| 棒状共晶的凝固模型 |
| 潘冶;孙国雄 |
| 东南大学 |
|
| SOLIDIFICATION MODEL OF ROD EUTECTIC |
| PAN Ye; SUN Guoxiong(Southeast University; Nanjing 210018)(Manuscript received 1995-04-24) |
引用本文:
潘冶;孙国雄. 棒状共晶的凝固模型[J]. 金属学报, 1996, 32(2): 120-126.
,
.
SOLIDIFICATION MODEL OF ROD EUTECTIC[J]. Acta Metall Sin, 1996, 32(2): 120-126.
| 1JacksonKA,KuntJD,TransAIME,1966;236:11292MagninP,TrivediR,ActaMetallMater,1991;39:4533SatoT,SayamaY.JCrystGrowth,1974;22:2594FisherDJ,KurzW.ActaMetall,1980;28:7775MagninP,KurzW.ActaMetall1987;35:11196MashaalM,AmarMB,Hakim.VPhyRev,1990;41:44217PelceP,PumirA.JCrystGrowth,1985;73:3378KarmaA.PhysRev,1986;34:43539KarmaA,PelceP,PhysRev,1990;41:674110TrivediR,MagninP,KurzW.ActaMetall1987;35:97111虞觉奇,易文质,陈邦迪,陈宏鉴.二元合金状态图集.上海:上海科学技术出版社,1987:46312HoganLM,SongH.MetallTrans,1987;18A:70713于金,东南大学博士论文,1992:3114NotisMR,ShahDM.IEEETransonMagn,1979,Mag-15:95715刘俊明.物理学报,1992;41:861t |
|