AZ31镁合金中拉伸孪晶静态再结晶的分析
收稿日期: 2009-08-10
修回日期: 2009-10-23
网络出版日期: 2010-02-10
基金资助
国家自然科学基金项目资助50571009
ANALYSIS OF THE STATIC RECRYSTALLIZATION AT TENSION TWINS IN AZ31 MAGNESIUM ALLOY
Received date: 2009-08-10
Revised date: 2009-10-23
Online published: 2010-02-10
Supported by
Supported by National Natural Science Foundation of China (No.50571009)
杨平 , 李萧 . AZ31镁合金中拉伸孪晶静态再结晶的分析[J]. 金属学报, 2010 , 46(2) : 147 -154 . DOI: 10.3724/SP.J.1037.2009.00533
Due to the poor plasticity of magnesium alloys at room temperature (about 15%), twinning plays an important role in the deformation of magnesium alloys, and twins will be the dominant recrystallization nucleation sites. There are at least two types of twinning in magnesium: the {1012}–type tension twinning and the {1011}–type compression twinning. Tension twinning proceeds much more easily than compression twinning since its volume fraction is much higher than that of compression twins, which may have a promotion effect on the recrystallization to a certain degree. Based on the previous research on the static recrystallization at compression twins, the evolution of microstructure and texture in AZ31 magnesium alloy during its static recystallization at tension twins was futher investigated; and the orientational characteristics of new grains formed at tension twins in the early stage of static recrystallization were analyzed by EBSD technique. The results showed that tension twins played only a subordinate role in recrystallization nucleation and suppressed recrystallization rate, thus failed to rfine grain size effectively. The strong basal texture waretained and weakened wih no new texture component being detectd dring annealing. New grains were observed to nucleae preferentially at the intersections of tension twin variants or the intersections between tension twins and compression twins. Their orientations were relative random and are strongly scattered from those of original tension twins or compression twins. A comparison of the recrystallization at tension twins and compression twins was made.
Key words: magnesium alloy; tension twin; texture; recystallization; orienaion
[1] Gehrmann R, Frommert M M, Gottstein G. Mater Sci Eng, 2005; A395: 338
[2] Agnew S R, Duygulu O. Int J Plast, 2005; 21: 1161
[3] Tucker M T, Horstemeyer M F, Gullett P M, Kadiri H E, Whittington W R. Scr Mater, 2009; 60: 182
[4] Kelley E W, Hosford Jr. W F. Trans AIME, 1968; 242: 5
[5] Wonsiewicz B C, Backofen W A. Trans AIME, 1967; 239: 1422
[6] Hartt WH, Reed–Hill R E. Trans Metall Soc AIME, 1968; 242: 1127
[7] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A490: 411
[8] P´erez–Prado M T, del Valle J A, Contreras J M, Ruano O A. Scr Mater, 2004; 50: 661
[9] Yin D L, Zhang K F, Wang G F, Han W B. Mater Sci Eng, 2005; A392: 320
[10] Prasad Y V R K, Rao K P. Mater Sci Eng, 2006; A432: 170
[11] del Valle J A, Ruano O A. Mater Sci Eng, 2008; A487: 473
[12] Nave M D, Barnett M R. Scr Mater, 2004; 51: 881
[13] Cottam R, Robson J, Lorimer G, Davis B. Ceram Trans, 2008; 200: 501
[14] Jager A, Luk´ac P, Gartnerov´a V, Haloda J, Dopita M. Mater Sci Eng, 2006; A432: 20
[15] Mackenzie L W F, Pekguleryuz M O. Scr Mater, 2008; 59: 665
[16] Yi S B, Zaefferer S, Brokmeier H G. Mater Sci Eng, 2006; A424: 275
[17] Yang X Y, Miura H, Sakai T. Trans Nonferrous Met Soc China, 2007; 17: 1139
[18] Beer A G, Barnett M R. Mater Sci Eng, 2008; A485: 318
[19] Cottam R, Robson J, Lorimer G, Davis B. Mater Sci Eng, 2008; A485: 375
[20] Li X, Yang P, Wang L N, Meng L, Cui F E. Mater Sci Eng, 2009; A517: 160
/
| 〈 |
|
〉 |