3DAP INVESTIGATION OF PRECIPITATION BEHAVIOR OF Cu-RICH PHASE IN SUPER304H HEAT RESISTANT STEEL

  • CHI Cheng-Yu ,
  • DONG Jian-Xin ,
  • LIU Wen-Qiang ,
  • XIE Ti-Shan
Expand
  • 1) School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2) Instrumental Analysis & Research Center, Shanghai University, Shanghai 200444

Received date: 2009-12-22

  Revised date: 2010-05-10

  Online published: 2010-09-11

Supported by

Supported by Key Project of National Natural Science Foundation of China (No.50931003)

摘要

利用三维原子探针(3DAP)研究了超超临界电站锅炉过热器/再热器管材Super304H在650℃时效富Cu相的析出行为. 结果表明, 富 Cu相的析出经历了富Cu原子偏聚区的快速形成以及Cu原子不断聚集到富Cu偏聚区中而渐变形成富Cu相. 富Cu相的析出速率极快, 时效仅5 h富Cu相已明显析出. 随时效时间的延长在富Cu相中逐步排斥出其它元素, 使Cu原子成为富Cu相的主要组成元素. 时效500 h富Cu相中Cu原子的浓度已经达到90%, 时效1000 h富Cu相仍然保持纳米级的尺度且均匀分布, 对Super304H耐热不锈钢具有非常好的强化作用.

本文引用格式

迟成宇 , 董建新 , 刘文庆 , 谢锡善 . 3DAP研究Super304H耐热不锈钢中富Cu相的析出行为[J]. 金属学报, 2010 , 46(9) : 1141 -1146 . DOI: 10.3724/SP.J.1037.2009.00853

Abstract

Super304H austenitic heat resistant steel is based on 18/8 Cr-Ni stainless steel alloyed mainly with 3%Cu and a small amount of Nb combined with N, which is used as superheater/reheater tubes in ultra-super critical (USC) power plants all over the world, due to its good combination of elevated temperature strength with hot corrosion resistance. The excellent high temperature strengths of this steel are mainly contributed by the precipitation strengthening effect of fine Cu-rich phase. Comprehensive study of the characteristic of Cu-rich phase is very important to understand strengthening effect on this steel. However, the Cu-rich phase is very fine< and difficult to be detected at the beginning of precipitation. In this paper, three dimensional atom probe (3DAP) was used to study the early stage of precipitation behavior and the composition change in Cu-rich phase of Super304H aged at 650℃ for different times after solution treatment at high temperature. Cu-rich phase is formed from Cu-rich segregated rigion by the concentration of Cu atoms in it at very beginning stage of aging. Homogeneously distributed Cu-rich phase precipitates with about 1 nm radius are obviously detected after aging at 650℃ for 5 h. With increasing aging time, Cu-rich phase is growing slowly while other elements in the Cu-rich phase decreased obviously. The copper element has almost concentrated to 90\% in the center part of Cu-rich phase after 500 h aging. The homogenous distribution of fine Cu-rich phase in austenitic matrix effects excellent hardening with increasing aging time. The stability of fine Cu-rich phase is one of the most important reasons for keeping good strength of Super304H heat resistant steel at high temperature.

参考文献

[1] Masuyama F. ISIJ Int, 2001; 41: 612
[2] Sawaragi Y, Ogawa K, Kato S, Matori A, Hirano S. Sumitomo Search, 1992; 48: 50
[3] Sourmail T, Bhadeshia H K D H. Metall Mater Trans, 2004; 36A: 23
[4] Mimura M, Ishitsuka H. In: Jaske C E ed., 2007 Proc ASME Pressure Vessels and Piping Conterence–8the International Conference on Creep and Fatigue at Elevated Temperatures–CREEP, New York: ASME, 2008: 197
[5] Viswanathan R, Henry J F, Tanzosh J, Stanko G, Shingledecker J, Vitalis B. J Mater Eng Perform, 2005; 14: 281
[6] Sawaragi Y, Hirano S. In: Jono M, Inone T eds., Proc Int Conf Mech Behav Mater, New York: Pergamon Press Inc, 1991; 4: 589
[7] Iseda A, Okada H, Semba H, Igarashi M. Energ Mater, 2007; 2: 199
[8] Tan S P, Wang Z H, Cheng S C, Liu Z D, Han J C, Fu W T. Mater Sci Eng, 2009; A517: 312
[9] Noguchi Y, Miyahara M, Okada H, Igarashi M. J Soc Mater Sci, 2007; 56: 136
[10] Prabha B, Sundaramoorthy P, Suresh S, Manimozhi S, Ravishankar B. J Mater Eng Perform, 2009; 18: 1294
[11] Igarashi M. CAMP–ISIJ, 2004; 17: 336
[12] Yang Y, Cheng S C, Yang G. Mater for Mech Eng, 2002; 26(10): 23
(杨岩, 程世长, 杨钢. 机械工程材料, 2002; 26(10): 23)
[13] Semba H, Sawaragi Y, Ogawa K, Natori A, Kan T. Materia Jpn, 2002; 41: 120
[14] Hono K. Acta Mater, 1999; 47: 3127
[15] Liu Q D, Chu Y L, Wang Z M, Liu W Q, Zhou B X. Acta Metall Sin, 2008; 44: 1281
(刘庆冬, 褚于良, 王泽民, 刘文庆, 周邦新. 金属学报, 2008; 44: 1281)
[16] Isheim D, Kolli R P, Fine M E, Seidman D N. Scr Mater, 2006; 55: 35

文章导航

/

〈 〉