| M2铸造高速钢的变质研究 |
| 李彦军;姜启川;赵宇光;何镇明 |
| 吉林工业大学 |
|
| MODIFICATION OF M2 CAST HIGH SPEED STEEL |
| LI Yanjun; JIANG Qichuan; ZHAO Yuguang; HE Zhenming(Jilin University of Technology; Changchun 130025) (Manuscript received 1 995-10-06) |
引用本文:
李彦军;姜启川;赵宇光;何镇明. M2铸造高速钢的变质研究[J]. 金属学报, 1996, 32(3): 313-317.
,
,
,
.
MODIFICATION OF M2 CAST HIGH SPEED STEEL[J]. Acta Metall Sin, 1996, 32(3): 313-317.
| 1GhomaschiMR,SellarsCM.MetSci,1984:18(1):442LentaEJ,TwentymanME,PesciH.Metallography,1983;16:3873WatmoughT,GouwensPR.AFSTrans,1966:7:524StutzmanGD.AmMachinist,1970;114(15):585XiaojunM,BeelyPR.BritishFoundryman,1991;2:666ShiGongqi,DingPeidao,ZhouShouze.MaterSciTechnol.1992;18:4497HoyleG.HighSpeedSteels.London:ButterWorth&Co.Ltd.,1988:31 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|