论文

考虑炉壁温度变化的高温合金叶片定向凝固过程模拟

  • 潘冬 ,
  • 许庆彦 ,
  • 柳百成
展开
  • 清华大学机械工程系先进成形制造教育部重点实验室; 北京 100084
潘 \ \ \ 冬, 男, 1981年生, 博士生

收稿日期: 2009-09-04

  修回日期: 2009-12-04

  网络出版日期: 2010-03-11

基金资助

国家重点基础研究发展计划项目2005CB724105, 国家自然科学基金项目10477010和国家高技术研究发展计划项目2007AA04Z141资助

MODELLING ON DIRECTIONAL SOLIDIFICATION OF SUPERALLOY BLADES WITH FURNACE WALL TEMPERATURE EVOLUTION

  • PAN Dong ,
  • XU Qiang-Pan ,
  • LIU Bai-Cheng
Expand
  • Key Laboratory for Advanced Materials Processing Technology; MOE; Department of Mechanical Engineering; Tsinghua University; Beijing 100084

Received date: 2009-09-04

  Revised date: 2009-12-04

  Online published: 2010-03-11

Supported by

Supported by National Basic Research Program of China (No.2005CB724105), National Natural Science Foundation of China (No.10477010) and National High Technology Research and Development Program of China (No.2007AA04Z141)

 

摘要

考虑炉壁温度的变化, 基于Monte Carlo射线追踪法建立了高温合金叶片定向凝固过程的温度场计算改进模型. 通过法向射线加密提高加热炉炉壁的辐射计算精度, 并采用叶片三维有限差分网格和加热炉二维网格混合使用的方法提高计算效率. 叶片和炉壁的温度曲线模拟与实验结果吻合良好, 改进模型反映了抽拉过程中炉壁温度的变化及其对叶片内部温度分布的影响, 提高了叶片温度的模拟精度.

本文引用格式

潘冬 , 许庆彦 , 柳百成 . 考虑炉壁温度变化的高温合金叶片定向凝固过程模拟[J]. 金属学报, 2010 , 46(3) : 294 -303 . DOI: 10.3724/SP.J.1037.2009.00578

Abstract

Ni--based superalloy turbine blades produced by Bridgman directional solidification technology are widely used in both aeronautic and energy industries as key parts of the gas turbine engines. Because of existence of complex heat radiation between the shell surface and the furnace wall, precise control of the temperature distribution within the blade is a challenging task. A modified model based on the Monte Carlo ray tracing method was proposed for the three dimensional temperature simulation of the turbine blades during directional solidification process, in which the furnace wall temperature evolution was considered and calculated. Ray refinement in normal direction was applied to improve the heat radiation calculation precision. Three dimensional finite differential grids for turbine blades and two dimensional differential grids for furnace wall were used together to increase simulation efficiency and save memory consumption. Heat transfer calculation of the blades with the modified model was performed and compared with that of the simplified model in which the furnace wall temperature was treated as constant. Experiments were carried out to validate the proposed model in this paper. It was demonstrated that the modified model revealed the furnace wall temperature change during the withdrawal process and its impact on the blade, and simulated the temperature distribution of the turbine blade with a higher accuracy.

参考文献

[1] Perepezko J H. Science, 2009; 326: 1068
[2] Kear B H, Thompson E R. Science, 1980; 208: 847
[3] Li C G, Fu H Z, Yu Q. Aerospace Materials. Beijing: National Defense Industry Press, 2002: 12
(李成功, 傅恒志, 于 翘. 航空航天材料. 北京: 国防工业出版社, 2002: 12)

[4] Roger C R. The Superalloys Fundamentals and Applications. Cambridge: Cambridge University Press, 2006: 18
[5] Huang Q Y, Li H K. Superalloys. Beijing: Metallurgical Industry Press, 2000: 2
(黄乾尧, 李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 2)
[6] Fu H Z. Directional Solidification and Processing of Advanced Materials. Beijing: Science Press, 2008: 591
(傅恒志. 先进材料定向凝固. 北京: 科学出版社, 2008: 591)

[7] McLean M, Lee P D, Shollock B A. In: Fuchs G, James A W, Gabb T, McLean M, Harada H, eds., Advanced Materials and Processes for Gas Turbines, Copper MT, CO: Warrendale, PA, TMS, 2003: 83
[8] Liu B C. Eng Sci, 2000; 2: 29
(柳百成. 中国工程科学, 2000; 2: 29)
[9] Xiong S M, Xu Q Y, Kang J W. Simulation Technology of Casting Process. Beijing: China Machine Press, 2004: 2
(熊守美, 许庆彦, 康进武. 铸造过程模拟仿真技术. 北京: 机械工业出版社, 2004: 2)

[10] Wang D, Overfelt R A. Proc Conf Computational Modeling of Materials, Minerals and Metals Processing. San Diego, CA, United States: Minerals, Metals and Materials Society, 2001: 461
[11] Liu S Z, Li J R, Tang D Z, Zhong Z G. Mater Eng, 1999; 7: 39
(刘世忠, 李嘉荣, 唐定忠, 钟振纲. 材料工程, 1999; 7: 39)

[12] Yu J, Xu Q Y, Cui K, Liu B C, Kimastsuka A, Kuroki Y, Hirata A. J Mater Sci Technol, 2007; 23: 47
[13] Cui K, Xu Q Y, Yu J, Liu B C, Kimatsuka A, Kuroki Y, Yukoyama F. Acta Metall Sin, 2007; 43: 464
(崔锴, 许庆彦, 于靖, 柳百成, 木间塚明彦, 黑木康德, 横山文彦. 金属学报, 2007; 43: 464)

[14] Yu J, Xu Q Y, Li J R, Yuan H L, Liu S Z, Liu B C. Acta Metall Sin, 2007; 43: 1113
(于靖, 许庆彦, 李嘉荣, 袁海龙, 刘世忠, 柳百成. 金属学报, 2007, 43: 1113)

[15] JiangWH. Heat Transfer. Beijing: High Education Press, 1989: 183
(姜为珩. 传热学. 北京: 高等教育出版社, 1989: 183)

[16] Elliott A J, Karney G B, Gigliotti M F X, Pollock T M. In: Green K A, Pollock T M, Harada H, Howson T E, Reed R C, Schirra J J, Walston W, eds., Superalloys 2004, Warrendale, PA, TMS, 2004: 421

文章导航

/

〈 〉