| 微细宏观结合的金属断裂理论方块图 |
| 邢修三 |
| 北京理工大学 |
|
| DIAGRAM OF MICRO-MESO-MACRO MULTILEVEL CONNECTED THEORY OF FRACTURE |
| XING Xiusan (Beijing Institute of Technology;Beijing 100081)(Manuscript received 1996-01-08;in revised form 1996-06-21) |
引用本文:
邢修三. 微细宏观结合的金属断裂理论方块图[J]. 金属学报, 1996, 32(12): 1265-1269.
.
DIAGRAM OF MICRO-MESO-MACRO MULTILEVEL CONNECTED THEORY OF FRACTURE[J]. Acta Metall Sin, 1996, 32(12): 1265-1269.
| 1邢修三.物理学报,1966;22:4872邢修三.物理学报,1980;29:7183邢修三.物理学报,1990:39:16024XingXS.EngFractMech,1986;24:455XingXS.EngFractMech,1987;26:3936邢修三.力学进展,1991,21:1537WeibullW.ProcRoySwedInstEngRes,1939:151:1538KOHTOPOBTA,1941;11:1739 ZhouST,CadssonAE,ThomsonR.PhysRevLett,1994;76:85210HolianBL,RaveloR.PhysRev,1995:B51:11275 |
|