不锈钢材料的高效率焊接新工艺

  • 陆善平 ,
  • 董文超 ,
  • 李殿中 ,
  • 李依依
展开
  • 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
陆善平, 男, 1970年生, 研究员

收稿日期: 2010-08-30

  修回日期: 2010-09-28

  网络出版日期: 2010-11-11

基金资助

国家自然科学基金资助项目50874101

HIGH EFFICIENCY WELDING PROCESS FOR STAINLESS STEEL MATERIALS

  • LU Shan-Beng ,
  • DONG Wen-Tiao ,
  • LI Dian-Zhong ,
  • LI Yi-Yi
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2010-08-30

  Revised date: 2010-09-28

  Online published: 2010-11-11

Supported by

Supported by National Natural Science Foundation of China (No.50874101)

摘要

针对不锈钢材料钨极惰性气体保护(TIG)焊熔深浅、焊接效率低的缺点开发了大深宽比高效率TIG焊接新工艺, 包括活性剂焊接工艺、混合气体联合保护焊工艺和双层气流保护焊工艺. 与涂覆活性剂法相比, 混合气体法不仅可获得深熔深, 而且操作方便, 易于实现工业化; 双层气流法可有效避免混合气体法中电极氧化烧损现象. 实验和模拟结果表明: 熔池中活性元素O含量变化导致的Marangoni对流方向的变化是TIG焊熔深增加的主要因素, 焊接过程中调整液态熔池中活性组元含量可获得大深宽比焊缝. 高效率TIG焊接工艺对焊接规范 (焊接速度、焊接电流和电极间距)不敏感, 有利于在工业生产中推广应用.

本文引用格式

陆善平 , 董文超 , 李殿中 , 李依依 . 不锈钢材料的高效率焊接新工艺[J]. 金属学报, 2010 , 46(11) : 1347 -1364 . DOI: 10.3724/SP.J.1037.2010.00437

Abstract

The high efficiency tungsten inert gas (TIG) welding process has been developed, including active flux welding process, mixed shielded welding process and double shielded welding process, to increase the weld depth/width ratio (D/W$) of conventional TIG welding method. Compared to the active flux method, mixed shielding method can make penetration deeper and the industrialization can be realized easily due to the simplification in operation. Double shielded method can avoid the oxidation of tungsten electrode. The results of experiment and simulation show that the change of the Marangoni convection direction which arises from the adjustment of the oxygen content in the weld pool is one of the main factors contributing to the increase in TIG weld penetration, and the large D/W ratio can be obtained by adjusting the active element content in the liquid pool. High efficiency TIG welding process is not sensitive to welding parameters (welding speed, welding current and electrode gap) and therefore is suitable to be applied in industry easily.

参考文献

[1] Gurevich S M, Zamkov V N, Kushmienko N A. Avtom Svarka, 1965; 9: 1 [2] Gurevich S M, Zamkov V N. Avtom Svarka, 1966; 12: 13 [3] Ludwig H C. Weld J, 1968; 47: 234s [4] Lucas W, Howse D S. Weld Met Fabr, 1996; 64: 11 [5] Howse D S, Lucas W. Sci Technol Weld Joi, 2000; 15: 189 [6] Tanaka M, Shimizu T, Terasaki H, Ushio M, Koshi–ishi F, Yang C L. Sci Technol Weld Join, 2000; 5: 397 [7] Anderson P C J, Wiktorowicz R. Weld Met Fabr, 1996; 64: 108 [8] Paskell T, Lundin C, Castner H. Weld J, 1997; 76: 57s [9] Modenesi P J, Apolinario E R, Pereira I M. J Mater Proc Technol, 2000; 9: 260 [10] Kou M, Sun Z, Pan D. Sci Technol Weld Join, 2001; 6: 17 [11] Savitskii M M, Leskov G I. Avtom Svarka, 1980; 9: 17 [12] Lowke J J, Tanaka M, Ushio M. The 57th Annual Assembly of International Institute of Welding. Osaka, Japan, 2004, IIW Doc. 212–1053–04 [13] Heiple C R, Burgardt P. Weld J, 1985; 64: 159s [14] Heiple C R, Roper J R. Weld J, 1982; 61: 97s [15] Heiple C R, Roper J R, Stagner R T, Aden R J. Weld J, 1983; 62: 72s [16] Heiple C R, Roper J R. Weld J, 1981; 60: 143s [17] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2006; 11: 389 [18] Leconte S, Paillard P, Chapelle P. Sci Technol Weld Join, 2007; 12: 120 [19] Lu S P, Fujii H, Sugiyama H, Nogi K. Metall Mater Trans, 2003; 34A: 1901 [20] Lu S P, Fujii H, Sugiyama H, Tanaka M, Nogi K. ISIJ Int, 2003; 43: 1590 [21] Lu S P, Fujii H, Nogi K. Scr Mater, 2004; 51: 271 [22] Lu S P, Fujii H, Nogi K. Sci Technol Weld Join, 2004; 9: 272 [23] Lu S P, Fujii H, Nogi K. Mater Sci Eng, 2004; A380: 290 [24] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2006; 22: 359 [25] Lu S P, Fujii H, Nogi K, Sato T. Sci Technol Weld Join, 2007; 12: 689 [26] Lu S P, Fujii H, Nogi K. J Mater Sci Technol, 2010; 26: 170 [27] Wu C H, Hao D Q. Physical Chemistry. 1st Ed., Beijing: Machine Building Press, 1988: 138, 287 (吴长春, 郝德庆. 物理化学. 第一版, 北京: 机械工业出版社, 1988: 138, 287) [28] Kraus H G. Weld J, 1989; 68: 269s [29] Bad’yanov B N, Davdov V A, Ivanov V A. Avtom Svarka, 1974; 1: 11 [30] Bad’yanov B N. Avtom Svarka, 1975; 1: 74 [31] Palmer T A, DebRoy T. Weld J, 1996; 75: 197s [32] Sato Y, Dong W, Kokawa H, Kuwana T. ISIJ Int Suppl, 2000; 40: S20 [33] Wada H, Pehlke R D. Metall Trans, 1977; 8B: 675 [34] Dong W, Kokawa H, Sato Y, Tsukamoto S. Metall Mater Trans, 2003; 34B: 75 [35] Katz J D, Kiong T B. Metall Trans, 1989; 20B: 175 [36] Palmer T A, DebRoy T. Sci Technol Weld Join, 1998; 3: 190 [37] Zhu P Y, Lowke J J, Morrow R. J Phys, 1992; 25D: 1221 [38] Lowke J J, Kovitya P, Schmidt H P. J Phys, 1992; 25D: 1601 [39] Zhu P Y, Lowke J J, Morrow R, Haidar J. J Phys, 1995; 28D: 1369 [40] Lowke J J, Morrow R, Haidar J. J Phys, 1997; 30D: 2033 [41] Scott D A, Kovitya P, Haddad G N. J Appl Phys, 1989; 66: 5232 [42] McKelliget J, Szekely J. Metall Trans, 1986; 17A: 1139 [43] Bini R, Monno M, Boulos M I. J Phys, 2006; 39D: 3253 [44] Ushio M, Szekely J, Chang C W. Iron Steel, 1981; 6: 279 [45] Wu C S, Ushio M, Tanaka M. Compt Mater Sci, 1997; 7: 308 [46] Lu S P, Dong W C, Li D Z, Li Y Y. Compt Mater Sci, 2009; 45: 327 [47] Sahoo P, DebRoy T, McNallan M J. Metall Mater Trans, 1988; 19B: 483 [48] DongWC, Lu S P, Li D Z, Li Y Y. Acta Metall Sin, 2008; 44: 249 (董文超, 陆善平, 李殿中, 李依依. 金属学报, 2008; 44: 249) [49] Lu S P, Dong W C, Li D Z, Li Y Y. Sci Tech Weld Join, 2009; 14: 509 [50] Hsu K C, Etemadi K, Pfender E. J Appl Phys, 1983; 54: 1293 [51] Nestor O H. J Appl Phys, 1962; 33: 1638