze casting of aluminum alloy has been developed, in which the heat transfer, solidification shrinkage, feeding flow, pressure transfer, and hydrogen conservation were taken into account. The shrinkage induced flow and the pressure drop in the mushy zone were calculated by solving continuity and momentum equations. A mechanical model was solved for obtaining the pressure transferred into the central area of the casting. By coupling the pressure drop with the pressure transferred into the central area, the pressure distribution in the mushy zone was calculated. Based on the hydrogen conservation equation, the microporosity volume fraction was calculated by referring to the pressure value in the mushy zone. The squeeze casting processes of aluminum alloy under different process conditions were simulated and the simulation results were compared with experimental results. It was shown that the simulation results agree well with the experimental results, and the increases in applied pressure and mould temperature tend to reduce the microporosity in the castings.

参考文献

[1] Ghomashchi M R, Vikhrov A. J Mater Process Technol, 2000; 101: 1

[2] Qi P X. Spec Cast Nonferrous Alloys, 1998; 18(4): 32

(齐丕骧. 特种铸造及有色合金, 1998; 18(4): 32)

[3] Luo S J, Chen B G, Qi P X. Liquid Forging and Squeeze Casting Technology. Beijing: Chemical Industry Press, 2007: 1

(罗守靖, 陈炳光, 齐丕骧. 液态模锻与挤压铸造技术. 北京: 化学工业出版社, 2007: 1)

[4] Major J F. AFS Trans, 1998; 105: 901

[5] Samuel A M, Samuel F H. Metall Mater Trans, 1995; 26A: 2359

[6] Lee C D. Mater Sci Eng, 2007; A464: 249

[7] Lee P D, Chirazi A, See D. J Light Met, 2001; (1): 15

[8] Stefanescu D M. Int J Cast Met Res, 2005; 18(3): 129

[9] Gui Z L, Dai T, Zhu M F. Spec Cast Nonferrous Alloys, 2007; 27: 766

(桂仲林, 戴挺, 朱鸣芳. 特种铸造及有色合金, 2007; 27: 766)

[10] Kubo K, Pehlke R D. Metall Trans, 1985; 16B: 359

[11] Poirier D R, Yeum K, Maples A L. Metall Trans, 1987; 18A: 1979

[12] Shivkumar S, Apelian D, Zou J. AFS Trans, 1990; 98: 897

[13] Sabau A S, Viswanathan S. Metall Mater Trans, 2002; 33B: 243

[14] Pequet C H, Gremaud M, Rappaz M. Metall Mater Trans, 2002; 33A: 2095

[15] Zhao H D, Wu C Z, Li Y Y, Ohnaka I. Acta Metall Sin, 2008; 44: 1340

(赵海东, 吴朝忠, 李元元, 大中逸雄. 金属学报, 2008; 44: 1340)

[16] Atwood R C, Sridhar S, Zhang W, Lee P D. Acta Mater, 2000; 48: 405

[17] Lee P D, Chirazi A, Atwood R C, Wang W. Mater Sci Eng, 2004; A365: 57

[18] Wang J S, Lee P D. Int J Cast Met Res, 2007; 20(3): 151

[19] Backer G, Wang Q G. Metall Mater Trans, 2007; 38B: 533

[20] Carlson K D, Lin Z P, Beckermann C. Metall Mater Trans, 2007; 38B: 541

[21] Han Z Q, Zhu W, Liu B C. Acta Metall Sin, 2009; 45: 356

(韩志强, 朱维, 柳百成. 金属学报, 2009 45: 356)

[22] Zhu W, Han Z Q, Liu B C. Acta Metall Sin, 2009 45: 363

(朱维, 韩志强, 柳百成. 金属学报, 2009; 45: 363)

[23] Anyalebechi P N. Acta Metall, 1995; 33: 1209

[24] Lewis R W, Han Z Q, Gethin D T. C R Mec, 2007: 335: 287

[25] Yang W, Li J X, Han Z Q, Zhao H D, Liu B C. Spec Cast Nonferrous Alloys, 2010; 30: 54

(杨文, 李金玺, 韩志强, 赵海东, 柳百成. 特种铸造及有色合金, 2010; 30: 54)
文章导航

/

〈 〉