| 含FeO熔渣的起泡过程及起泡参数间关系分析 |
| 黄宗泽;肖兴国;肖泽强 |
| 东北大学 |
|
| FOAMING BEHAVIOUR AND PARAMETERS OF FeO-BEARING SLAGS |
| HUANG Zongze;XIAO Hingguo;XIAO Zeqiang(Northeastern University; Shenyang 110006); S. D. SINGH(National Metallurgical Laboratory; Jamshedpur; India;831007) (Manuscript recieved 1995-06-29) |
引用本文:
黄宗泽;肖兴国;肖泽强. 含FeO熔渣的起泡过程及起泡参数间关系分析[J]. 金属学报, 1996, 32(3): 278-283.
,
,
.
FOAMING BEHAVIOUR AND PARAMETERS OF FeO-BEARING SLAGS[J]. Acta Metall Sin, 1996, 32(3): 278-283.
| 1黄宗泽,肖兴国,肖泽强,SinghSD.金属学报,1995;31:B2892黄宗泽,肖兴国,肖泽强,SinghSD,东北大学学报,1995;16:2883OgawaY,HuinD,GayeH,TokumitsuN.ISIJInt,1993;33:2244SzekelyJ.FluidFlowPhenomenainMetalsProcessing.AmericanAcademicPress,19795RoK,FruchanRJ.MetalTrans,1989;20B:5096FuwaT.TransJIM,1989;29:353 |
|