论文

压铸充型过程中卷气现象的数值模拟研究

  • 李帅君 ,
  • 熊守美 ,
  • Mei Li ,
  • John Allison
展开
  • 1) 清华大学机械工程系; 汽车安全与节能国家重点实验室;  北京 100084 2) Research $\&$ Advanced Engineering Department; Scientific Research Laboratory; Ford Motor Company; Dearborn; MI 48121; USA
李帅君, 男, 1981年生, 博士生

收稿日期: 2009-10-19

  修回日期: 2010-01-14

  网络出版日期: 2010-05-11

基金资助

国家重点基础研究发展计划项目2005CB724105和2006CB605208--2以及美国Ford汽车公司资助

NUMERICAL SIMULATION OF AIR ENTRAPMENT PHENOMENON DURING MOLD FILLING OF HIGH PRESSURE DIE CASTING PROCESS

  • LI Shuai-Jun ,
  • XIONG Shou-Mei
Expand
  • 1) State Key Laboratory of Automotive Safety and Energy; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 2) Research & Advanced Engineering Department; Scientific Research Laboratory; Ford Motor Company; Dearborn; MI 48121; USA

Received date: 2009-10-19

  Revised date: 2010-01-14

  Online published: 2010-05-11

Supported by

Supported by National Basic Research Program of China (Nos.2005CB724105 and 2006CB605208-2}) and Ford Motor Company, USA

摘要

采用一种液-气两相耦合模型模拟了压铸充型过程中的卷气现象, 对卷入金属液中的每个气泡均单独计算其压力变化的趋势, 通过压力传递将液-气两相联系在一起. 为了验证模型的可靠性和准确性, 开展了专门针对压铸的高速水模拟实验, 并采用液-气两相耦合模型以及单相流模型分别进行了模拟, 通过比较可以证实两相耦合模型在模拟卷气方面比单相流模型具有更高的精确度.

本文引用格式

李帅君 , 熊守美 , Mei Li , John Allison . 压铸充型过程中卷气现象的数值模拟研究[J]. 金属学报, 2010 , 46(5) : 554 -560 . DOI: 10.3724/SP.J.1037.2009.00683

Abstract

The most common defect found in the high pressure die casting (HPDC) process is gas porosity which significantly affects the mechanical properties of the final components. As it is known, the air entrapment of the liquid metal flow during the mold filling stage has a close relationship with the gas porosity distribution in die castings. The generation of the entrapped air is mainly due to the interaction between air and liquid metal in the die cavity. In the past few decades, extensive efforts have been made to develop numerical models for the simulation of mold filling. However, these efforts mainly focused on the single phase flow models which can only predict the liquid metal flow and assume that the effect of air in the die cavity is negligible. As a result, these models could not provide the quantity and location of entrapped air in die castings. Recently, several research results on tracking the entrapped air in the molten metal flow have been reported but some techniques still need to be improved further and much more researches are required. In this study, a liquid-gas coupled model is presented to simulate the air entrapment phenomenon during the HPDC mold filling process. The pressure of the entrapped air bubbles is solved at each time step.  The calculations of the liquid and gas phases are combined together through the pressure transfer. In order to verify the validity and stability of this model, a specially designed water analog experiment was carried out and compared with the numerical simulation results of the liquid-gas coupled model and the single phase flow model, respectively. The comparison shows that the liquid-gas coupled model has better prediction accuracy than the single phase flow model in tracking the entrapped air bubbles.

参考文献

[1] Cleary P W, Ha J, Prakash M, Nguyen T. Appl Math Model, 2006; 30: 1406
[2] Vinarcik E J. Adv Mater Process, 2001; 159: 49
[3] Cross M, Pericleous K, Croft T N, McBride D, Lawrence J A, Williams A J. In: Murat T ed., TMS Annual Meeting, San Francisco: Minerals, Metals and Materials Society, 2005: 305
[4] Huang W S, Stoehr R A. J Met, 1983; 35(10): 22
[5] Lin H J. AFS Trans, 1988; 96: 447
[6] Li Y B, Wei Z. Mater Technol, 2003; 18(1): 36
[7] Caboussat A, Picasso M, Rappaz J. J Comput Phys, 2005; 203: 626
[8] Hong J H, Choi Y S, Hwang H Y, Choi J K. In: Bellet M ed., Modeling of Casting, Welding and Advanced Solidification Processes–XI, Opio: Minerals, Metals and Materials Society, 2006: 611
[9] Hao J, Chen L L, Zhou J X. In: Materials Science Forum ed., 5th Int Conf on Physical and Numerical Simulation of Materials Processing, Zhengzhou: Trans Tech Publications Ltd., 2007: 43
[10] Anderson J D. Computational Fluid Dynamics. New York: McGraw–Hill Companies, 1995: 248
[11] Chorin A J. Math Comput, 1968; 22: 745
[12] Kim J, Moin P. J Comput Phys, 1985; 59: 308
[13] Armfield S, Street R. Int J Numer Methods Fluids, 2002; 38: 255
[14] Hirt C W, Nichols B D. J Comput Phys, 1981; 39: 201
[15] Homayonifar P, Babaei R, Attar E, Shahinfar S, Davami P. Int J Adv Manuf Technol, 2008; 39: 219

文章导航

/

〈 〉